Zhiyao Hou
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Zhiyao Hou has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
- Jun Lin
Chinese Academy of Sciences
5 shared publications Guogang Li
State Key Laboratory of Rare Earth Resource Utilization, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun, P. R. China
4 shared publicationsChong Peng
State Key Laboratory of Rare Earth Resource Utilization, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun, 130022, PR China
2 shared publicationsChunxia Li
State Key Laboratory of Rare Earth Resource Utilization, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun 130022, P. R. China
2 shared publicationsCuimiao Zhang
State Key Laboratory of Rare Earth Resource Utilization, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun 130022, P. R. China
2 shared publicationsHongzhou Lian
State Key Laboratory of Rare Earth Resource Utilization, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun, P. R. China
2 shared publications
Latest Publications
- 28 June 2016
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 6 (70) , 65600-65606
Controllable drug release system based on phase change molecules as gatekeepers for bimodal tumor therapy with enhanced efficacy
NIR- and pH-triggered DOX release in Cu9S5@mSiO2-PEG@DOX@TD multifunctional drug delivery.
- 28 June 2016
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 6 (70) , 65600-65606
Controllable drug release system based on phase change molecules as gatekeepers for bimodal tumor therapy with enhanced efficacy
NIR- and pH-triggered DOX release in Cu9S5@mSiO2-PEG@DOX@TD multifunctional drug delivery.
- Open Access
- 5 April 2013
- Published by Wiley in Advanced Healthcare Materials
- Vol. 2 (4) , 514
Drug Delivery: Platinum (IV) Pro-Drug Conjugated NaYF4:Yb3+/Er3+Nanoparticles for Targeted Drug Delivery and Up-Conversion Cell Imaging (Adv. Healthcare Mater. 4/2013)
- 5 April 2013
- Published by Wiley in Advanced Healthcare Materials
- Vol. 2 (4) , 514
Open AccessDrug Delivery: Platinum (IV) Pro-Drug Conjugated NaYF4:Yb3+/Er3+Nanoparticles for Targeted Drug Delivery and Up-Conversion Cell Imaging (Adv. Healthcare Mater. 4/2013)
- 1 March 2012
- Published by Royal Society of Chemistry (RSC) in Dalton Transactions
- Vol. 41 (16) , 4780-4788
Electrospinning synthesis and luminescence properties of one-dimensional La9.33(SiO4)6O2: Ln3+ (Ln = Ce, Eu, Tb) microfibers
One-dimensional La9.33(SiO4)6O2: Ln3+ (Ln = Ce, Eu, Tb) microfibers were fabricated by a simple and cost-effective electrospinning method. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), photoluminescence (PL) and low voltage cathodoluminescence (CL) as well as kinetic decay were used to characterize the resulting samples. SEM and TEM results indicated that the diameter of the microfibers annealed at 1000 °C for 3 h was 200–245 nm. The microfibers were further composed of fine and closely linked nanoparticles. La9.33(SiO4)6O2: Ln3+ (Ln = Ce, Eu, Tb) phosphors showed the characteristic emission of Ce3+ (5d → 4f), Eu3+ (5D0 → 7FJ) and Tb3+ (5D3,4 → 7FJ) under ultraviolet excitation and low-voltage electron beams (3–5 kV) excitation. An energy transfer from Ce3+ to Tb3+ was observed in the La9.33(SiO4)6O2: Ce3+, Tb3+ phosphor under ultraviolet excitation and low-voltage electron beam excitation. Luminescence mechanisms were proposed to explain the observed phenomena. Blue, red and green emission can be realized in La9.33(SiO4)6O2: Ln3+ (Ln = Ce, Eu, Tb) microfibers by changing the doping ions. So the La9.33(SiO4)6O2: Ln3+ (Ln = Ce, Eu, Tb) phosphors have potential applications in full-color field emission displays.
