Reinhold Braun
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Reinhold Braun has a total of 21 co-authors. Here are the top co-authors by number of shared publications:
- Christoph Leyens
TU Dresden
5 shared publications A. Lange
German Aerospace Center (DLR), Institute of Materials Research, Köln, Germany
2 shared publicationsM. Fröhlich
DLR—German Aerospace Center, Institute of Materials Research, D‐51170 Köln (Germany)
2 shared publications- Stéphane Mathieu
Université de Lorraine, CNRS, IJL, Nancy, France
2 shared publications A. Ebach‐Stahl
DLR—German Aerospace Center, Institute of Materials Research, D‐51170 Köln (Germany)
1 shared publication- D. Renusch
Karl-Winnacker-Institute of Dechema e.V., Frankfurt, Germany
1 shared publication
Latest Publications
- 1 February 2018
- Published by Elsevier in Intermetallics
- Vol. 93, 169-179
Environmental protection of Nb/Nb5Si3-based alloys by E/TBC systems
- 1 February 2018
- Published by Elsevier in Intermetallics
- Vol. 93, 169-179
Environmental protection of Nb/Nb5Si3-based alloys by E/TBC systems
- 19 October 2017
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 35 (1-3) , 195-203
PVD thermal barrier coating systems for Mo–Si–B alloys
Oxidation protective layers with chemical compositions of Mo–70Al, Mo–46Si–24B, Mo–37Si–15B and Mo–47Si–24Al (at.-%) were deposited on Mo–9Si–8B specimens by magnetron sputtering. After pre-oxidation of the coated samples, ceramic topcoats of yttria partially stabilized zirconia (YSZ) and gadolinium zirconate (GZO) were applied using electron-beam physical vapour deposition. Both as-deposited YSZ and GZO topcoats exhibited good adhesion to the pre-oxidised bond coats. The different thermal barrier coating (TBC) systems were exposed to air at 1000 °C for periods between 20 and 100 h. The YSZ topcoat was tightly-adherent to the borosilicate scale grown on the Mo–46Si–24B bond coat after 20 h of exposure. Similar results were obtained for GZO topcoats deposited on Mo–46Si–24B and Mo–37Si–15B bond coats. The TBC system consisting of GZO topcoat and Mo–47Si–24Al bond coat, which formed a mixed scale of silica and mullite-like oxides, survived 100 h at 1000 °C. However, after this exposure time, the bond coats were approaching their lifetime due to the low layer thickness (5–10 μm). Oxidation of the Mo–Si–B substrate at unprotected areas around the suspension hole of the samples caused severe deterioration of the Mo–70Al bond coat and substantial degradation of the outer region of the GZO topcoat due to chemical reactions with MoO3.
- 19 October 2017
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 35 (1-3) , 195-203
PVD thermal barrier coating systems for Mo–Si–B alloys
Oxidation protective layers with chemical compositions of Mo–70Al, Mo–46Si–24B, Mo–37Si–15B and Mo–47Si–24Al (at.-%) were deposited on Mo–9Si–8B specimens by magnetron sputtering. After pre-oxidation of the coated samples, ceramic topcoats of yttria partially stabilized zirconia (YSZ) and gadolinium zirconate (GZO) were applied using electron-beam physical vapour deposition. Both as-deposited YSZ and GZO topcoats exhibited good adhesion to the pre-oxidised bond coats. The different thermal barrier coating (TBC) systems were exposed to air at 1000 °C for periods between 20 and 100 h. The YSZ topcoat was tightly-adherent to the borosilicate scale grown on the Mo–46Si–24B bond coat after 20 h of exposure. Similar results were obtained for GZO topcoats deposited on Mo–46Si–24B and Mo–37Si–15B bond coats. The TBC system consisting of GZO topcoat and Mo–47Si–24Al bond coat, which formed a mixed scale of silica and mullite-like oxides, survived 100 h at 1000 °C. However, after this exposure time, the bond coats were approaching their lifetime due to the low layer thickness (5–10 μm). Oxidation of the Mo–Si–B substrate at unprotected areas around the suspension hole of the samples caused severe deterioration of the Mo–70Al bond coat and substantial degradation of the outer region of the GZO topcoat due to chemical reactions with MoO3.
