Tsutomu Ohzuku
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Tsutomu Ohzuku has a total of 29 co-authors. Here are the top co-authors by number of shared publications:
Kingo Ariyoshi
Department of Applied Chemistry, Graduate School of Engineering, Osaka City University (OCU), Osaka 558-8585, Japan
7 shared publicationsMitsuyasu Imazaki
Department of Applied Chemistry, Graduate School of Engineering, Osaka City University (OCU), Osaka 558-8585, Japan
3 shared publicationsKazuhiko Mukai
Toyota Central Research and Development Laboratories Inc., Nagakute, Aichi 480-1192, Japan
2 shared publications- Kingo Ariyoshi
Department of Chemistry and Bioengineering, Graduate School of Engineering, Osaka Metropolitan University
2 shared publications - Naoaki Yabuuchi
Department of Chemistry and Life Science Yokohama National University Yokohama Japan
2 shared publications Noriaki Nakayama
Department of Advanced Materials Science and Engineering, Faculty of Engineering, Yamaguchi University, Ube 755-8611, Japan
2 shared publications
Latest Publications
- Open Access
- 1 January 2012
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 159 (10) , A1710-A1715
Capacity Fading of Lithium-Ion Cells Having Li[Li1/3Ti5/3]O4(LTO)-Negative Electrodes for the First- and Second-Generation 12 V Lead-Free Batteries
Lithium-ion cells consisting of Li[Li1/3Ti5/3]O4 (LTO) and Li[Li0.1Al0.1Mn1.8]O4 (LAMO) or Li[Ni1/2Mn3/2]O4 (LiNiMO) were examined at currents higher than 1 mA cm−2 at room temperature. Capacity fading was observed for both LTO/LAMO and LTO/LiNiMO cells during the continuous charge and discharge at 1, 2, and 4 mA cm−2 when a microporous membrane usually used so far was applied. In order to understand the capacity fading, Li/LAMO and Li/LTO cells together with zero-volt lithium-ion cells consisting of LTO or LAMO were fabricated and examined. Among these cells, the rechargeable capacity of a zero-volt lithium-ion cell of LTO with a microporous membrane faded cycle by cycle, while the other cells did not show such obvious capacity fading. From these results, a possible source of capacity fading was discussed in terms of a mass transport problem due to the “zero-strain” insertion electrode combined with a microporous membrane. A solution of the problem is also given in such a way that a non-woven cloth is substituted for the microporous membrane as a separator in LTO/LAMO and LTO/LiNiMO cells for the first- and second-generation 12 V lead-free batteries, respectively.
- 1 January 2012
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 159 (10) , A1710-A1715
Open AccessCapacity Fading of Lithium-Ion Cells Having Li[Li1/3Ti5/3]O4(LTO)-Negative Electrodes for the First- and Second-Generation 12 V Lead-Free Batteries
Lithium-ion cells consisting of Li[Li1/3Ti5/3]O4 (LTO) and Li[Li0.1Al0.1Mn1.8]O4 (LAMO) or Li[Ni1/2Mn3/2]O4 (LiNiMO) were examined at currents higher than 1 mA cm−2 at room temperature. Capacity fading was observed for both LTO/LAMO and LTO/LiNiMO cells during the continuous charge and discharge at 1, 2, and 4 mA cm−2 when a microporous membrane usually used so far was applied. In order to understand the capacity fading, Li/LAMO and Li/LTO cells together with zero-volt lithium-ion cells consisting of LTO or LAMO were fabricated and examined. Among these cells, the rechargeable capacity of a zero-volt lithium-ion cell of LTO with a microporous membrane faded cycle by cycle, while the other cells did not show such obvious capacity fading. From these results, a possible source of capacity fading was discussed in terms of a mass transport problem due to the “zero-strain” insertion electrode combined with a microporous membrane. A solution of the problem is also given in such a way that a non-woven cloth is substituted for the microporous membrane as a separator in LTO/LAMO and LTO/LiNiMO cells for the first- and second-generation 12 V lead-free batteries, respectively.
