Mingbo Yang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Mingbo Yang has a total of 57 co-authors. Here are the top co-authors by number of shared publications:
- Li Hu
College of Material Science and Engineering, Chongqing University of Technology, Chongqing 400054, China
8 shared publications - Tao Zhou
College of Material Science and Engineering, Chongqing University of Technology, Chongqing, China
8 shared publications Fusheng Pan
Chongqing University
7 shared publications- Laixin Shi
College of Material Science and Engineering, Chongqing University of Technology, Chongqing, China
7 shared publications - Jin Zhang
University of Science and Technology Beijing
6 shared publications - Yong Lian
Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China
6 shared publications
Latest Publications
- Open Access
Tailoring Microstructure and Mechanical Properties of the Al-7Si-0.35Mg-0.35Fe Alloy by Cr Addition: A Study on Fe-Rich Phase Modification
Fe-rich phases are unavoidable intermetallic compounds in aluminum alloys, particularly in recycled aluminum. Their needle-like morphology not only impairs the mechanical performance of the alloy by disrupting the continuity of the matrix but also significantly reduces the allowable addition of recycled aluminum materials. Based on this, this study focuses on the Al-7Si-0.35Mg-0.35Fe alloy with a high Fe content. The Cr was introduced to modify the characteristics of the Fe-rich phase, and the microstructural evolution and mechanical properties of the aluminum alloy with different Cr content (0–0.25 wt.%) were investigated. Experimental results show that the secondary dendrite arm spacing of the alloy is significantly refined after Cr addition. Meanwhile, the Fe-rich phase gradually transitions from β-Al5FeSi with needle-like morphology to α-Al15(Fe,Cr)3Si2 with short rod-like or blocky morphology as the Cr content increases. Notably, the Fe-rich phase in the 0.20Cr alloy exhibits an approximately 65% increase in sphericity and an 84% reduction in equivalent diameter compared to those in the 0Cr alloy. The morphological blunting and dispersed distribution of Fe-rich phases lead to a broad effective Cr addition range of 0.05–0.20 wt% in the alloy. Among them, the 0.20Cr alloy exhibited the best comprehensive mechanical properties, with its ultimate tensile strength and elongation approximately 19% and 107% higher than those of the 0Cr alloy, respectively. Furthermore, the fracture morphology and the relationship between the Fe-rich phase and microcracks in Al-7Si-0.35Mg-0.35Fe alloys with different Cr contents were also analyzed.
Open AccessTailoring Microstructure and Mechanical Properties of the Al-7Si-0.35Mg-0.35Fe Alloy by Cr Addition: A Study on Fe-Rich Phase Modification
Fe-rich phases are unavoidable intermetallic compounds in aluminum alloys, particularly in recycled aluminum. Their needle-like morphology not only impairs the mechanical performance of the alloy by disrupting the continuity of the matrix but also significantly reduces the allowable addition of recycled aluminum materials. Based on this, this study focuses on the Al-7Si-0.35Mg-0.35Fe alloy with a high Fe content. The Cr was introduced to modify the characteristics of the Fe-rich phase, and the microstructural evolution and mechanical properties of the aluminum alloy with different Cr content (0–0.25 wt.%) were investigated. Experimental results show that the secondary dendrite arm spacing of the alloy is significantly refined after Cr addition. Meanwhile, the Fe-rich phase gradually transitions from β-Al5FeSi with needle-like morphology to α-Al15(Fe,Cr)3Si2 with short rod-like or blocky morphology as the Cr content increases. Notably, the Fe-rich phase in the 0.20Cr alloy exhibits an approximately 65% increase in sphericity and an 84% reduction in equivalent diameter compared to those in the 0Cr alloy. The morphological blunting and dispersed distribution of Fe-rich phases lead to a broad effective Cr addition range of 0.05–0.20 wt% in the alloy. Among them, the 0.20Cr alloy exhibited the best comprehensive mechanical properties, with its ultimate tensile strength and elongation approximately 19% and 107% higher than those of the 0Cr alloy, respectively. Furthermore, the fracture morphology and the relationship between the Fe-rich phase and microcracks in Al-7Si-0.35Mg-0.35Fe alloys with different Cr contents were also analyzed.
