GDG. K. Dey

G. K. Dey

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


G. K. Dey has a total of 27 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Precipitation in a Cu–4Ti–2Be alloy

    by R. Tewari, I.S. Batra, G.K. Dey, U.D. Kulkarni

    It is known that the binary Cu–2 wt.% Be alloy can be strengthened by ageing its supersaturated solution at 523 K. The increase in the strength arising from ageing is because of the formation of GP zones. The same level of strength is achieved by ageing the supersaturated solid solution of a dilute binary Cu–4 wt.% Ti alloy at 723 K. In contrast to Cu–2 wt.% Be alloy, the increase in strength in this alloy occurs on account of spinodal decomposition of the as-quenched microstructure through the mechanism of clustering and ordering. In the present study, decomposition of a supersaturated solid solution of the ternary Cu–4 wt.% Ti–2 wt.% Be alloy was studied. Whereas ageing of this alloy at 523 K resulted in the formation of GP zones like in a Cu–2 wt.% Be alloy, ageing at 723 K resulted in a spinodally decomposed microstructure as in a Cu–4 wt.% Ti alloy. The decomposition of the ternary alloy at the two temperatures by two different mechanisms indicates that Be and Ti in solution in Cu act, more or less, independently of each other during ageing.

  • Influence of free volume and medium-range order on the deformation response of rapidly solidified and bulk Zr-based (Zr52Ti6Al10Cu18Ni14) metallic glass

    by B. Vishwanadh, S.K. Sharma, P.K. Pujari, R. Kishore, G.K. Dey, R. Tewari

    Free volume and medium-range order (MRO) present in rapidly solidified ribbons (RSRs) and bulk metallic glasses (BMGs) of Zr52Ti6Al10Cu18Ni14 have been probed by high resolution electron microscopy, fluctuation microscopy, positron annihilation and differential scanning calorimetry. In the as-solidified condition, RSRs showed higher free volume and lower MRO in comparison to BMGs. Within BMGs, the central regions showed higher MRO and lower free volume than the peripheral regions. Uniform deformation of BMGs and RSRs modified their structures, where in, free volume increased in the former and reduced in the latter. These changes in structures led to work hardening in RSRs and work softening in BMGs. Such behaviour could be explained by invoking a concept of critical free volume in the glass phase. For samples (in as-solidified condition) having free volume higher than the critical value, free volume decreased with deformation and showed work-hardening behaviour. In contrast, the work softening behaviour was noticed in samples having free volume lower than the critical free volume.


  • A study on the formation of crystalline phases during solidification and crystallisation in the bulk metallic glass of Zr53Cu21Al10Ni8Ti8composition

    by S. Neogy, R. Tewari, G.K. Dey, S. Banerjee, S. Ranganathan

    The present paper considers the formation of crystalline phases during solidification and crystallisation of the Zr53Cu21Al10Ni8Ti8 alloy. Solidification was carried out by a copper mould casting technique, which yielded a partially crystalline microstructure comprising a ‘big cube phase’ in a dendritic morphology and a bct Zr2Ni phase. Detailed high-resolution microscopy was carried out to determine possible mechanisms for the formation of the crystalline phases. Based on microstructural examinations, it was established that the dendrites grew by the attachment of atomistic ledges. The bct Zr2Ni phase, formed during solidification and crystallisation, showed various types of faults depending on the crystallite size, and its crystallography was examined in detail. It has been shown that the presence of these faults could be explained by anti-site occupancy in the bct lattice of the Zr2Ni phase.

  • Novel defects in Al–Pd–Fe complex metallic alloys: A micromechanical modelling approach

    by K.V. Mani Krishna, A. Arya, M. Heggen, G.K. Dey, M. Feuerbacher, S. Banerjee


  • Nanostructural Studies on Lead Magnesium Niobate and Lead Iron Niobate by TEM

    by D. Mohan, D. D. Upadhyaya, Ram Prasad, G. K. Dey, S. Banerjee

    PMN and PFN are very interesting ferroelectric ceramics finding many useful applications in multilayer ceramic capacitors and electrostrictive devices. These ceramics prepared by semi-wet hydroxide route were observed by TEM for their nanostructural features such as ordering-disordering, grain boundary phase etc.

