Boyd W. Veal
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Boyd W. Veal has a total of 69 co-authors. Here are the top co-authors by number of shared publications:
A. P. Paulikas
Argonne National Laboratory
4 shared publicationsH Claus
3 shared publicationsA P Paulikas
2 shared publicationsA.P. Paulikas
2 shared publications- G. W. Crabtree
Materials Science Division, Argonne National Laboratory, Argonne, Illinois 60439
2 shared publications - P. Y. Hou
Lawrence Berkeley National Laboratory
2 shared publications
Latest Publications
- 4 May 2007
- Published by Springer Nature in Oxidation of Metals
- Vol. 68 (1-2) , 37-51
Chromium-oxide Growth on Fe–Cr–Ni Alloy Studied with Grazing-emission X-ray Fluorescence
- 4 May 2007
- Published by Springer Nature in Oxidation of Metals
- Vol. 68 (1-2) , 37-51
Chromium-oxide Growth on Fe–Cr–Ni Alloy Studied with Grazing-emission X-ray Fluorescence
- 16 October 2006
- Published by AIP Publishing in Applied Physics Letters
- Vol. 89 (16) , 161916
Mechanisms and control of phase transition in thermally grown aluminas
The oxidation rate of β-NiAl, at 1100°C in air, can be slowed by means of a mechanical polish with α-Al2O3 grit. Particles embedded during polishing act as nucleation sites for conversion of the initially formed θ-Al2O3 to the stable α-Al2O3 phase. Since θ-phase growth is much faster than α-phase growth, accelerated θ→α conversion results in a thinner oxide when conversion is complete. A model is presented to quantitatively describe this behavior.
- 16 October 2006
- Published by AIP Publishing in Applied Physics Letters
- Vol. 89 (16) , 161916
Mechanisms and control of phase transition in thermally grown aluminas
The oxidation rate of β-NiAl, at 1100°C in air, can be slowed by means of a mechanical polish with α-Al2O3 grit. Particles embedded during polishing act as nucleation sites for conversion of the initially formed θ-Al2O3 to the stable α-Al2O3 phase. Since θ-phase growth is much faster than α-phase growth, accelerated θ→α conversion results in a thinner oxide when conversion is complete. A model is presented to quantitatively describe this behavior.
- 9 April 2006
- Published by Springer Nature in Nature Materials
- Vol. 5 (5) , 349-351
Tensile stress and creep in thermally grown oxide
Structural components that operate at high temperatures (for example, turbine blades) rely on thermally grown oxide (TGO), commonly alumina, for corrosion protection. Strains that develop in TGOs during operation can reduce the protectiveness of the TGO. However, the occurrence of growth strains in TGOs, and mechanisms that cause them, are poorly understood. It is accepted that compressive strains can develop as oxygen and metal atoms meet to form new growth within constrained oxide. More controversial is the experimental finding that large tensile stresses, close to 1 GPa, develop during isothermal growth conditions in alumina TGO formed on a FeCrAlY alloy. Using a novel technique based on synchrotron radiation, we have confirmed these previous results, and show that the tensile strain develops as the early oxide, (Fe,Cr,Al)(2)O(3), converts to alpha-Al2O3 during the growth process. This allows us to model the strain behaviour by including creep and this diffusion-controlled phase change.
- 9 April 2006
- Published by Springer Nature in Nature Materials
- Vol. 5 (5) , 349-351
Tensile stress and creep in thermally grown oxide
Structural components that operate at high temperatures (for example, turbine blades) rely on thermally grown oxide (TGO), commonly alumina, for corrosion protection. Strains that develop in TGOs during operation can reduce the protectiveness of the TGO. However, the occurrence of growth strains in TGOs, and mechanisms that cause them, are poorly understood. It is accepted that compressive strains can develop as oxygen and metal atoms meet to form new growth within constrained oxide. More controversial is the experimental finding that large tensile stresses, close to 1 GPa, develop during isothermal growth conditions in alumina TGO formed on a FeCrAlY alloy. Using a novel technique based on synchrotron radiation, we have confirmed these previous results, and show that the tensile strain develops as the early oxide, (Fe,Cr,Al)(2)O(3), converts to alpha-Al2O3 during the growth process. This allows us to model the strain behaviour by including creep and this diffusion-controlled phase change.
