Murugasamy Kannan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Murugasamy Kannan has a total of 40 co-authors. Here are the top co-authors by number of shared publications:
- Kuruvilla Joseph
Indian Institute of Space Science and Technology
11 shared publications - Sabu Thomas
School of Energy Materials Mahatma Gandhi University Kottayam Kerala India
10 shared publications S. S. Bhagawan
Department of Chemical Engineering, Amrita Vishwa Vidyapeetham, Coimbatore, India
4 shared publicationsS.S. Bhagawan
Department of Chemical Engineering Amrita Vishwa Vidyapeetham Coimbatore 641112 India
4 shared publications- Sai Gopal Krishna Bhagavatula
Department of Chemical Engineering and Materials Science, Amrita School of Engineering, Amrita Vishwa Vidyapeetham, Coimbatore 641112, India
4 shared publications Achal Bhiogade
Center of Excellence in Advanced Materials and Green Technologies, Department of Chemical Engineering and Materials Science, Amrita School of Engineering, Amrita Vishwa Vidyapeetham, Coimbatore, Tamil Nadu, India
2 shared publications
Latest Publications
- 17 August 2026
- Published by Springer Nature in Iranian Polymer Journal
- p. 1-19
Improved mechanical and thermal properties of PLA-based green nanocomposites through TPU, EVA, and PBAT blending
- 17 August 2026
- Published by Springer Nature in Iranian Polymer Journal
- p. 1-19
Improved mechanical and thermal properties of PLA-based green nanocomposites through TPU, EVA, and PBAT blending
- 5 January 2026
- Published by SAGE Publications in Journal of Reinforced Plastics and Composites
- Vol. 45 (19-20) , 4523-4546
Nanoclay and copper oxide reinforced PLA/PBAT nanocomposites: EMI shielding, thermal stability, and mechanical properties
This research investigates bio-based green nanocomposites prepared by melt-mixing PLA and PBAT in a 70/30 weight ratio with nanoclay and copper oxide (CuO) as the nanoparticles. The study evaluated the effect of CuO on the electromagnetic interference shielding effectiveness (EMI SE), mechanical, thermal, and material dispersion properties of nanocomposites with and without nanoclay, even though CuO is generally used at less than 2% to improve the antimicrobial resistance of nanocomposites. The SEM image was used to evaluate the dispersion level of PBAT in PLA matrix. In the EMI study, the hybrid composition of 70/30/3/0.4 shows higher SE across the entire frequency range of the X-band (8.4 to 12.4 GHz). 5 parts (parts per hundred resin) nanoclay-based composites, the tensile strength increased from 31.0 MPa to 32.5 MPa, and elongation from 4.6 % to 30.2 %, along with improved thermal stability in the TGA analysis compared to the 70/30 blend. Nanocomposites with 0.4 and 0.8 parts CuO showed tensile properties comparable to the 70/30 blend, but a marginal decrease was observed with 1.2 parts. CuO-based composition showed lower thermal stability in the TGA analysis. The FTIR analysis indicates the absence of a chemical reaction or hydrogen bonding within the materials.
- 5 January 2026
- Published by SAGE Publications in Journal of Reinforced Plastics and Composites
- Vol. 45 (19-20) , 4523-4546
Nanoclay and copper oxide reinforced PLA/PBAT nanocomposites: EMI shielding, thermal stability, and mechanical properties
This research investigates bio-based green nanocomposites prepared by melt-mixing PLA and PBAT in a 70/30 weight ratio with nanoclay and copper oxide (CuO) as the nanoparticles. The study evaluated the effect of CuO on the electromagnetic interference shielding effectiveness (EMI SE), mechanical, thermal, and material dispersion properties of nanocomposites with and without nanoclay, even though CuO is generally used at less than 2% to improve the antimicrobial resistance of nanocomposites. The SEM image was used to evaluate the dispersion level of PBAT in PLA matrix. In the EMI study, the hybrid composition of 70/30/3/0.4 shows higher SE across the entire frequency range of the X-band (8.4 to 12.4 GHz). 5 parts (parts per hundred resin) nanoclay-based composites, the tensile strength increased from 31.0 MPa to 32.5 MPa, and elongation from 4.6 % to 30.2 %, along with improved thermal stability in the TGA analysis compared to the 70/30 blend. Nanocomposites with 0.4 and 0.8 parts CuO showed tensile properties comparable to the 70/30 blend, but a marginal decrease was observed with 1.2 parts. CuO-based composition showed lower thermal stability in the TGA analysis. The FTIR analysis indicates the absence of a chemical reaction or hydrogen bonding within the materials.
