Jarrod V. Crum
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Jarrod V. Crum has a total of 44 co-authors. Here are the top co-authors by number of shared publications:
- John D. Vienna
Pacific Northwest National Laboratory Richland Washington USA
6 shared publications David K. Peeler
Savannah River National Laboratory Aiken South Carolina 29808
3 shared publications- Dong-Sang Kim
Pacific Northwest National Laboratory (PNNL), Richland, WA (United States)
3 shared publications Michael J. Schweiger
3 shared publications- Carmen P. Rodriguez
Pacific Northwest National Laboratory Richland Washington USA
2 shared publications Donald E. Rinehart
2 shared publications
Latest Publications
- 22 May 2014
- Published by Office of Scientific and Technical Information (OSTI)
Silicate Based Glass Formulations for Immobilization of U.S. Defense Wastes Using Cold Crucible Induction Melters
The cold crucible induction melter (CCIM) is an alternative technology to the currently deployed liquid-fed, ceramic-lined, Joule-heated melter for immobilizing of U.S. tank waste generated from defense related reprocessing. In order to accurately evaluate the potential benefits of deploying a CCIM, glasses must be developed specifically for that melting technology. Related glass formulation efforts have been conducted since the 1990s including a recent study that is first documented in this report. The purpose of this report is to summarize the silicate base glass formulation efforts for CCIM testing of U.S. tank wastes. Summaries of phosphate based glass formulation and phosphate and silicate based CCIM demonstration tests are reported separately (Day and Ray 2013 and Marra 2013, respectively). Combined these three reports summarize the current state of knowledge related to waste form development and process testing of CCIM technology for U.S. tank wastes.
- 22 May 2014
- Published by Office of Scientific and Technical Information (OSTI)
Silicate Based Glass Formulations for Immobilization of U.S. Defense Wastes Using Cold Crucible Induction Melters
The cold crucible induction melter (CCIM) is an alternative technology to the currently deployed liquid-fed, ceramic-lined, Joule-heated melter for immobilizing of U.S. tank waste generated from defense related reprocessing. In order to accurately evaluate the potential benefits of deploying a CCIM, glasses must be developed specifically for that melting technology. Related glass formulation efforts have been conducted since the 1990s including a recent study that is first documented in this report. The purpose of this report is to summarize the silicate base glass formulation efforts for CCIM testing of U.S. tank wastes. Summaries of phosphate based glass formulation and phosphate and silicate based CCIM demonstration tests are reported separately (Day and Ray 2013 and Marra 2013, respectively). Combined these three reports summarize the current state of knowledge related to waste form development and process testing of CCIM technology for U.S. tank wastes.
- 8 May 2012
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 95 (7) , 2196-2205
DWPF Startup Frit Viscosity Measurement Round Robin Results
A viscosity standard is needed to replace the N ational I nstitute of S tandards and T echnology ( NIST ) glasses currently being used to calibrate viscosity measurement equipment. The current NIST glasses are either unavailable or less than ideal for calibrating equipment to measure the viscosity of high‐level waste glasses. This report documents the results of a viscosity round robin study conducted on the D efense W aste P rocessing F acility ( DWPF ) startup frit. DWPF startup frit was selected because its viscosity‐temperature relationship is similar to most DWPF and H anford high‐level waste glass compositions. The glass underwent grinding and blending to homogenize the large batch. Portions of the batch were supplied to eight laboratories for viscosity measurements, which were conducted following a specified temperature schedule with a temperature range of 1150°C–950°C, with an option to measure viscosity at temperatures below 950°C if their equipment was capable. Results were used to fit the V ogel‐ F ulcher‐ T amman‐ H esse and A rrhenius equations to viscosity as a function of temperature for the entire temperature range of 460°C through 1250°C as well as the limited temperature interval of ~ 950°C through 1250°C. The standard errors for confidence and prediction were determined for the fitted models.
