Kajetan Müller
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Kajetan Müller has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- Sven Sängerlaub
Department for Technical Systems, Processes and Communication Munich University of Applied Sciences HM Munich Germany
4 shared publications - Astrid Pant
TUM School of Life Sciences Weihenstephan, Chair of Food Packaging Technology, Technical University of Munich, Freising, Germany
1 shared publication - Camelia Stinga
BT3 Technologies, Impasse Bellevue 8, 38240 Meylan, France
1 shared publication Claudia Schoenweitz
Materials Development Fraunhofer Institute for Process Engineering and Packaging IVV Freising Germany
1 shared publication- Cornelia Stramm
Fraunhofer Institute for Process Engineering and Packaging IVV, Giggenhauser Straße 35, Freising 85354, Germany
1 shared publication - Daniel Samain
BT3 Technologies, Impasse Bellevue 8, 38240 Meylan, France
1 shared publication
Latest Publications
- Open Access
UV-Activated, Transparent Oxygen Scavenger Coating Based on Inorganic–Organic Hybrid Polymer (ORMOCER®) with High Oxygen Absorption Capacity
Oxygen scavengers are used to reduce the oxygen permeation of packaging (active barrier) and to absorb oxygen from its direct environment, e.g., a headspace of packaged food. Few oxygen scavenger coatings have been developed. Therefore, in this study, a novel oxygen scavenger coating has been developed. It is based on inorganic–organic polymers (ORMOCER®). The oxygen absorption reaction is activated by UV light. The scavenger was synthesized, coated on aluminum foil, subsequently dried and afterwards laminated with a polyethylene sealing layer. UV light activates the oxygen scavenging reaction. The oxygen absorption capacity, measured at 23 °C and 0% r.h., was 242 ± 8 mg oxygen/g scavenger coating. When the oxygen scavenger coating layer was laminated by using a two-component polyurethane laminating adhesive, the absorption capacity was hardly reduced, with a measured absorption capacity of 223 ± 18 mg oxygen/g scavenger coating. In an experimental packaging sample with the oxygen scavenger coating with a thickness (dry) of 3 µm and 18 µm, near-zero mbar oxygen partial pressure was reached by the non-laminated oxygen scavenger coatings within two days, and within about 20 days when laminated with a polyurethane laminating adhesive and a PE-layer on the oxygen scavenger layer. The oxygen partial pressure was kept near zero mbar for 500 days, whereas in the experimental packaging without oxygen scavenger, the oxygen partial pressure increased to 110 mbar during this time. The developed oxygen scavenger based on inorganic–organic polymers can be applied as wet chemical coating on various surfaces with standard application procedures. Application scenarios are oxygen-sensitive goods such as food, pharmaceutical products and cosmetics.
Open AccessUV-Activated, Transparent Oxygen Scavenger Coating Based on Inorganic–Organic Hybrid Polymer (ORMOCER®) with High Oxygen Absorption Capacity
Oxygen scavengers are used to reduce the oxygen permeation of packaging (active barrier) and to absorb oxygen from its direct environment, e.g., a headspace of packaged food. Few oxygen scavenger coatings have been developed. Therefore, in this study, a novel oxygen scavenger coating has been developed. It is based on inorganic–organic polymers (ORMOCER®). The oxygen absorption reaction is activated by UV light. The scavenger was synthesized, coated on aluminum foil, subsequently dried and afterwards laminated with a polyethylene sealing layer. UV light activates the oxygen scavenging reaction. The oxygen absorption capacity, measured at 23 °C and 0% r.h., was 242 ± 8 mg oxygen/g scavenger coating. When the oxygen scavenger coating layer was laminated by using a two-component polyurethane laminating adhesive, the absorption capacity was hardly reduced, with a measured absorption capacity of 223 ± 18 mg oxygen/g scavenger coating. In an experimental packaging sample with the oxygen scavenger coating with a thickness (dry) of 3 µm and 18 µm, near-zero mbar oxygen partial pressure was reached by the non-laminated oxygen scavenger coatings within two days, and within about 20 days when laminated with a polyurethane laminating adhesive and a PE-layer on the oxygen scavenger layer. The oxygen partial pressure was kept near zero mbar for 500 days, whereas in the experimental packaging without oxygen scavenger, the oxygen partial pressure increased to 110 mbar during this time. The developed oxygen scavenger based on inorganic–organic polymers can be applied as wet chemical coating on various surfaces with standard application procedures. Application scenarios are oxygen-sensitive goods such as food, pharmaceutical products and cosmetics.
