Young‐Wook Park
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Interests
Young‐Wook Park has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
Dong‐Sung Lee
Department of Polymer Science and Engineering and ERI, Gyeongsang National University, Jinju, 660-701, Korea
3 shared publicationsDong-Sung Lee
Department of Polymer Science and Engineering and ERI, Gyeongsang National University, Jinju, 660‐701, Korea
1 shared publicationSang‐Hyun Kim
Department of Electrical Engineering, Gyeongsang National University, Chinju, 660‐701, Korea
1 shared publication
Latest Publications
- 30 September 2004
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 94 (5) , 1947-1955
Surface and thermal characteristics of rubber‐modified aromatic polyamide
- 30 September 2004
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 94 (5) , 1947-1955
Surface and thermal characteristics of rubber‐modified aromatic polyamide
- 22 September 2004
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 94 (4) , 1780-1788
Mechanical and thermal properties of ceramic-modified poly(amide imide)
- 22 September 2004
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 94 (4) , 1780-1788
Mechanical and thermal properties of ceramic-modified poly(amide imide)
- 14 April 2004
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 93 (1) , 342-347
Surface and electrical characteristics of poly(amide imide)–poly(dimethylsiloxane) nanocomposites
A series of poly(amide imide)–poly(dimethylsiloxane) (PDMS) nanocomposites were fabricated through the reaction of poly(amide imide), epoxysilane (coupling agent), and diethoxydimethylsilane (DEDMS) via a sol–gel process. Nanocomposite films were obtained through the hydrolysis and condensation of DEDMS in poly(amide imide) solutions. The existence of the condensation product of DEDMS in the poly(amide imide) matrix was confirmed with Fourier transform infrared (FTIR). The concentration of PDMS on the surface of the poly(amide imide) matrix was observed through a comparison of FTIR and attenuated total reflection spectra. The contact angle of the poly(amide imide)–PDMS composites increased more than 40° with respect to that of pure poly(amide imide). The alternating‐current (ac) breakdown strength was obtained through the measurement of the ac breakdown voltage at the temperature of liquid nitrogen. As the PDMS concentration in poly(amide imide) increased, the characteristics of the insulation breakdown improved greatly. The best ac breakdown strength was observed in a poly(amide imide)–epoxysilane (30 wt %) nanocomposite with 30 wt % PDMS. The samples at the temperature of liquid nitrogen were brittle, as in a glassy state. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 93: 342–347, 2004
- 14 April 2004
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 93 (1) , 342-347
Surface and electrical characteristics of poly(amide imide)–poly(dimethylsiloxane) nanocomposites
A series of poly(amide imide)–poly(dimethylsiloxane) (PDMS) nanocomposites were fabricated through the reaction of poly(amide imide), epoxysilane (coupling agent), and diethoxydimethylsilane (DEDMS) via a sol–gel process. Nanocomposite films were obtained through the hydrolysis and condensation of DEDMS in poly(amide imide) solutions. The existence of the condensation product of DEDMS in the poly(amide imide) matrix was confirmed with Fourier transform infrared (FTIR). The concentration of PDMS on the surface of the poly(amide imide) matrix was observed through a comparison of FTIR and attenuated total reflection spectra. The contact angle of the poly(amide imide)–PDMS composites increased more than 40° with respect to that of pure poly(amide imide). The alternating‐current (ac) breakdown strength was obtained through the measurement of the ac breakdown voltage at the temperature of liquid nitrogen. As the PDMS concentration in poly(amide imide) increased, the characteristics of the insulation breakdown improved greatly. The best ac breakdown strength was observed in a poly(amide imide)–epoxysilane (30 wt %) nanocomposite with 30 wt % PDMS. The samples at the temperature of liquid nitrogen were brittle, as in a glassy state. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 93: 342–347, 2004
- 5 December 2003
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 91 (3) , 1774-1783
Mechanical, surface, and thermal properties of polyamideimide–polydimethylsiloxane nanocomposites fabricated by sol–gel process
Polyamideimide (PAI)–epoxysilane (coupling agent) composites were reacted with oligomeric polydimethylsiloxane (PDMS), a condensation product of difunctional silane, by using the sol–gel process, and were then dried into films. After this procedure, the surface, mechanical, and thermal properties were measured. The study showed that PDMS existed in the PAI matrix by the use of FTIR. With respect to mechanical properties, the maximum elongation and toughness were increased in the PAI with silane groups, although the maximum tensile strength was slightly decreased. In this experiment, PAI–30 wt % epoxysilane composite had the best mechanical properties. The intensive dispersion of the silane groups on the surface of PAI was confirmed through XPS measurement. As a function of the siloxane contents, the TGA curve shows less thermal stability in terms of their initial weight loss. However, in an oxygen atmosphere at about 700°C, the series of PAI–siloxane composites indicated a significant increase in char concentration. In the end, PAI with a relevant amount of silane groups was improved in both toughness and surface properties. This experiment showed that PDMS added to PAI had better properties than those of classical materials. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 91: 1774–1783, 2004
- 5 December 2003
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 91 (3) , 1774-1783
Mechanical, surface, and thermal properties of polyamideimide–polydimethylsiloxane nanocomposites fabricated by sol–gel process
Polyamideimide (PAI)–epoxysilane (coupling agent) composites were reacted with oligomeric polydimethylsiloxane (PDMS), a condensation product of difunctional silane, by using the sol–gel process, and were then dried into films. After this procedure, the surface, mechanical, and thermal properties were measured. The study showed that PDMS existed in the PAI matrix by the use of FTIR. With respect to mechanical properties, the maximum elongation and toughness were increased in the PAI with silane groups, although the maximum tensile strength was slightly decreased. In this experiment, PAI–30 wt % epoxysilane composite had the best mechanical properties. The intensive dispersion of the silane groups on the surface of PAI was confirmed through XPS measurement. As a function of the siloxane contents, the TGA curve shows less thermal stability in terms of their initial weight loss. However, in an oxygen atmosphere at about 700°C, the series of PAI–siloxane composites indicated a significant increase in char concentration. In the end, PAI with a relevant amount of silane groups was improved in both toughness and surface properties. This experiment showed that PDMS added to PAI had better properties than those of classical materials. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 91: 1774–1783, 2004