- 8 May 2012
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 95 (7) , 2196-2205
DWPF Startup Frit Viscosity Measurement Round Robin Results
A viscosity standard is needed to replace the N ational I nstitute of S tandards and T echnology ( NIST ) glasses currently being used to calibrate viscosity measurement equipment. The current NIST glasses are either unavailable or less than ideal for calibrating equipment to measure the viscosity of high‐level waste glasses. This report documents the results of a viscosity round robin study conducted on the D efense W aste P rocessing F acility ( DWPF ) startup frit. DWPF startup frit was selected because its viscosity‐temperature relationship is similar to most DWPF and H anford high‐level waste glass compositions. The glass underwent grinding and blending to homogenize the large batch. Portions of the batch were supplied to eight laboratories for viscosity measurements, which were conducted following a specified temperature schedule with a temperature range of 1150°C–950°C, with an option to measure viscosity at temperatures below 950°C if their equipment was capable. Results were used to fit the V ogel‐ F ulcher‐ T amman‐ H esse and A rrhenius equations to viscosity as a function of temperature for the entire temperature range of 460°C through 1250°C as well as the limited temperature interval of ~ 950°C through 1250°C. The standard errors for confidence and prediction were determined for the fitted models.
- 17 October 2011
- Published by Office of Scientific and Technical Information (OSTI)
Formulation and Characterization of Waste Glasses with Varying Processing Temperature
This report documents the preliminary results of glass formulation and characterization accomplished within the finished scope of the EM-31 technology development tasks for WP-4 and WP-5, including WP-4.1.2: Glass Formulation for Next Generation Melter, WP-5.1.2.3: Systematic Glass Studies, and WP-5.1.2.4: Glass Formulation for Specific Wastes. This report also presents the suggested studies for eventual restart of these tasks. The initial glass formulation efforts for the cold crucible induction melter (CCIM), operating at {approx}1200 C, with selected HLW (AZ-101) and LAW (AN-105) successfully developed glasses with significant increase of waste loading compared to that is likely to be achieved based on expected reference WTP formulations. Three glasses formulated for AZ-101HLW and one glass for AN-105 LAW were selected for the initial CCIM demonstration melter tests. Melter tests were not performed within the finished scope of the WP-4.1.2 task. Glass formulations for CCIM were expanded to cover additional HLWs that have high potential to successfully demonstrate the unique advantages of the CCIM technologies based on projected composition of Hanford wastes. However, only the preliminary scoping tests were completed with selected wastes within the finished scope. Advanced glass formulations for the reference WTP melter, operating at {approx}1200 C, were initiated with selected specificmore » wastes to determine the estimated maximum waste loading. The incomplete results from these initial formulation efforts are summarized. For systematic glass studies, a test matrix of 32 high-aluminum glasses was completed based on a new method developed in this study. « less
- 17 October 2011
- Published by Office of Scientific and Technical Information (OSTI)
Formulation and Characterization of Waste Glasses with Varying Processing Temperature
This report documents the preliminary results of glass formulation and characterization accomplished within the finished scope of the EM-31 technology development tasks for WP-4 and WP-5, including WP-4.1.2: Glass Formulation for Next Generation Melter, WP-5.1.2.3: Systematic Glass Studies, and WP-5.1.2.4: Glass Formulation for Specific Wastes. This report also presents the suggested studies for eventual restart of these tasks. The initial glass formulation efforts for the cold crucible induction melter (CCIM), operating at {approx}1200 C, with selected HLW (AZ-101) and LAW (AN-105) successfully developed glasses with significant increase of waste loading compared to that is likely to be achieved based on expected reference WTP formulations. Three glasses formulated for AZ-101HLW and one glass for AN-105 LAW were selected for the initial CCIM demonstration melter tests. Melter tests were not performed within the finished scope of the WP-4.1.2 task. Glass formulations for CCIM were expanded to cover additional HLWs that have high potential to successfully demonstrate the unique advantages of the CCIM technologies based on projected composition of Hanford wastes. However, only the preliminary scoping tests were completed with selected wastes within the finished scope. Advanced glass formulations for the reference WTP melter, operating at {approx}1200 C, were initiated with selected specificmore » wastes to determine the estimated maximum waste loading. The incomplete results from these initial formulation efforts are summarized. For systematic glass studies, a test matrix of 32 high-aluminum glasses was completed based on a new method developed in this study. « less