- Open Access
Correction: Lian et al. Microstructure and Mechanical Property of Mg-3Al-1Zn Magnesium Alloy Sheet Processed by Integrated High Temperature Rolling and Continuous Bending. Metals 2020, 10, 380
In the original publication, there were mistakes in Figures 2d, 3, 4b, 5, 6d and 7b as published
Open AccessCorrection: Lian et al. Microstructure and Mechanical Property of Mg-3Al-1Zn Magnesium Alloy Sheet Processed by Integrated High Temperature Rolling and Continuous Bending. Metals 2020, 10, 380
In the original publication, there were mistakes in Figures 2d, 3, 4b, 5, 6d and 7b as published
- RetractionOpen Access
RETRACTED: Shi et al. Effect of Final Rolling Temperature on Microstructures and Mechanical Properties of AZ31 Alloy Sheets Prepared by Equal Channel Angular Rolling and Continuous Bending. Materials 2020, 13, 3346
The journal retracts the article, “Effect of Final Rolling Temperature on Microstructures and Mechanical Properties of AZ31 Alloy Sheets Prepared by Equal Channel Angular Rolling and Continuous Bending”
RetractionOpen AccessRETRACTED: Shi et al. Effect of Final Rolling Temperature on Microstructures and Mechanical Properties of AZ31 Alloy Sheets Prepared by Equal Channel Angular Rolling and Continuous Bending. Materials 2020, 13, 3346
The journal retracts the article, “Effect of Final Rolling Temperature on Microstructures and Mechanical Properties of AZ31 Alloy Sheets Prepared by Equal Channel Angular Rolling and Continuous Bending”
- 9 January 2024
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (1) , 896-904
Preliminary Investigations about Effects of Aging Method on Microstructure and Tensile Properties of As-Eextruded Mg-Gd-Y-Mn-Based Magnesium Alloys
- 9 January 2024
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (1) , 896-904
Preliminary Investigations about Effects of Aging Method on Microstructure and Tensile Properties of As-Eextruded Mg-Gd-Y-Mn-Based Magnesium Alloys
- Open Access
Effects of Rapid Quenching on Grain Boundary Microstructure and Mechanical Properties of an Al-Mg-Si-Cu Alloy
Precipitate free zones (PFZs) near grain boundaries generally soften alloys. The quenching rate after solution treatment is an important factor influencing the width of PFZs in Al-Mg-Si-Cu alloy. This study explored the effects of high quenching rates on the grain boundary microstructures and mechanical properties of an Al-Mg-Si-Cu alloy. Samples of various thickness were quenched in water at room temperature and in ethylene glycol at −40 °C, respectively. The results showed that the rapidly quenched samples at −40 °C exhibited better comprehensive mechanical properties than the water-quenched samples. Transmission electron microscopy studies revealed the rapidly quenched samples had wider PFZs, shorter intragranular precipitates, and larger grain boundary precipitates (GBPs) than water-quenched samples. It is proposed that when the quenching rate exceeds the critical cooling rate, e.g., in water quenching or rapid quenching, the formation of PFZs is controlled by the solute depletion mechanism rather than the vacancy depletion mechanism. The nucleation and growth of GBPs thus lead to the depletion of solute atoms, resulting in wider PFZs rather than thinner PFZs according to previous knowledge. This research provides valuable insights into the application of rapid quenching technology for modifying alloys’ microstructures and properties.
Open AccessEffects of Rapid Quenching on Grain Boundary Microstructure and Mechanical Properties of an Al-Mg-Si-Cu Alloy
Precipitate free zones (PFZs) near grain boundaries generally soften alloys. The quenching rate after solution treatment is an important factor influencing the width of PFZs in Al-Mg-Si-Cu alloy. This study explored the effects of high quenching rates on the grain boundary microstructures and mechanical properties of an Al-Mg-Si-Cu alloy. Samples of various thickness were quenched in water at room temperature and in ethylene glycol at −40 °C, respectively. The results showed that the rapidly quenched samples at −40 °C exhibited better comprehensive mechanical properties than the water-quenched samples. Transmission electron microscopy studies revealed the rapidly quenched samples had wider PFZs, shorter intragranular precipitates, and larger grain boundary precipitates (GBPs) than water-quenched samples. It is proposed that when the quenching rate exceeds the critical cooling rate, e.g., in water quenching or rapid quenching, the formation of PFZs is controlled by the solute depletion mechanism rather than the vacancy depletion mechanism. The nucleation and growth of GBPs thus lead to the depletion of solute atoms, resulting in wider PFZs rather than thinner PFZs according to previous knowledge. This research provides valuable insights into the application of rapid quenching technology for modifying alloys’ microstructures and properties.