- 12 September 2025
- Published by Wiley in Polymer Composites
- Vol. 47 (5) , 4660-4684
Green Nanocomposites of PLA / PBAT Reinforced With Fe 3 O 4 and GNP : EMI Shielding, Mechanical, Thermal, and Morphological Analysis
This study focuses on the bio‐based green nanocomposites formed by melt‐mixing PLA and PBAT in a 70/30 weight ratio, with Fe 3 O 4 and Graphene Nanoplatelets (GNP) as the nanoparticles. Reinforcement with Fe 3 O 4 (3, 5, and 7 phr), GNP (3, 5, and 7 phr), and their hybrid was used to evaluate improvements in electromagnetic interference shielding effectiveness (EMI SE), thermal, mechanical, and morphological properties of the PLA/PBAT system. GNP 7 phr and hybrid 7 phr show high SE, primarily from absorption due to magnetic dipoles in Fe 3 O 4 based and interfacial polarization in GNP based nanocomposites. The 70/30 blend shows a tensile strength of 31 MPa and elongation of 4.6%, while the nanocomposites range from 22 to 30 MPa and 2%–3.2%, respectively—except for 3 phr Fe 3 O 4 , which reaches 35 MPa and 2.7%. However, in fracture toughness, the critical stress intensity factor (K IC ) increased from 1.56 to 5.7 MPa.m 0.5 and strain energy release rate per unit area (G IC ) increased from 1.68 to 18.39 kJ/m 2 for the 70/30 to 3 phr hybrid. XRD confirms Fe 3 O 4 phase retention in nanocomposites. TGA shows improved thermal stability for GNP and the hybrid composition. SEM evaluated PBAT dispersion in PLA, and FTIR showed no chemical interaction between the materials.
- 12 September 2025
- Published by Wiley in Polymer Composites
- Vol. 47 (5) , 4660-4684
Green Nanocomposites of PLA / PBAT Reinforced With Fe 3 O 4 and GNP : EMI Shielding, Mechanical, Thermal, and Morphological Analysis
This study focuses on the bio‐based green nanocomposites formed by melt‐mixing PLA and PBAT in a 70/30 weight ratio, with Fe 3 O 4 and Graphene Nanoplatelets (GNP) as the nanoparticles. Reinforcement with Fe 3 O 4 (3, 5, and 7 phr), GNP (3, 5, and 7 phr), and their hybrid was used to evaluate improvements in electromagnetic interference shielding effectiveness (EMI SE), thermal, mechanical, and morphological properties of the PLA/PBAT system. GNP 7 phr and hybrid 7 phr show high SE, primarily from absorption due to magnetic dipoles in Fe 3 O 4 based and interfacial polarization in GNP based nanocomposites. The 70/30 blend shows a tensile strength of 31 MPa and elongation of 4.6%, while the nanocomposites range from 22 to 30 MPa and 2%–3.2%, respectively—except for 3 phr Fe 3 O 4 , which reaches 35 MPa and 2.7%. However, in fracture toughness, the critical stress intensity factor (K IC ) increased from 1.56 to 5.7 MPa.m 0.5 and strain energy release rate per unit area (G IC ) increased from 1.68 to 18.39 kJ/m 2 for the 70/30 to 3 phr hybrid. XRD confirms Fe 3 O 4 phase retention in nanocomposites. TGA shows improved thermal stability for GNP and the hybrid composition. SEM evaluated PBAT dispersion in PLA, and FTIR showed no chemical interaction between the materials.
