D. J. Sellmyer
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
D. J. Sellmyer has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
- M. L. Yan
Center for Materials Research and Analysis and Department of Physics and Astronomy, University of Nebraska, Lincoln, Nebraska 68588-0113
5 shared publications Z. S. Shan
Komag Inc., 1710 Automation Parkway, San Jose, California 95131
3 shared publicationsN. Powers
Department of Physics and Astronomy and Center for Materials Research and Analysis, University of Nebraska, Lincoln, Nebraska 68588-0113
2 shared publications- Sy-Hwang Liou
Department of Physics and Astronomy, University of Nebraska-Lincoln, Lincoln, NE, USA
2 shared publications B. Bian
Komag Inc., 1710 Automation Parkway, San Jose, California 95131
1 shared publicationC. P. Reed
Center for Materials Research and Analysis, University of Nebraska-Lincoln, Lincoln, Nebraska 68588-0111
1 shared publication
Latest Publications
- 15 May 2003
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 93 (10) , 7768-7770
Studies of magnetic properties of the stabilizing layer for synthetic antiferromagnetically coupled media
The effects of the stabilizing layer thickness and its temperature dependence on the magnetic properties were investigated experimentally. These results were used to analyze the magnetic structure of the thin stabilizing layer and its effect on the coupling strength, which is valuable for improving the design of synthetic antiferromagnetically coupled media.
- 15 May 2003
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 93 (10) , 7768-7770
Studies of magnetic properties of the stabilizing layer for synthetic antiferromagnetically coupled media
The effects of the stabilizing layer thickness and its temperature dependence on the magnetic properties were investigated experimentally. These results were used to analyze the magnetic structure of the thin stabilizing layer and its effect on the coupling strength, which is valuable for improving the design of synthetic antiferromagnetically coupled media.
- 15 May 2003
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 93 (10) , 8152-8154
Effects of rapid thermal annealing on nanostructure, texture and magnetic properties of granular FePt:Ag films for perpendicular recording (invited)
We report effects of rapid thermal annealing on nanostructure, texture, and magnetic properties of granular FePt:Ag films. It was found that the orientations of FePt grains were dependent strongly on the as-deposited multilayer structure and the annealing processes. Through the control of the annealing processes, (001) textured granular FePt:Ag films were obtained. Magnetic measurements revealed that saturation magnetization perpendicular coercivity and remanence ratio were also dependent on the annealing temperature, annealing time and Ag content. Perpendicular values increased from 1.5 to 15 kOe when the annealing temperature changed from 400 to 600 °C for 600 s. Perpendicular values remained about 11 kOe when the annealing time changed from 5 to 600 s. The effect of Ag content on magnetic properties is reported.- 15 May 2003
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 93 (10) , 8152-8154
Effects of rapid thermal annealing on nanostructure, texture and magnetic properties of granular FePt:Ag films for perpendicular recording (invited)
We report effects of rapid thermal annealing on nanostructure, texture, and magnetic properties of granular FePt:Ag films. It was found that the orientations of FePt grains were dependent strongly on the as-deposited multilayer structure and the annealing processes. Through the control of the annealing processes, (001) textured granular FePt:Ag films were obtained. Magnetic measurements revealed that saturation magnetization perpendicular coercivity and remanence ratio were also dependent on the annealing temperature, annealing time and Ag content. Perpendicular values increased from 1.5 to 15 kOe when the annealing temperature changed from 400 to 600 °C for 600 s. Perpendicular values remained about 11 kOe when the annealing time changed from 5 to 600 s. The effect of Ag content on magnetic properties is reported.- 13 May 2002
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 91 (10) , 8641-8643
Magnetic intergranular interaction in nanocomposite CoxPt100−x:C thin films
Magnetization reversal and intergranular interactions have been studied in composite thin films using several magnetic characterization techniques. The intergranular interactions, as determined by curves, were strongly dependent on the ratio of Co and Pt concentration. For films with high Co content, the intergranular exchange coupling was predominant, while dipolar interactions were exhibited in the film with the equiatomic concentration of Co and Pt. Magnetic intergranular interaction was directly observed using magnetic force microscopy. There is a strong correlation between the value of the and magnetic correlation length obtained from the magnetic domain images.- 13 May 2002
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 91 (10) , 8641-8643
Magnetic intergranular interaction in nanocomposite CoxPt100−x:C thin films