- 6 September 2016
- Published by Wiley in Materials and Corrosion
- Vol. 67 (12) , 1252-1260
Lifetime of environmental/thermal barrier coatings deposited on a niobium silicide composite with boron containing M7Si6‐based bond coat
- 6 September 2016
- Published by Wiley in Materials and Corrosion
- Vol. 67 (12) , 1252-1260
Lifetime of environmental/thermal barrier coatings deposited on a niobium silicide composite with boron containing M7Si6‐based bond coat
- 6 January 2016
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 47 (3) , 1367-1377
Environmentally Assisted Cracking of Alloy 7050-T7451 Exposed to Aqueous Chloride Solutions
- 6 January 2016
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 47 (3) , 1367-1377
Environmentally Assisted Cracking of Alloy 7050-T7451 Exposed to Aqueous Chloride Solutions
- 10 August 2013
- Published by Springer Nature in Oxidation of Metals
- Vol. 81 (1-2) , 83-93
Lifetime of Thermal Barrier Coatings Deposited on γ-TiAl Based Alloys Using Intermetallic Ti–Al–Cr Bond Coats with Additions of Yttrium and Zirconium
- 10 August 2013
- Published by Springer Nature in Oxidation of Metals
- Vol. 81 (1-2) , 83-93
Lifetime of Thermal Barrier Coatings Deposited on γ-TiAl Based Alloys Using Intermetallic Ti–Al–Cr Bond Coats with Additions of Yttrium and Zirconium
- 15 May 2013
- Published by Elsevier in Surface and Coatings Technology
- Vol. 222, 128-134
Oxidation resistance of γ-TiAl based alloy Ti–45Al–8Nb coated with intermetallic Ti–Al–Cr–Y layers and EB-PVD zirconia topcoats at 950°C in air
- 15 May 2013
- Published by Elsevier in Surface and Coatings Technology
- Vol. 222, 128-134
Oxidation resistance of γ-TiAl based alloy Ti–45Al–8Nb coated with intermetallic Ti–Al–Cr–Y layers and EB-PVD zirconia topcoats at 950°C in air
- 30 April 2010
- Published by Elsevier in Intermetallics
- Vol. 18 (4) , 479-486
Environmental protection of γ-TiAl based alloy Ti-45Al-8Nb by CrAlYN thin films and thermal barrier coatings
- 30 April 2010
- Published by Elsevier in Intermetallics
- Vol. 18 (4) , 479-486
Environmental protection of γ-TiAl based alloy Ti-45Al-8Nb by CrAlYN thin films and thermal barrier coatings
- 12 March 2009
- Published by Springer Nature in Oxidation of Metals
- Vol. 71 (5-6) , 295-318
Oxidation Behaviour of TBC Systems on γ-TiAl Based Alloy Ti–45Al–8Nb
- 12 March 2009
- Published by Springer Nature in Oxidation of Metals
- Vol. 71 (5-6) , 295-318
Oxidation Behaviour of TBC Systems on γ-TiAl Based Alloy Ti–45Al–8Nb
- 10 July 2008
- Published by Wiley in Materials and Corrosion
- Vol. 59 (7) , 539-546
Investigation on the oxidation behaviour of gamma titanium aluminides coated with thermal barrier coatings
In the present study, the applicability of thermal barrier coatings (TBCs) on γ‐TiAl alloys was investigated. Two alloys with the chemical compositions of Ti‐45Al‐8Nb‐0.2B‐0.15C and Ti‐45Al‐1Cr‐6Nb‐0.4W‐0.2B‐0.5C‐0.2Si were used. Before TBC deposition, the specimens were pre‐oxidised in laboratory air or low partial pressure oxygen atmosphere. Yttria partially stabilised zirconia top coats were then deposited using electron‐beam physical vapour deposition (EB‐PVD). The oxidation behaviour of the γ‐TiAl specimens with TBC was studied by cyclic oxidation testing in air at 850 and 900 °C. Post‐oxidation analysis of the coating systems was performed using scanning electron microscopy with energy‐dispersive X‐ray spectroscopy (EDS). No spallation of the TBC was observed for pre‐oxidised specimens of both alloys when exposed to air at 850 °C for 1100 cycles of 1 h dwell time at high temperature. SEM micrographs of the thermally grown oxide scale revealed outer mixed TiO2/Al2O3 protrusions with a columnar structure. The protrusions contained small particles of zirconia and a low amount of about 0.5 at% zirconium was measured by EDS analysis throughout this outer oxide mixture. The TBCs exhibited excellent adherence on the oxide scale. Intercolumnar gaps and pores in the root area of the TBC were filled with titania and alumina. Below the outer columnar oxide scale, a broad porous zone of predominant titania was observed. The transition region between the oxide scale and substrate consisted of a discontinuous nitride layer intermixed with alumina particles and intermetallic phases rich in niobium formed at the nitride layer/substrate interface. When thermally cycled at 900 °C, the oxide scales on the alloy Ti‐45Al‐8Nb‐0.2B‐0.15C pre‐oxidised in low partial pressure oxygen spalled off after 540 cycles. For the sample with TBC, spallation was observed after 810 cycles. Failure occurred in the thermally grown oxide near the oxide/nitride layer interface. Microstructural examinations revealed again oxide scales with columnar structure beneath the zirconia top coat and good adherence of the TBC on the thermally grown oxides formed at 900 °C.
