Antti Niskanen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Antti Niskanen has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
- Kai Arstila
Accelerator Laboratory, Department of Physics, University of Jyvaskyla 1 , P.O. Box 35, FI-40014 Jyvaskyla, Finland
2 shared publications - Markku Leskelä
Department of Chemistry, University of Helsinki, P. O. Box 55, FI-00014, Finland
2 shared publications - Mikko Ritala
Department of Chemistry University of Helsinki Helsinki Finland
2 shared publications
Latest Publications
- 4 April 2007
- Published by Wiley in Chemical Vapor Deposition
- Vol. 13 (4) , 152-157
Radical Enhanced Atomic Layer Deposition of Titanium Dioxide
Titanium dioxide films are grown with radical‐enhanced atomic layer deposition (RE‐ALD) from titanium isopropoxide and oxygen radicals at between 50 and 300 °C on silicon, glass, platinum, and RuO2 surfaces. Additionally, the films are grown on polymers and natural fibers at 50 °C. The oxygen radicals are produced by dissociating molecular oxygen with a remote microwave plasma discharge. Purified argon is used as the carrier and purge gas. Growth rate saturation and conformal growth are observed, and thus the film growth in the ALD mode was proven. The saturated growth rate is 0.19 nm per cycle at 50 °C, with an overall cycle time of 11 s. The film grown at 50 °C has a dielectric constant of 20, and undergoes catastrophic breakdown at 0.6 MV cm–1 electric field. It contains 13 at.‐% hydrogen and 4 at.‐% carbon. As the deposition temperature is increased to 250 °C, the impurity contents decrease to 0.5 at.‐% for hydrogen and 0.4 at.‐% for carbon. The film density and refractive index are 3.2 g cm–3 and 2.2, respectively, for a film deposited at 50 °C, and increases to 3.8 g cm–3 and 2.4, respectively, for a film deposited at 250 °C. All the films grown below 250 °C are amorphous according to X‐ray diffraction (XRD).
- 4 April 2007
- Published by Wiley in Chemical Vapor Deposition
- Vol. 13 (4) , 152-157
Radical Enhanced Atomic Layer Deposition of Titanium Dioxide
Titanium dioxide films are grown with radical‐enhanced atomic layer deposition (RE‐ALD) from titanium isopropoxide and oxygen radicals at between 50 and 300 °C on silicon, glass, platinum, and RuO2 surfaces. Additionally, the films are grown on polymers and natural fibers at 50 °C. The oxygen radicals are produced by dissociating molecular oxygen with a remote microwave plasma discharge. Purified argon is used as the carrier and purge gas. Growth rate saturation and conformal growth are observed, and thus the film growth in the ALD mode was proven. The saturated growth rate is 0.19 nm per cycle at 50 °C, with an overall cycle time of 11 s. The film grown at 50 °C has a dielectric constant of 20, and undergoes catastrophic breakdown at 0.6 MV cm–1 electric field. It contains 13 at.‐% hydrogen and 4 at.‐% carbon. As the deposition temperature is increased to 250 °C, the impurity contents decrease to 0.5 at.‐% for hydrogen and 0.4 at.‐% for carbon. The film density and refractive index are 3.2 g cm–3 and 2.2, respectively, for a film deposited at 50 °C, and increases to 3.8 g cm–3 and 2.4, respectively, for a film deposited at 250 °C. All the films grown below 250 °C are amorphous according to X‐ray diffraction (XRD).
- 1 January 2005
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 152 (7) , F90-F93
Low-Temperature Deposition of Aluminum Oxide by Radical Enhanced Atomic Layer Deposition
Aluminum oxide was deposited by radical enhanced atomic layer deposition using trimethylaluminum (TMA) and oxygen radicals in the temperature range 25-300°C25-300°C . The radicals were produced by dissociating oxygen gas in a remote microwave plasma discharge. Oxygen was mixed with argon which was also used as the carrier and purge gas. Films were grown on silicon, glass, and indium tin oxide coated glass substrates. Additional growth experiments were conducted on heat-sensitive materials: polyethene, polypropene, and wool. The time to complete one deposition cycle was nearly independent of the deposition temperature, being around 10s10s for all deposition temperatures. Growth rates were between 1.5 and 2.9Åpercycle2.9Åpercycle , which is higher than what has been obtained with the TMA-H2OTMA-H2O process in similar reactor conditions. The films were amorphous according to X-ray diffraction. The films were also very smooth; the surface root-mean-square roughness was less than 0.8nm0.8nm for 180nm180nm thick films. The films had breakdown fields, defined as the field corresponding to the leakage current density of 1μA∕cm21μA∕cm2 , between 6 and 10MV∕cm10MV∕cm , and dielectric constants between 6.5 and 8.1. The film impurity levels according to time-of-flight elastic recoil detection analysis were between 0.8 and 15 atom % for hydrogen and 0.2 and 4 atom % for carbon. The refractive indexes at 580nm580nm were between 1.60 and 1.64.
- 1 January 2005
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 152 (7) , F90-F93
Low-Temperature Deposition of Aluminum Oxide by Radical Enhanced Atomic Layer Deposition
Aluminum oxide was deposited by radical enhanced atomic layer deposition using trimethylaluminum (TMA) and oxygen radicals in the temperature range 25-300°C25-300°C . The radicals were produced by dissociating oxygen gas in a remote microwave plasma discharge. Oxygen was mixed with argon which was also used as the carrier and purge gas. Films were grown on silicon, glass, and indium tin oxide coated glass substrates. Additional growth experiments were conducted on heat-sensitive materials: polyethene, polypropene, and wool. The time to complete one deposition cycle was nearly independent of the deposition temperature, being around 10s10s for all deposition temperatures. Growth rates were between 1.5 and 2.9Åpercycle2.9Åpercycle , which is higher than what has been obtained with the TMA-H2OTMA-H2O process in similar reactor conditions. The films were amorphous according to X-ray diffraction. The films were also very smooth; the surface root-mean-square roughness was less than 0.8nm0.8nm for 180nm180nm thick films. The films had breakdown fields, defined as the field corresponding to the leakage current density of 1μA∕cm21μA∕cm2 , between 6 and 10MV∕cm10MV∕cm , and dielectric constants between 6.5 and 8.1. The film impurity levels according to time-of-flight elastic recoil detection analysis were between 0.8 and 15 atom % for hydrogen and 0.2 and 4 atom % for carbon. The refractive indexes at 580nm580nm were between 1.60 and 1.64.