Tiago Aurelio Donassollo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Tiago Aurelio Donassollo has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Flávio Fernando Demarco
Federal University of Pelotas, Pelotas, Brazil
2 shared publications - Alvaro Della Bona
Postgraduate Program in Dentistry, School of Dentistry, University of Passo Fundo, Passo Fundo, RS, Brazil
1 shared publication André Strapasson
Federal University of Pelotas, Brazil
1 shared publicationLeandro Sommer
Federal University of Pelotas, Brazil
1 shared publication- Maximiliano Sérgio Cenci
Radboud University Medical Center, Department of Dentistry, Nijmegen, the Netherlands
1 shared publication - Tatiana Pereira-Cenci
Radboud University Medical Center, Department of Dentistry, Philips van Leydenlaan 25, Nijmegen 6525 EX, the Netherlands
1 shared publication
Latest Publications
- 12 November 2009
- Vol. 57 (4) , 374-9
Resin bond strength to a zirconia-reinforced ceramic after different surface treatments.
This study evaluated the microtensile bond strength between a composite resin and a zirconia-reinforced alumina-based glass-infiltrated ceramic after different ceramic surface treatments. Blocks (12 mm x 10 mm x 5 mm3) of a ceramic containing zirconia were fabricated, polished, and divided at random into seven groups, with each group receiving a different surface treatment. The adhesive system and composite resin were applied to the treated ceramic; these composite-ceramic blocks were stored in distilled water (37 degrees C) for seven days. At that point, they were cut along two axes to produce specimens with a cross-sectional area of 1.0 (+/- 0.1) mm2. The specimens (n = 20) were loaded in tension in a universal testing machine with a cross-head speed of 0.5 mm/minute. The microtensile bond strength values were calculated and statistically analyzed using ANOVA and Tukey's test (alpha = 0.05). Among the seven groups, specimens with both a silica coating and a silane coupling agent showed the highest mean microtensile bond strength values. All specimens treated with 9.5% hydrofluoric acid failed during the cutting procedure; among all specimens, the majority of the failures were cohesive. A positive correlation was observed between the fracture type and the microtensile bond strength (r = 0.63).
- 12 November 2009
- Vol. 57 (4) , 374-9
Resin bond strength to a zirconia-reinforced ceramic after different surface treatments.
This study evaluated the microtensile bond strength between a composite resin and a zirconia-reinforced alumina-based glass-infiltrated ceramic after different ceramic surface treatments. Blocks (12 mm x 10 mm x 5 mm3) of a ceramic containing zirconia were fabricated, polished, and divided at random into seven groups, with each group receiving a different surface treatment. The adhesive system and composite resin were applied to the treated ceramic; these composite-ceramic blocks were stored in distilled water (37 degrees C) for seven days. At that point, they were cut along two axes to produce specimens with a cross-sectional area of 1.0 (+/- 0.1) mm2. The specimens (n = 20) were loaded in tension in a universal testing machine with a cross-head speed of 0.5 mm/minute. The microtensile bond strength values were calculated and statistically analyzed using ANOVA and Tukey's test (alpha = 0.05). Among the seven groups, specimens with both a silica coating and a silane coupling agent showed the highest mean microtensile bond strength values. All specimens treated with 9.5% hydrofluoric acid failed during the cutting procedure; among all specimens, the majority of the failures were cohesive. A positive correlation was observed between the fracture type and the microtensile bond strength (r = 0.63).
- Open Access
- 1 April 2008
- Published by FapUNIFESP (SciELO) in Journal of Applied Oral Science
- Vol. 16 (2) , 106-110
Influence of thermal stress on marginal integrity of restorative materials
The aim of this study was to evaluate the influence of thermal stress on the marginal integrity of restorative materials with different adhesive and thermal properties. Three hundred and sixty Class V cavities were prepared in buccal and lingual surfaces of 180 bovine incisors. Cervical and incisal walls were located in dentin and enamel, respectively. Specimens were restored with resin composite (RC); glass ionomer (GI) or amalgam (AM), and randomly assigned to 18 groups (n=20) according to the material, number of cycles (500 or 1,000 cycles) and dwell time (30 s or 60 s). Dry and wet specimens served as controls Specimens were immersed in 1% basic fuchsine solution (24 h), sectioned, and microleakage was evaluated under x40 magnification. Data were analyzed by Kruskal-Wallis and Mann-Whitney tests: Thermal cycling regimens increased leakage in all AM restorations (p<0.05) and its effect on RC and GI restorations was only significant when a 60-s dwell time was used (p<0.05). Marginal integrity was more affected in AM restorations under thermal cycling stress, whereas RC and GI ionomer restoration margins were only significantly affected only under longer dwell times.
- 1 April 2008
- Published by FapUNIFESP (SciELO) in Journal of Applied Oral Science
- Vol. 16 (2) , 106-110
Open AccessInfluence of thermal stress on marginal integrity of restorative materials
The aim of this study was to evaluate the influence of thermal stress on the marginal integrity of restorative materials with different adhesive and thermal properties. Three hundred and sixty Class V cavities were prepared in buccal and lingual surfaces of 180 bovine incisors. Cervical and incisal walls were located in dentin and enamel, respectively. Specimens were restored with resin composite (RC); glass ionomer (GI) or amalgam (AM), and randomly assigned to 18 groups (n=20) according to the material, number of cycles (500 or 1,000 cycles) and dwell time (30 s or 60 s). Dry and wet specimens served as controls Specimens were immersed in 1% basic fuchsine solution (24 h), sectioned, and microleakage was evaluated under x40 magnification. Data were analyzed by Kruskal-Wallis and Mann-Whitney tests: Thermal cycling regimens increased leakage in all AM restorations (p<0.05) and its effect on RC and GI restorations was only significant when a 60-s dwell time was used (p<0.05). Marginal integrity was more affected in AM restorations under thermal cycling stress, whereas RC and GI ionomer restoration margins were only significantly affected only under longer dwell times.