Takataro Hamajima
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Takataro Hamajima has a total of 53 co-authors. Here are the top co-authors by number of shared publications:
M. Tsuda
Tohoku University, 05 Aoba Aramaki, Aoba-ku, Sendai, 980-8579, Japan
10 shared publicationsT. Yagai
Department of Electrical Engineering, Graduate School of Engineering, Sophia University, Tokyo, Japan
7 shared publicationsK. Takahata
National Institute for Fusion Science, Gifu, Japan
6 shared publicationsY. Nunoya
Japan Atomic Energy Agency, Naka., Ibaraki, Japan
4 shared publicationsK. Okuno
3 shared publicationsD. Miyagi
Tohoku University, 05 Aoba Aramaki, Aoba-ku, Sendai, 980-8579, Japan
2 shared publications
Latest Publications
- 25 January 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 28 (3) , 1-4
Superconducting Properties of a Prototype Pancake Coil Using a MgB2 Rutherford-Type Stranded Conductor
A prototype pancake coil using MgB2 Rutherford-type stranded conductors for SMES coil proposed in Advanced Superconducting Power Conditioning System (ASPCS) was fabricated and evaluated. A Rutherford-type stranded conductor, consists of CuNi former, 8 MgB2 wires and 4 Cu wires, with the twisted pitch was 51 mm, and a pancake coil of 200 mm in inner diameter, 269 mm in outer diameter and 7 mm in thickness was manufactured using Wind-and-React (W&R) method. The prototype coil was cooled by conduction cooling with use of refrigerators and critical current under 1.5 T at 25 K was over 700 A. These measurements suggest that several kJ class MgB2 SMES using MgB2 stranded conductors could be designed appropriately in terms from the view point of the bending strain.
- 25 January 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 28 (3) , 1-4
Superconducting Properties of a Prototype Pancake Coil Using a MgB2 Rutherford-Type Stranded Conductor
A prototype pancake coil using MgB2 Rutherford-type stranded conductors for SMES coil proposed in Advanced Superconducting Power Conditioning System (ASPCS) was fabricated and evaluated. A Rutherford-type stranded conductor, consists of CuNi former, 8 MgB2 wires and 4 Cu wires, with the twisted pitch was 51 mm, and a pancake coil of 200 mm in inner diameter, 269 mm in outer diameter and 7 mm in thickness was manufactured using Wind-and-React (W&R) method. The prototype coil was cooled by conduction cooling with use of refrigerators and critical current under 1.5 T at 25 K was over 700 A. These measurements suggest that several kJ class MgB2 SMES using MgB2 stranded conductors could be designed appropriately in terms from the view point of the bending strain.
- Open Access
- 21 April 2012
- Published by Elsevier in Physics Procedia
- Vol. 27, 396-399
Advanced superconducting power conditioning system with SMES for effective use of renewable energy
- 21 April 2012
- Published by Elsevier in Physics Procedia
- Vol. 27, 396-399
Open AccessAdvanced superconducting power conditioning system with SMES for effective use of renewable energy
- 29 November 2011
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 22 (3) , 4802004
Optimal Pitch Analysis Governing Contact Strand Number and Lengths With Cu Sleeves at CIC Joints
It is observed that measured critical current of Cable-in-Conduit-Conductor (CICC) for ITER TF coil are lower than expected. This is partly explained an imbalance of the contact resistance at the joint between double pancakes which causes an unbalanced current distribution in a cable and hence during a slow temperature increase some strands reach the critical current earlier than other. In order to estimate the contact resistances, we identify the three-dimensional positions of all strands inside the CICC, and then evaluate the contact parameters such as number and length of the strands which appear on the cable surface and have contact with a copper sleeve. It is observed that many strands do not appear on the surface of the cable, and can lead to unbalanced current distribution. We developed a numerical code to analyze all strand positions in the CICC. We evaluated the contact parameters by using the numerical code, and then compared them with those evaluated from the measured strand positions. It is found that since both results are in good agreement, the numerical code is available for evaluating the contact parameters. By using the code, we can optimize the contact parameters by varying the twist pitches of all staged subcables. The results show that all strands appear at the surface of the cable and have contact with the copper sleeve, and moreover the contact parameters have been improved.