- 10 July 2008
- Published by Wiley in Materials and Corrosion
- Vol. 59 (7) , 539-546
Investigation on the oxidation behaviour of gamma titanium aluminides coated with thermal barrier coatings
In the present study, the applicability of thermal barrier coatings (TBCs) on γ‐TiAl alloys was investigated. Two alloys with the chemical compositions of Ti‐45Al‐8Nb‐0.2B‐0.15C and Ti‐45Al‐1Cr‐6Nb‐0.4W‐0.2B‐0.5C‐0.2Si were used. Before TBC deposition, the specimens were pre‐oxidised in laboratory air or low partial pressure oxygen atmosphere. Yttria partially stabilised zirconia top coats were then deposited using electron‐beam physical vapour deposition (EB‐PVD). The oxidation behaviour of the γ‐TiAl specimens with TBC was studied by cyclic oxidation testing in air at 850 and 900 °C. Post‐oxidation analysis of the coating systems was performed using scanning electron microscopy with energy‐dispersive X‐ray spectroscopy (EDS). No spallation of the TBC was observed for pre‐oxidised specimens of both alloys when exposed to air at 850 °C for 1100 cycles of 1 h dwell time at high temperature. SEM micrographs of the thermally grown oxide scale revealed outer mixed TiO2/Al2O3 protrusions with a columnar structure. The protrusions contained small particles of zirconia and a low amount of about 0.5 at% zirconium was measured by EDS analysis throughout this outer oxide mixture. The TBCs exhibited excellent adherence on the oxide scale. Intercolumnar gaps and pores in the root area of the TBC were filled with titania and alumina. Below the outer columnar oxide scale, a broad porous zone of predominant titania was observed. The transition region between the oxide scale and substrate consisted of a discontinuous nitride layer intermixed with alumina particles and intermetallic phases rich in niobium formed at the nitride layer/substrate interface. When thermally cycled at 900 °C, the oxide scales on the alloy Ti‐45Al‐8Nb‐0.2B‐0.15C pre‐oxidised in low partial pressure oxygen spalled off after 540 cycles. For the sample with TBC, spallation was observed after 810 cycles. Failure occurred in the thermally grown oxide near the oxide/nitride layer interface. Microstructural examinations revealed again oxide scales with columnar structure beneath the zirconia top coat and good adherence of the TBC on the thermally grown oxides formed at 900 °C.
- 30 August 2007
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 38 (9) , 674-689
Environmentally assisted cracking of aluminium alloys
A short review of the stress corrosion cracking (SCC) behaviour of aluminium alloys is given. Mechanisms of environmentally assisted cracking are outlined. For aluminium alloys, in which stress corrosion cracks propagate predominantly along grain boundaries, anodic dissolution and hydrogen embrittlement have been proposed. Transgranular stress corrosion cracking occurring at severe loading conditions has found particular interest concerning localised corrosion‐deformation interactions. Accelerated test methods for assessing the SCC behaviour are described, including the slow strain rate testing technique and the breaking load method. Results of recent studies on environmentally assisted cracking of aluminium alloys are summarised. Most of the work published in the last two decades has been on aluminium‐lithium based alloys and improved high strength Al‐Zn‐Mg‐Cu alloys in corrosion resistant retrogressed and re‐aged tempers.
- 30 August 2007
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 38 (9) , 674-689
Environmentally assisted cracking of aluminium alloys
A short review of the stress corrosion cracking (SCC) behaviour of aluminium alloys is given. Mechanisms of environmentally assisted cracking are outlined. For aluminium alloys, in which stress corrosion cracks propagate predominantly along grain boundaries, anodic dissolution and hydrogen embrittlement have been proposed. Transgranular stress corrosion cracking occurring at severe loading conditions has found particular interest concerning localised corrosion‐deformation interactions. Accelerated test methods for assessing the SCC behaviour are described, including the slow strain rate testing technique and the breaking load method. Results of recent studies on environmentally assisted cracking of aluminium alloys are summarised. Most of the work published in the last two decades has been on aluminium‐lithium based alloys and improved high strength Al‐Zn‐Mg‐Cu alloys in corrosion resistant retrogressed and re‐aged tempers.