- 11 April 2011
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry
- Vol. 21 (27) , 10179-10188
High-capacity lithium insertion materials of lithium nickel manganese oxides for advanced lithium-ion batteries: toward rechargeable capacity more than 300 mA h g−1
Lithium nickel manganese oxides Li[NixLi(1/ 3−2x/3)Mn(2/ 3−x/3)]O2 (x = 1/2, 2/7, and 1/5) are prepared and characterized by XRD and FT-IR, and the samples are examined in non-aqueous lithium cells at room temperature and 55 °C. Among these materials LiNi1 / 2Mn1 / 2O2 (x = 1/2) shows the highest operating voltage and the smallest polarization with a rechargeable capacity of ca. 230 mA h g−1 and Li[Li1/ 5Ni1 / 5Mn3 /5]O2 (x = 1/5) shows the lowest operating voltage and the largest polarization with a rechargeable capacity more than 300 mA h g−1. Extraordinarily large rechargeable capacity of Li[Li1/ 5Ni1 / 5Mn3 /5]O2 together with an anomalously long voltage plateau at 4.5 V only observed at first charging process is examined by window-opening charge and discharge, continuous charge and discharge combined with differential chronopotentiometry at room temperature and at 55 °C, and possible mechanisms are discussed in terms of lithium insertion scheme.
- 11 April 2011
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry
- Vol. 21 (27) , 10179-10188
High-capacity lithium insertion materials of lithium nickel manganese oxides for advanced lithium-ion batteries: toward rechargeable capacity more than 300 mA h g−1
Lithium nickel manganese oxides Li[NixLi(1/ 3−2x/3)Mn(2/ 3−x/3)]O2 (x = 1/2, 2/7, and 1/5) are prepared and characterized by XRD and FT-IR, and the samples are examined in non-aqueous lithium cells at room temperature and 55 °C. Among these materials LiNi1 / 2Mn1 / 2O2 (x = 1/2) shows the highest operating voltage and the smallest polarization with a rechargeable capacity of ca. 230 mA h g−1 and Li[Li1/ 5Ni1 / 5Mn3 /5]O2 (x = 1/5) shows the lowest operating voltage and the largest polarization with a rechargeable capacity more than 300 mA h g−1. Extraordinarily large rechargeable capacity of Li[Li1/ 5Ni1 / 5Mn3 /5]O2 together with an anomalously long voltage plateau at 4.5 V only observed at first charging process is examined by window-opening charge and discharge, continuous charge and discharge combined with differential chronopotentiometry at room temperature and at 55 °C, and possible mechanisms are discussed in terms of lithium insertion scheme.
- 1 January 2011
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 158 (4) , A417-A421
Silicon-Based Negative Electrode for High-Capacity Lithium-Ion Batteries: “SiO”-Carbon Composite
The silicon-based materials were prepared and examined in lithium cells for high-capacity lithium-ion batteries. Among the materials examined, “SiO”-carbon composite showed remarkable improvements on capacity fading. “SiO” is composed of nanosized silicon crystallites highly dispersed in an amorphous silicon dioxide matrix. The “SiO”-carbon composite materials consisting of “SiO,” graphite, and carbon fiber with carbon coatings show the smallest irreversible capacity at the first cycle and the best capacity retention among the other silicon-based materials examined, such as carbon-coated silicon, the one-to-one mixture of “SiO” and graphite, or one-to-one mixture of carbon-coated “SiO” and graphite. Capacity of more than 85% compared to capacities observed for initial ten cycles is retained after 100 cycles when the laminate-type cell with a positive electrode is examined in voltage ranging from 2.5 to 4.2 V, which meets the requirement on the negative electrodes for practical high-capacity lithium-ion batteries.
- 1 January 2011
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 158 (4) , A417-A421
Silicon-Based Negative Electrode for High-Capacity Lithium-Ion Batteries: “SiO”-Carbon Composite
The silicon-based materials were prepared and examined in lithium cells for high-capacity lithium-ion batteries. Among the materials examined, “SiO”-carbon composite showed remarkable improvements on capacity fading. “SiO” is composed of nanosized silicon crystallites highly dispersed in an amorphous silicon dioxide matrix. The “SiO”-carbon composite materials consisting of “SiO,” graphite, and carbon fiber with carbon coatings show the smallest irreversible capacity at the first cycle and the best capacity retention among the other silicon-based materials examined, such as carbon-coated silicon, the one-to-one mixture of “SiO” and graphite, or one-to-one mixture of carbon-coated “SiO” and graphite. Capacity of more than 85% compared to capacities observed for initial ten cycles is retained after 100 cycles when the laminate-type cell with a positive electrode is examined in voltage ranging from 2.5 to 4.2 V, which meets the requirement on the negative electrodes for practical high-capacity lithium-ion batteries.
