Sukanda Jiansirisomboon
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Sukanda Jiansirisomboon has a total of 22 co-authors. Here are the top co-authors by number of shared publications:
Anucha Watcharapasorn
Department of Physics and Materials Science, Faculty of Science, Chiang Mai University, Chiang Mai, Thailand; Materials Science Research Center, Faculty of Science, Chiang Mai University, Chiang Mai, Thailand
12 shared publicationsPharatree Jaita
Department of Physics and Materials Science, Faculty of Science, Chiang Mai University, Chiang Mai, Thailand
5 shared publicationsMethee Promsawat
Department of Physics and Materials Science, Faculty of Science, Chiang Mai University, 239 Huay Kaew Road, Muang, Chiang Mai, 50200, Thailand; Materials Science Research Center, Faculty of Science, Chiang Mai University, 239 Huay Kaew Road, Muang, Chiang Mai, 50200, Thailand
3 shared publicationsOrapim Namsar
Department of Physics and Materials Science, Faculty of Science, Chiang Mai University, Chiang Mai, Thailand
3 shared publications- Zuo-Guang Ye
Department of Chemistry and 4D LABS, Simon Fraser University, Burnaby, British Columbia V5A 1S6, Canada
3 shared publications A. Watcharapasorn
Chiang Mai University
2 shared publications
Latest Publications
- 12 August 2016
- Published by Taylor & Francis in Integrated Ferroelectrics
- Vol. 175 (1) , 1-8
Electrical properties of ternary system Bi0.5(Na0.80K0.20)0.5TiO3-0.005LiNbO3-BaTiO3lead-free piezoelectric ceramics
Ternary system of lead-free piezoelectric ceramics with the formula of (1-x-y)Bi0.5(Na0.80K0.20)0.5TiO3-xLiNbO3-yBaTiO3 or (1-x-y)BNKT-xLN-yBT (x = 0.005 and y = 0, 0.01, 0.02, 0.03, 0.04, 0.05, 0.06 and 0.07 mol fraction) were sintered at the temperature of 1125°C for 2 h. All samples have the density ranging of 5.59 - 5.73 g/cm3. X-ray diffraction pattern exhibited a single perovskite structure without any secondary phase. Scanning electron micrographs indicated a cubic-like grain shape occurred for all compositions with side length of 0.49 - 0.77 μm. At a composition BNKT-0.005LN-0.04BT showed the highest piezoelectric coefficient (d33 = 198 pC/N) with good dielectric (ϵr = 1775, tanδ = 0.0534) and ferroelectric properties (Pr = 17.36 μC/cm2, Rsq = 1.67).
- 12 August 2016
- Published by Taylor & Francis in Integrated Ferroelectrics
- Vol. 175 (1) , 1-8
Electrical properties of ternary system Bi0.5(Na0.80K0.20)0.5TiO3-0.005LiNbO3-BaTiO3lead-free piezoelectric ceramics
Ternary system of lead-free piezoelectric ceramics with the formula of (1-x-y)Bi0.5(Na0.80K0.20)0.5TiO3-xLiNbO3-yBaTiO3 or (1-x-y)BNKT-xLN-yBT (x = 0.005 and y = 0, 0.01, 0.02, 0.03, 0.04, 0.05, 0.06 and 0.07 mol fraction) were sintered at the temperature of 1125°C for 2 h. All samples have the density ranging of 5.59 - 5.73 g/cm3. X-ray diffraction pattern exhibited a single perovskite structure without any secondary phase. Scanning electron micrographs indicated a cubic-like grain shape occurred for all compositions with side length of 0.49 - 0.77 μm. At a composition BNKT-0.005LN-0.04BT showed the highest piezoelectric coefficient (d33 = 198 pC/N) with good dielectric (ϵr = 1775, tanδ = 0.0534) and ferroelectric properties (Pr = 17.36 μC/cm2, Rsq = 1.67).
