F. J. Boerio
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
F. J. Boerio has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
R. G. Dillingham
Brighton Technologies Group, Inc. , Cincinnati , Ohio , USA
3 shared publicationsS. Wirasate
Department of Chemical and Materials Engineering , University of Cincinnati , Cincinnati, Ohio, USA
2 shared publicationsB. Bengu
Department of Chemical and Materials Engineering , University of Cincinnati , Cincinnnati , Ohio , USA
1 shared publicationC. A. Gosselin
Department of Materials Science and Metallurgical Engineering , University of Cincinnati , Cincinnati , Ohio , 45221 , U.S.A.
1 shared publicationE. J. Krusling
Department of Chemical and Materials Engineering, University of Cincinnati Cincinnati, Ohio 45221–0012
1 shared publicationH. W. Liu
Department of Materials Science and Metallurgical Engineering , University of Cincinnati , Cincinnati , Ohio , 45221 , U.S.A.
1 shared publication
Latest Publications
- 3 December 2008
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 84 (10) , 872-895
AFM/FTIR: A New Technique for Materials Characterization
A new type of infrared spectroscopy for obtaining the molecular composition of the surfaces of materials at ultra-high spatial resolution has been developed by combining atomic force microscopy (AFM) with Fourier-transform infrared spectroscopy (FTIR). This new analytical technique involves the use of an AFM to detect the response of a material to the absorption of modulated infrared radiation from an FTIR spectrometer and is referred to as AFM/FTIR spectroscopy. When the technique of AFM/FTIR spectroscopy is completely developed, we plan to use it to probe the molecular structure of interphases in polymer composites and adhesive bonds. Two approaches have been used to measure the response of polymer systems to infrared absorption. The first involves the use of a contact mode AFM probe to measure the thermal expansion of the polymer; the second involves using a scanning thermal microscopy (SThM) probe to measure the polymer's temperature increase. In either case, the output of the probe resembles an interferogram to which a Fourier-transform can be applied to obtain the infrared absorption spectrum. The first approach was used to obtain excellent quality AFM/FTIR spectra from various neat polymer films, including polystyrene, polycarbonate, and a model adhesive system consisting of an epoxy resin cross-linked with dicyandiamide. Excellent spectra were also obtained from polystyrene beads having a diameter of about 2 µm. The second approach, using an SThM probe to determine the temperature increase that accompanies infrared absorption, was also used to obtain interferograms of polymer samples such as polystyrene. However, the interferograms were noisy and the AFM/FTIR spectra obtained from them had a low signal-to-noise ratio. The present results, thus, show that AFM/FTIR spectroscopy is feasible but the spatial resolution of the technique remains to be shown.
- 3 December 2008
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 84 (10) , 872-895
AFM/FTIR: A New Technique for Materials Characterization
A new type of infrared spectroscopy for obtaining the molecular composition of the surfaces of materials at ultra-high spatial resolution has been developed by combining atomic force microscopy (AFM) with Fourier-transform infrared spectroscopy (FTIR). This new analytical technique involves the use of an AFM to detect the response of a material to the absorption of modulated infrared radiation from an FTIR spectrometer and is referred to as AFM/FTIR spectroscopy. When the technique of AFM/FTIR spectroscopy is completely developed, we plan to use it to probe the molecular structure of interphases in polymer composites and adhesive bonds. Two approaches have been used to measure the response of polymer systems to infrared absorption. The first involves the use of a contact mode AFM probe to measure the thermal expansion of the polymer; the second involves using a scanning thermal microscopy (SThM) probe to measure the polymer's temperature increase. In either case, the output of the probe resembles an interferogram to which a Fourier-transform can be applied to obtain the infrared absorption spectrum. The first approach was used to obtain excellent quality AFM/FTIR spectra from various neat polymer films, including polystyrene, polycarbonate, and a model adhesive system consisting of an epoxy resin cross-linked with dicyandiamide. Excellent spectra were also obtained from polystyrene beads having a diameter of about 2 µm. The second approach, using an SThM probe to determine the temperature increase that accompanies infrared absorption, was also used to obtain interferograms of polymer samples such as polystyrene. However, the interferograms were noisy and the AFM/FTIR spectra obtained from them had a low signal-to-noise ratio. The present results, thus, show that AFM/FTIR spectroscopy is feasible but the spatial resolution of the technique remains to be shown.