- 1 March 2012
- Published by Royal Society of Chemistry (RSC) in Dalton Transactions
- Vol. 41 (16) , 4780-4788
Electrospinning synthesis and luminescence properties of one-dimensional La9.33(SiO4)6O2: Ln3+ (Ln = Ce, Eu, Tb) microfibers
One-dimensional La9.33(SiO4)6O2: Ln3+ (Ln = Ce, Eu, Tb) microfibers were fabricated by a simple and cost-effective electrospinning method. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), photoluminescence (PL) and low voltage cathodoluminescence (CL) as well as kinetic decay were used to characterize the resulting samples. SEM and TEM results indicated that the diameter of the microfibers annealed at 1000 °C for 3 h was 200–245 nm. The microfibers were further composed of fine and closely linked nanoparticles. La9.33(SiO4)6O2: Ln3+ (Ln = Ce, Eu, Tb) phosphors showed the characteristic emission of Ce3+ (5d → 4f), Eu3+ (5D0 → 7FJ) and Tb3+ (5D3,4 → 7FJ) under ultraviolet excitation and low-voltage electron beams (3–5 kV) excitation. An energy transfer from Ce3+ to Tb3+ was observed in the La9.33(SiO4)6O2: Ce3+, Tb3+ phosphor under ultraviolet excitation and low-voltage electron beam excitation. Luminescence mechanisms were proposed to explain the observed phenomena. Blue, red and green emission can be realized in La9.33(SiO4)6O2: Ln3+ (Ln = Ce, Eu, Tb) microfibers by changing the doping ions. So the La9.33(SiO4)6O2: Ln3+ (Ln = Ce, Eu, Tb) phosphors have potential applications in full-color field emission displays.
- 3 February 2012
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry
- Vol. 22 (12) , 5254-5276
One-dimensional luminescent materials derived from the electrospinning process: preparation, characteristics and application
This feature article highlights the recent advances on the preparation, characteristics and application of one-dimensional (1D) luminescent materials (including rare earth based inorganic materials, rare earth based composite materials and non rare earth materials) by an electrospinning process. Electrospinning is an effective method to prepare 1D polymer, composite and inorganic submicro- or nano-materials. The key strategy of the electrospinning method is to form an electrospinning solution with viscoelastic behavior similar to that of a conventional polymer solution. It utilizes an electrical force on the surface of an electrospinning solution to overcome the surface tension and produce a very thin charged jet. This jet moves straight for a certain distance, and then bends into looping and spiraling paths. During the elongation of the liquid jet, solvent evaporates and 1D hybrid materials accumulate on a grounded collector. Dispersing complexes or inorganic nanoparticles into polymer and inorganic matrices, composite luminescent materials viaelectrospinning combine both inorganic and organic characters. Annealing the inorganic/polymer hybrid precursors can yield various kinds of inorganic luminescent materials with fiber, wire, belt and tube-like morphologies, which have potential applications in fluorescent lamps and color displays. Furthermore, with the addition of some surfactants, it is possible to prepare 1D luminescent and porous multifunctional materials, which can act as potential drug carriers in the biomedical area.
- 3 February 2012
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry
- Vol. 22 (12) , 5254-5276
One-dimensional luminescent materials derived from the electrospinning process: preparation, characteristics and application
This feature article highlights the recent advances on the preparation, characteristics and application of one-dimensional (1D) luminescent materials (including rare earth based inorganic materials, rare earth based composite materials and non rare earth materials) by an electrospinning process. Electrospinning is an effective method to prepare 1D polymer, composite and inorganic submicro- or nano-materials. The key strategy of the electrospinning method is to form an electrospinning solution with viscoelastic behavior similar to that of a conventional polymer solution. It utilizes an electrical force on the surface of an electrospinning solution to overcome the surface tension and produce a very thin charged jet. This jet moves straight for a certain distance, and then bends into looping and spiraling paths. During the elongation of the liquid jet, solvent evaporates and 1D hybrid materials accumulate on a grounded collector. Dispersing complexes or inorganic nanoparticles into polymer and inorganic matrices, composite luminescent materials viaelectrospinning combine both inorganic and organic characters. Annealing the inorganic/polymer hybrid precursors can yield various kinds of inorganic luminescent materials with fiber, wire, belt and tube-like morphologies, which have potential applications in fluorescent lamps and color displays. Furthermore, with the addition of some surfactants, it is possible to prepare 1D luminescent and porous multifunctional materials, which can act as potential drug carriers in the biomedical area.