- 13 April 2016
- Published by Springer Nature in Journal of Electroceramics
- Vol. 36 (1-4) , 70-75
Dielectric properties, electric-field-induced polarization and strain behavior of Lead Zirconate Titanate-Strontium bismuth Niobate ceramics
- 13 April 2016
- Published by Springer Nature in Journal of Electroceramics
- Vol. 36 (1-4) , 70-75
Dielectric properties, electric-field-induced polarization and strain behavior of Lead Zirconate Titanate-Strontium bismuth Niobate ceramics
- 7 February 2016
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 99 (5) , 1615-1624
Lead‐Free (Ba0.70Sr0.30)TiO3‐Modified Bi0.5(Na0.80K0.20)0.5TiO3 Ceramics with Large Electric Field–Induced Strains
The dielectric, ferroelectric, and electric field–induced strain behavior of Bi0.5(Na0.80K0.20)0.5TiO3 (BNKT) ceramics modified with (Ba0.70Sr0.30)O3 (BST) were investigated as a function of composition and temperature. The ceramic samples were synthesized by a solid‐state mixed oxide method and sintered at 1125°C for 2 h. The XRD and Raman spectra showed coexisting rhombohedral and tetragonal phases throughout the entire compositional range with the tetragonal phase becoming dominant at higher BST concentrations. For all compositions, the temperature dependence of the dielectric spectra revealed a frequency dependence that is characteristic of a relaxor mechanism. This suggests that these ceramics lacked long‐range order and it appears that the maximum disorder was observed for the composition with 5 mol% BST (BNKT–0.05BST sample). This was evidenced by the observation of pinched hysteresis loops, even at room temperature, and a significant decrease in the Pr and Ec values which resulted in large electric field–induced strains (Smax) of 0.40% and a normalized strain coefficient ( = Smax/Emax) of 732 pm/V. This significant strain enhancement at the composition of x = 0.05 may be attributed to both a composition‐induced structural phase transition and a field‐induced relaxor to ferroelectric phase transition.
- 7 February 2016
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 99 (5) , 1615-1624
Lead‐Free (Ba0.70Sr0.30)TiO3‐Modified Bi0.5(Na0.80K0.20)0.5TiO3 Ceramics with Large Electric Field–Induced Strains
The dielectric, ferroelectric, and electric field–induced strain behavior of Bi0.5(Na0.80K0.20)0.5TiO3 (BNKT) ceramics modified with (Ba0.70Sr0.30)O3 (BST) were investigated as a function of composition and temperature. The ceramic samples were synthesized by a solid‐state mixed oxide method and sintered at 1125°C for 2 h. The XRD and Raman spectra showed coexisting rhombohedral and tetragonal phases throughout the entire compositional range with the tetragonal phase becoming dominant at higher BST concentrations. For all compositions, the temperature dependence of the dielectric spectra revealed a frequency dependence that is characteristic of a relaxor mechanism. This suggests that these ceramics lacked long‐range order and it appears that the maximum disorder was observed for the composition with 5 mol% BST (BNKT–0.05BST sample). This was evidenced by the observation of pinched hysteresis loops, even at room temperature, and a significant decrease in the Pr and Ec values which resulted in large electric field–induced strains (Smax) of 0.40% and a normalized strain coefficient ( = Smax/Emax) of 732 pm/V. This significant strain enhancement at the composition of x = 0.05 may be attributed to both a composition‐induced structural phase transition and a field‐induced relaxor to ferroelectric phase transition.
- 20 November 2015
- Published by Taylor & Francis in Ferroelectrics
- Vol. 489 (1) , 118-128
X-ray Photoelectron Spectroscopy Analysis and Electrical Properties of Bi0.5(Na0.80K0.20)0.5TiO3-LiNbO3Lead-Free Piezoelectrics
Lead-free piezoelectric ceramics with formula of (1-x)Bi0.5(Na0.80K0.20)0.5TiO3-xLiNbO3 or (1-x)BNKT-xLN (when x = 0, 0.005, 0.010, 0.015 and 0.020 mol fraction) were produced by a solid-state mixed oxide method. The ceramics with density ranging 5.38 - 5.68 g/cm3 were obtained by sintering at 1100°C. X-ray diffraction pattern showed that (1-x)BNKT-xLN ceramics exhibited pure perovskite structure. X-ray photoelectron spectroscopy analysis was used to identify of chemical composition, chemical state and binding energy of ionic species in the ceramics. Dielectric, ferroelectric and piezoelectric properties of all ceramics were investigated and found to be optimized at the composition of x = 0.005.