- 8 March 2007
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 83 (3) , 267-287
Molecular Structure of the Interphase Formed by Plasma-Polymerized Acetylene Films and Steel Substrates
The molecular structure of the interphase between plasma-polymerized acetylene films and steel substrates was determined using in situ reflection–absorption infrared spectroscopy (RAIR) and X-ray photoelectron spectroscopy (XPS). Plasma-polymerized acetylene films were deposited onto polished steel substrates using argon as a carrier gas and inductively coupled, radio frequency (RF)-powered plasma reactors that were interfaced directly to the XPS and Fourier transform infrared (FTIR) spectrometers. RAIR showed that the plasma polymerized films contained large numbers of methyl and methylene groups but only a small number of mono substituted acetylene groups, indicating that there was substantial rearrangement of the monomer molecules during plasma polymerization. Bands were observed near 1020 and 855 cm−1 in the RAIR spectra that were attributed to skeletal stretching vibrations in C–C–O–Fe groups, indicating that the plasma-polymerized films interacted with the substrate through formation of alkoxide bonds. Another band was observed near 1565 cm−1 and attributed to carboxylate groups in the interphase between the films and the oxidized surface of the substrate. Results obtained from XPS showed that the surface of the iron substrate consisted mostly of a mixture of Fe2O3 and FeOOH and that iron was mostly present in the Fe(III) oxidation state. However, during plasma polymerization of acetylene, there was a tendency for the concentration of FeOOH groups to decrease and for the concentration of Fe(II) to increase, due to the reducing nature of argon/acetylene plasmas. Results from XPS also confirmed the formation of alkoxide and carboxylate groups in the interphase during plasma polymerization of acetylene.
- 8 March 2007
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 83 (3) , 267-287
Molecular Structure of the Interphase Formed by Plasma-Polymerized Acetylene Films and Steel Substrates
The molecular structure of the interphase between plasma-polymerized acetylene films and steel substrates was determined using in situ reflection–absorption infrared spectroscopy (RAIR) and X-ray photoelectron spectroscopy (XPS). Plasma-polymerized acetylene films were deposited onto polished steel substrates using argon as a carrier gas and inductively coupled, radio frequency (RF)-powered plasma reactors that were interfaced directly to the XPS and Fourier transform infrared (FTIR) spectrometers. RAIR showed that the plasma polymerized films contained large numbers of methyl and methylene groups but only a small number of mono substituted acetylene groups, indicating that there was substantial rearrangement of the monomer molecules during plasma polymerization. Bands were observed near 1020 and 855 cm−1 in the RAIR spectra that were attributed to skeletal stretching vibrations in C–C–O–Fe groups, indicating that the plasma-polymerized films interacted with the substrate through formation of alkoxide bonds. Another band was observed near 1565 cm−1 and attributed to carboxylate groups in the interphase between the films and the oxidized surface of the substrate. Results obtained from XPS showed that the surface of the iron substrate consisted mostly of a mixture of Fe2O3 and FeOOH and that iron was mostly present in the Fe(III) oxidation state. However, during plasma polymerization of acetylene, there was a tendency for the concentration of FeOOH groups to decrease and for the concentration of Fe(II) to increase, due to the reducing nature of argon/acetylene plasmas. Results from XPS also confirmed the formation of alkoxide and carboxylate groups in the interphase during plasma polymerization of acetylene.
