Subutay Han Altintas
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Subutay Han Altintas has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
Aslihan Usumez
Department of Prosthodontics, Faculty of Dentistry Bezmialem Vakif University Istanbul Turkey
3 shared publicationsSaadettin Kayipmaz
Department of Oral Diagnosis and Radiology, Faculty of Dentistry Karadeniz Technical University Trabzon Turkey
1 shared publicationTahsin Yildirim
Department of Restorative Dentistry, Faculty of Dentistry Karadeniz Technical University Trabzon Turkey
1 shared publication
Latest Publications
- 25 October 2012
- Published by Wiley in Journal of Prosthodontics
- Vol. 22 (4) , 282-286
Evaluation of the Radiopacity of Luting Cements by Digital Radiography
Purpose: The aim of this study was to evaluate the radiopacity of eight contemporary luting cements using direct digital radiography.Materials and Methods: Ten specimens, (5 mm diameter, 1 mm high) were prepared for each material tested (RelyX ARC, RelyX U100, RelyX Unicem, Nexus 2, Nexus 3, Metacem, Breeze, Adhesor zinc phosphate). The specimens were stored in a moist chamber at 37°C until completely set, then radiographed using a Kodak digital sensor and an aluminum step wedge with variable thicknesses (1 to 13 mm in 1‐mm increments) used for reference. A Kodak 2100 intraoral X‐ray unit was operated at 60 kV, 7 mA, and 0.20 seconds. According to international standards, the radiopacity of the specimens was compared with that of the aluminum step wedge using the equal‐density area tool of the Kodak Dental Imaging software (ver. 6.7). Data were analyzed by ANOVA and Tukey's test.Results: Adhesor zinc phosphate cement showed the highest radiopacity of all materials and dentin. Breeze showed the lowest radiopacity (p < 0.05). No significant difference in radiopacity was observed between dentin and RelyX ARC, Nexus 2, or Metacem (p > 0.05). The radiopacities of Nexus 3 and RelyX Unicem were significantly higher than those of other resin cements and dentin (p < 0.05).Conclusions: All materials showed radiopacity above the minimum recommended by the International Organization for Standardization and the American National Standards/American Dental Association. Breeze had less radiopacity than dentin.
- 25 October 2012
- Published by Wiley in Journal of Prosthodontics
- Vol. 22 (4) , 282-286
Evaluation of the Radiopacity of Luting Cements by Digital Radiography
Purpose: The aim of this study was to evaluate the radiopacity of eight contemporary luting cements using direct digital radiography.Materials and Methods: Ten specimens, (5 mm diameter, 1 mm high) were prepared for each material tested (RelyX ARC, RelyX U100, RelyX Unicem, Nexus 2, Nexus 3, Metacem, Breeze, Adhesor zinc phosphate). The specimens were stored in a moist chamber at 37°C until completely set, then radiographed using a Kodak digital sensor and an aluminum step wedge with variable thicknesses (1 to 13 mm in 1‐mm increments) used for reference. A Kodak 2100 intraoral X‐ray unit was operated at 60 kV, 7 mA, and 0.20 seconds. According to international standards, the radiopacity of the specimens was compared with that of the aluminum step wedge using the equal‐density area tool of the Kodak Dental Imaging software (ver. 6.7). Data were analyzed by ANOVA and Tukey's test.Results: Adhesor zinc phosphate cement showed the highest radiopacity of all materials and dentin. Breeze showed the lowest radiopacity (p < 0.05). No significant difference in radiopacity was observed between dentin and RelyX ARC, Nexus 2, or Metacem (p > 0.05). The radiopacities of Nexus 3 and RelyX Unicem were significantly higher than those of other resin cements and dentin (p < 0.05).Conclusions: All materials showed radiopacity above the minimum recommended by the International Organization for Standardization and the American National Standards/American Dental Association. Breeze had less radiopacity than dentin.