- Open Access
- 1 July 2023
- Published by Springer Nature in China Foundry
- Vol. 20 (4) , 307-314
Effects of aging treatment processes on microstructures and mechanical properties of AZ63 casting magnesium alloy
- 1 July 2023
- Published by Springer Nature in China Foundry
- Vol. 20 (4) , 307-314
Open AccessEffects of aging treatment processes on microstructures and mechanical properties of AZ63 casting magnesium alloy
- Open Access
Hot Deformation Behavior and Constitutive Analysis of As-Extruded Mg–6Zn–5Ca–3Ce Alloy Fabricated by Rapid Solidification
The plasticity of Mg–6Zn–5Ca–3Ce alloy fabricated by rapid solidification (RS) at room temperature is poor due to its hexagonal-close-packed (HCP) structure. Therefore, hot deformation of RS Mg–6Zn–5Ca–3Ce alloy at elevated temperature would be a major benefit for manufacturing products with complex shapes. In the present study, hot deformation behavior of as-extruded Mg–6Zn–5Ca–3Ce alloy fabricated by RS was investigated by an isothermal compression test at a temperature (T) of 573–673 K and strain rate () of 0.0001–0.01 s−1. Results indicated that the flow stress increases along with the declining temperature and the rising strain rate. The flow stress behavior was then depicted by the hyperbolic sine constitutive equation where the value of activation energy (Q) was calculated to be 186.3 kJ/mol. This issue is mainly attributed to the existence of fine grain and numerous second phases, such as Mg2Ca and Mg–Zn–Ce phase (T’ phase), acting as barriers to restrict dislocation motion effectively. Furthermore, strain compensation was introduced to incorporate the effect of plastic strain on material constants (,,,) and the predicted flow stresses under various conditions were roughly consistent with the experimental results. Moreover, the processing maps based on the Murty criterion were constructed and visualized to find out the optimal deformation conditions during hot working. The preferential hot deformation windows were identified as follows: T = 590–640 K, = 0.0001–0.0003 s−1 and T = 650–670 K, = 0.0003–0.004 s−1 for the studied material.Open AccessHot Deformation Behavior and Constitutive Analysis of As-Extruded Mg–6Zn–5Ca–3Ce Alloy Fabricated by Rapid Solidification
The plasticity of Mg–6Zn–5Ca–3Ce alloy fabricated by rapid solidification (RS) at room temperature is poor due to its hexagonal-close-packed (HCP) structure. Therefore, hot deformation of RS Mg–6Zn–5Ca–3Ce alloy at elevated temperature would be a major benefit for manufacturing products with complex shapes. In the present study, hot deformation behavior of as-extruded Mg–6Zn–5Ca–3Ce alloy fabricated by RS was investigated by an isothermal compression test at a temperature (T) of 573–673 K and strain rate () of 0.0001–0.01 s−1. Results indicated that the flow stress increases along with the declining temperature and the rising strain rate. The flow stress behavior was then depicted by the hyperbolic sine constitutive equation where the value of activation energy (Q) was calculated to be 186.3 kJ/mol. This issue is mainly attributed to the existence of fine grain and numerous second phases, such as Mg2Ca and Mg–Zn–Ce phase (T’ phase), acting as barriers to restrict dislocation motion effectively. Furthermore, strain compensation was introduced to incorporate the effect of plastic strain on material constants (,,,) and the predicted flow stresses under various conditions were roughly consistent with the experimental results. Moreover, the processing maps based on the Murty criterion were constructed and visualized to find out the optimal deformation conditions during hot working. The preferential hot deformation windows were identified as follows: T = 590–640 K, = 0.0001–0.0003 s−1 and T = 650–670 K, = 0.0003–0.004 s−1 for the studied material. - RetractedOpen Access
RETRACTED: Effect of Final Rolling Temperature on Microstructures and Mechanical Properties of AZ31 Alloy Sheets Prepared by Equal Channel Angular Rolling and Continuous Bending
The effects of final rolling temperature on the microstructures, texture and mechanical properties of AZ31 Mg alloy sheets prepared by equal channel angular rolling and continuous bending (ECAR-CB) were investigated. Extension twins {10–12} could be observed in the ECAR-CB deformed sheets. The increase in the number of {10–12} extension twins with increasing final rolling temperature might be attributed to the larger grain size and faster grain boundary migration. For all the ECAR-CB sheets at different final rolling temperatures, the deformation texture contains a basal texture component and a prismatic texture component, whereas the annealing recrystallization texture becomes a non-basal (pyramidal) texture with double peaks tilting away from normal direction (ND) to rolling direction (RD). With increasing final rolling temperature, the tilted angle of double peaks of annealing recrystallization non-basal texture increases. In addition, the plasticity and formability of ECAR-CB-A (ECAR-CB and then annealing) AZ31 Mg alloy sheets at room temperature can be improved by increasing the final rolling temperature.
RetractedOpen AccessRETRACTED: Effect of Final Rolling Temperature on Microstructures and Mechanical Properties of AZ31 Alloy Sheets Prepared by Equal Channel Angular Rolling and Continuous Bending
The effects of final rolling temperature on the microstructures, texture and mechanical properties of AZ31 Mg alloy sheets prepared by equal channel angular rolling and continuous bending (ECAR-CB) were investigated. Extension twins {10–12} could be observed in the ECAR-CB deformed sheets. The increase in the number of {10–12} extension twins with increasing final rolling temperature might be attributed to the larger grain size and faster grain boundary migration. For all the ECAR-CB sheets at different final rolling temperatures, the deformation texture contains a basal texture component and a prismatic texture component, whereas the annealing recrystallization texture becomes a non-basal (pyramidal) texture with double peaks tilting away from normal direction (ND) to rolling direction (RD). With increasing final rolling temperature, the tilted angle of double peaks of annealing recrystallization non-basal texture increases. In addition, the plasticity and formability of ECAR-CB-A (ECAR-CB and then annealing) AZ31 Mg alloy sheets at room temperature can be improved by increasing the final rolling temperature.