- 21 December 2006
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 82 (12) , 1133-1155
Interaction of Epoxy/Dicyandiamide Adhesives with Metal Substrates
The molecular structure of the interphase formed by curing a model adhesive system consisting of the diglycidyl ether of bisphenol-A (DGEBA) and dicyandiamide (DDA) against mechanically polished aluminum and electrogalvanized steel (EGS) substrates was determined using reflection–absorption infrared spectroscopy (RAIR) and X-ray photoelectron spectroscopy (XPS). RAIR analysis suggested that DGEBA/DDA mixtures created an interphase with a different molecular structure from the bulk of the adhesive when cured in contact with aluminum. The formation of this unique interphase was mainly due to interactions between DDA and the Al surface. XPS analysis indicated that aluminum ions exposed by heating the substrate surface were necessary for this interaction. DDA was found to adsorb onto the aluminum surface via the lone pair of electrons on the nitrogen atoms of the nitrile groups. A slight decrease in the nitrile stretching frequency suggested an additional back-bonding interaction between aluminum ions and the nitrile groups. Slight back donation of electrons from the metal to DDA resulted in a reduction product that led to the formation of the carbodiimide form of DDA. This specific reaction caused a decrease in the concentration of nitrile groups in the interphase and changed the extent of the reaction between DDA and DGEBA by inhibiting the formation of oxazolidine structures. The interaction of DDA with EGS surfaces followed a similar trend. However, the effects were much more pronounced with EGS and the extent of the curing reaction and the cross-linking rate near the metal surface were strongly affected by EGS/DDA interactions.
- 21 December 2006
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 82 (12) , 1133-1155
Interaction of Epoxy/Dicyandiamide Adhesives with Metal Substrates
The molecular structure of the interphase formed by curing a model adhesive system consisting of the diglycidyl ether of bisphenol-A (DGEBA) and dicyandiamide (DDA) against mechanically polished aluminum and electrogalvanized steel (EGS) substrates was determined using reflection–absorption infrared spectroscopy (RAIR) and X-ray photoelectron spectroscopy (XPS). RAIR analysis suggested that DGEBA/DDA mixtures created an interphase with a different molecular structure from the bulk of the adhesive when cured in contact with aluminum. The formation of this unique interphase was mainly due to interactions between DDA and the Al surface. XPS analysis indicated that aluminum ions exposed by heating the substrate surface were necessary for this interaction. DDA was found to adsorb onto the aluminum surface via the lone pair of electrons on the nitrogen atoms of the nitrile groups. A slight decrease in the nitrile stretching frequency suggested an additional back-bonding interaction between aluminum ions and the nitrile groups. Slight back donation of electrons from the metal to DDA resulted in a reduction product that led to the formation of the carbodiimide form of DDA. This specific reaction caused a decrease in the concentration of nitrile groups in the interphase and changed the extent of the reaction between DDA and DGEBA by inhibiting the formation of oxazolidine structures. The interaction of DDA with EGS surfaces followed a similar trend. However, the effects were much more pronounced with EGS and the extent of the curing reaction and the cross-linking rate near the metal surface were strongly affected by EGS/DDA interactions.
- 1 August 2006
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 82 (8) , 805-829
Adhesion and Scratch Resistance of Polycarbonate Films on Ferroplate Substrates: Effect of γ-APS Primers
The influence of γ-aminopropyltriethoxysilane (γ-APS) primers on the adhesion and scratch resistance of polycarbonate (PC) films on ferroplate substrates was determined from the critical normal loads at which debonding of the films from the substrates occurred during scratch testing. The critical load was a strong function of the concentration of the aqueous solutions from which the γ-APS primers were adsorbed and of the thickness of the primer films. Thus, the critical normal load increased from 0.09 ± 0.02 N to 0.31 ± 0.07 N as the concentration of the γ-APS solutions increased from 0.05% to 0.2%, respectively. However, the critical load increased only slightly as the solution concentration increased beyond 0.2%. The increase in critical load as concentration of γ-APS solutions increased was related to the formation of an interphase involving chemical reaction and physical entanglement of PC and γ-APS molecules. The critical load for debonding of PC films from the substrates also depended strongly on the temperature at which the γ-APS films were dried before application of the PC films. Thus, the critical normal loads for debonding were 0.31 ± 0.07, 0.20 ± 0.02, and 0.05 ± 0.01 N for γ-APS films that were dried for 15 min at room temperature, 60°C, or 110°C, respectively. The decrease in critical load with increasing drying temperature was attributed to the greater cross-link density in γ-APS films that were dried at elevated temperatures, which limited interdiffusion and physical entanglement of PC and γ-APS molecules. High reaction temperature of γ-APS and PC induced a fragmentation of amine. However, it also increased the probability of amines to react with carbonate because of increasing mobility of PC chains. Optimization of these two factors was required to obtain the greatest adhesion and scratch resistance. Chemical reactions occurring between PC films and γ-APS primers were investigated by reflection–absorption infrared spectroscopy (RAIR) and X-ray photoelectron spectroscopy (XPS) using diphenyl carbonate (DPC) as a model compound. The carbonyl absorption band of neat DPC was observed at 1780 cm−1. However, two carbonyl bands were observed at 1738 and 1652 cm−1 in RAIR spectra of γ-APS films that were reacted with DPC and were assigned to urethane and urea groups, respectively. XPS results revealed that urethane was the main reaction product between DPC and γ-APS. It was concluded that urethane groups formed by the reaction of PC with γ-APS were responsible for adhesion and scratch resistance of PC to ferroplate substrates that were primed with γ-APS.