- 7 April 2025
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 142 (26)
Modifying the Mechanical, Viscoelastic, Thermal, and Degradation Properties of PLA/PBAT Blends With Nanoclay and PEG
In this research, polylactic acid (PLA) was blended with polybutylene adipate terephthalate (PBAT) to enhance PLA's processability, heat resistance, toughness, and flexibility. In this context, the biodegradability of PLA can be maximized in PLA/PBAT blends, as PBAT is also biodegradable and offers an alternative resource for the biobased components of PLA, despite PBAT's primary derivation from fossil fuel sources. However, the immiscibility of these two neat polymers restricts the overall effectiveness of polymer blends. To address this issue, plasticizers such as polyethylene glycol (PEG) and nanoparticles like nanoclay were added to the blends to enhance their miscibility. The polymer blend underwent analysis through static mechanical testing, creep testing, differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), Fourier transform infrared spectroscopy (FTIR), and scanning electron microscopy (SEM). The results show that nanoclay plays a significant role in improving elongation in tensile properties. The addition of 5 parts nanoclay to the 70/30 PLA/PBAT composition shows an elongation‐at‐break of 30%, compared to 4.7% for the 70/30 blend, without significant changes in modulus and strength. TGA analysis shows that neat PBAT has better thermal stability than PLA, whereas the thermal stability of the PLA/PBAT blend was observed to be lower than that of neat PLA.
- 7 April 2025
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 142 (26)
Modifying the Mechanical, Viscoelastic, Thermal, and Degradation Properties of PLA/PBAT Blends With Nanoclay and PEG
In this research, polylactic acid (PLA) was blended with polybutylene adipate terephthalate (PBAT) to enhance PLA's processability, heat resistance, toughness, and flexibility. In this context, the biodegradability of PLA can be maximized in PLA/PBAT blends, as PBAT is also biodegradable and offers an alternative resource for the biobased components of PLA, despite PBAT's primary derivation from fossil fuel sources. However, the immiscibility of these two neat polymers restricts the overall effectiveness of polymer blends. To address this issue, plasticizers such as polyethylene glycol (PEG) and nanoparticles like nanoclay were added to the blends to enhance their miscibility. The polymer blend underwent analysis through static mechanical testing, creep testing, differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), Fourier transform infrared spectroscopy (FTIR), and scanning electron microscopy (SEM). The results show that nanoclay plays a significant role in improving elongation in tensile properties. The addition of 5 parts nanoclay to the 70/30 PLA/PBAT composition shows an elongation‐at‐break of 30%, compared to 4.7% for the 70/30 blend, without significant changes in modulus and strength. TGA analysis shows that neat PBAT has better thermal stability than PLA, whereas the thermal stability of the PLA/PBAT blend was observed to be lower than that of neat PLA.
- 24 February 2023
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 140 (17)
Synergistic behavior of dual filler system (n‐Si3N4/COOH‐MWCNT) on the mechanical, tribological, curing, and corrosion characteristics of epoxy hybrid nanocomposites
Epoxy hybrid nanocomposites reinforced with silicon nitride nanoparticles (SiN) and carboxylic acid‐modified multiwalled carbon nanotubes (COOH‐MWCNT) were prepared by hand layup. These hybrid nanocomposites have not undergone thorough investigation in the fields of mechanical, tribological, and corrosion‐resistant characteristics. The 0.25/0.5 SiN/MWCNT hybrid nanocomposite displayed improvement in elongation by 190% and fracture toughness by 360%. The effect of dual filler system on the wear and friction properties of the composite was investigated. The influence of silicon nitride and hybrid fillers the curing characteristics of epoxy was examined using Fourier transform infrared spectroscopy (FTIR). From differential scanning calorimetry (DSC), it was found that the use of dual fillers in the epoxy system reduced the residual heat of reaction and curing time by 15%. In a highly corrosive environment (3.5% NaCl), TAFEL polarization showed that 0.5/0.5 SiN/MWCNT epoxy hybrid coating on mild steel (MS) increased protection against corrosion by 30%. The dispersion of nanofillers and their interactions were verified using high‐resolution transmission electron microscopy (HR‐TEM). The morphology of the fracture, wear, and corroded surfaces were examined by field emission scanning electron microscopy (FE‐SEM). SiN manifested a synergistic effect with MWCNTs making it a superior reinforcement at very low content.
