Horst Fischer
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Horst Fischer has a total of 37 co-authors. Here are the top co-authors by number of shared publications:
R. Marx
8 shared publicationsR. Telle
4 shared publicationsRainer Telle
Department of Ceramics and Refractory Materials, RWTH Aachen University, Mauerstrasse 5, 52064 Aachen, Germany
4 shared publicationsRudolf Marx
4 shared publicationsNadine Kaltenborn
Department of Ceramics and Refractory Materials, RWTH Aachen University, 52064 Aachen, Germany
2 shared publicationsA. Erdrich
1 shared publication
Latest Publications
- 1 May 2008
- Published by Elsevier in Dental Materials
- Vol. 24 (5) , 618-622
Influence of preparation of ceramic SEVNB specimens on fracture toughness testing results
- 1 May 2008
- Published by Elsevier in Dental Materials
- Vol. 24 (5) , 618-622
Influence of preparation of ceramic SEVNB specimens on fracture toughness testing results
- 1 March 2008
- Published by Elsevier in Dental Materials
- Vol. 24 (3) , 328-332
Crack healing in alumina bioceramics
- 1 March 2008
- Published by Elsevier in Dental Materials
- Vol. 24 (3) , 328-332
Crack healing in alumina bioceramics
- 9 January 2008
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 87A (3) , 582-587
Chemical strengthening of a dental lithium disilicate glass–ceramic material
Chemical strengthening of dental ceramics by ion exchange has hitherto only been confirmed for feldspathic porcelains. The objective of this study was to examine whether the strength of lithium disilicate glass–ceramics can be increased by ion exchange as well. A lithium disilicate glass–ceramic material was treated in different molten salts. The concentration gradients of the relevant ions in the surface layer were investigated by means of electron probe microanalysis and secondary ion mass spectroscopy. Characteristic strength and Weibull modulus data were determined. An increase in strength of 25% was achieved by treatment in potassium nitrate. The chemical analyses revealed that the increase in strength resulted from an exchange of potassium for lithium ions. We conclude that ion‐exchange treatments can increase the strength of lithium disilicate glass–ceramics. The improved material could be used for highly stressed applications, such as posterior crowns or inlay‐retained bridges, with higher mechanical reliability. © 2008 Wiley Periodicals, Inc. J Biomed Mater Res, 2008
- 9 January 2008
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 87A (3) , 582-587
Chemical strengthening of a dental lithium disilicate glass–ceramic material
Chemical strengthening of dental ceramics by ion exchange has hitherto only been confirmed for feldspathic porcelains. The objective of this study was to examine whether the strength of lithium disilicate glass–ceramics can be increased by ion exchange as well. A lithium disilicate glass–ceramic material was treated in different molten salts. The concentration gradients of the relevant ions in the surface layer were investigated by means of electron probe microanalysis and secondary ion mass spectroscopy. Characteristic strength and Weibull modulus data were determined. An increase in strength of 25% was achieved by treatment in potassium nitrate. The chemical analyses revealed that the increase in strength resulted from an exchange of potassium for lithium ions. We conclude that ion‐exchange treatments can increase the strength of lithium disilicate glass–ceramics. The improved material could be used for highly stressed applications, such as posterior crowns or inlay‐retained bridges, with higher mechanical reliability. © 2008 Wiley Periodicals, Inc. J Biomed Mater Res, 2008
- 10 May 2007
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 90 (5) , 1644-1646
Coupling of Phosphates on Alumina Surfaces for Bioactivation
This paper reports on a new surface treatment, coupling phosphates on alumina surfaces for bioactivation. Alumina samples were treated in monoaluminumphosphate solution at 1400°C. Strongly coupled aluminum phosphates due to the treatment were proved by X‐ray diffraction and infrared spectroscopy. Contact angle measurements proved the hydrophilic nature of the treated surface. In vitro tests in simulated body fluid indicated a bioactive behavior by means of apatite‐forming ability. Such functionalized alumina ceramics imply the potential for a new class of bioactive high‐strength ceramic implant materials, due to a pronounced affinity of bioactive phosphate groups to particular amino acid sequences of proteins.