- Open Access
Desiccant Films Made of Low-Density Polyethylene with Dispersed Silica Gel—Water Vapor Absorption, Permeability (H2O, N2, O2, CO2), and Mechanical Properties
Silica gel is a well-known desiccant. Through dispersion of silica gel in a polymer, films can be made that absorb and desorb water vapor. The water vapor absorption becomes reversible by exposing such films to a water vapor pressure below that of the water vapor pressure during absorption, or by heating the film. The intention of this study was to achieve a better understanding about the water vapor absorption, permeability (H2O, N2, O2, CO2), and mechanical properties of films with dispersed silica gel. Low-density polyethylene (PE-LD) monolayer films with a nominal silica gel concentration of 0.2, 0.4, and 0.6 g dispersed silica gel per 1 g film (PE-LD) were prepared and they absorbed up to 0.08 g water vapor per 1 g of film. The water vapor absorption as a function of time was described by using effective diffusion coefficients. The steady state (effective) water vapor permeation coefficients of the films with dispersed silica gel were a factor of 2 to 14 (8.4 to 60.2·10−12 mg·cm·(cm2·s·Pa)−1, 23 °C) higher than for pure PE-LD films (4.3·10−12 mg·cm·(cm²·s·Pa)−1, 23 °C). On the other hand, the steady state gas permeabilities for N2, O2, and CO2 were reduced to around one-third of the pure PE-LD films. An important result is that (effective) water vapor permeation coefficients calculated from results of sorption and measured by permeation experiments yielded similar values. It has been found that it is possible to describe the sorption and diffusion behavior of water by knowing the permeability coefficient and the sorption capacity of the film ( ). The tensile stress changed only slightly (values between 10 and 14 N mm−2), while the tensile strain at break was reduced with higher nominal silica gel concentration from 318 length-% (pure PE-LD film) to 5 length-% (PE-LD with 0.6 g dispersed silica gel per 1 g film).Open AccessDesiccant Films Made of Low-Density Polyethylene with Dispersed Silica Gel—Water Vapor Absorption, Permeability (H2O, N2, O2, CO2), and Mechanical Properties
Silica gel is a well-known desiccant. Through dispersion of silica gel in a polymer, films can be made that absorb and desorb water vapor. The water vapor absorption becomes reversible by exposing such films to a water vapor pressure below that of the water vapor pressure during absorption, or by heating the film. The intention of this study was to achieve a better understanding about the water vapor absorption, permeability (H2O, N2, O2, CO2), and mechanical properties of films with dispersed silica gel. Low-density polyethylene (PE-LD) monolayer films with a nominal silica gel concentration of 0.2, 0.4, and 0.6 g dispersed silica gel per 1 g film (PE-LD) were prepared and they absorbed up to 0.08 g water vapor per 1 g of film. The water vapor absorption as a function of time was described by using effective diffusion coefficients. The steady state (effective) water vapor permeation coefficients of the films with dispersed silica gel were a factor of 2 to 14 (8.4 to 60.2·10−12 mg·cm·(cm2·s·Pa)−1, 23 °C) higher than for pure PE-LD films (4.3·10−12 mg·cm·(cm²·s·Pa)−1, 23 °C). On the other hand, the steady state gas permeabilities for N2, O2, and CO2 were reduced to around one-third of the pure PE-LD films. An important result is that (effective) water vapor permeation coefficients calculated from results of sorption and measured by permeation experiments yielded similar values. It has been found that it is possible to describe the sorption and diffusion behavior of water by knowing the permeability coefficient and the sorption capacity of the film ( ). The tensile stress changed only slightly (values between 10 and 14 N mm−2), while the tensile strain at break was reduced with higher nominal silica gel concentration from 318 length-% (pure PE-LD film) to 5 length-% (PE-LD with 0.6 g dispersed silica gel per 1 g film). - Open Access
Gallic Acid as an Oxygen Scavenger in Bio-Based Multilayer Packaging Films