- 21 November 2009
- Published by Oxford University Press (OUP) in Chemistry Letters
- Vol. 38 (12) , 1202-1203
An Approach to 12-V Lead-free Batteries: High Temperature 3600-cycle Examinations on a 2.5-V LTO/LAMO Battery
- 21 November 2009
- Published by Oxford University Press (OUP) in Chemistry Letters
- Vol. 38 (12) , 1202-1203
An Approach to 12-V Lead-free Batteries: High Temperature 3600-cycle Examinations on a 2.5-V LTO/LAMO Battery
- 8 May 2009
- Published by American Physical Society (APS) in Physical Review B
- Vol. 79 (18) , 184411
investigation of local magnetic order inIn order to elucidate the magnetic nature of the lithium chromium dioxide , in which the ions form a two-dimensional triangular lattice in the plane, we have performed a positive muon-spin rotation and relaxation experiment using a powder sample in the temperature range 1.7–155 K. Weak-transverse-field measurements indicated the existence of a bulk antiferromagnetic (AF) transition at . Below , zero-field (ZF) measurements demonstrated the formation of static long-range order; the observed ZF spectrum was well reproduced by the AF spin structure proposed by neutron measurements. The measurements also indicated that is a pure paramagnet for , since its internal magnetic field can be explained by solely nuclear magnetic moments. This means that, contrary to previous suggestions by susceptibility and heat capacity measurements, no short-range order exists for . However, detected the change in from a low- static state to a high- dynamic state at 115 K, most likely connected to a change in the position/motion of the Li ions.- 8 May 2009
- Published by American Physical Society (APS) in Physical Review B
- Vol. 79 (18) , 184411
investigation of local magnetic order inIn order to elucidate the magnetic nature of the lithium chromium dioxide , in which the ions form a two-dimensional triangular lattice in the plane, we have performed a positive muon-spin rotation and relaxation experiment using a powder sample in the temperature range 1.7–155 K. Weak-transverse-field measurements indicated the existence of a bulk antiferromagnetic (AF) transition at . Below , zero-field (ZF) measurements demonstrated the formation of static long-range order; the observed ZF spectrum was well reproduced by the AF spin structure proposed by neutron measurements. The measurements also indicated that is a pure paramagnet for , since its internal magnetic field can be explained by solely nuclear magnetic moments. This means that, contrary to previous suggestions by susceptibility and heat capacity measurements, no short-range order exists for . However, detected the change in from a low- static state to a high- dynamic state at 115 K, most likely connected to a change in the position/motion of the Li ions.- 1 January 2009
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 156 (10) , A780-A786
An Approach to 12 V “Lead-Free” Batteries: Tolerance toward Overcharge of 2.5 V Battery Consisting of LTO and LAMO
The 2.5 V cell consisting of lithium titanium oxide (LTO) Li[Li1/3Ti5/3]O4Li[Li1/3Ti5/3]O4 and lithium aluminum manganese oxide (LAMO) Li[Li0.1Al0.1Mn1.8]O4Li[Li0.1Al0.1Mn1.8]O4 is examined in terms of tolerance toward overcharge in voltages up to 5.2 V. LTO can be cycled with ca. 225mAhg−1225mAhg−1 of rechargeable capacity in voltages ranging from 0 to 2 V in a Li/LTO cell. The fatal damage was not observed even after LTO at 0 V was stored at 25°C25°C for 2 weeks. LAMO can be cycled with ca. 120mAhg−1120mAhg−1 of rechargeable capacity in voltages ranging from 3 to 5.2 V in a Li/LAMO cell without a dramatic capacity fading during 52 cycles. Because the 12 V batteries consist of five 2.5 V cells connected in series, occasional 26 V input is possible for the 12 V batteries. X-ray diffraction measurements on the positive and negative electrodes under overcharged conditions are also performed and show that both LTO and LAMO are resistive against overcharge. From the results, we discuss whether or not the materials selection based on a spinel-framework structure is correct for the 12 V “lead-free” batteries.