- 17 December 2010
- Published by Office of Scientific and Technical Information (OSTI)
Development of Crystal-Tolerant High-Level Waste Glasses
Twenty five glasses were formulated. They were batched from HLW AZ-101 simulant or raw chemicals and melted and tested with a series of tests to elucidate the effect of spinel-forming components (Ni, Fe, Cr, Mn, and Zn), Al, and noble metals (Rh2O3 and RuO2) on the accumulation rate of spinel crystals in the glass discharge riser of the high-level waste (HLW) melter. In addition, the processing properties of glasses, such as the viscosity and TL, were measured as a function of temperature and composition. Furthermore, the settling of spinel crystals in transparent low-viscosity fluids was studied at room temperature to access the shape factor and hindered settling coefficient of spinel crystals in the Stokes equation. The experimental results suggest that Ni is the most troublesome component of all the studied spinel-forming components producing settling layers of up to 10.5 mm in just 20 days in Ni-rich glasses if noble metals or a higher concentration of Fe was not introduced in the glass. The layer of this thickness can potentially plug the bottom of the riser, preventing glass from being discharged from the melter. The noble metals, Fe, and Al were the components that significantly slowed down or stopped the accumulationmore » of spinel at the bottom. Particles of Rh2O3 and RuO2, hematite and nepheline, acted as nucleation sites significantly increasing the number of crystals and therefore decreasing the average crystal size. The settling rate of ≤10-μm crystal size around the settling velocity of crystals was too low to produce thick layers. The experimental data for the thickness of settled layers in the glasses prepared from AZ-101 simulant were used to build a linear empirical model that can predict crystal accumulation in the riser of the melter as a function of concentration of spinel-forming components in glass. The developed model predicts the thicknesses of accumulated layers quite well, R2 = 0.985, and can be become an efficient tool for the formulation of the crystal-tolerant HLW glasses for higher waste loading. A physical modeling effort revealed that the Stokes and Richardson-Zaki equations can be used to adequately predict the accumulation rate of spinel crystals of different sizes and concentrations in the glass discharge riser of HLW melters. The determined shape factor for the glass beads was only 0.73% lower than the theoretical shape factor for a perfect sphere. The shape factor for the spinel crystals matched the theoretically predicted value to within 10% and was smaller than that of the beads, given the larger drag force caused by the larger surface area-to-volume ratio of the octahedral crystals. In the hindered settling experiments, both the glass bead and spinel suspensions were found to follow the predictions of the Richardson-Zaki equation with the exponent n = 3.6 and 2.9 for glass beads and spinel crystals, respectively. « less
- 17 December 2010
- Published by Office of Scientific and Technical Information (OSTI)
Development of Crystal-Tolerant High-Level Waste Glasses
Twenty five glasses were formulated. They were batched from HLW AZ-101 simulant or raw chemicals and melted and tested with a series of tests to elucidate the effect of spinel-forming components (Ni, Fe, Cr, Mn, and Zn), Al, and noble metals (Rh2O3 and RuO2) on the accumulation rate of spinel crystals in the glass discharge riser of the high-level waste (HLW) melter. In addition, the processing properties of glasses, such as the viscosity and TL, were measured as a function of temperature and composition. Furthermore, the settling of spinel crystals in transparent low-viscosity fluids was studied at room temperature to access the shape factor and hindered settling coefficient of spinel crystals in the Stokes equation. The experimental results suggest that Ni is the most troublesome component of all the studied spinel-forming components producing settling layers of up to 10.5 mm in just 20 days in Ni-rich glasses if noble metals or a higher concentration of Fe was not introduced in the glass. The layer of this thickness can potentially plug the bottom of the riser, preventing glass from being discharged from the melter. The noble metals, Fe, and Al were the components that significantly slowed down or stopped the accumulationmore » of spinel at the bottom. Particles of Rh2O3 and RuO2, hematite and nepheline, acted as nucleation sites significantly increasing the number of crystals and therefore decreasing the average crystal size. The settling rate of ≤10-μm crystal size around the settling velocity of crystals was too low to produce thick layers. The experimental data for the thickness of settled layers in the glasses prepared from AZ-101 simulant were used to build a linear empirical model that can predict crystal accumulation in the riser of the melter as a function of concentration of spinel-forming components in glass. The developed model predicts the thicknesses of accumulated layers quite well, R2 = 0.985, and can be become an efficient tool for the formulation of the crystal-tolerant HLW glasses for higher waste loading. A physical modeling effort revealed that the Stokes and Richardson-Zaki equations can be used to adequately predict the accumulation rate of spinel crystals of different sizes and concentrations in the glass discharge riser of HLW melters. The determined shape factor for the glass beads was only 0.73% lower than the theoretical shape factor for a perfect sphere. The shape factor for the spinel crystals matched the theoretically predicted value to within 10% and was smaller than that of the beads, given the larger drag force caused by the larger surface area-to-volume ratio of the octahedral crystals. In the hindered settling experiments, both the glass bead and spinel suspensions were found to follow the predictions of the Richardson-Zaki equation with the exponent n = 3.6 and 2.9 for glass beads and spinel crystals, respectively. « less
- 23 March 2010
- Published by Office of Scientific and Technical Information (OSTI)
Hanford Sludge Simulant Selection for Soil Mechanics Property Measurement
The current System Plan for the Hanford Tank Farms uses relaxed buoyant displacement gas release event (BDGRE) controls for deep sludge (i.e., high level waste [HLW]) tanks, which allows the tank farms to use more storage space, i.e., increase the sediment depth, in some of the double-shell tanks (DSTs). The relaxed BDGRE controls are based on preliminary analysis of a gas release model from van Kessel and van Kesteren. Application of the van Kessel and van Kesteren model requires parametric information for the sediment, including the lateral earth pressure at rest and shear modulus. No lateral earth pressure at rest and shear modulus in situ measurements for Hanford sludge are currently available. The two chemical sludge simulants will be used in follow-on work to experimentally measure the van Kessel and van Kesteren model parameters, lateral earth pressure at rest, and shear modulus.
- 23 March 2010
- Published by Office of Scientific and Technical Information (OSTI)
Hanford Sludge Simulant Selection for Soil Mechanics Property Measurement
The current System Plan for the Hanford Tank Farms uses relaxed buoyant displacement gas release event (BDGRE) controls for deep sludge (i.e., high level waste [HLW]) tanks, which allows the tank farms to use more storage space, i.e., increase the sediment depth, in some of the double-shell tanks (DSTs). The relaxed BDGRE controls are based on preliminary analysis of a gas release model from van Kessel and van Kesteren. Application of the van Kessel and van Kesteren model requires parametric information for the sediment, including the lateral earth pressure at rest and shear modulus. No lateral earth pressure at rest and shear modulus in situ measurements for Hanford sludge are currently available. The two chemical sludge simulants will be used in follow-on work to experimentally measure the van Kessel and van Kesteren model parameters, lateral earth pressure at rest, and shear modulus.
- 20 November 2009
- Published by Office of Scientific and Technical Information (OSTI)
Laboratory Tests on Post-Filtration Precipitation in the WTP Pretreatment Process
Pacific Northwest National Laboratory (PNNL) has been tasked by Bechtel National Inc. (BNI) on the River Protection Project-Hanford Tank Waste Treatment and Immobilization Plant (RPP-WTP) project to perform research and development activities to resolve technical issues identified for the Pretreatment Facility (PTF). The Pretreatment Engineering Platform (PEP) was designed, constructed, and operated as part of a plan to respond to issue M12, "Undemonstrated Leaching Processes," of the External Flowsheet Review Team (EFRT) issue response plan (Barnes et al. 2006). The PEP is a 1/4.5-scale test platform designed to simulate the WTP pretreatment caustic leaching, oxidative leaching, ultrafiltration solids concentration, and slurry washing processes. The PEP replicates the WTP leaching processes using prototypic equipment and control strategies. A simplified flow diagram of the PEP system is shown in Figure 1.1. Two operating scenarios are currently being evaluated for the ultrafiltration process (UFP) and leaching operations. The first scenario has caustic leaching performed in the UFP-2 ultrafiltration feed vessels (i.e., vessel UFP-VSL-T02A in the PEP; and vessels UFP-VSL-00002A and B in the WTP PTF). The second scenario has caustic leaching conducted in the UFP-1 ultrafiltration feed preparation vessels (i.e., vessels UFP-VSL-T01A and B in the PEP; vessels UFP-VSL-00001A and B in themore » WTP PTF).« less
- 20 November 2009
- Published by Office of Scientific and Technical Information (OSTI)
Laboratory Tests on Post-Filtration Precipitation in the WTP Pretreatment Process