- 15 August 2005
- Published by Maney Publishing in Materials at High Temperatures
- Vol. 22 (3) , 535-543
Stress development and relaxation in Al2O3 during early stage oxidation of β-NiAl
- 15 August 2005
- Published by Maney Publishing in Materials at High Temperatures
- Vol. 22 (3) , 535-543
Stress development and relaxation in Al2O3 during early stage oxidation of β-NiAl
- 2 January 2005
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 22 (3) , 535-543
Stress development and relaxation in Al 2 O 3 during early stage oxidation of β-NiAl
- 2 January 2005
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 22 (3) , 535-543
Stress development and relaxation in Al 2 O 3 during early stage oxidation of β-NiAl
- 18 April 2002
- Published by IOP Publishing in Superconductor Science and Technology
- Vol. 15 (5) , 672-674
Joining of melt-textured YBCO: a direct contact method
We report a method for making weld joints, capable of transmitting high supercurrent densities, in bulk samples of melt-textured YBCO. The joining procedure is carried out in a flowing atmosphere of O2 to eliminate problems associated with nitrogen gas, which can become trapped in the joint. No filler or fluxing material is used. The method can be used to join large areas (several cm2) that are capable of transmitting supercurrent densities exceeding 104 A cm−2.
- 18 April 2002
- Published by IOP Publishing in Superconductor Science and Technology
- Vol. 15 (5) , 672-674
Joining of melt-textured YBCO: a direct contact method
We report a method for making weld joints, capable of transmitting high supercurrent densities, in bulk samples of melt-textured YBCO. The joining procedure is carried out in a flowing atmosphere of O2 to eliminate problems associated with nitrogen gas, which can become trapped in the joint. No filler or fluxing material is used. The method can be used to join large areas (several cm2) that are capable of transmitting supercurrent densities exceeding 104 A cm−2.
- 17 November 1999
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 86 (11) , 6282-6286
Contactless characterization of melt-textured superconducting junctions using micro-Hall sensor arrays
We use spatially resolved Hall-probe magnetometry and magneto-optical imaging to study current-carrying properties of melt-textured high-temperature superconducting welds at high magnetic fields. Magneto-optical images show no deterioration of the current-carrying properties of the sample in the presence of the superconducting weld. The study of the vortex dynamics near the junction using high-resolution Hall-probe magnetometry revealed enhanced relaxation of the magnetization at the junction at high temperatures. We attribute this behavior to an increased local concentration of defects near the weld that, depending on the temperature range, either facilitates enhanced relaxation or strengthens the local pinning properties.
- 17 November 1999
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 86 (11) , 6282-6286
Contactless characterization of melt-textured superconducting junctions using micro-Hall sensor arrays
We use spatially resolved Hall-probe magnetometry and magneto-optical imaging to study current-carrying properties of melt-textured high-temperature superconducting welds at high magnetic fields. Magneto-optical images show no deterioration of the current-carrying properties of the sample in the presence of the superconducting weld. The study of the vortex dynamics near the junction using high-resolution Hall-probe magnetometry revealed enhanced relaxation of the magnetization at the junction at high temperatures. We attribute this behavior to an increased local concentration of defects near the weld that, depending on the temperature range, either facilitates enhanced relaxation or strengthens the local pinning properties.
- 1 September 1999
- Published by Elsevier in Physica C: Superconductivity and its Applications
- Vol. 322 (1-2) , 1-8
High critical current “weld” joints in textured YBa2Cu3Ox
- 1 September 1999
- Published by Elsevier in Physica C: Superconductivity and its Applications
- Vol. 322 (1-2) , 1-8
High critical current “weld” joints in textured YBa2Cu3Ox
- 1 February 1995
- Published by American Physical Society (APS) in Physical Review B
- Vol. 51 (6) , 3981-3984
Hall-effect studies of the mixed state ofY1−xPrxBa2Cu3O7−δ(0≤x≤0.42) andYBa2Cu3Oy(6.65≤y≤6.84) single crystals
The maximum value Δ of the negative Hall resistivity of (0≤x≲0.13) and (6.73≲y≤6.84) single crystals scales with T/, exhibiting a maximum for T/≊0.96 and vanishing for T/≲0.87. scales with and decreases monotonically with decreasing to zero for ≲70 K. The Hall conductivity vs B data have been analyzed using the expression =/B+B, where the two terms are associated with motion of the magnetic vortices and the quasiparticles in the vortex cores, respectively, yielding and as functions of x, y, and T.- 1 February 1995
- Published by American Physical Society (APS) in Physical Review B
- Vol. 51 (6) , 3981-3984
Hall-effect studies of the mixed state ofY1−xPrxBa2Cu3O7−δ(0≤x≤0.42) andYBa2Cu3Oy(6.65≤y≤6.84) single crystals
The maximum value Δ of the negative Hall resistivity of (0≤x≲0.13) and (6.73≲y≤6.84) single crystals scales with T/, exhibiting a maximum for T/≊0.96 and vanishing for T/≲0.87. scales with and decreases monotonically with decreasing to zero for ≲70 K. The Hall conductivity vs B data have been analyzed using the expression =/B+B, where the two terms are associated with motion of the magnetic vortices and the quasiparticles in the vortex cores, respectively, yielding and as functions of x, y, and T.