- 1 January 2011
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 158 (7) , J208-J214
Fabrication and Luminescence Properties of Ca2RE8(SiO4)6O2: Pb2+, Dy3+ (RE = Y, Gd) One-dimensional Phosphors by Electrospinning Method
One-dimensional Ca2RE8(SiO4)6O2: Pb2+, Dy3+ (RE = Y, Gd) nanobelts and microfibers were fabricated by a simple and cost-effective electrospinning method. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermogravimetric and differential scanning calorimetry (TG-DSC), scanning electron microscopy (SEM), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), photoluminescence (PL) and low voltage cathodoluminescence (CL) were used to characterize the resulting samples. SEM and TEM results indicated that the width and the thickness of Ca2Gd8 (SiO4)6O2: Pb2+, Dy3+ nanobelts annealed at 1000°C for 4 h were 220–250 and 90–100 nm, respectively. The diameter of the Ca2Gd8(SiO4)6O2: Pb2+, Dy3+ microfibers annealed at 1000°C for 4 h was 140–190 nm. When the samples were excited by ultraviolet (254 nm), the Pb2+ can sensitize the Gd3+ sublattice, and the energy can be efficiently transferred from Pb2+ to Dy3+ in Ca2Gd8(SiO4)6O2. Under low-voltage electron beams (4–6 kV) excitation, the Ca2RE8(SiO4)6O2: Pb2+, Dy3+ (RE = Y, Gd) samples showed strong white emission. The PL and CL intensities of Ca2Gd8(SiO4)6O2: Pb2+, Dy3+ microfibers were higher than those of Ca2Gd8(SiO4)6O2: Pb2+, Dy3+ nanobelts. The CIE chromaticity coordinates of Ca2Y8(SiO4)6O2: Pb2+, Dy3+ microfibers were x = 0.323, y = 0.333, very close to the ideal white region.
- 1 January 2011
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 158 (7) , J208-J214
Fabrication and Luminescence Properties of Ca2RE8(SiO4)6O2: Pb2+, Dy3+ (RE = Y, Gd) One-dimensional Phosphors by Electrospinning Method
One-dimensional Ca2RE8(SiO4)6O2: Pb2+, Dy3+ (RE = Y, Gd) nanobelts and microfibers were fabricated by a simple and cost-effective electrospinning method. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermogravimetric and differential scanning calorimetry (TG-DSC), scanning electron microscopy (SEM), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), photoluminescence (PL) and low voltage cathodoluminescence (CL) were used to characterize the resulting samples. SEM and TEM results indicated that the width and the thickness of Ca2Gd8 (SiO4)6O2: Pb2+, Dy3+ nanobelts annealed at 1000°C for 4 h were 220–250 and 90–100 nm, respectively. The diameter of the Ca2Gd8(SiO4)6O2: Pb2+, Dy3+ microfibers annealed at 1000°C for 4 h was 140–190 nm. When the samples were excited by ultraviolet (254 nm), the Pb2+ can sensitize the Gd3+ sublattice, and the energy can be efficiently transferred from Pb2+ to Dy3+ in Ca2Gd8(SiO4)6O2. Under low-voltage electron beams (4–6 kV) excitation, the Ca2RE8(SiO4)6O2: Pb2+, Dy3+ (RE = Y, Gd) samples showed strong white emission. The PL and CL intensities of Ca2Gd8(SiO4)6O2: Pb2+, Dy3+ microfibers were higher than those of Ca2Gd8(SiO4)6O2: Pb2+, Dy3+ nanobelts. The CIE chromaticity coordinates of Ca2Y8(SiO4)6O2: Pb2+, Dy3+ microfibers were x = 0.323, y = 0.333, very close to the ideal white region.
- 7 July 2009
- Published by American Chemical Society (ACS) in Langmuir
- Vol. 25 (20) , 12340-12348
Fabrication and Luminescence Properties of One-Dimensional CaMoO4: Ln3+ (Ln = Eu, Tb, Dy) Nanofibers via Electrospinning Process
One-dimensional CaMoO4:Ln3+ (Ln = Eu, Tb, Dy) nanofibers have been prepared by a combination method of sol−gel and electrospinning process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), photoluminescence (PL), and low voltage cathodoluminescence (CL) as well as kinetic decays were used to characterize the resulting samples. SEM and TEM analyses indicate that the obtained precursor fibers have a uniform size, and the as-formed CaMoO4:Ln3+ nanofibers consist of nanoparticles. Under ultraviolet excitation, the CaMoO4 samples exhibit a blue-green emission band with a maximum at 500 nm originating from the MoO42− groups. Due to an efficient energy transfer from molybdate groups to dopants, CaMoO4:Ln3+ phosphors show their strong characteristic emission under ultraviolet excitation and low-voltage electron beam excitation. The energy transfer process was further studied by the emission spectra and the kinetic decay curves of Ln3+ upon excitation into the MoO42− groups in the CaMoO4:x mol % Ln3+ samples (x = 0−5). Furthermore, the emission colors of CaMoO4:Ln3+ nanofibers can be tuned from blue-green to green, yellow, and orange-red easily by changing the doping concentrations (x) of Ln3+ ions, making the materials have potential applications in fluorescent lamps and field emission displays (FEDs).