- 1 August 2006
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 82 (8) , 805-829
Adhesion and Scratch Resistance of Polycarbonate Films on Ferroplate Substrates: Effect of γ-APS Primers
The influence of γ-aminopropyltriethoxysilane (γ-APS) primers on the adhesion and scratch resistance of polycarbonate (PC) films on ferroplate substrates was determined from the critical normal loads at which debonding of the films from the substrates occurred during scratch testing. The critical load was a strong function of the concentration of the aqueous solutions from which the γ-APS primers were adsorbed and of the thickness of the primer films. Thus, the critical normal load increased from 0.09 ± 0.02 N to 0.31 ± 0.07 N as the concentration of the γ-APS solutions increased from 0.05% to 0.2%, respectively. However, the critical load increased only slightly as the solution concentration increased beyond 0.2%. The increase in critical load as concentration of γ-APS solutions increased was related to the formation of an interphase involving chemical reaction and physical entanglement of PC and γ-APS molecules. The critical load for debonding of PC films from the substrates also depended strongly on the temperature at which the γ-APS films were dried before application of the PC films. Thus, the critical normal loads for debonding were 0.31 ± 0.07, 0.20 ± 0.02, and 0.05 ± 0.01 N for γ-APS films that were dried for 15 min at room temperature, 60°C, or 110°C, respectively. The decrease in critical load with increasing drying temperature was attributed to the greater cross-link density in γ-APS films that were dried at elevated temperatures, which limited interdiffusion and physical entanglement of PC and γ-APS molecules. High reaction temperature of γ-APS and PC induced a fragmentation of amine. However, it also increased the probability of amines to react with carbonate because of increasing mobility of PC chains. Optimization of these two factors was required to obtain the greatest adhesion and scratch resistance. Chemical reactions occurring between PC films and γ-APS primers were investigated by reflection–absorption infrared spectroscopy (RAIR) and X-ray photoelectron spectroscopy (XPS) using diphenyl carbonate (DPC) as a model compound. The carbonyl absorption band of neat DPC was observed at 1780 cm−1. However, two carbonyl bands were observed at 1738 and 1652 cm−1 in RAIR spectra of γ-APS films that were reacted with DPC and were assigned to urethane and urea groups, respectively. XPS results revealed that urethane was the main reaction product between DPC and γ-APS. It was concluded that urethane groups formed by the reaction of PC with γ-APS were responsible for adhesion and scratch resistance of PC to ferroplate substrates that were primed with γ-APS.