  • Phase-separation kinetics of a multicomponent alloy

    by S. Mazumder, D. Sen, I. S. Batra, R. Tewari, G. K. Dey, S. Banerjee, A. Sequeira, H. Amenitsch, S. Bernstorff

    Phase separation kinetics of multicomponent 350-grade maraging steel has been investigated on both recrystallized as well as cold-worked specimens by small-angle x-ray scattering, wide angle x-ray scattering, and transmission electron microscopy at two different temperatures, viz. 430 °C and 510 °C, for different aging times. Unlike previous observations, at both the temperatures, dynamical scaling behavior is observed at the early stages of phase separation accompanied by diffuse interface of the secondary phases. Porod exponents have been found to be greater than 4. At late stages, the precipitate-matrix interface becomes sharp — the Porod exponent is close to 4 but clear deviation from the dynamical scaling behavior is evident. At 430°C, the phase separation is attributed to the formation of an ordered ω phase through a mechanism involving chemical ordering and the ω-like lattice collapse in the bcc structure. Time (t) dependent population averaged precipitate radius follows t1/5 power law indicating cluster diffusion mechanism of Binder-Stauffer type for the entire range, 30 min–72 h, of aging time. At 510°C,the phase separation is attributed to the formation of Ni3(Ti,Mo) with DO24 structure through the process of nucleation and growth. Average precipitate radius follows t1/3 Lifshitz-Slyozov power law for the entire range, 5 min–18 h, of aging time. The system, despite being multicomponent and complex, appears to follow two distinct time-temperature-transformation curves. As far as the effect of cold work on phase-separation behavior is concerned, it has been found that cold work facilitates the growth of the precipitates. Also, it narrows down the size distribution and enforces strong spatial correlation of the precipitates. Cold working the material is found to be detrimental to the dynamical scaling behavior.


  • Ordered Omega Derivatives in (Zr3Al)-Nb Alloys

    by R. Tewari, G. K. Dey, P. Mukhopadhyay, S. Banerjee, L. A. Bendersky


  • Dynamic recrystallisation during hot working of Zr–2·5Nb: characterisation using processing maps

    by J. K. Chakravartty, G. K. Dey, S. Banerjee, Y. V. R. K. Prasad

    The characteristics of the hot deformation of Zr–2·5Nb (wt-%) in the temperature range 650–950°C and in the strain rate range 0·001–100 s−1 have been studied using hot compression testing. Two different preform microstructures: equiaxed (α+β) and β transformed, have been investigated. For this study, the approach of processing maps has been adopted and their interpretation carried out using the dynamic materials model. The efficiency of power dissipation given by [2m/(m+1)], where m is the strain rate sensitivity, is plotted as a function of temperature and strain rate to obtain a processing map. A domain of dynamic recrystallisation has been identified in the maps of equiaxed (α+β) and β transformed preforms. In the case of equiaxed (α+β), the stress–strain curves are steady state and the dynamic recrystallisation domain in the map occurs with a peak efficiency of 45% at 850°C and 0·001 s−1. On the other hand, the β transformed preform exhibits stress–strain curves with continuous flow softening. The corresponding processing map shows a domain of dynamic recrystallisation occurring by the shearing of α platelets followed by globularisation with a peak efficiency of 54% at 750°C and 0·001 s−1. The characteristics of dynamic recrystallisation are analysed on the basis of a simple model which considers the rates of nucleation and growth of recrystallised grains. Calculations show that these two rates are nearly equal and that the nucleation of dynamic recrystallisation is essentially controlled by mechanical recovery involving the cross-slip of screw dislocations. Analysis of flow instabilities using a continuum criterion revealed that Zr–2·5Nb exhibits flow localisation at temperatures lower than 700°C and strain rates higher than 1 s−1. MST/3103