- 24 February 2023
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 140 (17)
Synergistic behavior of dual filler system (n‐Si3N4/COOH‐MWCNT) on the mechanical, tribological, curing, and corrosion characteristics of epoxy hybrid nanocomposites
Epoxy hybrid nanocomposites reinforced with silicon nitride nanoparticles (SiN) and carboxylic acid‐modified multiwalled carbon nanotubes (COOH‐MWCNT) were prepared by hand layup. These hybrid nanocomposites have not undergone thorough investigation in the fields of mechanical, tribological, and corrosion‐resistant characteristics. The 0.25/0.5 SiN/MWCNT hybrid nanocomposite displayed improvement in elongation by 190% and fracture toughness by 360%. The effect of dual filler system on the wear and friction properties of the composite was investigated. The influence of silicon nitride and hybrid fillers the curing characteristics of epoxy was examined using Fourier transform infrared spectroscopy (FTIR). From differential scanning calorimetry (DSC), it was found that the use of dual fillers in the epoxy system reduced the residual heat of reaction and curing time by 15%. In a highly corrosive environment (3.5% NaCl), TAFEL polarization showed that 0.5/0.5 SiN/MWCNT epoxy hybrid coating on mild steel (MS) increased protection against corrosion by 30%. The dispersion of nanofillers and their interactions were verified using high‐resolution transmission electron microscopy (HR‐TEM). The morphology of the fracture, wear, and corroded surfaces were examined by field emission scanning electron microscopy (FE‐SEM). SiN manifested a synergistic effect with MWCNTs making it a superior reinforcement at very low content.
- 13 January 2021
- Published by SAGE Publications in Polymers and Polymer Composites
- Vol. 29 (9_suppl) , S85-S98
Studies on thermal and degradation kinetics of cellulose micro/nanoparticle filled polylactic acid (PLA) based nanocomposites
The aim of this work is to understand the effect of concentration of plasticizer, particle size and wt% of nanoparticles on nanocomposites by fabricating poly lactic acid (PLA) based bio-nanocomposites. The bio-nanocomposites were prepared by a solution casting method with PLA as the matrix, chloroform as solvent and poly ethylene glycol (PEG) as plasticizer. Microcrystalline cellulose (MCC) and cellulose nanocrystal (CNC) were used as reinforcements in 1, 3 and 5 wt% to modify the properties of the bio-nanocomposite. The degradation kinetics of the PLA based composites were determined by using the Coats-Redfern equation over the range of 0-5 wt% of MCC and CNC. Fabricated PLA based composite films were analyzed by differential scanning calorimetry (DSC), thermo gravimetric analysis (TGA), X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), dynamic light scattering (DLS) and field emission scanning electron microscopy (FE-SEM). The analyses showed that the amount of PEG, MCC and CNC affected the degree of crystallinity. DSC results showed that the MCC/CNC content level affected the degree of crystallinity compared to neat PLA. The FTIR showed a free hydroxyl group (−OH) present in the system. The TGA analysis showed that the PLA/MCC3%/ PEG 10% composition had the highest stability compared to the other compositions but less than neat PLA.
- 13 January 2021
- Published by SAGE Publications in Polymers and Polymer Composites
- Vol. 29 (9_suppl) , S85-S98
Studies on thermal and degradation kinetics of cellulose micro/nanoparticle filled polylactic acid (PLA) based nanocomposites
The aim of this work is to understand the effect of concentration of plasticizer, particle size and wt% of nanoparticles on nanocomposites by fabricating poly lactic acid (PLA) based bio-nanocomposites. The bio-nanocomposites were prepared by a solution casting method with PLA as the matrix, chloroform as solvent and poly ethylene glycol (PEG) as plasticizer. Microcrystalline cellulose (MCC) and cellulose nanocrystal (CNC) were used as reinforcements in 1, 3 and 5 wt% to modify the properties of the bio-nanocomposite. The degradation kinetics of the PLA based composites were determined by using the Coats-Redfern equation over the range of 0-5 wt% of MCC and CNC. Fabricated PLA based composite films were analyzed by differential scanning calorimetry (DSC), thermo gravimetric analysis (TGA), X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), dynamic light scattering (DLS) and field emission scanning electron microscopy (FE-SEM). The analyses showed that the amount of PEG, MCC and CNC affected the degree of crystallinity. DSC results showed that the MCC/CNC content level affected the degree of crystallinity compared to neat PLA. The FTIR showed a free hydroxyl group (−OH) present in the system. The TGA analysis showed that the PLA/MCC3%/ PEG 10% composition had the highest stability compared to the other compositions but less than neat PLA.