- 1 June 2005
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 81 (6) , 645-675
Adhesion of Injection Molded PVC to Steel Substrates
Interactions occurring at the interface between injection-molded poly (vinyl chloride) (PVC) and steel substrates that were coated with thin films of aminosilanes were investigated by X-ray photoelectron spectroscopy (XPS) and Fourier-transform infrared spectroscopy (FTIR). The silane films were formed by adsorption of γ-aminopropyltriethoxysilane (γ-APS) or N-(2-aminoethyl-3-aminopropyl)trimethoxysilane (γ-AEAPS) from 2% aqueous solutions onto polished steel substrates. PVC was injection molded onto the silane-primed steel substrates and annealed at temperatures up to 170°C for times as long as 30 min. PVC was peeled off of the primed steel substrates using a 90° peel test and the substrate failure surfaces were thoroughly rinsed with tetrahydrofuran (THF) and distilled water to remove PVC and other compounds that were not strongly bonded to the substrates. The PVC failure surfaces were characterized by attenuated total reflection infrared spectroscopy (ATR) and PVC rinsed off of the substrate failure surfaces was characterized by transmission infrared spectroscopy. The resulting transmission and ATR spectra showed an absorption band near 1650 cm−1 that was attributed to unsaturation in PVC. The substrate failure surfaces were characterized by XPS; curve-fitting of N(1s) and Cl(2p) high-resolution spectra showed the formation of amine hydrochloride complexes by protonation of amino groups of the silanes with HCl that was liberated from PVC during the onset of thermal dehydrochlorination. Furthermore, quaternization or nucleophilic substitution of labile pendent allylic chloride groups by amino groups on the silanes took place, thus grafting PVC onto the aminosilanes. It was determined that PVC that had β-chloroallyl groupings along its chains showed better adhesion with steel primed with aminosilanes and that generation of allylic chloride groups in PVC chains was the rate-limiting step in the reaction between PVC and aminosilane. Moreover, the effect of crosslinking of silane films on adhesion between PVC and aminosilane primed steel was investigated and it was concluded that interdiffusion of the polymer phase and the silane phase was also critical in obtaining good adhesion.
- 1 June 2005
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 81 (6) , 645-675
Adhesion of Injection Molded PVC to Steel Substrates
Interactions occurring at the interface between injection-molded poly (vinyl chloride) (PVC) and steel substrates that were coated with thin films of aminosilanes were investigated by X-ray photoelectron spectroscopy (XPS) and Fourier-transform infrared spectroscopy (FTIR). The silane films were formed by adsorption of γ-aminopropyltriethoxysilane (γ-APS) or N-(2-aminoethyl-3-aminopropyl)trimethoxysilane (γ-AEAPS) from 2% aqueous solutions onto polished steel substrates. PVC was injection molded onto the silane-primed steel substrates and annealed at temperatures up to 170°C for times as long as 30 min. PVC was peeled off of the primed steel substrates using a 90° peel test and the substrate failure surfaces were thoroughly rinsed with tetrahydrofuran (THF) and distilled water to remove PVC and other compounds that were not strongly bonded to the substrates. The PVC failure surfaces were characterized by attenuated total reflection infrared spectroscopy (ATR) and PVC rinsed off of the substrate failure surfaces was characterized by transmission infrared spectroscopy. The resulting transmission and ATR spectra showed an absorption band near 1650 cm−1 that was attributed to unsaturation in PVC. The substrate failure surfaces were characterized by XPS; curve-fitting of N(1s) and Cl(2p) high-resolution spectra showed the formation of amine hydrochloride complexes by protonation of amino groups of the silanes with HCl that was liberated from PVC during the onset of thermal dehydrochlorination. Furthermore, quaternization or nucleophilic substitution of labile pendent allylic chloride groups by amino groups on the silanes took place, thus grafting PVC onto the aminosilanes. It was determined that PVC that had β-chloroallyl groupings along its chains showed better adhesion with steel primed with aminosilanes and that generation of allylic chloride groups in PVC chains was the rate-limiting step in the reaction between PVC and aminosilane. Moreover, the effect of crosslinking of silane films on adhesion between PVC and aminosilane primed steel was investigated and it was concluded that interdiffusion of the polymer phase and the silane phase was also critical in obtaining good adhesion.
- 1 May 2005
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 81 (5) , 509-528
Effect of Adhesion, Film Thickness, and Substrate Hardness on the Scratch Behavior of Poly(carbonate) Films
The effect of adhesion, film thickness, and substrate hardness on the scratch behavior of poly(carbonate) (PC) films was investigated. Films of various thickness were prepared by spin-coating solutions of PC in chloroform onto glass, ferroplate, Al 1100, Al 6022, and Al 6111 substrates. Adhesion between the films and the substrates was controlled by pretreatment of the substrates and the thickness of the films was controlled by the concentration of the PC solutions. Adhesion of the films to the glass substrates was measured by a blister test. Scratch tests were performed using a custom-built, progressive-load scratch tester with interchangeable diamond indenters; the resulting scratches were observed by optical microscopy, atomic force microscopy (AFM), and environmental scanning electron microscopy (ESEM). The critical normal load (i.e., the smallest applied normal load for which delamination of the film from the substrate was observed) was used as a criterion to determine the scratch resistance of the films. It was found that better film/substrate adhesion resulted in a higher critical load for delamination. As film thickness increased, the critical load and, thus, scratch resistance also increased. Substrate hardness had a strong influence on the scratch behavior of the PC films. For a low-hardness substrate (i.e., Al 1100), the work from scratching was mainly consumed by deforming the substrate. In the case of substrates with intermediate hardness (i.e., Al 6022, Al 6111, and ferroplate), the substrates were more resistant to the stresses that were generated in the films; hence, the deformation of the substrates was less severe. A high-hardness substrate (i.e., glass) resisted the applied load and resulted in higher stress concentrations in the films and at the interface. Consequently, a rougher surface inside the scratch track was observed.
