Fernanda Tranchesi Sadek
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Fernanda Tranchesi Sadek has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Marco Ferrari
Department of Prosthodontics, University of Siena, 53100 Siena, Italy
6 shared publications - Paulo Eduardo Capel Cardoso
University of São Paulo, Brazil
5 shared publications - Francesca Monticelli
Periodontics, Faculty of Health and Sport Sciences, Universidad de Zaragoza, C/Velódromo S/N, 22006 Huesca, Spain
3 shared publications - Cecilia Goracci
Department of Medical Biotechnologies, University of Siena, 53100 Siena, Italy
2 shared publications Antonio Muench
Department of Dental Materials, University of São Paulo, São Paulo, Brazil
1 shared publicationByoung I Suh
1 shared publication
Latest Publications
- 1 February 2008
- Vol. 21 (1) , 30-4
Early and 24-hour bond strength and degree of conversion of etch-and-rinse and self-etch adhesives.
To evaluate early and 24-hour microtensile bond strength (microTBS) and the degree of conversion (DC) of one representative adhesive system from each of the four current bonding approaches. 40 human molars were sectioned occluso-gingivally into two halves. Resin composite was bonded incrementally to flat, mid-coronal dentin, using the adhesives Adper Scotchbond MP (MP); Adper Scotchbond 2 (SB); Clearfil SE Bond (SE); and Adper Prompt L-Pop (LP) according to the respective manufacturer's instructions (n = 10). One half was immediately sectioned into sticks and subjected to muTBS test. As the sectioning process took approximately 1 hour, the results were designated as 1-hour bond strengths. The other half was stored in distilled water at 37 degrees C for 24 hours before being sectioned and tested. The DC of these systems was measured using Fourier Transform-Raman spectroscopy in three periods: immediately, 1 and 24 hours after polymerization. Data were analyzed with ANOVA and Tukey's tests. There were no significant differences between the 1-hour and 24-hour bond strengths (P > 0.05), or among the DC measured immediately, 1 hour and 24 hours after polymerization (P > 0.05). However, significant differences were observed among adhesives (P < 0.05). microTBS values obtained, in MPa (1 hour/24 hour), were: SB (48.6 + 1.3/48.4 + 3.5) = SE (51.9 + 4.7/53.3 +/- 2.9) > MP (35.3 +/- 10.9/38.6 + 6.7) > LP (25.5 + 1.1/26.0 + 1.5). The DC, in percentage (immediately/1 hour/24 hour), were: SE (81/82/87) > MP (79/77/81) > SB (60/63/65) > LP (39/37/42).
- 1 February 2008
- Vol. 21 (1) , 30-4
Early and 24-hour bond strength and degree of conversion of etch-and-rinse and self-etch adhesives.
To evaluate early and 24-hour microtensile bond strength (microTBS) and the degree of conversion (DC) of one representative adhesive system from each of the four current bonding approaches. 40 human molars were sectioned occluso-gingivally into two halves. Resin composite was bonded incrementally to flat, mid-coronal dentin, using the adhesives Adper Scotchbond MP (MP); Adper Scotchbond 2 (SB); Clearfil SE Bond (SE); and Adper Prompt L-Pop (LP) according to the respective manufacturer's instructions (n = 10). One half was immediately sectioned into sticks and subjected to muTBS test. As the sectioning process took approximately 1 hour, the results were designated as 1-hour bond strengths. The other half was stored in distilled water at 37 degrees C for 24 hours before being sectioned and tested. The DC of these systems was measured using Fourier Transform-Raman spectroscopy in three periods: immediately, 1 and 24 hours after polymerization. Data were analyzed with ANOVA and Tukey's tests. There were no significant differences between the 1-hour and 24-hour bond strengths (P > 0.05), or among the DC measured immediately, 1 hour and 24 hours after polymerization (P > 0.05). However, significant differences were observed among adhesives (P < 0.05). microTBS values obtained, in MPa (1 hour/24 hour), were: SB (48.6 + 1.3/48.4 + 3.5) = SE (51.9 + 4.7/53.3 +/- 2.9) > MP (35.3 +/- 10.9/38.6 + 6.7) > LP (25.5 + 1.1/26.0 + 1.5). The DC, in percentage (immediately/1 hour/24 hour), were: SE (81/82/87) > MP (79/77/81) > SB (60/63/65) > LP (39/37/42).
- 1 February 2007
- Vol. 9 (1) , 25-31
Composite-to-composite microtensile bond strength in the repair of a microfilled hybrid resin: effect of surface treatment and oxygen inhibition.
