Hideki Yamane
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Hideki Yamane has a total of 66 co-authors. Here are the top co-authors by number of shared publications:
- Huaizhong Xu
Department of Biobased Materials Science Kyoto Institute of Technology Kyoto Japan
5 shared publications Masaki Yamamoto
Textile Research Institute of Gunma, Gunma 376-0011, Japan
4 shared publicationsJae-Chang Lee
Korea Research Institute of Chemical Technology
3 shared publicationsShinichi Sakurai
Department of Biobased Materials Science, Kyoto Institute of Technology, Matsugasaki, Sakyo-Ku, Kyoto 606-8585, Japan; Department of Chemical Engineering, Indian Institute of Technology Guwahati (IITG), Guwahati, Assam 781039, India
3 shared publications- Hitomi Ohara
Department of Biobased Materials Science, Kyoto Institute of Technology, Kyoto, Japan
2 shared publications Huaizhong Xu
Dept. of Biobased Materials Science, Kyoto Institute of Technology, Kyoto 606-8585, Japan
2 shared publications
Latest Publications
- 3 August 2022
- Published by Wiley in Polymers for Advanced Technologies
- Vol. 33 (10) , 3658-3665
Melt spinning of polyamide 4
Polyamide 4 (PA 4), a biobased and biodegradable polymer, is firstly produced into fibers by melt spinning. PA 4 is a thermally‐sensitive polymer that is difficult to be processed by melting methods, while through mixing with an ionic liquid (IL)—1‐butyl‐3‐methylimidazolium chloride (BmimCl), the melting point of the PA 4 decreases 40°C when 30 wt% ILs are incorporated. Homogeneous and circular cross‐sectional PA 4 fibers are produced at winding speeds of 19, 79, 228 and 396 m/min. The as‐spun PA 4 fibers produced at 19 m/min winding speed can maximally be drawn four times in a water bath with temperatures ranging 60–75°C. The mechanical properties of the PA 4 fiber reach an optimum value as the fiber is drawn at 65°C. The ILs are fully removed when the fibers immerse in water for 3 min. In the meanwhile, the melting point of PA 4 is gradually enhanced with washing. Moreover, the crystallization of the washed PA 4 fibers increases, while the orientation of the crystals slightly decreases. The application of IL can be extended to improve the processibility of thermally‐sensitive polymers that cannot be directly manufactured by melt‐extrusion based technologies.
- 3 August 2022
- Published by Wiley in Polymers for Advanced Technologies
- Vol. 33 (10) , 3658-3665
Melt spinning of polyamide 4
Polyamide 4 (PA 4), a biobased and biodegradable polymer, is firstly produced into fibers by melt spinning. PA 4 is a thermally‐sensitive polymer that is difficult to be processed by melting methods, while through mixing with an ionic liquid (IL)—1‐butyl‐3‐methylimidazolium chloride (BmimCl), the melting point of the PA 4 decreases 40°C when 30 wt% ILs are incorporated. Homogeneous and circular cross‐sectional PA 4 fibers are produced at winding speeds of 19, 79, 228 and 396 m/min. The as‐spun PA 4 fibers produced at 19 m/min winding speed can maximally be drawn four times in a water bath with temperatures ranging 60–75°C. The mechanical properties of the PA 4 fiber reach an optimum value as the fiber is drawn at 65°C. The ILs are fully removed when the fibers immerse in water for 3 min. In the meanwhile, the melting point of PA 4 is gradually enhanced with washing. Moreover, the crystallization of the washed PA 4 fibers increases, while the orientation of the crystals slightly decreases. The application of IL can be extended to improve the processibility of thermally‐sensitive polymers that cannot be directly manufactured by melt‐extrusion based technologies.