- 1 January 2009
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 156 (10) , A780-A786
An Approach to 12 V “Lead-Free” Batteries: Tolerance toward Overcharge of 2.5 V Battery Consisting of LTO and LAMO
The 2.5 V cell consisting of lithium titanium oxide (LTO) Li[Li1/3Ti5/3]O4Li[Li1/3Ti5/3]O4 and lithium aluminum manganese oxide (LAMO) Li[Li0.1Al0.1Mn1.8]O4Li[Li0.1Al0.1Mn1.8]O4 is examined in terms of tolerance toward overcharge in voltages up to 5.2 V. LTO can be cycled with ca. 225mAhg−1225mAhg−1 of rechargeable capacity in voltages ranging from 0 to 2 V in a Li/LTO cell. The fatal damage was not observed even after LTO at 0 V was stored at 25°C25°C for 2 weeks. LAMO can be cycled with ca. 120mAhg−1120mAhg−1 of rechargeable capacity in voltages ranging from 3 to 5.2 V in a Li/LAMO cell without a dramatic capacity fading during 52 cycles. Because the 12 V batteries consist of five 2.5 V cells connected in series, occasional 26 V input is possible for the 12 V batteries. X-ray diffraction measurements on the positive and negative electrodes under overcharged conditions are also performed and show that both LTO and LAMO are resistive against overcharge. From the results, we discuss whether or not the materials selection based on a spinel-framework structure is correct for the 12 V “lead-free” batteries.
- 21 November 2007
- Published by Springer Nature in Journal of Solid State Electrochemistry
- Vol. 12 (7) , 979-985
Steady-state polarization measurements of lithium insertion electrodes for high-power lithium-ion batteries
- 21 November 2007
- Published by Springer Nature in Journal of Solid State Electrochemistry
- Vol. 12 (7) , 979-985
Steady-state polarization measurements of lithium insertion electrodes for high-power lithium-ion batteries
- 1 January 2007
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 154 (4) , A314-A321
Solid-State Chemistry and Electrochemistry of LiCo[sub 1∕3]Ni[sub 1∕3]Mn[sub 1∕3]O[sub 2] for Advanced Lithium-Ion Batteries
Reaction mechanism of LiCo1∕3Ni1∕3Mn1∕3O2LiCo1∕3Ni1∕3Mn1∕3O2 was examined by ex situ X-ray diffraction (XRD) and electrochemical methods. According to XRD results, the change in hexagonal lattice parameters was quite similar to that of Li1−xCo1∕2Ni1∕2O2Li1−xCo1∕2Ni1∕2O2 , i.e., the unit cell volume was almost constant at 0≤x<2∕30≤xLi1−xCo1∕3Ni1∕3Mn1∕3O2Li1−xCo1∕3Ni1∕3Mn1∕3O2 , indicating homogeneous phase reaction over an entire range. Reversible-potential measurements on Li1−xCo1∕3Ni1∕3Mn1∕3O2Li1−xCo1∕3Ni1∕3Mn1∕3O2 (0≤x<1)(0≤xLi+◻Co1∕3Ni1∕3Mn1∕3O2→LiCo1∕3Ni1∕3Mn1∕3O2Li+◻Co1∕3Ni1∕3Mn1∕3O2→LiCo1∕3Ni1∕3Mn1∕3O2 was obtained to be ΔG=−398kJmol−1ΔG=−398kJmol−1 , which was slightly higher than that for LiCo1∕2Ni1∕2O2LiCo1∕2Ni1∕2O2 (−393kJmol−1)(−393kJmol−1) . Rechargeable capacity (Q)(Q) as a function of charge-end voltage (Ece)(Ece) was examined for Li∕LiCo1∕3Ni1∕3Mn1∕3O2Li∕LiCo1∕3Ni1∕3Mn1∕3O2 cells and the relation between QQ in mAhg−1mAhg−1 and EceEce in V was given to be Q=151+121Q=151+121 (Ece−4.2)(Ece−4.2) . From these results, rechargeable capacity and cycleability as a function of charge-end voltage are discussed in relation to the reaction mechanism of LiCo1∕3Ni1∕3Mn1∕3O2LiCo1∕3Ni1∕3Mn1∕3O2 .
