Hitoshi Morioka
Research Subjects
Hitoshi Morioka has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
- Hiroshi Funakubo
Institute of Science Tokyo
4 shared publications - Keisuke Saito
Application Laboratory, Analytical Department, Philips Japan, Limited, 35-1, Sagamiono 7-chome, Sagamihara-shi 223-0803, Japan
3 shared publications - Shintaro Yokoyama
Tokyo Institute of Technology, Department of Innovative and Engineered Materials, Japan
3 shared publications - Mitsumasa Nakajima
Department of Innovative and Engineered Materials, Tokyo Institute of Technology, Yokohama, Kanagawa 226-8502, JAPAN
2 shared publications - Mutsuo Ishikawa
Depertment of Clinical Engineering, Faculty of Biomedical Engineering, Toin University of Yokohama (1614 Kurogane-cho, Aoba-ku, Yokohama, Kanagawa, 225-8503 JAPAN), Japan
2 shared publications Takahiro Oikawa
Department of Innovative and Engineered Materials, Tokyo Institute of Technology, Yokohama, Kanagawa 226-8502, JAPAN
2 shared publications
Latest Publications
- 15 February 2013
- Published by Springer Nature in MRS Proceedings
- Vol. 1507
Crystal Structure Change with Applied Electric Field for (100)/(001)-oriented Polycrystalline Lead Zirconate Titanate Films
- 15 February 2013
- Published by Springer Nature in MRS Proceedings
- Vol. 1507
Crystal Structure Change with Applied Electric Field for (100)/(001)-oriented Polycrystalline Lead Zirconate Titanate Films
- 28 October 2009
- Published by Taylor & Francis in Ferroelectrics
- Vol. 389 (1) , 10-17
Composition Dependency of Epitaxial Pb(Zr,Ti)O3Films with Different Film Thickness
Epitaxial Pb(ZrxTi1 - x)O3 films with 200 nm and 2 μm thickness were grown by metal organic chemical vapor deposition. Crystal symmetry changed from tetragonal to rhombohedral with increasing x value in Pb(ZrxTi1 - x)O3 [x = Zr/(Zr+Ti)] for both film thickness and a region for the co-existence of the mixture of tetragonal and rhombohedral exists around x = 0.5, becoming a little wider with increasing film thickness. Saturation and remanent polarizations (P sat and P r ) showed a minimum near x = 0.5 irrespective of the film thickness. The P r /P sat ratio also showed a minimum in case of 200 nm thick films, but such a minimum in P r /P sat was not observed in case of 2 μm thickness. Relative dielectric constant showed a maximum near x = 0.5 for both film thickness, but the effective longitudinal piezoelectric constant did not show any noticeable maximum near x = 0.5 irrespective of the film thickness, differently from the reported data for the sintered body.
- 28 October 2009
- Published by Taylor & Francis in Ferroelectrics
- Vol. 389 (1) , 10-17
Composition Dependency of Epitaxial Pb(Zr,Ti)O3Films with Different Film Thickness
Epitaxial Pb(ZrxTi1 - x)O3 films with 200 nm and 2 μm thickness were grown by metal organic chemical vapor deposition. Crystal symmetry changed from tetragonal to rhombohedral with increasing x value in Pb(ZrxTi1 - x)O3 [x = Zr/(Zr+Ti)] for both film thickness and a region for the co-existence of the mixture of tetragonal and rhombohedral exists around x = 0.5, becoming a little wider with increasing film thickness. Saturation and remanent polarizations (P sat and P r ) showed a minimum near x = 0.5 irrespective of the film thickness. The P r /P sat ratio also showed a minimum in case of 200 nm thick films, but such a minimum in P r /P sat was not observed in case of 2 μm thickness. Relative dielectric constant showed a maximum near x = 0.5 for both film thickness, but the effective longitudinal piezoelectric constant did not show any noticeable maximum near x = 0.5 irrespective of the film thickness, differently from the reported data for the sintered body.
- 1 January 2005
- Published by Springer Nature in MRS Proceedings
- Vol. 902
Observation of Domain Switching in Fatigued Epitaxial Pb(Zr,Ti)O3 Thin Films
- 1 January 2005
- Published by Springer Nature in MRS Proceedings
- Vol. 902
Observation of Domain Switching in Fatigued Epitaxial Pb(Zr,Ti)O3 Thin Films
- 22 September 2003
- Published by AIP Publishing in Applied Physics Letters
- Vol. 83 (12) , 2408-2410
Large piezoelectric response in (111)-oriented epitaxial Pb(Zr,Ti)O3 films consisting of mixed phases with rhombohedral and tetragonal symmetry
films with a ratio of 0.48 having 1.5 μm in thickness were grown on -, -, and -oriented substrates by metalorganic chemical vapor deposition. It was ascertained by θ–2θ scans of x-ray diffraction that -, {110}-, and {111}-oriented films were epitaxially grown on -, -, and -oriented substrates. Polarization and field-induced strain in these films were simultaneously observed through a scanning probe microscope that was attached to a ferroelectric test system. About three times larger field-induced strain than that on other substrates was observed together with the largest spontaneous polarization for a film grown on a substrate. High-resolution x-ray diffraction analysis suggested that the film grown on the substrate consisted of rhombohedral and tetragonal mixture phases. Its crystal structure possibly contributed to the large piezoelectric response.- 22 September 2003
- Published by AIP Publishing in Applied Physics Letters
- Vol. 83 (12) , 2408-2410
Large piezoelectric response in (111)-oriented epitaxial Pb(Zr,Ti)O3 films consisting of mixed phases with rhombohedral and tetragonal symmetry
films with a ratio of 0.48 having 1.5 μm in thickness were grown on -, -, and -oriented substrates by metalorganic chemical vapor deposition. It was ascertained by θ–2θ scans of x-ray diffraction that -, {110}-, and {111}-oriented films were epitaxially grown on -, -, and -oriented substrates. Polarization and field-induced strain in these films were simultaneously observed through a scanning probe microscope that was attached to a ferroelectric test system. About three times larger field-induced strain than that on other substrates was observed together with the largest spontaneous polarization for a film grown on a substrate. High-resolution x-ray diffraction analysis suggested that the film grown on the substrate consisted of rhombohedral and tetragonal mixture phases. Its crystal structure possibly contributed to the large piezoelectric response.