Pacific Northwest National Laboratory (PNNL) has been tasked by Bechtel National Inc. (BNI) on the River Protection Project-Hanford Tank Waste Treatment and Immobilization Plant (RPP-WTP) project to perform research and development activities to resolve technical issues identified for the Pretreatment Facility (PTF). The Pretreatment Engineering Platform (PEP) was designed, constructed, and operated as part of a plan to respond to issue M12, "Undemonstrated Leaching Processes," of the External Flowsheet Review Team (EFRT) issue response plan (Barnes et al. 2006). The PEP is a 1/4.5-scale test platform designed to simulate the WTP pretreatment caustic leaching, oxidative leaching, ultrafiltration solids concentration, and slurry washing processes. The PEP replicates the WTP leaching processes using prototypic equipment and control strategies. A simplified flow diagram of the PEP system is shown in Figure 1.1. Two operating scenarios are currently being evaluated for the ultrafiltration process (UFP) and leaching operations. The first scenario has caustic leaching performed in the UFP-2 ultrafiltration feed vessels (i.e., vessel UFP-VSL-T02A in the PEP; and vessels UFP-VSL-00002A and B in the WTP PTF). The second scenario has caustic leaching conducted in the UFP-1 ultrafiltration feed preparation vessels (i.e., vessels UFP-VSL-T01A and B in the PEP; vessels UFP-VSL-00001A and B in themore » WTP PTF).« less
- 25 September 2009
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 92 (10) , 2378-2384
Binary Phase Diagram of the Manganese Oxide–Iron Oxide System
The phase equilibrium of the MnO x –FeO y binary system was measured within a temperature range of 750°–1590°C in air to examine inconsistencies found in literature, i.e., discrepancies related to the boundary between the spinel and hausmannite+spinel phase fields. Several studies are available in the literature that describe this boundary however the results and methods by which they were studied vary namely in terms of the atmosphere (air versus reducing) used and heat treatment/analysis methods. In addition, samples in the discrepancy region of the diagram revert to the hausmannite phase spontaneously upon cooling due to a displacive transformation. In order to accurately measure the phase boundaries, the following measurement methods were used: isothermal heat treatments followed by rapid quenching (in air or water), dilatometry, differential thermal analysis with thermogravimetric analysis, as well as room temperature and hot‐stage X‐ray diffraction (XRD). Phase assemblage(s) in each specimen were determined by XRD. Data were compared with literature and a new, self consistent phase diagram was developed. The results are reported along with background information and a comparison with previously reported data. This study will support development of a model for thermodynamic equilibria in complex, multioxide silicate melts.
- 25 September 2009
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 92 (10) , 2378-2384
Binary Phase Diagram of the Manganese Oxide–Iron Oxide System
The phase equilibrium of the MnO x –FeO y binary system was measured within a temperature range of 750°–1590°C in air to examine inconsistencies found in literature, i.e., discrepancies related to the boundary between the spinel and hausmannite+spinel phase fields. Several studies are available in the literature that describe this boundary however the results and methods by which they were studied vary namely in terms of the atmosphere (air versus reducing) used and heat treatment/analysis methods. In addition, samples in the discrepancy region of the diagram revert to the hausmannite phase spontaneously upon cooling due to a displacive transformation. In order to accurately measure the phase boundaries, the following measurement methods were used: isothermal heat treatments followed by rapid quenching (in air or water), dilatometry, differential thermal analysis with thermogravimetric analysis, as well as room temperature and hot‐stage X‐ray diffraction (XRD). Phase assemblage(s) in each specimen were determined by XRD. Data were compared with literature and a new, self consistent phase diagram was developed. The results are reported along with background information and a comparison with previously reported data. This study will support development of a model for thermodynamic equilibria in complex, multioxide silicate melts.
- 30 March 2005
- Published by Office of Scientific and Technical Information (OSTI)
Tc Reductant Chemistry and Crucible Melting Studies with Simulated Hanford Low-Activity Waste
The FY 2003 risk assessment (RA) of bulk vitrification (BV) waste packages used 0.3 wt% of the technetium (Tc) inventory as a leachable salt and found it sufficient to create a significant peak in the groundwater concentration in a 100-meter down-gradient well. Although this peak met regulatory limits, considering uncertainty in the actual Tc salt fraction, peak concentrations could exceed the maximum concentration limit (MCL) under some scenarios so reducing the leachable salt inventory is desirable. The main objective of this study was to reduce the mobile Tc species available within a BV disposal package by reducing the oxidation state of the Tc in the waste feed and/or during melting because Tc in its reduced form of Tc(IV) has a much lower volatility than Tc(VII). Reduced Tc volatility has a secondary benefit of increasing the Tc retention in glass.