- 29 November 2011
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 22 (3) , 4802004
Optimal Pitch Analysis Governing Contact Strand Number and Lengths With Cu Sleeves at CIC Joints
It is observed that measured critical current of Cable-in-Conduit-Conductor (CICC) for ITER TF coil are lower than expected. This is partly explained an imbalance of the contact resistance at the joint between double pancakes which causes an unbalanced current distribution in a cable and hence during a slow temperature increase some strands reach the critical current earlier than other. In order to estimate the contact resistances, we identify the three-dimensional positions of all strands inside the CICC, and then evaluate the contact parameters such as number and length of the strands which appear on the cable surface and have contact with a copper sleeve. It is observed that many strands do not appear on the surface of the cable, and can lead to unbalanced current distribution. We developed a numerical code to analyze all strand positions in the CICC. We evaluated the contact parameters by using the numerical code, and then compared them with those evaluated from the measured strand positions. It is found that since both results are in good agreement, the numerical code is available for evaluating the contact parameters. By using the code, we can optimize the contact parameters by varying the twist pitches of all staged subcables. The results show that all strands appear at the surface of the cable and have contact with the copper sleeve, and moreover the contact parameters have been improved.
- 18 March 2010
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 20 (3) , 1365-1368
Suitable Method for Increasing Current Carrying Capacity of HTS Toroidal Coils for SMES and DC Reactor
Non-uniform current distribution in a conductor composed of multiple HTS tapes is one of the important problems for increasing current carrying capacity of a large-scale coil system such as Superconducting Magnetic Energy Storage (SMES) and DC reactor. We focused on a manufacturing error in the HTS tape thickness and analytically investigated the relationship between the manufacturing error and the non-uniform current distribution. Even in a transposed conductor, the non-uniform current distribution is easily occurred by a small error in the tape thickness due to high coupling constant among the tapes. The non-uniformity of the current distribution reduces the current carrying capacity. However, the non-uniform current distribution can be improved by adopting a pancake coil with a large radius and small number of turns. An HTS tape with large thickness is also effective for reducing the non-uniformity of current distribution. Adopting parallel double pancake coils composed of single HTS tape is one of the promising candidates for increasing current carrying capacity effectively without any problems of the non-uniform current distribution. The suitable connecting method among the parallel double pancake coils for uniform current distribution, however, should be developed.
- 18 March 2010
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 20 (3) , 1365-1368
Suitable Method for Increasing Current Carrying Capacity of HTS Toroidal Coils for SMES and DC Reactor
Non-uniform current distribution in a conductor composed of multiple HTS tapes is one of the important problems for increasing current carrying capacity of a large-scale coil system such as Superconducting Magnetic Energy Storage (SMES) and DC reactor. We focused on a manufacturing error in the HTS tape thickness and analytically investigated the relationship between the manufacturing error and the non-uniform current distribution. Even in a transposed conductor, the non-uniform current distribution is easily occurred by a small error in the tape thickness due to high coupling constant among the tapes. The non-uniformity of the current distribution reduces the current carrying capacity. However, the non-uniform current distribution can be improved by adopting a pancake coil with a large radius and small number of turns. An HTS tape with large thickness is also effective for reducing the non-uniformity of current distribution. Adopting parallel double pancake coils composed of single HTS tape is one of the promising candidates for increasing current carrying capacity effectively without any problems of the non-uniform current distribution. The suitable connecting method among the parallel double pancake coils for uniform current distribution, however, should be developed.
- 31 December 2009
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 20 (3) , 560-563
Conceptual Design of Coaxial Multi-Layer Type CIC for SC Magnet of FFHR
An imbalanced current distribution is often observed in cable-in-conduit (CIC) superconductors which are composed of triplet type multi-staged sub-cables, and hence deteriorates the performance of the coils. Since it is very difficult to control homogeneous current distribution in the triplet type CIC, we propose a coaxial multi-layer type CIC to obtain the homogeneous current distribution. We use a circuit model to analyse the current distribution in the coaxial multi-layer CIC. After calculating inductances between adjacent layers in the coaxial multilayer cable, we can derive a generalized formula governing the current distribution as explicit functions of the superconducting cable construction parameters, such as twist pitch, twist direction, layer radius and SC and Cu strands number. We apply the formula to design the coaxial multi-layer CIC for SC magnet of Force Free Helical-type Fusion Reactor (FFHR). We can design the coaxial multi-layer CIC with the homogeneous current distribution, and investigate several SC strand arrangements in the CIC, and optimize the superconducting strand volume.
- 31 December 2009
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 20 (3) , 560-563
Conceptual Design of Coaxial Multi-Layer Type CIC for SC Magnet of FFHR
An imbalanced current distribution is often observed in cable-in-conduit (CIC) superconductors which are composed of triplet type multi-staged sub-cables, and hence deteriorates the performance of the coils. Since it is very difficult to control homogeneous current distribution in the triplet type CIC, we propose a coaxial multi-layer type CIC to obtain the homogeneous current distribution. We use a circuit model to analyse the current distribution in the coaxial multi-layer CIC. After calculating inductances between adjacent layers in the coaxial multilayer cable, we can derive a generalized formula governing the current distribution as explicit functions of the superconducting cable construction parameters, such as twist pitch, twist direction, layer radius and SC and Cu strands number. We apply the formula to design the coaxial multi-layer CIC for SC magnet of Force Free Helical-type Fusion Reactor (FFHR). We can design the coaxial multi-layer CIC with the homogeneous current distribution, and investigate several SC strand arrangements in the CIC, and optimize the superconducting strand volume.