- 10 May 2007
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 90 (5) , 1644-1646
Coupling of Phosphates on Alumina Surfaces for Bioactivation
This paper reports on a new surface treatment, coupling phosphates on alumina surfaces for bioactivation. Alumina samples were treated in monoaluminumphosphate solution at 1400°C. Strongly coupled aluminum phosphates due to the treatment were proved by X‐ray diffraction and infrared spectroscopy. Contact angle measurements proved the hydrophilic nature of the treated surface. In vitro tests in simulated body fluid indicated a bioactive behavior by means of apatite‐forming ability. Such functionalized alumina ceramics imply the potential for a new class of bioactive high‐strength ceramic implant materials, due to a pronounced affinity of bioactive phosphate groups to particular amino acid sequences of proteins.
- 24 January 2007
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 81A (4) , 982-986
Hemocompatibility of high strength oxide ceramic materials: An in vitro study
High strength oxide ceramic materials like alumina and zirconia are frequently used for artificial joints because of their biocompatibility and high wear resistance. Their suitability as materials for implants and biomedical devices with direct blood contact, such as cardiovascular implants or components for blood pumps and dialyzers, has not been confirmed to date. The objective of this study was to investigate whether oxide ceramics show sufficient hemocompatibility. Dense specimens were made out of alumina, zirconia, titanium oxide, and aluminum titanate. Polyvinylchloride and silicone were additionally tested as reference materials. Interactions of human blood with the surfaces were studied by investigating partial thromboplastin time (PTT), thrombin antithrombin III complex (TAT), free plasma hemoglobin concentration, complete blood count, complement factor 5a, and protein adsorption. The results from the PTT and TAT tests clearly indicated higher blood activation by the ceramic materials when compared to the two polymer materials. However, alumina and zirconia showed lower C5a concentrations and less protein adsorption than the reference materials. Our results revealed that oxide ceramic materials alone cannot be used for implants in direct blood contact without modification of the ceramic surface, for example, by made‐to‐measure inert nanocoatings. © 2007 Wiley Periodicals, Inc. J Biomed Mater Res, 2007
- 24 January 2007
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 81A (4) , 982-986
Hemocompatibility of high strength oxide ceramic materials: An in vitro study
High strength oxide ceramic materials like alumina and zirconia are frequently used for artificial joints because of their biocompatibility and high wear resistance. Their suitability as materials for implants and biomedical devices with direct blood contact, such as cardiovascular implants or components for blood pumps and dialyzers, has not been confirmed to date. The objective of this study was to investigate whether oxide ceramics show sufficient hemocompatibility. Dense specimens were made out of alumina, zirconia, titanium oxide, and aluminum titanate. Polyvinylchloride and silicone were additionally tested as reference materials. Interactions of human blood with the surfaces were studied by investigating partial thromboplastin time (PTT), thrombin antithrombin III complex (TAT), free plasma hemoglobin concentration, complete blood count, complement factor 5a, and protein adsorption. The results from the PTT and TAT tests clearly indicated higher blood activation by the ceramic materials when compared to the two polymer materials. However, alumina and zirconia showed lower C5a concentrations and less protein adsorption than the reference materials. Our results revealed that oxide ceramic materials alone cannot be used for implants in direct blood contact without modification of the ceramic surface, for example, by made‐to‐measure inert nanocoatings. © 2007 Wiley Periodicals, Inc. J Biomed Mater Res, 2007
- 1 November 2005
- Published by Elsevier in Biomaterials
- Vol. 26 (31) , 6151-6157
Bioactivation of inert alumina ceramics by hydroxylation
- 1 November 2005
- Published by Elsevier in Biomaterials
- Vol. 26 (31) , 6151-6157
Bioactivation of inert alumina ceramics by hydroxylation
- 1 July 2005
- Published by Elsevier in Dental Materials
- Vol. 21 (7) , 671-677
Influence of annealing temperature on the strength of dental glass ceramic materials
- 1 July 2005
- Published by Elsevier in Dental Materials
- Vol. 21 (7) , 671-677
Influence of annealing temperature on the strength of dental glass ceramic materials
- 30 November 2004
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 72A (2) , 175-179
Effect of ion exchange of glazed dental glass ceramics on strength parameters