- 7 July 2009
- Published by American Chemical Society (ACS) in Langmuir
- Vol. 25 (20) , 12340-12348
Fabrication and Luminescence Properties of One-Dimensional CaMoO4: Ln3+ (Ln = Eu, Tb, Dy) Nanofibers via Electrospinning Process
One-dimensional CaMoO4:Ln3+ (Ln = Eu, Tb, Dy) nanofibers have been prepared by a combination method of sol−gel and electrospinning process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), photoluminescence (PL), and low voltage cathodoluminescence (CL) as well as kinetic decays were used to characterize the resulting samples. SEM and TEM analyses indicate that the obtained precursor fibers have a uniform size, and the as-formed CaMoO4:Ln3+ nanofibers consist of nanoparticles. Under ultraviolet excitation, the CaMoO4 samples exhibit a blue-green emission band with a maximum at 500 nm originating from the MoO42− groups. Due to an efficient energy transfer from molybdate groups to dopants, CaMoO4:Ln3+ phosphors show their strong characteristic emission under ultraviolet excitation and low-voltage electron beam excitation. The energy transfer process was further studied by the emission spectra and the kinetic decay curves of Ln3+ upon excitation into the MoO42− groups in the CaMoO4:x mol % Ln3+ samples (x = 0−5). Furthermore, the emission colors of CaMoO4:Ln3+ nanofibers can be tuned from blue-green to green, yellow, and orange-red easily by changing the doping concentrations (x) of Ln3+ ions, making the materials have potential applications in fluorescent lamps and field emission displays (FEDs).
- 1 January 2009
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 156 (8) , J209-J214
Preparation and Luminescence Properties of Gd[sub 2]MoO[sub 6]:Eu[sup 3+] Nanofibers and Nanobelts by Electrospinning
Gd2MoO6:Eu3+Gd2MoO6:Eu3+ nanofibers and nanobelts have been prepared by a combination method of the sol–gel process and electrospinning. X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, scanning electron microscopy (SEM), transmission electron microscopy (TEM), high resolution transmission electron microscopy, photoluminescence, and low voltage cathodoluminescence as well as kinetic decays were used to characterize the resulting samples. The results of XRD and FTIR indicate that the Gd2MoO6:Eu3+Gd2MoO6:Eu3+ samples have crystallized at 600°C600°C with the monoclinic (α)(α) structure. The SEM and TEM results indicate that the as-formed precursor fibers and belts are uniform and that the as-prepared nanofibers and nanobelts consist of nanoparticles. Gd2MoO6:Eu3+Gd2MoO6:Eu3+ phosphors show their strong characteristic emission under UV excitation (353 nm) and low voltage electron-beam excitation (3 kV), making the materials have potential applications in fluorescent lamps and field-emission displays.
- 1 January 2009
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 156 (8) , J209-J214
Preparation and Luminescence Properties of Gd[sub 2]MoO[sub 6]:Eu[sup 3+] Nanofibers and Nanobelts by Electrospinning
Gd2MoO6:Eu3+Gd2MoO6:Eu3+ nanofibers and nanobelts have been prepared by a combination method of the sol–gel process and electrospinning. X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, scanning electron microscopy (SEM), transmission electron microscopy (TEM), high resolution transmission electron microscopy, photoluminescence, and low voltage cathodoluminescence as well as kinetic decays were used to characterize the resulting samples. The results of XRD and FTIR indicate that the Gd2MoO6:Eu3+Gd2MoO6:Eu3+ samples have crystallized at 600°C600°C with the monoclinic (α)(α) structure. The SEM and TEM results indicate that the as-formed precursor fibers and belts are uniform and that the as-prepared nanofibers and nanobelts consist of nanoparticles. Gd2MoO6:Eu3+Gd2MoO6:Eu3+ phosphors show their strong characteristic emission under UV excitation (353 nm) and low voltage electron-beam excitation (3 kV), making the materials have potential applications in fluorescent lamps and field-emission displays.