- 23 June 2009
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 19 (3) , 1748-1751
Balanced Three-Phase Distributions of Tri-Axial Cable for Transmission Line
High Temperature Superconducting (HTS) cables have been intensively developed because of low loss and compactness, compared with conventional copper cables. A tri-axial cable composed of three concentric phases has been studied, because it has advantages such as reduced amount of HTS tapes and low heat-in-leak, compared with the three single-phase cables. However, there is an inherent imbalance in the three-phase distribution in the tri-axial cable due to differences in radii of the three-phase layers. We proposed a theory to obtain the balanced three-phase distribution for the tri-axial cable by treating two longitudinal cable sections together and adjusting all twist pitches. We derived a generalized formula as functions of winding pitches satisfying the balanced distribution. We designed and fabricated a short HTS tri-axial cable composed of 1 layer/phase to verify the proposed theory. The test results demonstrated that the theory is right for an equivalent impedance circuit model. The theory should be applied to the unbalanced three phase distributions caused by fabrication errors and inherent imbalance of capacitances in the tri-axial cable. We calculate the unbalanced three phase currents and voltages in steady state, and resolve them into symmetrical components to evaluate an imbalance ratio, which is defined as zero-sequence or negative-sequence to positive-sequence component. It is found that the fabrication errors of twist pitch and radius cause the imbalance ratios less than 1%, and the unbalanced capacitances of the cable of 10 km in length cause imbalance ratios of about 1%.
- 23 June 2009
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 19 (3) , 1748-1751
Balanced Three-Phase Distributions of Tri-Axial Cable for Transmission Line
High Temperature Superconducting (HTS) cables have been intensively developed because of low loss and compactness, compared with conventional copper cables. A tri-axial cable composed of three concentric phases has been studied, because it has advantages such as reduced amount of HTS tapes and low heat-in-leak, compared with the three single-phase cables. However, there is an inherent imbalance in the three-phase distribution in the tri-axial cable due to differences in radii of the three-phase layers. We proposed a theory to obtain the balanced three-phase distribution for the tri-axial cable by treating two longitudinal cable sections together and adjusting all twist pitches. We derived a generalized formula as functions of winding pitches satisfying the balanced distribution. We designed and fabricated a short HTS tri-axial cable composed of 1 layer/phase to verify the proposed theory. The test results demonstrated that the theory is right for an equivalent impedance circuit model. The theory should be applied to the unbalanced three phase distributions caused by fabrication errors and inherent imbalance of capacitances in the tri-axial cable. We calculate the unbalanced three phase currents and voltages in steady state, and resolve them into symmetrical components to evaluate an imbalance ratio, which is defined as zero-sequence or negative-sequence to positive-sequence component. It is found that the fabrication errors of twist pitch and radius cause the imbalance ratios less than 1%, and the unbalanced capacitances of the cable of 10 km in length cause imbalance ratios of about 1%.
- 5 June 2009
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 19 (3) , 2387-2390
Irregular Flux Linkage for Coupling Current Loops in Different Type CIC Conductors
Coupling current losses in large scale cable-in-conduit conductors (CICCs) for fusion apparatuses are sometimes annoyance because nobody can estimate how large the coupling loss is before fabricating hundred-meters of long conductor. Our approach for analyzing and estimating the loss based on real strand traces is unique compared with that of other research groups. In process of this approach, we have already measured the traces in two types of CICCs, one has circular cross section and the other has rectangular one. The cabling pattern of the former is 34 = 81 the latter is 34 times 6 = 486. The flux linkage area in a coupling current loop which consists of two contacting strands is evaluated as an indicator of driving force of the coupling current, which is proportional to the square root of AC loss per unit time. The flux linkage areas showed that the losses of rectangular-shape CICC would be larger than that of circular-shape CICC.
- 5 June 2009
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 19 (3) , 2387-2390
Irregular Flux Linkage for Coupling Current Loops in Different Type CIC Conductors
Coupling current losses in large scale cable-in-conduit conductors (CICCs) for fusion apparatuses are sometimes annoyance because nobody can estimate how large the coupling loss is before fabricating hundred-meters of long conductor. Our approach for analyzing and estimating the loss based on real strand traces is unique compared with that of other research groups. In process of this approach, we have already measured the traces in two types of CICCs, one has circular cross section and the other has rectangular one. The cabling pattern of the former is 34 = 81 the latter is 34 times 6 = 486. The flux linkage area in a coupling current loop which consists of two contacting strands is evaluated as an indicator of driving force of the coupling current, which is proportional to the square root of AC loss per unit time. The flux linkage areas showed that the losses of rectangular-shape CICC would be larger than that of circular-shape CICC.
