Adriana Faria Azevedo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Adriana Faria Azevedo has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Neidenei Gomes Ferreira
Instituto Nacional de Pesquisas Espaciais
5 shared publications - Mauricio Ribeiro Baldan
National Space Research Institute, Avenida dos astronautas 1758, São José dos Campos 12227-010, SP, Brazil
3 shared publications Carlos Giles
Universidade Estadual de Campinas – UNICAMP, Inst. de Física Gleb Wataghin, Departamento de Física da Matéria Condensada Barão Geraldo, Campinas, SP/13083-970 (Brazil)
1 shared publication- Eduardo Saito
Universidade Federal de Sao Paulo, Brasil
1 shared publication Evaldo J. Corat
Faculdade de Engenharia Química de Lorena, Brazil
1 shared publicationF. A. Souza
Instituto Nacional de Pesquisas Espaciais, INPE/LAS
1 shared publication
Latest Publications
- 7 May 2012
- Published by Wiley in Chemical Vapor Deposition
- Vol. 18 (4-6) , 159-165
The Effect of Boron Doping Level on The Morphology and Structure of Ultra/Nanocrystalline Diamond Films
In this work, boron‐doped nanocrystalline diamond (BDND) films are grown on silicon substrates by hot‐filament (HF)CVD in Ar/H2/CH4 gas mixtures. In this study, the transition from ultra‐nanocrystalline to nanocrystalline diamond films is clearly shown by the addition of boron dopant to the growth of the gas mixture. The doping process consists of an additional H2 line passing through a bubbler containing B2O3 dissolved in methanol with various B/C ratios. Five sample sets are obtained with doping in the methanol bubbler solution of 2 000, 5 000, 10 000, 20 000, and 30 000 ppm for a 16 h growth time. The morphology, roughness, and structure of these films have markedly different properties. The cross‐section of the films is characterized by scanning electron microscopy (SEM) showing the transition from ultra‐nanocrystalline growth (renucleation process) to a columnar structure of nanocrystalline films. The acceptor density values, evaluated by Raman spectra and by Mott‐Schottky plot analysis, vary from 1020 to 1021 B cm−3 as the doping level increases. The grain size and the relative intensity of the (111)/(220) peaks are obtained from X‐ray diffraction (XRD) patterns of the films. The diamond average grain size increases from 10 to 35 nm for films with 2 000 and 30 000 ppm B/C, respectively, in the methanol bubbler solution. The preferential orientation also changes, from (220) to (111), as the boron doping level increases.
- 7 May 2012
- Published by Wiley in Chemical Vapor Deposition
- Vol. 18 (4-6) , 159-165
The Effect of Boron Doping Level on The Morphology and Structure of Ultra/Nanocrystalline Diamond Films
In this work, boron‐doped nanocrystalline diamond (BDND) films are grown on silicon substrates by hot‐filament (HF)CVD in Ar/H2/CH4 gas mixtures. In this study, the transition from ultra‐nanocrystalline to nanocrystalline diamond films is clearly shown by the addition of boron dopant to the growth of the gas mixture. The doping process consists of an additional H2 line passing through a bubbler containing B2O3 dissolved in methanol with various B/C ratios. Five sample sets are obtained with doping in the methanol bubbler solution of 2 000, 5 000, 10 000, 20 000, and 30 000 ppm for a 16 h growth time. The morphology, roughness, and structure of these films have markedly different properties. The cross‐section of the films is characterized by scanning electron microscopy (SEM) showing the transition from ultra‐nanocrystalline growth (renucleation process) to a columnar structure of nanocrystalline films. The acceptor density values, evaluated by Raman spectra and by Mott‐Schottky plot analysis, vary from 1020 to 1021 B cm−3 as the doping level increases. The grain size and the relative intensity of the (111)/(220) peaks are obtained from X‐ray diffraction (XRD) patterns of the films. The diamond average grain size increases from 10 to 35 nm for films with 2 000 and 30 000 ppm B/C, respectively, in the methanol bubbler solution. The preferential orientation also changes, from (220) to (111), as the boron doping level increases.
- Open Access
- 1 January 2012
- Published by Wiley in International Journal of Electrochemistry
- Vol. 2012 (1) , 1-16
Nanodiamond Films for Applications in Electrochemical Systems
The purpose of the present paper is to give an overview on the current development status of nanocrystalline diamond electrodes for electrochemical applications. Firstly, we describe a brief comparison between the general properties of nanocrystalline diamond (undoped and boron-doped) and boron-doped microcrystalline diamond films. This is followed by a summary of the nanodiamond preparation methods. Finally, we present a discussion about the undoped and boron-doped nanocrystalline diamond and their characteristics, electrochemical properties, and practical applications.
- 1 January 2012
- Published by Wiley in International Journal of Electrochemistry
- Vol. 2012 (1) , 1-16
Open AccessNanodiamond Films for Applications in Electrochemical Systems
The purpose of the present paper is to give an overview on the current development status of nanocrystalline diamond electrodes for electrochemical applications. Firstly, we describe a brief comparison between the general properties of nanocrystalline diamond (undoped and boron-doped) and boron-doped microcrystalline diamond films. This is followed by a summary of the nanodiamond preparation methods. Finally, we present a discussion about the undoped and boron-doped nanocrystalline diamond and their characteristics, electrochemical properties, and practical applications.