- 20 November 2015
- Published by Taylor & Francis in Ferroelectrics
- Vol. 489 (1) , 118-128
X-ray Photoelectron Spectroscopy Analysis and Electrical Properties of Bi0.5(Na0.80K0.20)0.5TiO3-LiNbO3Lead-Free Piezoelectrics
Lead-free piezoelectric ceramics with formula of (1-x)Bi0.5(Na0.80K0.20)0.5TiO3-xLiNbO3 or (1-x)BNKT-xLN (when x = 0, 0.005, 0.010, 0.015 and 0.020 mol fraction) were produced by a solid-state mixed oxide method. The ceramics with density ranging 5.38 - 5.68 g/cm3 were obtained by sintering at 1100°C. X-ray diffraction pattern showed that (1-x)BNKT-xLN ceramics exhibited pure perovskite structure. X-ray photoelectron spectroscopy analysis was used to identify of chemical composition, chemical state and binding energy of ionic species in the ceramics. Dielectric, ferroelectric and piezoelectric properties of all ceramics were investigated and found to be optimized at the composition of x = 0.005.
- 30 October 2015
- Published by Taylor & Francis in Ferroelectrics
- Vol. 488 (1) , 79-88
Dielectric, Polarization and Strain Response of Enhanced Complex Ceramics: The Study through Pb(Zr0.52Ti0.48)O3-SrBi2Ta2O9
Electrical properties of the (1-x)PZT-xSBT ceramics (0.1≤x≤0.3) were investigated in comparison with pure PZT and SBT ceramics. It was found that the dielectric constant increased with small addition of SBT (x = 0.1) into PZT. The hysteresis loop measurement demonstrated that the PZT-SBT ceramics showed larger remanent polarization than pure PZT and less coercive filed than pure SBT ceramic. Strain behavior showed a symmetric butterfly curve in the compositions with 0≤x≤0.3 but the low strain obtained was found in pure SBT. This research suggested that 0.9PZT-0.1SBT ceramic is a promising material to be further utilized in ferroelectric memory devices.
- 30 October 2015
- Published by Taylor & Francis in Ferroelectrics
- Vol. 488 (1) , 79-88
Dielectric, Polarization and Strain Response of Enhanced Complex Ceramics: The Study through Pb(Zr0.52Ti0.48)O3-SrBi2Ta2O9
Electrical properties of the (1-x)PZT-xSBT ceramics (0.1≤x≤0.3) were investigated in comparison with pure PZT and SBT ceramics. It was found that the dielectric constant increased with small addition of SBT (x = 0.1) into PZT. The hysteresis loop measurement demonstrated that the PZT-SBT ceramics showed larger remanent polarization than pure PZT and less coercive filed than pure SBT ceramic. Strain behavior showed a symmetric butterfly curve in the compositions with 0≤x≤0.3 but the low strain obtained was found in pure SBT. This research suggested that 0.9PZT-0.1SBT ceramic is a promising material to be further utilized in ferroelectric memory devices.
- 8 October 2015
- Published by Taylor & Francis in Ferroelectrics
- Vol. 487 (1) , 1-8
Phase Development and Dielectric, Ferroelectric and Piezoelectric Properties of Pb(Mg1/3Nb2/3)0.9Ti0.1O3-Bi0.5(Na0.74K0.26)0.5TiO3Ceramics
In this work, the relationships between phase development and the properties of a new relaxor based ferroelectric (1-x)Pb(Mg1/3Nb2/3)0.9Ti0.1O3-xBi0.5(Na0.74K0.26)0.5TiO3 ceramics (when x = 0.0, 0.1, 0.3, 0.5, 0.7, 0.9 and 1.0 mole fraction) was studied. The pseudo-cubic structure was observed in the ceramics with x ≤ 0.7 mole fraction. The rhombohedral and tetragonal phases were found to coexist when x increased to 0.9, which transformed into the single tetragonal phase when x increased to 1.0. The dielectric constant measured at room temperature decreased with increasing x. The remnant polarization and piezoelectric constant of the ceramics significantly increased when x increased to 0.9 and 1.0.
- 8 October 2015
- Published by Taylor & Francis in Ferroelectrics
- Vol. 487 (1) , 1-8
Phase Development and Dielectric, Ferroelectric and Piezoelectric Properties of Pb(Mg1/3Nb2/3)0.9Ti0.1O3-Bi0.5(Na0.74K0.26)0.5TiO3Ceramics
In this work, the relationships between phase development and the properties of a new relaxor based ferroelectric (1-x)Pb(Mg1/3Nb2/3)0.9Ti0.1O3-xBi0.5(Na0.74K0.26)0.5TiO3 ceramics (when x = 0.0, 0.1, 0.3, 0.5, 0.7, 0.9 and 1.0 mole fraction) was studied. The pseudo-cubic structure was observed in the ceramics with x ≤ 0.7 mole fraction. The rhombohedral and tetragonal phases were found to coexist when x increased to 0.9, which transformed into the single tetragonal phase when x increased to 1.0. The dielectric constant measured at room temperature decreased with increasing x. The remnant polarization and piezoelectric constant of the ceramics significantly increased when x increased to 0.9 and 1.0.