- 30 January 2009
- Published by Wiley in IEEJ Transactions on Electrical and Electronic Engineering
- Vol. 4 (1) , 18-19
Expectation of implementation of superconduction applied equipment
- 30 January 2009
- Published by Wiley in IEEJ Transactions on Electrical and Electronic Engineering
- Vol. 4 (1) , 18-19
Expectation of implementation of superconduction applied equipment
- 6 June 2008
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 18 (2) , 832-835
Dependence of Horizontal Vibration Characteristics on Load Weight Distribution in Magnetic Levitation Type Seismic Isolation Device
We have developed a magnetic levitation type seismic isolation device. The device could remove any horizontal vibrations very effectively. Three-layer structure was adopted in the device. The bottom layer was composed of permanent magnets. The middle layer comprised HTS bulks and permanent magnets. The top layer consisted of HTS bulks. The horizontal vibration characteristics in the middle layer depended on the air gap between the bottom and middle layers; the air gap was closely related to the load weight distribution in the top and middle layers. Inhomogeneous load weight distribution caused the different air gap in each bulk. Horizontal levitation against the inhomogeneous load weight distribution, however, could be obtained by adjusting the initial offset angle of each bulk in field-cooling process. The smaller initial air gap was effective in realizing horizontal levitation; the difficulty of horizontal levitation increased with the initial air gap. Independent of the load weight distribution, almost the same characteristics of horizontal vibration were obtained in the small initial air gap.
- 6 June 2008
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 18 (2) , 832-835
Dependence of Horizontal Vibration Characteristics on Load Weight Distribution in Magnetic Levitation Type Seismic Isolation Device
We have developed a magnetic levitation type seismic isolation device. The device could remove any horizontal vibrations very effectively. Three-layer structure was adopted in the device. The bottom layer was composed of permanent magnets. The middle layer comprised HTS bulks and permanent magnets. The top layer consisted of HTS bulks. The horizontal vibration characteristics in the middle layer depended on the air gap between the bottom and middle layers; the air gap was closely related to the load weight distribution in the top and middle layers. Inhomogeneous load weight distribution caused the different air gap in each bulk. Horizontal levitation against the inhomogeneous load weight distribution, however, could be obtained by adjusting the initial offset angle of each bulk in field-cooling process. The smaller initial air gap was effective in realizing horizontal levitation; the difficulty of horizontal levitation increased with the initial air gap. Independent of the load weight distribution, almost the same characteristics of horizontal vibration were obtained in the small initial air gap.
- 6 June 2008
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 18 (2) , 1123-1126
Investigation of a Mechanism Forming Irregular Loops in Large CIC Conductor
Coupling loss with long time constants has been found a troublesome phenomenon for large size magnet application of superconductor because it would not be simply estimated from AC loss measurement of short sample conductor. In order to investigate the mechanism of the loss, we measured trajectories of strands of sample CIC (34 = 81) conductor. The measured length is 1 m along the conductor axis. By analyzing those trajectories, two important facts are cleared. One is that contact periods between two strands are calculated by the function of twisting pitches, not always by the Least Common Multiplier of twisting pitches. The other is that contact probabilities of two strands at each contactable point of sub cables depend on the difference of rotation angles of sub cables. To confirm the validity of this method, we calculated lengths of coupling current loops within 1 m in length by using experimentally obtained contact probabilities. The results are in very good agreement with lengths obtained from experimental results of strand trajectories. Then we computed the loop length in the long conductor (<100 m), it was obtained that the average loop length would reached about 3 m.
- 6 June 2008
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 18 (2) , 1123-1126
Investigation of a Mechanism Forming Irregular Loops in Large CIC Conductor
Coupling loss with long time constants has been found a troublesome phenomenon for large size magnet application of superconductor because it would not be simply estimated from AC loss measurement of short sample conductor. In order to investigate the mechanism of the loss, we measured trajectories of strands of sample CIC (34 = 81) conductor. The measured length is 1 m along the conductor axis. By analyzing those trajectories, two important facts are cleared. One is that contact periods between two strands are calculated by the function of twisting pitches, not always by the Least Common Multiplier of twisting pitches. The other is that contact probabilities of two strands at each contactable point of sub cables depend on the difference of rotation angles of sub cables. To confirm the validity of this method, we calculated lengths of coupling current loops within 1 m in length by using experimentally obtained contact probabilities. The results are in very good agreement with lengths obtained from experimental results of strand trajectories. Then we computed the loop length in the long conductor (<100 m), it was obtained that the average loop length would reached about 3 m.