- Open Access
- 1 July 2012
- Published by Georg Thieme Verlag KG in European Journal of Dentistry
- Vol. 06 (03) , 255-262
Evaluation of TEGDMA leaching from four resin cements by HPLC
Objectives: The aim of this study was to evaluate the elution of TEGDMA from dual cured resin cements, used for bonding of ceramic restoration by high performance liquid chromatography (HPLC).Methods: Forty freshly extracted caries and restoration free molar teeth used in this study. Standardized Class I preparations were prepared in all teeth. Ceramic inlays were cemented with one of the dual cured resin cements (Variolink II, Rely X ARC, Rely X Unicem and Resilute). After cementation, specimens were stored in 75% ethanol solution. HPLC was used to analyze the amounts of TEGDMA in different time intervals. Two-way ANOVA and Tukey HSD tests were used to evaluate the results (P<.05).Results: The amount of TEGDMA eluted from Resilute was the highest and the amount of TEGDMA eluted from Rely X Unicem was the lowest (P<.05). The total amount of monomers was the highest after 21 days (P<.05).Conclusions: The five soft drinks caused surface softening of enamel (erosion). In respect to the chemical variables tested, despite not statistically significant, the pH seems to have more influence on the erosive potential of these drinks. (Eur J Dent 2007;1:10-13)
- 1 July 2012
- Published by Georg Thieme Verlag KG in European Journal of Dentistry
- Vol. 06 (03) , 255-262
Open AccessEvaluation of TEGDMA leaching from four resin cements by HPLC
Objectives: The aim of this study was to evaluate the elution of TEGDMA from dual cured resin cements, used for bonding of ceramic restoration by high performance liquid chromatography (HPLC).Methods: Forty freshly extracted caries and restoration free molar teeth used in this study. Standardized Class I preparations were prepared in all teeth. Ceramic inlays were cemented with one of the dual cured resin cements (Variolink II, Rely X ARC, Rely X Unicem and Resilute). After cementation, specimens were stored in 75% ethanol solution. HPLC was used to analyze the amounts of TEGDMA in different time intervals. Two-way ANOVA and Tukey HSD tests were used to evaluate the results (P<.05).Results: The amount of TEGDMA eluted from Resilute was the highest and the amount of TEGDMA eluted from Rely X Unicem was the lowest (P<.05). The total amount of monomers was the highest after 21 days (P<.05).Conclusions: The five soft drinks caused surface softening of enamel (erosion). In respect to the chemical variables tested, despite not statistically significant, the pH seems to have more influence on the erosive potential of these drinks. (Eur J Dent 2007;1:10-13)
- 21 March 2008
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 86B (2) , 523-529
Evaluation of monomer leaching from a dual cured resin cement
Purpose: An increasing number of inlay cavities is restored with tooth‐colored materials, especially ceramics are cemented with resin cements. The comonomer TEGDMA and other monomers Bis‐GMA and UDMA have been identified as the main compounds released from polymerized resin cements into aqueous media. The present investigation was conducted to clarify the leaching behavior of the monomers of dual polymerized resin cement. Material and methods: Ten freshly extracted caries and restoration free molar teeth were used in this study. Standardized Class I preparations were prepared in all teeth. Lithium disilicate based (IPS Empress Esthetic) ceramic inlays were cemented with dual polymerized resin cement (Variolink II). After cementation, specimens were stored in 75% ethanol solution. High‐performance liquid chromatography (HPLC) was used to analyze the amounts of three monomers in the solution (after 10 min, 1 h, 24 h, 3, 7, 14, and 21 days). Two‐way ANOVA and Tukey HSD tests were used to evaluate the results (p < 0.05). Results: There were statistically significant differences among the amounts of the monomers (p < 0.01) and also among time periods (p < 0.01). While the TEGDMA resulted in significantly higher amount than Bis‐GMA and UDMA, there were no statistically significant differences between amounts of Bis‐GMA, UDMA (p = 0.06). The cumulative amount of monomers was the highest after 21 days (p < 0.01). Conclusion: In the case of resin cement, leaching of TEGDMA was the highest and the cumulative amount of leaching monomers from resin cement was influenced by the time. © 2008 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 2008
- 21 March 2008
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 86B (2) , 523-529
Evaluation of monomer leaching from a dual cured resin cement
Purpose: An increasing number of inlay cavities is restored with tooth‐colored materials, especially ceramics are cemented with resin cements. The comonomer TEGDMA and other monomers Bis‐GMA and UDMA have been identified as the main compounds released from polymerized resin cements into aqueous media. The present investigation was conducted to clarify the leaching behavior of the monomers of dual polymerized resin cement. Material and methods: Ten freshly extracted caries and restoration free molar teeth were used in this study. Standardized Class I preparations were prepared in all teeth. Lithium disilicate based (IPS Empress Esthetic) ceramic inlays were cemented with dual polymerized resin cement (Variolink II). After cementation, specimens were stored in 75% ethanol solution. High‐performance liquid chromatography (HPLC) was used to analyze the amounts of three monomers in the solution (after 10 min, 1 h, 24 h, 3, 7, 14, and 21 days). Two‐way ANOVA and Tukey HSD tests were used to evaluate the results (p < 0.05). Results: There were statistically significant differences among the amounts of the monomers (p < 0.01) and also among time periods (p < 0.01). While the TEGDMA resulted in significantly higher amount than Bis‐GMA and UDMA, there were no statistically significant differences between amounts of Bis‐GMA, UDMA (p = 0.06). The cumulative amount of monomers was the highest after 21 days (p < 0.01). Conclusion: In the case of resin cement, leaching of TEGDMA was the highest and the cumulative amount of leaching monomers from resin cement was influenced by the time. © 2008 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 2008