- 31 January 2022
- Published by Elsevier in Materials Science and Engineering: C
- Vol. 135, 112686
Enhancing the bioactivity of melt electrowritten PLLA scaffold by convenient, green, and effective hydrophilic surface modification
- 31 January 2022
- Published by Elsevier in Materials Science and Engineering: C
- Vol. 135, 112686
Enhancing the bioactivity of melt electrowritten PLLA scaffold by convenient, green, and effective hydrophilic surface modification
- Open Access
Fabrication and Properties of Electrospun Collagen Tubular Scaffold Crosslinked by Physical and Chemical Treatments
Tissue engineered scaffold was regarded as a promising approach instead of the autograft. In this study, small diameter electrospun collagen tubular scaffold with random continuous smooth nanofibers was successfully fabricated. However, the dissolution of collagen in concentrated aqueous (conc. aq.) acetic acid caused to the serious denaturation of collagen. A novel method ammonia treatment here was adopted which recovered the collagen triple helix structure according to the analysis of IR spectra. Further dehydrothermal (DHT) and glutaraldehyde (GTA) treatments were applied to introduce the crosslinks to improve the properties of collagen tube. The nanofibrous structure of collagen tube in a wet state was preserved by the crosslinking treatments. Swelling ratio and weight loss decreased by at least two times compared to those of the untreated collagen tube. Moreover, tensile strength was significantly enhanced by DHT treatment (about 0.0076 cN/dTex) and by GTA treatment (about 0.075 cN/dTex). In addition, the surface of crosslinked collagen tube kept the hydrophilic property. These results suggest that DHT and GTA treatments can be utilized to improve the properties of electrospun collagen tube which could become a suitable candidate for tissue engineered scaffold.
Open AccessFabrication and Properties of Electrospun Collagen Tubular Scaffold Crosslinked by Physical and Chemical Treatments
Tissue engineered scaffold was regarded as a promising approach instead of the autograft. In this study, small diameter electrospun collagen tubular scaffold with random continuous smooth nanofibers was successfully fabricated. However, the dissolution of collagen in concentrated aqueous (conc. aq.) acetic acid caused to the serious denaturation of collagen. A novel method ammonia treatment here was adopted which recovered the collagen triple helix structure according to the analysis of IR spectra. Further dehydrothermal (DHT) and glutaraldehyde (GTA) treatments were applied to introduce the crosslinks to improve the properties of collagen tube. The nanofibrous structure of collagen tube in a wet state was preserved by the crosslinking treatments. Swelling ratio and weight loss decreased by at least two times compared to those of the untreated collagen tube. Moreover, tensile strength was significantly enhanced by DHT treatment (about 0.0076 cN/dTex) and by GTA treatment (about 0.075 cN/dTex). In addition, the surface of crosslinked collagen tube kept the hydrophilic property. These results suggest that DHT and GTA treatments can be utilized to improve the properties of electrospun collagen tube which could become a suitable candidate for tissue engineered scaffold.
- Open Access
Effect of the Application of a Dehydrothermal Treatment on the Structure and the Mechanical Properties of Collagen Film
Dehydrothermal (DHT) treatment was used to improve the properties of collagen casings because of its non-cytotoxicity. Understanding the effects of DHT treatment on the structure and mechanical properties of collagen films is beneficial to developing satisfying collagen casings. Herein, DHT treatment with various temperatures (85–145 °C) and timescales (1–7 days) were investigated. It was clarified that the chemical crosslinking covalent bond between collagen molecules was formed after the DHT treatment. Crosslinking density increased with increasing DHT treatment temperatures, contributing to the increase of tensile strength up to over three times of that of the untreated collagen film. The increased crosslinking density was also found when increasing the DHT treatment time, and the maximum was obtained in 3 days. Further DHT treatment time did not change the crosslinking density. The damage in the triple helix structure and the self-assembly of collagen molecules were observed from IR and SAXS. The extent of denaturation increased with increasing DHT treatment temperature and time, although the effect of the DHT treatment time on the denaturation was more moderate. When the DHT treatment temperature was as high as 145 °C or the DHT treatment time exceeded 5 days, serious denaturation occurs, leading to the deterioration of mechanical properties.