- 26 May 2020
- Published by Elsevier in Materials Today: Proceedings
- Vol. 24, 1138-1146
Tuning parameters for flame-retardant coatings on wood and polymer
- 26 May 2020
- Published by Elsevier in Materials Today: Proceedings
- Vol. 24, 1138-1146
Tuning parameters for flame-retardant coatings on wood and polymer
- 1 January 2020
- Published by Elsevier in Materials Today: Proceedings
- Vol. 24, 806-814
Degradation kinetics study of Poly lactic acid(PLA) based biodegradable green composites
- 1 January 2020
- Published by Elsevier in Materials Today: Proceedings
- Vol. 24, 806-814
Degradation kinetics study of Poly lactic acid(PLA) based biodegradable green composites
- 17 June 2019
- Published by SAGE Publications in Plastics, Rubber and Composites: Macromolecular Engineering
- Vol. 48 (8) , 356-363
Studies on thermal degradation kinetics and dielectric properties of polyether imide foam/nanosilica-based nanocomposites
In this paper, polyether imide (PEI) having properties such as a high glass transition temperature of 216°C, high heat resistance, high flame resistance, low smoke generation and a high melting point within the range of 400°C, having low thermal conductivity and low dielectric constant was chosen to be a polymeric foam. Water vapor-induced phase separation method was used to prepare PEI foams. PEI foams were reinforced with nano-silica (weight 1, 3 and 5%) in order to alter the dielectric properties, thermal conductivity and degradation kinetics of foamed polymer. The tested samples showed a reduction in dielectric constant than that of solid PEI but at a higher loading, it showed a higher value due to threshold percolation and a reduction in thermal conductivity was observed for foamed PEI. From thermogravimetric analysis, we can conclude that PEI with 3% filler loading showed better thermal stability compared to other PEI foam compositions.
- 17 June 2019
- Published by SAGE Publications in Plastics, Rubber and Composites: Macromolecular Engineering
- Vol. 48 (8) , 356-363
Studies on thermal degradation kinetics and dielectric properties of polyether imide foam/nanosilica-based nanocomposites
In this paper, polyether imide (PEI) having properties such as a high glass transition temperature of 216°C, high heat resistance, high flame resistance, low smoke generation and a high melting point within the range of 400°C, having low thermal conductivity and low dielectric constant was chosen to be a polymeric foam. Water vapor-induced phase separation method was used to prepare PEI foams. PEI foams were reinforced with nano-silica (weight 1, 3 and 5%) in order to alter the dielectric properties, thermal conductivity and degradation kinetics of foamed polymer. The tested samples showed a reduction in dielectric constant than that of solid PEI but at a higher loading, it showed a higher value due to threshold percolation and a reduction in thermal conductivity was observed for foamed PEI. From thermogravimetric analysis, we can conclude that PEI with 3% filler loading showed better thermal stability compared to other PEI foam compositions.
- 20 July 2017
- Published by Springer Nature in Journal of Inorganic and Organometallic Polymers and Materials
- Vol. 27 (6) , 1649-1663
Microstructure Development, Wear Characteristics and Kinetics of Thermal Decomposition of Hybrid Nanocomposites Based on Poly Aryl Ether Ketone, Boron Carbide and Multi Walled Carbon Nanotubes
- 20 July 2017
- Published by Springer Nature in Journal of Inorganic and Organometallic Polymers and Materials
- Vol. 27 (6) , 1649-1663
Microstructure Development, Wear Characteristics and Kinetics of Thermal Decomposition of Hybrid Nanocomposites Based on Poly Aryl Ether Ketone, Boron Carbide and Multi Walled Carbon Nanotubes