- 17 July 2011
- Published by Springer Nature in Journal of Nanoparticle Research
- Vol. 13 (11) , 6133-6139
The influence of hydrogen plasma pre-treatment on the structure of BDND electrode surface applied for phenol detection
- 17 July 2011
- Published by Springer Nature in Journal of Nanoparticle Research
- Vol. 13 (11) , 6133-6139
The influence of hydrogen plasma pre-treatment on the structure of BDND electrode surface applied for phenol detection
- Open Access
- 28 April 2011
- Published by Elsevier in Journal of Electroanalytical Chemistry
- Vol. 658 (1-2) , 38-45
Detection of phenol at boron-doped nanocrystalline diamond electrodes
- 28 April 2011
- Published by Elsevier in Journal of Electroanalytical Chemistry
- Vol. 658 (1-2) , 38-45
Open AccessDetection of phenol at boron-doped nanocrystalline diamond electrodes
- Open Access
- 1 February 2006
- Published by FapUNIFESP (SciELO) in Química Nova
- Vol. 29 (1) , 129-136
Filmes de nanodiamantes para aplicações em sistemas eletroquímicos e tecnologia aeroespacial
The goal of this work is to show the use of undoped nanodiamond films as a new material for electrochemical and aerospace applications. Correlation between the applications and physico-chemical features of nano and conventional CVD polycrystalline diamond films are presented. An important and innovative application of these nanodiamonds is organic electrosynthesis, including pharmaceutical and water disinfection products, as well as electroanalytical applications, for example, development of biosensors for detection of glucose, glutamate and dopamine. In aeronautics and space developments, these nanodiamonds could be used as electrodes in rechargable batteries and in tribological investigations
- 1 February 2006
- Published by FapUNIFESP (SciELO) in Química Nova
- Vol. 29 (1) , 129-136
Open AccessFilmes de nanodiamantes para aplicações em sistemas eletroquímicos e tecnologia aeroespacial
The goal of this work is to show the use of undoped nanodiamond films as a new material for electrochemical and aerospace applications. Correlation between the applications and physico-chemical features of nano and conventional CVD polycrystalline diamond films are presented. An important and innovative application of these nanodiamonds is organic electrosynthesis, including pharmaceutical and water disinfection products, as well as electroanalytical applications, for example, development of biosensors for detection of glucose, glutamate and dopamine. In aeronautics and space developments, these nanodiamonds could be used as electrodes in rechargable batteries and in tribological investigations
- Open Access
- 1 January 2003
- Published by FapUNIFESP (SciELO) in Materials Research
- Vol. 6 (1) , 51-56
Raman analyses of residual stress in diamond thin films grown on Ti6Al4V alloy
The stress evolution in diamond films grown on Ti6Al4V was investigated in order to develop a comprehensive view of the residual stress formation. Residual stress is composed of intrinsic stress induced during diamond film growth and extrinsic stress caused by the different thermal expansion coefficients between the film and substrate. In the coalescence stage it has been observed that the residual stress is dominated by the microstructure, whereas on continuous films, the thermal stress is more important. In this work diamond thin films with small grain size and good size and good quality were obtained in a surface wave-guide microwave discharge, the Surfatron system, with a negative bias voltage applied between the plasma shell and substrate. For above of -100V applied bias, the ratio of carbon sp³/sp² bond may increase and the nucleation rate increase arising the high value at the -250V applied bias. Stress measurements and sp³ content in the film were studied by Raman scattering spectroscopy. The total residual stress is compressive and varied from -1.52 to -1.48 GPa between 0 and -200 V applied bias, respectively, and above the -200 V, the compressive residual stress increased drastically to -1.80 GPa. The diamond nucleation density was evaluated by top view SEM images
- 1 January 2003
- Published by FapUNIFESP (SciELO) in Materials Research
- Vol. 6 (1) , 51-56
Open AccessRaman analyses of residual stress in diamond thin films grown on Ti6Al4V alloy
The stress evolution in diamond films grown on Ti6Al4V was investigated in order to develop a comprehensive view of the residual stress formation. Residual stress is composed of intrinsic stress induced during diamond film growth and extrinsic stress caused by the different thermal expansion coefficients between the film and substrate. In the coalescence stage it has been observed that the residual stress is dominated by the microstructure, whereas on continuous films, the thermal stress is more important. In this work diamond thin films with small grain size and good size and good quality were obtained in a surface wave-guide microwave discharge, the Surfatron system, with a negative bias voltage applied between the plasma shell and substrate. For above of -100V applied bias, the ratio of carbon sp³/sp² bond may increase and the nucleation rate increase arising the high value at the -250V applied bias. Stress measurements and sp³ content in the film were studied by Raman scattering spectroscopy. The total residual stress is compressive and varied from -1.52 to -1.48 GPa between 0 and -200 V applied bias, respectively, and above the -200 V, the compressive residual stress increased drastically to -1.80 GPa. The diamond nucleation density was evaluated by top view SEM images