To compare the 24-h microtensile bond strength of a microfilled hybrid composite to the same material after mechanical and/or chemical treatment and assess the effect of oxygen inhibition on the composite-composite bond. Forty composite cylinders of Gradia Direct Anterior (GC) were prepared and stored 24 h prior to the following surface treatments: 50-microm aluminum oxide air abrasion and 37% phosphoric acid etching (group 1); hydrochloric acid and 6.9% hydrofluoric acid etching (group 2); diamond bur roughening and 37% phosphoric acid etching (group 3); diamond bur roughening (group 4). In all groups, Prime & Bond NT (Dentsply De Trey) was applied and light cured in air or under a nitrogen atmosphere, prior to layering a buildup of the repairing resin composite. Microtensile bond strength measurements were performed. Data were statistically analyzed with two-way ANOVA and Tukey's test (alpha = 0.05). The curing atmosphere did not significantly influence the interfacial strength (p < 0.05). Surface treatment significantly affected the composite-composite bond (p > 0.05). Air abrasion, regardless of curing atmosphere, resulted in the strongest bond (p < 0.05). The other treatments were comparable. Air abrasion and the application of a bonding agent offer satisfactory bond strengths for composite repair. The oxygen inhibition layer on a light-cured adhesive is not crucial to the success of the 24-h composite-composite bond.
- 1 February 2007
- Vol. 9 (1) , 25-31
Composite-to-composite microtensile bond strength in the repair of a microfilled hybrid resin: effect of surface treatment and oxygen inhibition.
To compare the 24-h microtensile bond strength of a microfilled hybrid composite to the same material after mechanical and/or chemical treatment and assess the effect of oxygen inhibition on the composite-composite bond. Forty composite cylinders of Gradia Direct Anterior (GC) were prepared and stored 24 h prior to the following surface treatments: 50-microm aluminum oxide air abrasion and 37% phosphoric acid etching (group 1); hydrochloric acid and 6.9% hydrofluoric acid etching (group 2); diamond bur roughening and 37% phosphoric acid etching (group 3); diamond bur roughening (group 4). In all groups, Prime & Bond NT (Dentsply De Trey) was applied and light cured in air or under a nitrogen atmosphere, prior to layering a buildup of the repairing resin composite. Microtensile bond strength measurements were performed. Data were statistically analyzed with two-way ANOVA and Tukey's test (alpha = 0.05). The curing atmosphere did not significantly influence the interfacial strength (p < 0.05). Surface treatment significantly affected the composite-composite bond (p > 0.05). Air abrasion, regardless of curing atmosphere, resulted in the strongest bond (p < 0.05). The other treatments were comparable. Air abrasion and the application of a bonding agent offer satisfactory bond strengths for composite repair. The oxygen inhibition layer on a light-cured adhesive is not crucial to the success of the 24-h composite-composite bond.
- 1 January 2007
- Published by Elsevier in Dental Materials
- Vol. 23 (1) , 95-99
Bond strength performance of different resin composites used as core materials around fiber posts
- 1 January 2007
- Published by Elsevier in Dental Materials
- Vol. 23 (1) , 95-99
Bond strength performance of different resin composites used as core materials around fiber posts
- 1 December 2005
- Published by Elsevier in Dental Materials
- Vol. 21 (12) , 1144-1149
The influence of the cutting speed on bond strength and integrity of microtensile specimens
- 1 December 2005
- Published by Elsevier in Dental Materials
- Vol. 21 (12) , 1144-1149
The influence of the cutting speed on bond strength and integrity of microtensile specimens
- 16 November 2005
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 78B (1) , 7-14
A novel method to obtain microtensile specimens minimizing cut flaws
Cutting procedures conventionally used for microtensile specimens' preparation induce mechanical stress and attrition, leading to cracks in dental structure. Enamel is mainly affected due to its high module of elasticity and brittleness. As an alternative to the conventional diamond saw, a diamond wire was used for cutting. The two techniques were compared in efficacy in the preparation of two different sample shapes. Forty human molars, flattened in dentin or enamel, were used for sample preparation. After bonding procedures, resin block was built incrementally. Half of the teeth were cut using a diamond disc and the other half using a diamond wire, obtaining slabs and stick‐shaped specimens. Slabs were then shaped to obtain hourglass samples. Five samples from each subgroup were randomly selected for Scanning electron microscopy (SEM) analysis. Remaining samples underwent microtensile test and the results were analyzed, including/excluding premature failures (pf), with three‐way ANOVA and Tukey test, performed separately, by substrate. On dentin, only the exclusion of pf showed a significant higher bond strength values than when pf were included (p < 0.05); however, on enamel, all factors (equipment, shape and including/excluding pf) had a significant effect on bond strength (p<0.05). The most remarkable finding from SEM was the incidence of specimens' cracks and defects when diamond blade was used. Scratches and cracks in the hourglass‐shaped specimens were also detected. In both cases, enamel was more affected than dentin. © 2005 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 2006