- 1 January 2007
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 154 (4) , A314-A321
Solid-State Chemistry and Electrochemistry of LiCo[sub 1∕3]Ni[sub 1∕3]Mn[sub 1∕3]O[sub 2] for Advanced Lithium-Ion Batteries
Reaction mechanism of LiCo1∕3Ni1∕3Mn1∕3O2LiCo1∕3Ni1∕3Mn1∕3O2 was examined by ex situ X-ray diffraction (XRD) and electrochemical methods. According to XRD results, the change in hexagonal lattice parameters was quite similar to that of Li1−xCo1∕2Ni1∕2O2Li1−xCo1∕2Ni1∕2O2 , i.e., the unit cell volume was almost constant at 0≤x<2∕30≤xLi1−xCo1∕3Ni1∕3Mn1∕3O2Li1−xCo1∕3Ni1∕3Mn1∕3O2 , indicating homogeneous phase reaction over an entire range. Reversible-potential measurements on Li1−xCo1∕3Ni1∕3Mn1∕3O2Li1−xCo1∕3Ni1∕3Mn1∕3O2 (0≤x<1)(0≤xLi+◻Co1∕3Ni1∕3Mn1∕3O2→LiCo1∕3Ni1∕3Mn1∕3O2Li+◻Co1∕3Ni1∕3Mn1∕3O2→LiCo1∕3Ni1∕3Mn1∕3O2 was obtained to be ΔG=−398kJmol−1ΔG=−398kJmol−1 , which was slightly higher than that for LiCo1∕2Ni1∕2O2LiCo1∕2Ni1∕2O2 (−393kJmol−1)(−393kJmol−1) . Rechargeable capacity (Q)(Q) as a function of charge-end voltage (Ece)(Ece) was examined for Li∕LiCo1∕3Ni1∕3Mn1∕3O2Li∕LiCo1∕3Ni1∕3Mn1∕3O2 cells and the relation between QQ in mAhg−1mAhg−1 and EceEce in V was given to be Q=151+121Q=151+121 (Ece−4.2)(Ece−4.2) . From these results, rechargeable capacity and cycleability as a function of charge-end voltage are discussed in relation to the reaction mechanism of LiCo1∕3Ni1∕3Mn1∕3O2LiCo1∕3Ni1∕3Mn1∕3O2 .
- 1 May 2006
- Published by Springer Nature in Research on Chemical Intermediates
- Vol. 32 (5) , 507-521
Formation of solid solution and its effect on lithium insertion schemes for advanced lithium-ion batteries: X-ray absorption spectroscopy and X-ray diffraction of LiCoO2, LiCo1/2Ni1/2O2 and LiNiO2
The X-ray absorption spectra (XAS) of LiCoO2, LiCo1/2Ni1/2O2 and LiNiO2 were examined together with X-ray diffraction (XRD). Co and Ni K-edge XANES spectra
- 1 May 2006
- Published by Springer Nature in Research on Chemical Intermediates
- Vol. 32 (5) , 507-521
Formation of solid solution and its effect on lithium insertion schemes for advanced lithium-ion batteries: X-ray absorption spectroscopy and X-ray diffraction of LiCoO2, LiCo1/2Ni1/2O2 and LiNiO2
The X-ray absorption spectra (XAS) of LiCoO2, LiCo1/2Ni1/2O2 and LiNiO2 were examined together with X-ray diffraction (XRD). Co and Ni K-edge XANES spectra
- 1 January 2006
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 9 (12) , A557-A560
Lithium Aluminum Manganese Oxide Having Spinel-Framework Structure for Long-Life Lithium-Ion Batteries
Lithium aluminum manganese oxide (LAMO) having a spinel-framework structure was prepared and examined in lithium nonaqueous cells. LAMO shows extremely small irreversible capacity with rechargeable capacity of ca. in lithium cells operated in voltage of 3 to . To show durability for long-life applications, a lithium-ion cell of and LAMO was fabricated and accelerated cycle tests were done at room temperature in voltage of 2 to for 3600 cycles, and an empirical relation between capacity and number of cycle was obtained to be .
- 1 January 2006
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 9 (12) , A557-A560
Lithium Aluminum Manganese Oxide Having Spinel-Framework Structure for Long-Life Lithium-Ion Batteries
Lithium aluminum manganese oxide (LAMO) having a spinel-framework structure was prepared and examined in lithium nonaqueous cells. LAMO shows extremely small irreversible capacity with rechargeable capacity of ca. in lithium cells operated in voltage of 3 to . To show durability for long-life applications, a lithium-ion cell of and LAMO was fabricated and accelerated cycle tests were done at room temperature in voltage of 2 to for 3600 cycles, and an empirical relation between capacity and number of cycle was obtained to be .