Silvia Sestini
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Silvia Sestini has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
Antonio Pelagalli
**** Department of Dentistry, University of Siena, Italy
1 shared publicationBarbara Cerboni
Department of Molecular Biology, University of Siena, Italy
1 shared publicationCarlo Alessandrini
** Department of Biomedical Sciences, University of Siena, Italy
1 shared publicationG. Jacomelli
1 shared publicationG. Pompucci
1 shared publicationLaura Notarantonio
Department of Molecular Biology, University of Siena, Italy
1 shared publication
Latest Publications
- Open Access
- 11 October 2006
- Published by Oxford University Press (OUP) in European Journal of Orthodontics
- Vol. 28 (6) , 567-572
In vitro toxicity evaluation of silver soldering, electrical resistance, and laser welding of orthodontic wires
The long-term effects of orthodontic appliances in the oral environment and the subsequent leaching of metals are relatively unknown. A method for determining the effects of various types of soldering and welding, both of which in turn could lead to leaching of metal ions, on the growth of osteoblasts, fibroblasts, and oral keratinocytes in vitro, is proposed. The effects of cell behaviour of metal wires on osteoblast differentiation, expressed by alkaline phosphatase (ALP) activity; on fibroblast proliferation, assayed by the 3-(4,5-dimethylthiazol-2-yl)-5-(3-carboxymethoxyphenyl)-2-(4-sulphophenil)-2H-tetrazolium–phenazine ethosulphate method; and on keratinocyte viability and migration on the wires, observed by scanning electron microscopy (SEM), were tested. Two types of commercially available wires normally used for orthodontic appliances, with a similar chemical composition (iron, carbon, silicon, chromium, molybdenum, phosphorus, sulphur, vanadium, and nitrogen) but differing in nickel and manganese content, were examined, as well as the joints obtained by electrical resistance welding, traditional soldering, and laser welding. Nickel and chromium, known as possible toxic metals, were also examined using pure nickel- and chromium-plated titanium wires. Segments of each wire, cut into different lengths, were added to each well in which the cells were grown to confluence. The high nickel and chromium content of orthodontic wires damaged both osteoblasts and fibroblasts, but did not affect keratinocytes. Chromium strongly affected fibroblast growth. The joint produced by electrical resistance welding was well tolerated by both osteoblasts and fibroblasts, whereas traditional soldering caused a significant (P < 0.05) decrease in both osteoblast ALP activity and fibroblast viability, and prevented the growth of keratinocytes in vitro. Laser welding was the only joining process well tolerated by all tested cells.
- 11 October 2006
- Published by Oxford University Press (OUP) in European Journal of Orthodontics
- Vol. 28 (6) , 567-572
Open AccessIn vitro toxicity evaluation of silver soldering, electrical resistance, and laser welding of orthodontic wires
The long-term effects of orthodontic appliances in the oral environment and the subsequent leaching of metals are relatively unknown. A method for determining the effects of various types of soldering and welding, both of which in turn could lead to leaching of metal ions, on the growth of osteoblasts, fibroblasts, and oral keratinocytes in vitro, is proposed. The effects of cell behaviour of metal wires on osteoblast differentiation, expressed by alkaline phosphatase (ALP) activity; on fibroblast proliferation, assayed by the 3-(4,5-dimethylthiazol-2-yl)-5-(3-carboxymethoxyphenyl)-2-(4-sulphophenil)-2H-tetrazolium–phenazine ethosulphate method; and on keratinocyte viability and migration on the wires, observed by scanning electron microscopy (SEM), were tested. Two types of commercially available wires normally used for orthodontic appliances, with a similar chemical composition (iron, carbon, silicon, chromium, molybdenum, phosphorus, sulphur, vanadium, and nitrogen) but differing in nickel and manganese content, were examined, as well as the joints obtained by electrical resistance welding, traditional soldering, and laser welding. Nickel and chromium, known as possible toxic metals, were also examined using pure nickel- and chromium-plated titanium wires. Segments of each wire, cut into different lengths, were added to each well in which the cells were grown to confluence. The high nickel and chromium content of orthodontic wires damaged both osteoblasts and fibroblasts, but did not affect keratinocytes. Chromium strongly affected fibroblast growth. The joint produced by electrical resistance welding was well tolerated by both osteoblasts and fibroblasts, whereas traditional soldering caused a significant (P < 0.05) decrease in both osteoblast ALP activity and fibroblast viability, and prevented the growth of keratinocytes in vitro. Laser welding was the only joining process well tolerated by all tested cells.
- 1 July 2000
- Published by Elsevier in Archives of Biochemistry and Biophysics
- Vol. 379 (2) , 277-282
Enzyme Activities Leading to NAD Synthesis in Human Lymphocytes
- 1 July 2000
- Published by Elsevier in Archives of Biochemistry and Biophysics
- Vol. 379 (2) , 277-282
Enzyme Activities Leading to NAD Synthesis in Human Lymphocytes