Eduardo Perez Tijerina
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Eduardo Perez Tijerina has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Alan Castillo Roderiguez
UANL, FIME, san Nicolas de Los garza, Mexico
1 shared publication - Ana Maria Arato Tovar
Facultad de Ingeniería Mecánica y Eléctrica (FIME), Universidad Autónoma de Nuevo León (UANL), 66450 San Nicolás de los Garza, N.L., México
1 shared publication - Bindu Krishnan
Facultad de Ingeniería Mecánica y Eléctrica, Universidad Autónoma de Nuevo León. San Nicolás de los Garza, Nuevo León, 66455, Méxicohttps://ror.org/01fh86n78https://www.isni.org/isni
1 shared publication - Joaquín Bohigas
Instituto de Astronomía, Universidad Nacional Autónoma de México, Km. 103 Carretera Tijuana-Ensenada, 22860 Ensenada, Baja California, Mexico
1 shared publication Jorge G. Garza
UANL, FIME, san Nicolas de Los garza, Mexico
1 shared publication- Roberto Machorro
Centro de Ciencias de la Materia Condensada-UNAM, Apdo. Postal 2681, Ensenada, B.C., 22800, México
1 shared publication
Latest Publications
- 1 January 2009
- Published by Springer Nature in MRS Proceedings
- Vol. 1165
Chemically Deposited Silver Antimony Selenide Thin Films for Photovoltaic Applications
Silver antimony selenide (AgSbSe2) thin films were prepared by heating sequentially deposited antimony sulphide (Sb2S3), silver selenide (Ag2Se) and Ag thin films in close contact with a selenium thin film. Sb2S3 thin film was prepared from chemical bath containing SbCl3 and Na2S2O3, Ag2Se from the bath containing AgNO3 and Na2SeSO3 and Se thin films from an acidified solution of Na2SeSO3, at room temperature on cleaned glass substrates. Ag thin film was deposited by vacuum thermal evaporation. The annealing temperature was varied from 300-390°C in vacuum (∼10−3 Torr) for 1 h. X-ray diffraction analysis showed the films formed at 350 °C was polycrystalline AgSb(S,Se)2 or AgSbSe2 depending on selenium thin film thickness. Morphology of these films was analyzed using Atomic Force Microscopy and Scanning Electron Microscopy. The elemental analysis was done using Energy Dispersive X-ray technique. Optical characterization of the thin films was done by optical transmittance spectra. The electrical characterizations were done using Hall effect and photocurrent measurements. A photovoltaic structure: Glass/ITO/CdS/AgSbSe2/Ag was formed, in which CdS was deposited by chemical bath deposition. J-V characteristics of this PV structure showed Voc=370 mV and Jsc=0.5 mA/cm2 under illumination using a tungsten halogen lamp.
- 1 January 2009
- Published by Springer Nature in MRS Proceedings
- Vol. 1165
Chemically Deposited Silver Antimony Selenide Thin Films for Photovoltaic Applications
Silver antimony selenide (AgSbSe2) thin films were prepared by heating sequentially deposited antimony sulphide (Sb2S3), silver selenide (Ag2Se) and Ag thin films in close contact with a selenium thin film. Sb2S3 thin film was prepared from chemical bath containing SbCl3 and Na2S2O3, Ag2Se from the bath containing AgNO3 and Na2SeSO3 and Se thin films from an acidified solution of Na2SeSO3, at room temperature on cleaned glass substrates. Ag thin film was deposited by vacuum thermal evaporation. The annealing temperature was varied from 300-390°C in vacuum (∼10−3 Torr) for 1 h. X-ray diffraction analysis showed the films formed at 350 °C was polycrystalline AgSb(S,Se)2 or AgSbSe2 depending on selenium thin film thickness. Morphology of these films was analyzed using Atomic Force Microscopy and Scanning Electron Microscopy. The elemental analysis was done using Energy Dispersive X-ray technique. Optical characterization of the thin films was done by optical transmittance spectra. The electrical characterizations were done using Hall effect and photocurrent measurements. A photovoltaic structure: Glass/ITO/CdS/AgSbSe2/Ag was formed, in which CdS was deposited by chemical bath deposition. J-V characteristics of this PV structure showed Voc=370 mV and Jsc=0.5 mA/cm2 under illumination using a tungsten halogen lamp.
- Open Access
- 1 January 2004
- Published by Cambridge University Press (CUP) in International Astronomical Union Colloquium
- Vol. 194, 258
Possible Density Determination of the Nebular Component of Cataclysmic Variables with the N III 4641/4635 Line Ratio
The dependence of the N III 4641/4635 line ratio on the electron density is presented. It is shown that this ratio may be an important diagnostic tool in cataclysmic variables.Pérez-Tijerina, Bohigas & Machorro (2001) used the Chianti code and database developed by the U.S. Nautical Observatory (Landi, 200) in order to find density and temperature sensitive line ratios in the conditions occuring in plasmas produced in pulsed laser deposition experiments for thin film deposition, i.e., around 1018 cm 3 and 104 K. Level populations are determined considering only radiative decay and collisional excitation and de-excitation.
- 1 January 2004
- Published by Cambridge University Press (CUP) in International Astronomical Union Colloquium
- Vol. 194, 258
Open AccessPossible Density Determination of the Nebular Component of Cataclysmic Variables with the N III 4641/4635 Line Ratio
The dependence of the N III 4641/4635 line ratio on the electron density is presented. It is shown that this ratio may be an important diagnostic tool in cataclysmic variables.Pérez-Tijerina, Bohigas & Machorro (2001) used the Chianti code and database developed by the U.S. Nautical Observatory (Landi, 200) in order to find density and temperature sensitive line ratios in the conditions occuring in plasmas produced in pulsed laser deposition experiments for thin film deposition, i.e., around 1018 cm 3 and 104 K. Level populations are determined considering only radiative decay and collisional excitation and de-excitation.