- 1 May 2005
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 81 (5) , 509-528
Effect of Adhesion, Film Thickness, and Substrate Hardness on the Scratch Behavior of Poly(carbonate) Films
The effect of adhesion, film thickness, and substrate hardness on the scratch behavior of poly(carbonate) (PC) films was investigated. Films of various thickness were prepared by spin-coating solutions of PC in chloroform onto glass, ferroplate, Al 1100, Al 6022, and Al 6111 substrates. Adhesion between the films and the substrates was controlled by pretreatment of the substrates and the thickness of the films was controlled by the concentration of the PC solutions. Adhesion of the films to the glass substrates was measured by a blister test. Scratch tests were performed using a custom-built, progressive-load scratch tester with interchangeable diamond indenters; the resulting scratches were observed by optical microscopy, atomic force microscopy (AFM), and environmental scanning electron microscopy (ESEM). The critical normal load (i.e., the smallest applied normal load for which delamination of the film from the substrate was observed) was used as a criterion to determine the scratch resistance of the films. It was found that better film/substrate adhesion resulted in a higher critical load for delamination. As film thickness increased, the critical load and, thus, scratch resistance also increased. Substrate hardness had a strong influence on the scratch behavior of the PC films. For a low-hardness substrate (i.e., Al 1100), the work from scratching was mainly consumed by deforming the substrate. In the case of substrates with intermediate hardness (i.e., Al 6022, Al 6111, and ferroplate), the substrates were more resistant to the stresses that were generated in the films; hence, the deformation of the substrates was less severe. A high-hardness substrate (i.e., glass) resisted the applied load and resulted in higher stress concentrations in the films and at the interface. Consequently, a rougher surface inside the scratch track was observed.
- 1 February 2005
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 81 (2) , 115-142
Vapor-Phase Silanation of Plasma-Polymerized Silica-Like Films by γ-Aminopropyltriethoxysilane
Silica-like films were deposited onto aluminum substrates by plasma polymerization of hexamethyldisiloxane (HMDSO) in the presence of oxygen using a capacitively coupled Radio-Frequency (RF)-powered plasma reactor. Two types of films, referred to as low hydroxyl and high hydroxyl, were obtained by varying parameters such as the power and the flow rates of oxygen and HMDSO. Two bands that were assigned to hydrogen-bonded silanol groups were observed in reflection–absorption infrared (RAIR) spectra of high-hydroxyl films. The first band was near 3400 cm−1 and was very broad; this band was assigned to the OH-stretching mode of silanol groups in which the hydrogen atom was hydrogen bonded to the oxygen atom of an adjacent silanol group. The second band was near 3650 cm−1 and was assigned to OH stretching in isolated silanol groups in which the hydrogen atom was hydrogen bonded to the oxygen atom of an Si‒O‒Si group. Only the band near 3650 cm−1 was observed in RAIR spectra of low-hydroxyl films. RAIR spectra of the high-hydroxyl films were characterized by a band near 934 cm−1 assigned to the Si‒O-stretching mode of silanol groups. This band was not observed in spectra of the low-hydroxyl films. γ-Aminopropyltriethoxysilane (γ-APS) was adsorbed onto the silica-like films from the vapor phase at a substrate temperature of 100°C. Results obtained from X-ray photoelectron spectroscopy (XPS) showed that some of the nitrogen atoms in the adsorbed γ-APS films were protonated, probably by strong hydrogen bonding with silanol groups on the surface of the silica-like films. However, most of the amino groups were not protonated, indicating that adsorption in that case involved condensation of ethoxy groups with surface silanol groups. Thus, a band observed near 1100 cm−1in RAIR spectra of γ-APS that adsorbed onto silica-like films was tentatively assigned to a vibrational mode characteristic of Si‒O‒Sisubstrate bonds. Lap joints were prepared using a two-part epoxy adhesive and aluminum substrates that were primed with silica-like films. Joints prepared from substrates that were primed with low-hydroxyl films had an average strength of about 23.4 MPa whereas those prepared from substrates primed with high-hydroxyl films had an average strength of about 14.3 MPa. Vapor-phase silanation of the primer films did not have a significant effect on the initial strength of the joints. However, it did have an effect on the locus of failure as determined by XPS. When no silane was used, joints prepared using substrates primed with the low-hydroxyl films failed near the adhesive–primer interface. Joints prepared using substrates primed with the low-hydroxyl films and coated with γ-APS failed cohesively, within the adhesive.