Ion exchange treatments can significantly increase the strength of dental glass ceramic core materials by induced compressive residual stresses. However, the core materials of dental restorations need to be veneered or at least to be stained and glazed for esthetic and functional reasons. The objective of this study was to determine the effect of different ion exchange treatments on the strength parameters of stained and glazed glass ceramics. Batches of specimens made of a leucite reinforced dental glass with and without staining and glazing layer, untreated, single ion exchanged (KNO3), and dual ion exchanged (1. KNO3/27, 2. 30 mol% NaNO3/70 mol% KNO3) were tested. The strength of the core material was increased from 117 to 213 MPa by single ion exchange. Staining and glazing increased the strength up to 165 MPa. Single ion exchange of the stained and glazed core caused only a slight additional strength increase up to 173 MPa. The dual ion exchanged stained and glazed core exhibit a strength of 195 MPa and decreased the large strength scatter because of a well‐designed residual stress profile. We conclude that dual ion exchange treatments could significantly increase the mechanical reliability of stained and glazed glass ceramic restorations. © 2004 Wiley Periodicals, Inc. J Biomed Mater Res 72A: 175–179, 2005
- 30 November 2004
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 72A (2) , 175-179
Effect of ion exchange of glazed dental glass ceramics on strength parameters
Ion exchange treatments can significantly increase the strength of dental glass ceramic core materials by induced compressive residual stresses. However, the core materials of dental restorations need to be veneered or at least to be stained and glazed for esthetic and functional reasons. The objective of this study was to determine the effect of different ion exchange treatments on the strength parameters of stained and glazed glass ceramics. Batches of specimens made of a leucite reinforced dental glass with and without staining and glazing layer, untreated, single ion exchanged (KNO3), and dual ion exchanged (1. KNO3/27, 2. 30 mol% NaNO3/70 mol% KNO3) were tested. The strength of the core material was increased from 117 to 213 MPa by single ion exchange. Staining and glazing increased the strength up to 165 MPa. Single ion exchange of the stained and glazed core caused only a slight additional strength increase up to 173 MPa. The dual ion exchanged stained and glazed core exhibit a strength of 195 MPa and decreased the large strength scatter because of a well‐designed residual stress profile. We conclude that dual ion exchange treatments could significantly increase the mechanical reliability of stained and glazed glass ceramic restorations. © 2004 Wiley Periodicals, Inc. J Biomed Mater Res 72A: 175–179, 2005
- 1 March 2004
- Published by Elsevier in Journal of Biomechanics
- Vol. 37 (3) , 289-294
Finite element and experimental analyses of polymer-based dental bridges reinforced by ceramic bars
- 1 March 2004
- Published by Elsevier in Journal of Biomechanics
- Vol. 37 (3) , 289-294
Finite element and experimental analyses of polymer-based dental bridges reinforced by ceramic bars
- 1 December 2003
- Published by SAGE Publications in Journal of Dental Research
- Vol. 82 (12) , 972-975
Effect of Surface Roughness on Flexural Strength of Veneer Ceramics
The strength of ceramic restorations depends on the occlusal surface roughness of the veneering porcelain, which is influenced by the final preparation. The hypothesis of the study was that roughnesses below a critical microscopic defect size—based only on fracture mechanics considerations—also affect flexural strength. The bending failure stress was evaluated on standard specimens of 4 veneer ceramics with 4 different surfaces of defined roughnesses, respectively. A linear correlation was found between roughness and failure stress. A "roughness-free" failure stress value was predicted for each tested material. This theoretical value can represent the "true" strength of the respective ceramic material. We conclude from our results that the final preparation of a ceramic restoration is critical to the strength of the material, and that ceramic veneering materials can be compared more objectively with respect to their strength by means of roughness-free strength values.
- 1 December 2003
- Published by SAGE Publications in Journal of Dental Research
- Vol. 82 (12) , 972-975
Effect of Surface Roughness on Flexural Strength of Veneer Ceramics
The strength of ceramic restorations depends on the occlusal surface roughness of the veneering porcelain, which is influenced by the final preparation. The hypothesis of the study was that roughnesses below a critical microscopic defect size—based only on fracture mechanics considerations—also affect flexural strength. The bending failure stress was evaluated on standard specimens of 4 veneer ceramics with 4 different surfaces of defined roughnesses, respectively. A linear correlation was found between roughness and failure stress. A "roughness-free" failure stress value was predicted for each tested material. This theoretical value can represent the "true" strength of the respective ceramic material. We conclude from our results that the final preparation of a ceramic restoration is critical to the strength of the material, and that ceramic veneering materials can be compared more objectively with respect to their strength by means of roughness-free strength values.