- 10 September 2015
- Published by Springer Nature in Electronic Materials Letters
- Vol. 11 (5) , 881-889
Polarization fatigue in ferroelectric Pb(Zr0.52Ti0.48)O3-SrBi2Nb2O9 ceramics
- 10 September 2015
- Published by Springer Nature in Electronic Materials Letters
- Vol. 11 (5) , 881-889
Polarization fatigue in ferroelectric Pb(Zr0.52Ti0.48)O3-SrBi2Nb2O9 ceramics
- 10 September 2015
- Published by Springer Nature in Electronic Materials Letters
- Vol. 11 (5) , 828-835
Large electric field-induced strain and piezoelectric responses of lead-free Bi0.5(Na0.80K0.20)0.5TiO3-Ba(Ti0.90Sn0.10)O3 ceramics near morphotropic phase boundary
- 10 September 2015
- Published by Springer Nature in Electronic Materials Letters
- Vol. 11 (5) , 828-835
Large electric field-induced strain and piezoelectric responses of lead-free Bi0.5(Na0.80K0.20)0.5TiO3-Ba(Ti0.90Sn0.10)O3 ceramics near morphotropic phase boundary
- 10 December 2014
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 98 (3) , 848-854
Enhanced Dielectric and Ferroelectric Properties of Pb(Mg1/3Nb2/3)0.65Ti0.35O3 Ceramics by ZnO Modification
Phase formation, microstructures, dielectric, and ferroelectric properties of ZnO‐modified Pb(Mg1/3Nb2/3)0.65Ti0.35O3 (PMNT/xZnO, where x = 0, 0.4, 2.0, 4.0, and 11.0 mol%) ceramics were studied. A coexistence of rhombohedral and tetragonal ferroelectric phases was observed at room temperature in all samples. The ceramics with the relative densities of 93%–95% were prepared. The modification by ZnO led to an increase in grain sizes of PMNT ceramics. The maximum dielectric constant of the pure PMNT ceramic was increased with x = 0.4–4.0 mol% ZnO doping, with the highest value being observed in the 2.0 mol% sample. Both the temperature at which the transition between rhombohedral and tetragonal ferroelectric phases took place (TR‐T) and the Curie temperature of the ceramics tended to increase with increasing x. The ferroelectric properties were enhanced with increased remanent polarization and P(E) loop squareness in the compositions with x = 0.4–4.0 mol%. However, the ferroelectric properties were attenuated with x = 11.0 mol%.
- 10 December 2014
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 98 (3) , 848-854
Enhanced Dielectric and Ferroelectric Properties of Pb(Mg1/3Nb2/3)0.65Ti0.35O3 Ceramics by ZnO Modification
Phase formation, microstructures, dielectric, and ferroelectric properties of ZnO‐modified Pb(Mg1/3Nb2/3)0.65Ti0.35O3 (PMNT/xZnO, where x = 0, 0.4, 2.0, 4.0, and 11.0 mol%) ceramics were studied. A coexistence of rhombohedral and tetragonal ferroelectric phases was observed at room temperature in all samples. The ceramics with the relative densities of 93%–95% were prepared. The modification by ZnO led to an increase in grain sizes of PMNT ceramics. The maximum dielectric constant of the pure PMNT ceramic was increased with x = 0.4–4.0 mol% ZnO doping, with the highest value being observed in the 2.0 mol% sample. Both the temperature at which the transition between rhombohedral and tetragonal ferroelectric phases took place (TR‐T) and the Curie temperature of the ceramics tended to increase with increasing x. The ferroelectric properties were enhanced with increased remanent polarization and P(E) loop squareness in the compositions with x = 0.4–4.0 mol%. However, the ferroelectric properties were attenuated with x = 11.0 mol%.
- 31 May 2014
- Published by Springer Nature in Journal of Electroceramics
- Vol. 33 (1-2) , 96-104
Enhanced ferroelectric order in Pb(Mg1/3Nb2/3)0.9Ti0.1O3 ceramics by ZnO modification
- 31 May 2014
- Published by Springer Nature in Journal of Electroceramics
- Vol. 33 (1-2) , 96-104
Enhanced ferroelectric order in Pb(Mg1/3Nb2/3)0.9Ti0.1O3 ceramics by ZnO modification