Oxygen scavengers are used in food packaging to protect oxygen-sensitive food products. A mixture of gallic acid (GA) and sodium carbonate was used as an oxygen scavenger (OSc) in bio-based multilayer packaging films produced in a three-step process: compounding, flat film extrusion, and lamination. We investigated the film surface color as well as oxygen absorption at different relative humidities (RHs) and temperatures, and compared the oxygen absorption of OSc powder, monolayer films, and multilayer films. The films were initially brownish-red in color but changed to greenish-black during oxygen absorption under humid conditions. We observed a maximum absorption capacity of 447 mg O2/g GA at 21 °C and 100% RH. The incorporation of GA into a polymer matrix reduced the rate of oxygen absorption compared to the GA powder because the polymer acted as a barrier to oxygen and water vapor diffusion. As expected, the temperature had a significant effect on the initial absorption rate of the multilayer films; the corresponding activation energy was 75.4 kJ/mol. Higher RH significantly increased the oxygen absorption rate. These results demonstrate for the first time the production and the properties of a bio-based multilayer packaging film with GA as the oxygen scavenger. Potential applications include the packaging of food products with high water activity (aw > 0.86).
Open AccessGallic Acid as an Oxygen Scavenger in Bio-Based Multilayer Packaging Films
Oxygen scavengers are used in food packaging to protect oxygen-sensitive food products. A mixture of gallic acid (GA) and sodium carbonate was used as an oxygen scavenger (OSc) in bio-based multilayer packaging films produced in a three-step process: compounding, flat film extrusion, and lamination. We investigated the film surface color as well as oxygen absorption at different relative humidities (RHs) and temperatures, and compared the oxygen absorption of OSc powder, monolayer films, and multilayer films. The films were initially brownish-red in color but changed to greenish-black during oxygen absorption under humid conditions. We observed a maximum absorption capacity of 447 mg O2/g GA at 21 °C and 100% RH. The incorporation of GA into a polymer matrix reduced the rate of oxygen absorption compared to the GA powder because the polymer acted as a barrier to oxygen and water vapor diffusion. As expected, the temperature had a significant effect on the initial absorption rate of the multilayer films; the corresponding activation energy was 75.4 kJ/mol. Higher RH significantly increased the oxygen absorption rate. These results demonstrate for the first time the production and the properties of a bio-based multilayer packaging film with GA as the oxygen scavenger. Potential applications include the packaging of food products with high water activity (aw > 0.86).
- Open Access
Water Repellence and Oxygen and Water Vapor Barrier of PVOH-Coated Substrates before and after Surface Esterification
This study investigates chemical grafting with fatty acid chlorides as a method for the surface modification of hydrophilic web materials. The resulting changes in the water repellence and barrier properties were studied. For this purpose, different grades of polyvinyl alcohol (PVOH) were coated on regenerated cellulose films (“cellophane”) and paper and then grafted with fatty acid chlorides. The PVOH grades varied in their degree of hydrolysis and average molecular weight. The surface was esterified with two fatty acid chlorides, palmitoyl (C16) and stearoyl chloride (C18), by chemical grafting. The chemical grafting resulted in water-repellent surfaces and reduced water vapor transmission rates by a factor of almost 19. The impact of the surface modification was greater for a higher degree of hydrolysis of the polyvinyl alcohol and for shorter fatty acid chains. Although the water vapor barrier for palmitoyl-grafted PVOH was higher than for stearoyl-grafted PVOH, the contact angle with water was lower. Additionally, it was shown that a higher degree of hydrolysis led to higher water vapor barrier improvement factors after grafting. Furthermore, the oxygen permeability decreased after grafting significantly, due to the fact that the grafting protects the PVOH against humidity when the humidity is applied on the grafted side. It can be concluded that the carbon chain length of the fatty acid chlorides is the limiting factor for water vapor adsorption, but the grafting density is the bottleneck for water diffusing in the polymer.