- 1 February 2005
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 81 (2) , 115-142
Vapor-Phase Silanation of Plasma-Polymerized Silica-Like Films by γ-Aminopropyltriethoxysilane
Silica-like films were deposited onto aluminum substrates by plasma polymerization of hexamethyldisiloxane (HMDSO) in the presence of oxygen using a capacitively coupled Radio-Frequency (RF)-powered plasma reactor. Two types of films, referred to as low hydroxyl and high hydroxyl, were obtained by varying parameters such as the power and the flow rates of oxygen and HMDSO. Two bands that were assigned to hydrogen-bonded silanol groups were observed in reflection–absorption infrared (RAIR) spectra of high-hydroxyl films. The first band was near 3400 cm−1 and was very broad; this band was assigned to the OH-stretching mode of silanol groups in which the hydrogen atom was hydrogen bonded to the oxygen atom of an adjacent silanol group. The second band was near 3650 cm−1 and was assigned to OH stretching in isolated silanol groups in which the hydrogen atom was hydrogen bonded to the oxygen atom of an Si‒O‒Si group. Only the band near 3650 cm−1 was observed in RAIR spectra of low-hydroxyl films. RAIR spectra of the high-hydroxyl films were characterized by a band near 934 cm−1 assigned to the Si‒O-stretching mode of silanol groups. This band was not observed in spectra of the low-hydroxyl films. γ-Aminopropyltriethoxysilane (γ-APS) was adsorbed onto the silica-like films from the vapor phase at a substrate temperature of 100°C. Results obtained from X-ray photoelectron spectroscopy (XPS) showed that some of the nitrogen atoms in the adsorbed γ-APS films were protonated, probably by strong hydrogen bonding with silanol groups on the surface of the silica-like films. However, most of the amino groups were not protonated, indicating that adsorption in that case involved condensation of ethoxy groups with surface silanol groups. Thus, a band observed near 1100 cm−1in RAIR spectra of γ-APS that adsorbed onto silica-like films was tentatively assigned to a vibrational mode characteristic of Si‒O‒Sisubstrate bonds. Lap joints were prepared using a two-part epoxy adhesive and aluminum substrates that were primed with silica-like films. Joints prepared from substrates that were primed with low-hydroxyl films had an average strength of about 23.4 MPa whereas those prepared from substrates primed with high-hydroxyl films had an average strength of about 14.3 MPa. Vapor-phase silanation of the primer films did not have a significant effect on the initial strength of the joints. However, it did have an effect on the locus of failure as determined by XPS. When no silane was used, joints prepared using substrates primed with the low-hydroxyl films failed near the adhesive–primer interface. Joints prepared using substrates primed with the low-hydroxyl films and coated with γ-APS failed cohesively, within the adhesive.