Magnetization reversal and intergranular interactions have been studied in composite thin films using several magnetic characterization techniques. The intergranular interactions, as determined by curves, were strongly dependent on the ratio of Co and Pt concentration. For films with high Co content, the intergranular exchange coupling was predominant, while dipolar interactions were exhibited in the film with the equiatomic concentration of Co and Pt. Magnetic intergranular interaction was directly observed using magnetic force microscopy. There is a strong correlation between the value of the and magnetic correlation length obtained from the magnetic domain images.- 1 January 2002
- Published by Springer Nature in MRS Proceedings
- Vol. 721
Non-epitaxial, Highly Textured (001) CoPt:B2O3 Composite Films for Perpendicular Recording
- 1 January 2002
- Published by Springer Nature in MRS Proceedings
- Vol. 721
Non-epitaxial, Highly Textured (001) CoPt:B2O3 Composite Films for Perpendicular Recording
- 15 April 1997
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 81 (8) , 4785-4787
Interlayer coupling in NiFe/Mo multilayers and effect of Fe underlayer
We report our studies of exchange coupling in NiFe/Mo multilayers with and without Fe underlayer. The interlayer coupling of NiFe layers across the Mo spacer as well as the magnetic exchange coupling between Fe underlayer and the NiFe/Mo multilayers were observed: The interlayer coupling in NiFe/Mo multilayers exhibits the typical oscillations as a function of the Mo spacer with a period of about 11 Å, and the magnetic exchange coupling between Fe underlayer and the NiFe/Mo multilayers is strongly dependent on the thickness of the Mo spacer t Mo and the bilayer number N of NiFe/Mo multilayers. For the [ NiFe(20 Å)/Mo (t Mo )] 30 samples with a 100 Å Fe underlayer, the hysteresis loops with thinner Mo spacer ( t Mo <4 Å) are single loops indicating that the Fe underlayer is strongly magnetic exchange coupled with the NiFe/Mo multilayers; whereas hysteresis loops with thicker Mo spacer ( t Mo ⩾5 Å) show a two-magnetic-phase feature. For the [ NiFe(20 Å)/Mo(10 Å)] 30 sample with 100 Å Fe underlayer, the hysteresis loops are single loops for bilayer number N<15 , while hysteresis loops show the two-phase feature for N⩾15 .
- 15 April 1997
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 81 (8) , 4785-4787
Interlayer coupling in NiFe/Mo multilayers and effect of Fe underlayer
We report our studies of exchange coupling in NiFe/Mo multilayers with and without Fe underlayer. The interlayer coupling of NiFe layers across the Mo spacer as well as the magnetic exchange coupling between Fe underlayer and the NiFe/Mo multilayers were observed: The interlayer coupling in NiFe/Mo multilayers exhibits the typical oscillations as a function of the Mo spacer with a period of about 11 Å, and the magnetic exchange coupling between Fe underlayer and the NiFe/Mo multilayers is strongly dependent on the thickness of the Mo spacer t Mo and the bilayer number N of NiFe/Mo multilayers. For the [ NiFe(20 Å)/Mo (t Mo )] 30 samples with a 100 Å Fe underlayer, the hysteresis loops with thinner Mo spacer ( t Mo <4 Å) are single loops indicating that the Fe underlayer is strongly magnetic exchange coupled with the NiFe/Mo multilayers; whereas hysteresis loops with thicker Mo spacer ( t Mo ⩾5 Å) show a two-magnetic-phase feature. For the [ NiFe(20 Å)/Mo(10 Å)] 30 sample with 100 Å Fe underlayer, the hysteresis loops are single loops for bilayer number N<15 , while hysteresis loops show the two-phase feature for N⩾15 .
- 15 November 1991
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 70 (10) , 5882-5884
The process-controlled magnetic properties of nanostructured Co/Ag composite films
Nanostructured Co/Ag composite films were prepared by magnetron sputtering using a single target. The average crystallite sizes of Co and Ag in the films depend on the deposition conditions. As the substrate temperature increases from 100 °C to 600 °C, the average Ag crystallite size increases from 39 to 452 Å, and the average Co crystallite size increases from <30 to 297 Å in the film with 39 vol. % of Co. The films with 39 vol. % of Co and prepared at 400 °C substrate temperature showed a maximum magnetic coercivity of 565 Oe at 6 K. We have studied the correlation between the structure and magnetic properties of these films.
- 15 November 1991
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 70 (10) , 5882-5884
The process-controlled magnetic properties of nanostructured Co/Ag composite films
Nanostructured Co/Ag composite films were prepared by magnetron sputtering using a single target. The average crystallite sizes of Co and Ag in the films depend on the deposition conditions. As the substrate temperature increases from 100 °C to 600 °C, the average Ag crystallite size increases from 39 to 452 Å, and the average Co crystallite size increases from <30 to 297 Å in the film with 39 vol. % of Co. The films with 39 vol. % of Co and prepared at 400 °C substrate temperature showed a maximum magnetic coercivity of 565 Oe at 6 K. We have studied the correlation between the structure and magnetic properties of these films.