Open AccessWater Repellence and Oxygen and Water Vapor Barrier of PVOH-Coated Substrates before and after Surface Esterification
This study investigates chemical grafting with fatty acid chlorides as a method for the surface modification of hydrophilic web materials. The resulting changes in the water repellence and barrier properties were studied. For this purpose, different grades of polyvinyl alcohol (PVOH) were coated on regenerated cellulose films (“cellophane”) and paper and then grafted with fatty acid chlorides. The PVOH grades varied in their degree of hydrolysis and average molecular weight. The surface was esterified with two fatty acid chlorides, palmitoyl (C16) and stearoyl chloride (C18), by chemical grafting. The chemical grafting resulted in water-repellent surfaces and reduced water vapor transmission rates by a factor of almost 19. The impact of the surface modification was greater for a higher degree of hydrolysis of the polyvinyl alcohol and for shorter fatty acid chains. Although the water vapor barrier for palmitoyl-grafted PVOH was higher than for stearoyl-grafted PVOH, the contact angle with water was lower. Additionally, it was shown that a higher degree of hydrolysis led to higher water vapor barrier improvement factors after grafting. Furthermore, the oxygen permeability decreased after grafting significantly, due to the fact that the grafting protects the PVOH against humidity when the humidity is applied on the grafted side. It can be concluded that the carbon chain length of the fatty acid chlorides is the limiting factor for water vapor adsorption, but the grafting density is the bottleneck for water diffusing in the polymer.
- 26 September 2011
- Published by Wiley in Packaging Technology and Science
- Vol. 25 (3) , 137-148
Thin Laminate Films for Barrier Packaging Application – Influence of Down Gauging and Substrate Surface Properties on the Permeation Properties
A reduction in thickness of barrier laminated film systems generally leads to a quality decrease of the resulting packaging materials' functional properties. Especially for food packaging applications, adequate oxygen and water barrier properties are indispensable. The focus of this study was therefore the development of thin film systems using metallized aluminium or ethyl vinyl alcohol barrier laminates with low oxygen and water vapour transmission properties. Biaxially oriented polyethylene terephthalate and biaxially oriented polypropylene aluminium‐coated thin film laminates as well as corresponding ethyl vinyl alcohol film systems could be successfully produced with oxygen transmission rates of <0.5 cm³(STP)/(m² d bar) and water barrier values of <0.1 g/(m² d). It could be confirmed that the film thickness of these materials within the range of the investigated dimensions does not have an influence on the barrier properties. In fact, the parameters of the production process influence the functional properties of the film systems and must therefore be adapted. Machinability of these excellent thin film systems requires further investigation on packaging lines before they can be transferred to packaging application. Copyright © 2011 John Wiley & Sons, Ltd.
- 26 September 2011
- Published by Wiley in Packaging Technology and Science
- Vol. 25 (3) , 137-148
Thin Laminate Films for Barrier Packaging Application – Influence of Down Gauging and Substrate Surface Properties on the Permeation Properties
A reduction in thickness of barrier laminated film systems generally leads to a quality decrease of the resulting packaging materials' functional properties. Especially for food packaging applications, adequate oxygen and water barrier properties are indispensable. The focus of this study was therefore the development of thin film systems using metallized aluminium or ethyl vinyl alcohol barrier laminates with low oxygen and water vapour transmission properties. Biaxially oriented polyethylene terephthalate and biaxially oriented polypropylene aluminium‐coated thin film laminates as well as corresponding ethyl vinyl alcohol film systems could be successfully produced with oxygen transmission rates of <0.5 cm³(STP)/(m² d bar) and water barrier values of <0.1 g/(m² d). It could be confirmed that the film thickness of these materials within the range of the investigated dimensions does not have an influence on the barrier properties. In fact, the parameters of the production process influence the functional properties of the film systems and must therefore be adapted. Machinability of these excellent thin film systems requires further investigation on packaging lines before they can be transferred to packaging application. Copyright © 2011 John Wiley & Sons, Ltd.