- 16 November 2005
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 78B (1) , 7-14
A novel method to obtain microtensile specimens minimizing cut flaws
Cutting procedures conventionally used for microtensile specimens' preparation induce mechanical stress and attrition, leading to cracks in dental structure. Enamel is mainly affected due to its high module of elasticity and brittleness. As an alternative to the conventional diamond saw, a diamond wire was used for cutting. The two techniques were compared in efficacy in the preparation of two different sample shapes. Forty human molars, flattened in dentin or enamel, were used for sample preparation. After bonding procedures, resin block was built incrementally. Half of the teeth were cut using a diamond disc and the other half using a diamond wire, obtaining slabs and stick‐shaped specimens. Slabs were then shaped to obtain hourglass samples. Five samples from each subgroup were randomly selected for Scanning electron microscopy (SEM) analysis. Remaining samples underwent microtensile test and the results were analyzed, including/excluding premature failures (pf), with three‐way ANOVA and Tukey test, performed separately, by substrate. On dentin, only the exclusion of pf showed a significant higher bond strength values than when pf were included (p < 0.05); however, on enamel, all factors (equipment, shape and including/excluding pf) had a significant effect on bond strength (p<0.05). The most remarkable finding from SEM was the incidence of specimens' cracks and defects when diamond blade was used. Scratches and cracks in the hourglass‐shaped specimens were also detected. In both cases, enamel was more affected than dentin. © 2005 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 2006
- 1 January 2002
- Vol. 4 (4) , 291-7
Adhesion testing with the microtensile method: effects of dental substrate and adhesive system on bond strength measurements.
To evaluate the bond strength of a self-etching primer (SE, Clearfil SE Bond) and a one-bottle adhesive system (EX, Excite) on enamel and dentin. Twenty-eight sound human molars were used. The teeth were randomly divided into four groups (n = 7): SE applied to enamel (SE-E); SE applied to dentin (SE-D); EX applied to enamel (EX-E); EX applied to dentin (EX-D). A resin (Tetric Ceram) block of approximately 5 x 5 x 5 mm was built up on the tooth and cured for 40 s. After 24 h, samples were obtained by cutting along the x and y axis of the tooth. Stick-shaped samples of approximately 0.8 mm2 cross-sectional area were obtained. The sticks underwent microtensile testing. The tensile bond strength (MPa) values of the test groups were: SE-E, 38.9 (+/- 4.8); SE-D, 44.5 (+/- 7.7); EX-E, 45.8 (+/- 4.7); EX-D, 42.9 (+/- 7.1). These values were not statistically significantly different. The null hypothesis was accepted that there is no difference between the self-etching primer and the one-bottle adhesive tested here. In addition, the bonding conditions provided by either bonding material on enamel were not significantly more favorable than on dentin. The majority of the specimens failed adhesively under load.
- 1 January 2002
- Vol. 4 (4) , 291-7
Adhesion testing with the microtensile method: effects of dental substrate and adhesive system on bond strength measurements.
To evaluate the bond strength of a self-etching primer (SE, Clearfil SE Bond) and a one-bottle adhesive system (EX, Excite) on enamel and dentin. Twenty-eight sound human molars were used. The teeth were randomly divided into four groups (n = 7): SE applied to enamel (SE-E); SE applied to dentin (SE-D); EX applied to enamel (EX-E); EX applied to dentin (EX-D). A resin (Tetric Ceram) block of approximately 5 x 5 x 5 mm was built up on the tooth and cured for 40 s. After 24 h, samples were obtained by cutting along the x and y axis of the tooth. Stick-shaped samples of approximately 0.8 mm2 cross-sectional area were obtained. The sticks underwent microtensile testing. The tensile bond strength (MPa) values of the test groups were: SE-E, 38.9 (+/- 4.8); SE-D, 44.5 (+/- 7.7); EX-E, 45.8 (+/- 4.7); EX-D, 42.9 (+/- 7.1). These values were not statistically significantly different. The null hypothesis was accepted that there is no difference between the self-etching primer and the one-bottle adhesive tested here. In addition, the bonding conditions provided by either bonding material on enamel were not significantly more favorable than on dentin. The majority of the specimens failed adhesively under load.