Wu Kai
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Wu Kai has a total of 79 co-authors. Here are the top co-authors by number of shared publications:
R. T. Huang
National Taiwan Ocean University
5 shared publicationsP.K. Liaw
Department of Materials Science and Engineering, University of Tennessee, 434 Dougherty Hall, Knoxville, TN 37996, USA
4 shared publicationsH.H. Hsieh
Institute of Materials Engineering, National Taiwan Ocean University, Keelung 20224, Taiwan, ROC
3 shared publicationsT.H. Ho
Institute of Materials Engineering, National Taiwan Ocean University, Keelung 20224, Taiwan, ROC
3 shared publicationsW. Zhang
Dalian University of Technology
3 shared publicationsY.R. Chen
Institute of Materials Engineering, National Taiwan Ocean University, Keelung 20224, Taiwan, ROC
3 shared publications
Latest Publications
- 15 March 2026
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1061
Effect of Nb content on the oxidation of NbxTiAlCrSi light-weight refractory high-entropy alloys
- 15 March 2026
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1061
Effect of Nb content on the oxidation of NbxTiAlCrSi light-weight refractory high-entropy alloys
- 24 March 2025
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1022
Effects of Cr and Al additions on the oxidation of FeCoNi-based medium- and high-entropy alloys in CO2/CO mixed gases
- 24 March 2025
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1022
Effects of Cr and Al additions on the oxidation of FeCoNi-based medium- and high-entropy alloys in CO2/CO mixed gases
- Open Access
Failure Analysis of a C-276 Alloy Pipe in a Controlled Decomposition Reactor
Failure analysis was carried out on a ruptured C-276 pipe heated externally at 1050 °C, which had been used for a few months in a controlled decomposition reactor (CDR) system. To catch the decomposed perfluorinated compounds (PFCs, e.g., CF4, SF6, NF3, C3F8 and C4F8) present in the exhaust gas, the C-276 reactor was periodically purged with water mist, which caused a temperature gradient from the external to the inner surface of the pipe. The precipitation of large amounts of intermetallic compounds along the grain boundaries were found to be corroded preferentially. The internal surface of the used pipe was covered with many fine cracks. The corrosion and cracking of grain boundary precipitates accounted for the short service life of the C-276 pipe. Compositional measurements by electron probe micro-analyzer (EPMA) and phase identification by electron backscatter diffraction (EBSD) confirmed the presence of δ and μ phases in the ruptured pipe. The coarse intergranular precipitates were the δ phase (Mo7Ni7), which were enriched in Mo and Cr. Moreover, the fine precipitates dispersed intergranularly and intragranularly were the μ phase (Mo6Ni7), which were abundant in Mo and W. The numerous precipitates present in the matrix and along the grain boundaries were responsible for an obvious loss in the strength and ductility of the used C-276 pipe.
Open AccessFailure Analysis of a C-276 Alloy Pipe in a Controlled Decomposition Reactor
Failure analysis was carried out on a ruptured C-276 pipe heated externally at 1050 °C, which had been used for a few months in a controlled decomposition reactor (CDR) system. To catch the decomposed perfluorinated compounds (PFCs, e.g., CF4, SF6, NF3, C3F8 and C4F8) present in the exhaust gas, the C-276 reactor was periodically purged with water mist, which caused a temperature gradient from the external to the inner surface of the pipe. The precipitation of large amounts of intermetallic compounds along the grain boundaries were found to be corroded preferentially. The internal surface of the used pipe was covered with many fine cracks. The corrosion and cracking of grain boundary precipitates accounted for the short service life of the C-276 pipe. Compositional measurements by electron probe micro-analyzer (EPMA) and phase identification by electron backscatter diffraction (EBSD) confirmed the presence of δ and μ phases in the ruptured pipe. The coarse intergranular precipitates were the δ phase (Mo7Ni7), which were enriched in Mo and Cr. Moreover, the fine precipitates dispersed intergranularly and intragranularly were the μ phase (Mo6Ni7), which were abundant in Mo and W. The numerous precipitates present in the matrix and along the grain boundaries were responsible for an obvious loss in the strength and ductility of the used C-276 pipe.
- 1 January 2021
- Published by Elsevier in Surface and Coatings Technology
- Vol. 405
Oxidation behavior and interdiffusion of Ta Al multilayer films and Inconel 617 alloy
- 1 January 2021
- Published by Elsevier in Surface and Coatings Technology
- Vol. 405
Oxidation behavior and interdiffusion of Ta Al multilayer films and Inconel 617 alloy
- 21 February 2019
- Published by Springer Nature in Oxidation of Metals
- Vol. 91 (3-4) , 437-449
The Corrosion of an Amorphous Fe70C10P10B5Mo5 Alloy in Various CO2/CO Mixed Gases at 500 °C
- 21 February 2019
- Published by Springer Nature in Oxidation of Metals
- Vol. 91 (3-4) , 437-449
The Corrosion of an Amorphous Fe70C10P10B5Mo5 Alloy in Various CO2/CO Mixed Gases at 500 °C
- 1 September 2018
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 763, 209-215
Air-oxidation of an amorphous Fe70C10P10B5Mo5 alloy at 400–500 °C
- 1 September 2018
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 763, 209-215
Air-oxidation of an amorphous Fe70C10P10B5Mo5 alloy at 400–500 °C
- 10 February 2018
- Published by Springer Nature in Oxidation of Metals
- Vol. 90 (3-4) , 279-290
Air Oxidation Behavior of (Fe41Cr15Mo14C12B9Co7Y2)97Ta3 Bulk Metallic Glass
- 10 February 2018
- Published by Springer Nature in Oxidation of Metals
- Vol. 90 (3-4) , 279-290
Air Oxidation Behavior of (Fe41Cr15Mo14C12B9Co7Y2)97Ta3 Bulk Metallic Glass
- 5 July 2016
- Published by Springer Nature in Oxidation of Metals
- Vol. 86 (3-4) , 205-219
Air Oxidation of a Ni53Nb20Ti10Zr8Co6Cu3 Glassy Alloy at 400–550 °C
- 5 July 2016
- Published by Springer Nature in Oxidation of Metals
- Vol. 86 (3-4) , 205-219
Air Oxidation of a Ni53Nb20Ti10Zr8Co6Cu3 Glassy Alloy at 400–550 °C
- 1 November 2013
- Published by Springer Nature in Oxidation of Metals
- Vol. 81 (3-4) , 453-465
The Effect of Er Addition on the Air-Oxidation of a Zr55Cu30Al10Ni5-Based Bulk Metallic Glass
- 1 November 2013
- Published by Springer Nature in Oxidation of Metals
- Vol. 81 (3-4) , 453-465
The Effect of Er Addition on the Air-Oxidation of a Zr55Cu30Al10Ni5-Based Bulk Metallic Glass
- 25 September 2012
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 536, S103-S108
Air-oxidation of a Cu50Zr50 binary amorphous ribbon at 350–425°C
- 25 September 2012
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 536, S103-S108
Air-oxidation of a Cu50Zr50 binary amorphous ribbon at 350–425°C