Open AccessEffect of the Application of a Dehydrothermal Treatment on the Structure and the Mechanical Properties of Collagen Film
Dehydrothermal (DHT) treatment was used to improve the properties of collagen casings because of its non-cytotoxicity. Understanding the effects of DHT treatment on the structure and mechanical properties of collagen films is beneficial to developing satisfying collagen casings. Herein, DHT treatment with various temperatures (85–145 °C) and timescales (1–7 days) were investigated. It was clarified that the chemical crosslinking covalent bond between collagen molecules was formed after the DHT treatment. Crosslinking density increased with increasing DHT treatment temperatures, contributing to the increase of tensile strength up to over three times of that of the untreated collagen film. The increased crosslinking density was also found when increasing the DHT treatment time, and the maximum was obtained in 3 days. Further DHT treatment time did not change the crosslinking density. The damage in the triple helix structure and the self-assembly of collagen molecules were observed from IR and SAXS. The extent of denaturation increased with increasing DHT treatment temperature and time, although the effect of the DHT treatment time on the denaturation was more moderate. When the DHT treatment temperature was as high as 145 °C or the DHT treatment time exceeded 5 days, serious denaturation occurs, leading to the deterioration of mechanical properties.
- 1 January 2019
- Published by Japan Society of Mechanical Engineers in The Proceedings of Mechanical Engineering Congress, Japan
- Vol. 2019, J24104
Research and development of uterine cervical cell harvestion brush using braid and modified cross section fiber
Cervical cell harvesting instruments used in cervical cancer screening mainly there are swabs and brushes. The examination using these is almost pain-free in a short period of time, it has advantages such as early detection and treatment being possible. But, the accuracy of cell harvest is about 50-70%, not necessarily high, there are demerits such as few re-examination due to errors, too. In this study, we can reduce re-examination due to error at the time of cell harvesting ② High harvest precision can be stabilized ③ Fiber structure that can absorb a much larger number of harvested cells than current commercial brush. Research and development of a new cervical cell harvesting instrument having such multifunctionality it is aiming. We are aiming at the research and development of a new cervical cell harvesting instrument having such multifunctionality. Then, a cell harvesting brush using the braiding technique was prototyped, and the amount of adsorption was measured using a uterus model of the same size as the actual one. We compared them with commercial brushes and examined its usefulness.
- 1 January 2019
- Published by Japan Society of Mechanical Engineers in The Proceedings of Mechanical Engineering Congress, Japan
- Vol. 2019, J24104
Research and development of uterine cervical cell harvestion brush using braid and modified cross section fiber
Cervical cell harvesting instruments used in cervical cancer screening mainly there are swabs and brushes. The examination using these is almost pain-free in a short period of time, it has advantages such as early detection and treatment being possible. But, the accuracy of cell harvest is about 50-70%, not necessarily high, there are demerits such as few re-examination due to errors, too. In this study, we can reduce re-examination due to error at the time of cell harvesting ② High harvest precision can be stabilized ③ Fiber structure that can absorb a much larger number of harvested cells than current commercial brush. Research and development of a new cervical cell harvesting instrument having such multifunctionality it is aiming. We are aiming at the research and development of a new cervical cell harvesting instrument having such multifunctionality. Then, a cell harvesting brush using the braiding technique was prototyped, and the amount of adsorption was measured using a uterus model of the same size as the actual one. We compared them with commercial brushes and examined its usefulness.
- 1 December 2018
- Published by Elsevier in Carbohydrate Polymers
- Vol. 201, 182-188
Regeneration of cellulose dissolved in ionic liquid using laser-heated melt-electrospinning
- 1 December 2018
- Published by Elsevier in Carbohydrate Polymers
- Vol. 201, 182-188
Regeneration of cellulose dissolved in ionic liquid using laser-heated melt-electrospinning
- 31 May 2018
- Published by SAGE Publications in Textile Research Journal
- Vol. 89 (9) , 1770-1781
Structure and properties of poly(3-hydroxybutyrate-co-3-hydroxyhexanoate)/poly(L-lactic acid) quasi core/sheath melt-electrospun microfibers
A facile route was proposed to fabricate core–sheath microfibers, and the relationships among processing parameters, crystalline structures and the mechanical properties were investigated. The compression molded poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) (PHBH)/poly(L-lactic acid) (PLLA) strip enhanced the spinnability of PHBH and the mechanical properties of PLLA as well. The core–sheath ratio of the fibers was determined by the prefab strip, while the PLLA sheath component did not completely cover the PHBH core component due to the weak interfacial tension between the melts of PHBH and PLLA. A rotational target was applied to collect aligned fibers, which were further drawn in a water bath. The tensile strength and the modulus of as-spun and drawn fibers increased with increasing the take-up velocities. When the take-up velocity was above 500 m/min, the jet became unstable and started to break up at the tip of the Taylor cone, decreasing the mechanical properties of the fibers. The drawing process facilitated the crystallization of PLLA and PHBH, and the tensile strength and the modulus increased linearly with the increasing the draw ratio. The crystal information displayed from wide-angle X-ray diffraction patterns and differential scanning calorimetry heating curves supported the results of the tensile tests.
