MTMaria Antonella Tagliente

Maria Antonella Tagliente

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Maria Antonella Tagliente has a total of 20 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Size-dependent oxidation in ZnO nanoparticles embedded in ion-implanted silica

    by M. A. Tagliente, M. Massaro, G. Mattei, P. Mazzoldi, V. Bello, G. Pellegrini

    ZnO – SiO 2 nanocomposites were synthesized by ion implanting a Zn+ beam in a silica slide and by annealing in oxidizing atmosphere at 800 °C. A detailed structural and optical characterization was performed by using glancing incidence x-ray diffraction, transmission electron microscopy combined with selected area electron diffraction and energy dispersive spectrometry, optical absorption, and photoluminescence spectroscopies. Samples obtained with three different Zn+ fluences in the range 1–2×1017 ions/cm2 have been investigated. According to the results, Zn crystalline nanoparticles were found in the as-implanted Zn–SiO2 samples. The size of the Zn nanoparticles was proportional to the implantation fluence. The annealing in oxidizing atmosphere promotes the total oxidation of the Zn nanoparticles with a preferential migration of the nanoparticles toward the surface of the sample along with an opposite and less pronounced diffusion toward the bulk of the matrix. A relatively strong excitonic peak from the ZnO nanoparticles was observed both in the optical absorption and photoluminescence spectra. We found that the oxidation of the Zn nanoparticles is size-dependent because the time necessary for the total oxidation of the nanoparticles increases with the decreasing in the size of the nanoparticles. This size-oxidation correlation has been explained in terms of arguments related to the stress of the Zn nanoparticles.


  • On the Structural and Optical Properties of ZnO Nanoparticles Formed in Silica by Ion Implantation

    by Maria Antonella Tagliente, Marcello Massaro, Giovanni Mattei, Paolo Mazzoldi, Giovanni Pellegrini, Valentina Bello, Daniela Carbone

    Zinc Oxide (ZnO) is a II-VI semiconductor material with a wide direct band-gap of 3.37 eV at room temperature (RT). In the past decades, the material has been used for a variety of applications such as gas sensors, surface acoustic wave devices, or transparent contacts. Recently, ZnO has gained a new substantial interest primarily because to its potentialities for optoelectronic and spintronic applications. The renewed interest has been fueled by the availability of high-quality bulk substrates, reports of p-type conduction and theoretical predictions of its ferromagnetic behavior at room temperature when doped with transition metals. In the domain of optoelectronics, its main applications include devices emitting in the blue and UV regions by exploiting its wide band-gap such as light-emitting and laser diodes. With respect to several wide band-gap semiconductor materials, ZnO has the advantage of a larger exciton binding energy (about 60 meV) which paves the way for an intense near-band-edge excitonic emission at room and higher temperatures. On the other hand, a band gap engineering can be also achieved by the incorporation of Cadmium and Magnesium atoms into the ZnO lattice.Many techniques have been used to prepare ZnO in various forms, such as single crystals, powders and films. In the past few years, the great attention toward materials with nanometric size have motivated a number of studies on the synthesis of ZnO nanocrystals. Ion implantation is one of the most effective and versatile technique to obtain nanoparticles. ZnO particles embedded in silica matrix have been successfully prepared by ion implantation followed by thermal oxidation.In this work, we report on a detailed structural and optical characterization of the ZnO-silica nanocomposites by using several complementary techniques; in particular, Glancing Incidence X-ray Diffraction (GIXRD), Rutherford Backscattering Spectrometry (RBS), linear Optical Absorption (OA) in the UV-near IR spectrum and Photo-Luminescence (PL). The ZnO nanoparticles embedded in SiO2matrix were prepared by implanting the substrates with 130 keV Zn+ions at doses of 1, 1.5 and 2´1017 ions/cm2. Subsequently, the implanted samples were annealed for 1h in a furnace at a temperature between 500 and 800°C under flowing O2 gas. X-ray diffraction results indicate the formation of Zn and ZnO nanoparticles in the as-implanted and annealed samples, respectively. Moreover, the ZnO nanocrystals embedded in the SiO2matrix have a (002) preferred orientation. After the oxidation, the optical absorption spectra show an absorption edge at about 374 nm by confirming the presence of the ZnO particles. A relatively strong exciton photoluminescence peak was observed at room temperature under pulsed N2 laser excitation at l=337nm. The results obtained, peculiarly related to the implantation doses and annealing temperature, are discussed.


  • Thermal behavior of indium nanoclusters in ion-implanted silica

    by M. A. Tagliente, G. Mattei, L. Tapfer, M. Vittori Antisari, P. Mazzoldi

    Fused silica substrates were implanted with 2×1017In2+∕cm2 ions at 320keV. Indium crystalline nanoclusters with an average size of about 15–20nm were found in the as-implanted samples. The thermal behavior of the nanoclusters was studied by performing heating-cooling cycles in vacuum and by using in-situ techniques based on glancing-incidence x-ray diffraction and transmission electron microscopy. The precipitates showed both superheating and supercooling. Moreover, no evidence of clusters growth or reorientation during the thermal cycle was found. A detailed study of the heating sequence showed that the melting temperature of the Indium precipitates depended on their size, i.e., the smallest particles melt first and at a temperature which is about 7K below the bulk melting point, while the largest ones were superheated until about 13K above it. Moreover, a remarkable stability of the In cluster well above their melting temperature (up to about 980K) was evidenced by in-situ transmission electron microscopy analysis. From a thermodynamic point of view, the experimental results were explained by considering two effects acting on the clusters: the thermodynamic size effect and the pressure of the silica matrix.


  • Properties of (In,Ga)N/GaN quantum wells grown by plasma-assisted molecular beam epitaxy

    by O. Brandt, P. Waltereit, S. Dhar, U. Jahn, Y. J. Sun, A. Trampert, K. H. Ploog, M. A. Tagliente, L. Tapfer

    We investigate the synthesis of (In,Ga)N/GaN multiple quantum wells by plasma-assisted molecular beam epitaxy (MBE). For metal-stable growth, unexpectedly strong In surface segregation is revealed. The In depth profiles obtained by secondary ion-mass spectrometry exhibit a top-hat In distribution and are thus indicative of a zeroth order segregation mechanism instead of a first order process as observed for other materials systems. As additionally evidenced by transmission electron microscopy, the segregation of In during metal-stable growth results in quantum wells with smooth interfaces but significantly larger width than intended. The resulting blueshift of the transition energy may be the reason for the frequent conclusion that the theoretical polarization fields of Bernardini et al. [Phys. Rev. B 56, R10024 (1997)] are too large for (In,Ga)N. Being in possession of the (at least approximately) correct structural parameters, we find the theoretical fields to be in very satisfactory agreement with those deduced from experimental data. For a thorough understanding of the spontaneous emission from these structures both electrostatic fields and compositional fluctuations have to be taken into account. Both the transition energies and radiative decay times in photoluminescence are shown to be in agreement with the quantum-confined Stark effect in these structures. Using cathodoluminescence spectroscopy, we investigate the dependence of transition energy and quantum efficiency on both temperature and excitation density. At low temperatures, recombination is governed by localized states, whereas for high temperatures extended states dominate. This finding is in agreement with the temperature dependence of the radiative decay time which is utilized as a probe of the dimensionality of the system. A quantitative analysis of these experiments via coupled rate equations shows that the localization depth in these MBE-grown (In,Ga)N/GaN quantum wells is around 20–30 meV. This shallow localization is found to significantly enhance the internal quantum efficiency up to a temperature of about 100 K.