- 30 March 2005
- Published by Office of Scientific and Technical Information (OSTI)
Tc Reductant Chemistry and Crucible Melting Studies with Simulated Hanford Low-Activity Waste
The FY 2003 risk assessment (RA) of bulk vitrification (BV) waste packages used 0.3 wt% of the technetium (Tc) inventory as a leachable salt and found it sufficient to create a significant peak in the groundwater concentration in a 100-meter down-gradient well. Although this peak met regulatory limits, considering uncertainty in the actual Tc salt fraction, peak concentrations could exceed the maximum concentration limit (MCL) under some scenarios so reducing the leachable salt inventory is desirable. The main objective of this study was to reduce the mobile Tc species available within a BV disposal package by reducing the oxidation state of the Tc in the waste feed and/or during melting because Tc in its reduced form of Tc(IV) has a much lower volatility than Tc(VII). Reduced Tc volatility has a secondary benefit of increasing the Tc retention in glass.
- 30 March 2001
- Published by Office of Scientific and Technical Information (OSTI)
Formulation Efforts for Direct Vitrification of INEEL Blend Calcine Waste Simulate: Fiscal Year 2000
This report documents the results of glass formulation efforts for Idaho National Engineering and Environmental Laboratory (INEEL) high level waste (HWL) calcine. Two waste compositions were used during testing. Testing started by using the Run 78 calcine composition and switched to simulated Blend calcine composition when it became available. The goal of the glass formulation efforts was to develop a frit composition that will accept higher waste loading that satisfies the glass processing and product acceptance constraints. 1. Melting temperature of 1125 ? 25?C 2. Viscosity between 2 and 10 Pa?s at the melting temperature 3. Liquidus temperature at least 100?C below the melting temperature 4. Normalized release of B, Li and Na each below 1 g/m2 (per ASTM C 1285-97) Glass formulation efforts tested several frit compositions with variable waste loadings of Run 78 calcine waste simulant. Frit 107 was selected as the primary candidate for processing since it met all process and performance criteria up to 45 mass% waste loading. When the simulated Blend calcine waste composition became available Frits 107 and 108 compositions were retested and again Frit 107 remained the primary candidate. However, both frits suffered a decrease in waste loading when switching from the Runmore » 78 calcine to simulated Blend calcine waste composition. This was due to increase concentrations of both F and Al2O3 along with a decrease in CaO and Na2O in the simulate Blend calcine waste all of which have strong impacts on the glass properties that limit waste loading of this type of waste.« less
- 30 March 2001
- Published by Office of Scientific and Technical Information (OSTI)
Formulation Efforts for Direct Vitrification of INEEL Blend Calcine Waste Simulate: Fiscal Year 2000
This report documents the results of glass formulation efforts for Idaho National Engineering and Environmental Laboratory (INEEL) high level waste (HWL) calcine. Two waste compositions were used during testing. Testing started by using the Run 78 calcine composition and switched to simulated Blend calcine composition when it became available. The goal of the glass formulation efforts was to develop a frit composition that will accept higher waste loading that satisfies the glass processing and product acceptance constraints. 1. Melting temperature of 1125 ? 25?C 2. Viscosity between 2 and 10 Pa?s at the melting temperature 3. Liquidus temperature at least 100?C below the melting temperature 4. Normalized release of B, Li and Na each below 1 g/m2 (per ASTM C 1285-97) Glass formulation efforts tested several frit compositions with variable waste loadings of Run 78 calcine waste simulant. Frit 107 was selected as the primary candidate for processing since it met all process and performance criteria up to 45 mass% waste loading. When the simulated Blend calcine waste composition became available Frits 107 and 108 compositions were retested and again Frit 107 remained the primary candidate. However, both frits suffered a decrease in waste loading when switching from the Runmore » 78 calcine to simulated Blend calcine waste composition. This was due to increase concentrations of both F and Al2O3 along with a decrease in CaO and Na2O in the simulate Blend calcine waste all of which have strong impacts on the glass properties that limit waste loading of this type of waste.« less