Seok Hern Jang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Seok Hern Jang has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
- Jinho Joo
Sch. of Adv. Mater. Sci. & Eng., Sungkyunkwan Univ., Suwon, South Korea
4 shared publications Jun Hyung Lim
Sungkyunkwan Univ., Suwon
3 shared publicationsKyu Tae Kim
Sungkyunkwan Univ., Suwon
3 shared publications- Seung-Boo Jung
School of Advanced Materials Science and Engineering, Sungkyunkwan University, Suwon, Republic of Korea
3 shared publications Kyung Min Yoon
Sungkyunkwan Univ., Suwon
2 shared publicationsSeung Yi Lee
Sungkyunkwan Univ., Suwon
2 shared publications
Latest Publications
- 23 July 2007
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 17 (2) , 3004-3007
A Study on the Processing Variables of the BSCCO-2212 Bulk Superconductors
Bi-2212/SrSO4 bulk superconductors were fabricated using a casting process, and the effects of the powder mixing method, annealing temperature, and SrSO4 content on the texture, microstructure, and critical properties were evaluated. The Bi-2212 powders were mixed with SrSO4 either by hand-mixing (HM) or planetary ball milling (PBM), followed by melting at 1100degC-1200degC, solidification, and annealing. The rod produced by PBM had a more homogeneous microstructure and smaller grain size of SrSO4 and minor phases, resulting in increased Ic, than the rod made by HM. The Ic of the rod was also dependent on the annealing temperature with the highest Ic of 200 A being obtained at an annealing temperature of 810degC. This was attributed to the moderate density and 2212 texture as well as the smaller and less minor phase than that observed at higher temperature. In addition, the optimum SrSO4 content was found to be 6 wt.% for an increased Ic. SEM, EPMA, and DTA analyses indicated that the differences in microstructural evolution caused the variations of the Ic with the powder mixing method, annealing temperature, and SrSO4 addition.
- 23 July 2007
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 17 (2) , 3004-3007
A Study on the Processing Variables of the BSCCO-2212 Bulk Superconductors
Bi-2212/SrSO4 bulk superconductors were fabricated using a casting process, and the effects of the powder mixing method, annealing temperature, and SrSO4 content on the texture, microstructure, and critical properties were evaluated. The Bi-2212 powders were mixed with SrSO4 either by hand-mixing (HM) or planetary ball milling (PBM), followed by melting at 1100degC-1200degC, solidification, and annealing. The rod produced by PBM had a more homogeneous microstructure and smaller grain size of SrSO4 and minor phases, resulting in increased Ic, than the rod made by HM. The Ic of the rod was also dependent on the annealing temperature with the highest Ic of 200 A being obtained at an annealing temperature of 810degC. This was attributed to the moderate density and 2212 texture as well as the smaller and less minor phase than that observed at higher temperature. In addition, the optimum SrSO4 content was found to be 6 wt.% for an increased Ic. SEM, EPMA, and DTA analyses indicated that the differences in microstructural evolution caused the variations of the Ic with the powder mixing method, annealing temperature, and SrSO4 addition.
- 23 July 2007
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 17 (2) , 3302-3305
Fabrication of the YBCO Films Made by TFA-MOD Using the 211-Process
YBCO films were fabricated using TFA-MOD method with a precursor solution of and powders dissolved in trifluoroacetic acid (TFA) (the so called "211-film"). The effect of the calcining temperature on the phase formation, texture evolution, and thermal and critical properties were investigated. The microstructure and critical current density of the 211-film varied significantly with the calcining temperature. The highest of 1.9 (corresponding critical current is 39 A/cm-width) was obtained for the film calcined at 460, which is probably due to the enhanced degree of texture and increased film density and grain size. In addition, the microstructure and properties of the 211-films were compared with those of the film made using the conventional TFA-MOD method with the precursor of the acetates being dissolved in TFA. The of the 211-film was higher than that produced by the conventional TFA-MOD method. TG, DTA, pole-figure, and SEM analyses indicated that the higher was due to the improved microstructure resulting from the enhanced reaction kinetics in the 211-film.
- 23 July 2007
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 17 (2) , 3302-3305
Fabrication of the YBCO Films Made by TFA-MOD Using the 211-Process
YBCO films were fabricated using TFA-MOD method with a precursor solution of and powders dissolved in trifluoroacetic acid (TFA) (the so called "211-film"). The effect of the calcining temperature on the phase formation, texture evolution, and thermal and critical properties were investigated. The microstructure and critical current density of the 211-film varied significantly with the calcining temperature. The highest of 1.9 (corresponding critical current is 39 A/cm-width) was obtained for the film calcined at 460, which is probably due to the enhanced degree of texture and increased film density and grain size. In addition, the microstructure and properties of the 211-films were compared with those of the film made using the conventional TFA-MOD method with the precursor of the acetates being dissolved in TFA. The of the 211-film was higher than that produced by the conventional TFA-MOD method. TG, DTA, pole-figure, and SEM analyses indicated that the higher was due to the improved microstructure resulting from the enhanced reaction kinetics in the 211-film.
- 23 July 2007
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 17 (2) , 3298-3301
The Effects of the Humidity and Thickness on YBCO Film Prepared Using the TFA-MOD Method
This study examined the epitaxial growth of YBa2Cu3O7-x (YBCO) films on (00l) LaAlO3 substrates prepared by metal organic deposition (MOD) using a trifluoroacetate (TFA) solution. The effects of humidity (0-20% of PH2O) and film thickness (0.4-2.1 mum) on the phase formation, texture, and microstructures of the YBCO films were examined by X-ray diffraction, pole-figure, and scanning electron microscopy (SEM). The microstructure and resultant critical properties varied remarkably with humidity. With increasing humidity, the amount of the second phase (BaF2) decreased, the degree of texture was enhanced, and consequently the critical current (IC) and temperature (TC ) were improved. In the case of multi-coated films, the IC value increased from 35 to 152 A/cm-width with an increasing number of coatings from one to three, while the corresponding critical current density (JC) was in the range of 0.9-1.5 MA/cm2 . Both the IC and JC decreased when an additional coating was applied due to microstructural degradation.
- 23 July 2007
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 17 (2) , 3298-3301
The Effects of the Humidity and Thickness on YBCO Film Prepared Using the TFA-MOD Method
This study examined the epitaxial growth of YBa2Cu3O7-x (YBCO) films on (00l) LaAlO3 substrates prepared by metal organic deposition (MOD) using a trifluoroacetate (TFA) solution. The effects of humidity (0-20% of PH2O) and film thickness (0.4-2.1 mum) on the phase formation, texture, and microstructures of the YBCO films were examined by X-ray diffraction, pole-figure, and scanning electron microscopy (SEM). The microstructure and resultant critical properties varied remarkably with humidity. With increasing humidity, the amount of the second phase (BaF2) decreased, the degree of texture was enhanced, and consequently the critical current (IC) and temperature (TC ) were improved. In the case of multi-coated films, the IC value increased from 35 to 152 A/cm-width with an increasing number of coatings from one to three, while the corresponding critical current density (JC) was in the range of 0.9-1.5 MA/cm2 . Both the IC and JC decreased when an additional coating was applied due to microstructural degradation.
- 1 January 2006
- Published by Springer Nature in MRS Proceedings
- Vol. 946
Development of YBCO film approached by TFA-MOD method using the Y2Ba1Cu1Ox and Ba3Cu5O8 powders
- 1 January 2006
- Published by Springer Nature in MRS Proceedings
- Vol. 946
Development of YBCO film approached by TFA-MOD method using the Y2Ba1Cu1Ox and Ba3Cu5O8 powders