- 1 January 2002
- Published by Springer Nature in MRS Proceedings
- Vol. 734
Molecular Structure of Interphases Formed by Plasma Polymerized Acetylene Films and Steel Substrates
- 1 January 2002
- Published by Springer Nature in MRS Proceedings
- Vol. 734
Molecular Structure of Interphases Formed by Plasma Polymerized Acetylene Films and Steel Substrates
- 1 January 1992
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 6 (1) , 207-225
The effect of a multicomponent silane primer on the interphase structure of aluminum/epoxy adhesive joints
The structure of films formed by a multicomponent silane primer applied to an aluminum adherend and the interactions of this primer with an amine-cured epoxy adhesive were studied using X-ray photoelectron spectroscopy, reflection-absorption infrared spectroscopy, and attenuated total reflectance infrared spectroscopy. The failure in joints prepared from primed adherends occurred extremely close to the adherend surface in a region that contained much interpenetrated primer and epoxy. IR spectra showed evidence of oxidation in the primer. Fracture occurred in a region of interpenetrated primer and adhesive with higher than normal crosslink density. The primer films have a stratified structure that is retained even after curing of the adhesive.
- 1 January 1992
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 6 (1) , 207-225
The effect of a multicomponent silane primer on the interphase structure of aluminum/epoxy adhesive joints
The structure of films formed by a multicomponent silane primer applied to an aluminum adherend and the interactions of this primer with an amine-cured epoxy adhesive were studied using X-ray photoelectron spectroscopy, reflection-absorption infrared spectroscopy, and attenuated total reflectance infrared spectroscopy. The failure in joints prepared from primed adherends occurred extremely close to the adherend surface in a region that contained much interpenetrated primer and epoxy. IR spectra showed evidence of oxidation in the primer. Fracture occurred in a region of interpenetrated primer and adhesive with higher than normal crosslink density. The primer films have a stratified structure that is retained even after curing of the adhesive.
- 13 December 1981
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 13 (2) , 159-176
Analysis of Thin Films on Metal Surfaces
External reflection infrared spectroscopy was used in combination with other surface analysis techniques such as ellipsometry, Auger electron spectroscopy (AES), and X-ray photoelectron spectroscopy (XPS) to determine the structure of organofunctional silanes adsorbed onto 2024 aluminum and titanium-6 Al, 4V mirrors. The results obtained indicated that the adsorption of γ-aminopropyltriethoxysilane (γ-APS) onto aluminum was a strong function of pH and adsorption time. Films formed by adsorption of γ-APS at pH = 8.5 were composed of polysiloxanes containing amine hydrochlorides. The structure of films formed by adsorption of γ-APS at pH-10.4 depended on time. Films obtained after one minute were composed of polysiloxanes that did not interact strongly with the oxide but during 15 minutes adsorption the air-formed oxide was dissolved and copper accumulated near the surface of the mirrors. Films formed by the adsorption of γ-glycidoxypropyltrimethoxysilane (γ-GPS) onto aluminum were composed of polysiloxanes that did not interact strongly with the oxide. The structure of films formed by adsorption of γ-APS onto titanium did not depend on adsorption time. Films formed at pH = 10.4 were composed of low molecular weight oligomers that gradually polymerized to polysiloxanes during atmospheric exposure.
- 13 December 1981
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 13 (2) , 159-176
Analysis of Thin Films on Metal Surfaces
External reflection infrared spectroscopy was used in combination with other surface analysis techniques such as ellipsometry, Auger electron spectroscopy (AES), and X-ray photoelectron spectroscopy (XPS) to determine the structure of organofunctional silanes adsorbed onto 2024 aluminum and titanium-6 Al, 4V mirrors. The results obtained indicated that the adsorption of γ-aminopropyltriethoxysilane (γ-APS) onto aluminum was a strong function of pH and adsorption time. Films formed by adsorption of γ-APS at pH = 8.5 were composed of polysiloxanes containing amine hydrochlorides. The structure of films formed by adsorption of γ-APS at pH-10.4 depended on time. Films obtained after one minute were composed of polysiloxanes that did not interact strongly with the oxide but during 15 minutes adsorption the air-formed oxide was dissolved and copper accumulated near the surface of the mirrors. Films formed by the adsorption of γ-glycidoxypropyltrimethoxysilane (γ-GPS) onto aluminum were composed of polysiloxanes that did not interact strongly with the oxide. The structure of films formed by adsorption of γ-APS onto titanium did not depend on adsorption time. Films formed at pH = 10.4 were composed of low molecular weight oligomers that gradually polymerized to polysiloxanes during atmospheric exposure.