- 31 May 2018
- Published by SAGE Publications in Textile Research Journal
- Vol. 89 (9) , 1770-1781
Structure and properties of poly(3-hydroxybutyrate-co-3-hydroxyhexanoate)/poly(L-lactic acid) quasi core/sheath melt-electrospun microfibers
A facile route was proposed to fabricate core–sheath microfibers, and the relationships among processing parameters, crystalline structures and the mechanical properties were investigated. The compression molded poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) (PHBH)/poly(L-lactic acid) (PLLA) strip enhanced the spinnability of PHBH and the mechanical properties of PLLA as well. The core–sheath ratio of the fibers was determined by the prefab strip, while the PLLA sheath component did not completely cover the PHBH core component due to the weak interfacial tension between the melts of PHBH and PLLA. A rotational target was applied to collect aligned fibers, which were further drawn in a water bath. The tensile strength and the modulus of as-spun and drawn fibers increased with increasing the take-up velocities. When the take-up velocity was above 500 m/min, the jet became unstable and started to break up at the tip of the Taylor cone, decreasing the mechanical properties of the fibers. The drawing process facilitated the crystallization of PLLA and PHBH, and the tensile strength and the modulus increased linearly with the increasing the draw ratio. The crystal information displayed from wide-angle X-ray diffraction patterns and differential scanning calorimetry heating curves supported the results of the tensile tests.
- 1 August 2017
- Published by Elsevier in Polymer Degradation and Stability
- Vol. 142, 188-197
Thermal properties of the multi-stereo block poly(lactic acid)s with various block lengths
- 1 August 2017
- Published by Elsevier in Polymer Degradation and Stability
- Vol. 142, 188-197
Thermal properties of the multi-stereo block poly(lactic acid)s with various block lengths
- 16 July 2017
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 134 (44)
Effect of the melt‐mixing condition on the physical property of poly(l‐lactic acid)/poly(d‐lactic acid) blends
The effect of the mixing condition in a mill‐type mixer on the thermal property and the crystal formation of the poly(l‐lactide)/poly(d‐lactide) blends is investigated. The blends melt‐mixed at 200 and 210 °C under application of a high shear flow tend to show a single melting peak of the stereocomplex crystal (SC) in the differential scanning calorimetry first and second heating processes without indicating the trace of the melting of homo‐chiral crystal. The mixing at an elevated temperature causes a serious thermal degradation. Further kneading of the blends at an elevated temperature higher than Tm of SC causes the transesterification between the same enatiomeric chains forming block copolymers of l‐ and d‐chains. This block copolymer acts as a nucleating agent of SC and the compatibilizing agent between poly(l‐lactide) and poly(d‐lactide) and promotes the formation of SC. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2017, 134, 45489.
- 16 July 2017
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 134 (44)
Effect of the melt‐mixing condition on the physical property of poly(l‐lactic acid)/poly(d‐lactic acid) blends
The effect of the mixing condition in a mill‐type mixer on the thermal property and the crystal formation of the poly(l‐lactide)/poly(d‐lactide) blends is investigated. The blends melt‐mixed at 200 and 210 °C under application of a high shear flow tend to show a single melting peak of the stereocomplex crystal (SC) in the differential scanning calorimetry first and second heating processes without indicating the trace of the melting of homo‐chiral crystal. The mixing at an elevated temperature causes a serious thermal degradation. Further kneading of the blends at an elevated temperature higher than Tm of SC causes the transesterification between the same enatiomeric chains forming block copolymers of l‐ and d‐chains. This block copolymer acts as a nucleating agent of SC and the compatibilizing agent between poly(l‐lactide) and poly(d‐lactide) and promotes the formation of SC. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2017, 134, 45489.