Ganna Bogdan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Ganna Bogdan has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Ken Haenen
Institute for Materials Research (IMO), Hasselt University, Wetenschapspark 1, 3590 Diepenbeek, Belgium
3 shared publications M. Nesládek
Institute for Materials Research (IMO), Hasselt University, Diepenbeek, Belgium
2 shared publicationsAndrey Bogdan
CEA Saclay, DRT, Bat 451, p. 84, Gif Sur Yvette, N/A, France, +33169088704
1 shared publicationJ. D'HAen
IMEC vzw, Division IMOMEC, Wetenschapspark 1, 3590 Diepenbeek, Belgium
1 shared publicationJ. Maes
Katholieke Universiteit Leuven, Laboratory for Solid State Physics and Magnetism, Pulsed Field Group, Celestijnenlaan 200D, 3001 Leuven, Belgium
1 shared publicationK. De Corte
HRD Research, Lier, Belgium
1 shared publication
Latest Publications
- 11 September 2006
- Published by Wiley in Physica Status Solidi (a)
- Vol. 203 (12) , 3063-3069
Thick single crystal CVD diamond prepared from CH4‐rich mixtures
Recent interests in freestanding single‐crystal CVD diamond (SC‐CVD) discs for several applications in electronics led to an intense study of SC‐CVD layer growth and properties. In this work we have investigated the growth mechanism of monocrystalline CVD diamond films with surfaces smooth in nanometer scale taking into account the defect incorporation in the SC‐CVD layers. Specifically we discuss the surface structure characteristics for these conditions as studied with high‐resolution AFM mapping. The as‐grown CVD layers were removed from the substrate by laser cutting, followed by a polishing step, yielding freestanding plates. Subsequently, microscopic and colour studies as well as infrared absorption spectroscopy were performed. These investigations revealed the presence of several characteristic defects and impurities.
- 11 September 2006
- Published by Wiley in Physica Status Solidi (a)
- Vol. 203 (12) , 3063-3069
Thick single crystal CVD diamond prepared from CH4‐rich mixtures
Recent interests in freestanding single‐crystal CVD diamond (SC‐CVD) discs for several applications in electronics led to an intense study of SC‐CVD layer growth and properties. In this work we have investigated the growth mechanism of monocrystalline CVD diamond films with surfaces smooth in nanometer scale taking into account the defect incorporation in the SC‐CVD layers. Specifically we discuss the surface structure characteristics for these conditions as studied with high‐resolution AFM mapping. The as‐grown CVD layers were removed from the substrate by laser cutting, followed by a polishing step, yielding freestanding plates. Subsequently, microscopic and colour studies as well as infrared absorption spectroscopy were performed. These investigations revealed the presence of several characteristic defects and impurities.
- 1 January 2006
- Published by Springer Nature in MRS Proceedings
- Vol. 956
Electrical Transport and Defect Spectroscopy of Free Standing Single Crystal CVD Diamond Prepared from Methane Rich Mixtures
Transient photocurrent measurements in the Time-of-Flight (TOF) configuration were used to study the electrical transport in single crystalline diamond layers using a Nd:YAG - pumped OPO (2.7 nsec) laser pulse excitation source working at a wavelength of ∼ 218 nm. The amount of collected charge was measured and the hole and electron drift mobilities were determined at room temperature for natural IIa diamond and intrinsic single crystalline CVD diamond samples. A variation of the laser intensity over several orders of magnitude enabled switching between the so called “small signal TOF” and “space charge limited current” (SCLC) modes. Experiments were done using electrical fields in the range of 0.05-1.2 V/μm.
- 1 January 2006
- Published by Springer Nature in MRS Proceedings
- Vol. 956
Electrical Transport and Defect Spectroscopy of Free Standing Single Crystal CVD Diamond Prepared from Methane Rich Mixtures
Transient photocurrent measurements in the Time-of-Flight (TOF) configuration were used to study the electrical transport in single crystalline diamond layers using a Nd:YAG - pumped OPO (2.7 nsec) laser pulse excitation source working at a wavelength of ∼ 218 nm. The amount of collected charge was measured and the hole and electron drift mobilities were determined at room temperature for natural IIa diamond and intrinsic single crystalline CVD diamond samples. A variation of the laser intensity over several orders of magnitude enabled switching between the so called “small signal TOF” and “space charge limited current” (SCLC) modes. Experiments were done using electrical fields in the range of 0.05-1.2 V/μm.
- 12 August 2005
- Published by Wiley in Physica Status Solidi (a)
- Vol. 202 (11) , 2066-2072
Growth and characterization of near‐atomically flat, thick homoepitaxial CVD diamond films
Diamond films were grown in an ASTeX MW PE CVD reactor. The effect of pre‐growth etching with a O2/H2 plasma and the influence of the methane concentration on growth on type Ib (100) HPHT synthetic diamonds were investigated. By controlling step flow growth we were able to prepare optical quality thick diamond films, free of hillocks and unepitaxial crystallites, with a relatively high growth rate of 4 to 5 µm/h using higher pressures and methane concentrations than standard growth conditions in combination with a modified substrate holder. All diamond films were characterized by optical microscopy, SEM, AFM and Raman spectroscopy. The mean roughness (Rms) of the films grown with a thickness of 120 µm was approximately 0.5 to 0.8 nm for scanning regions of 5 × 5 µm2. For the first time nearatomically flat films thicker than 200 µm could be prepared.
- 12 August 2005
- Published by Wiley in Physica Status Solidi (a)
- Vol. 202 (11) , 2066-2072
Growth and characterization of near‐atomically flat, thick homoepitaxial CVD diamond films
Diamond films were grown in an ASTeX MW PE CVD reactor. The effect of pre‐growth etching with a O2/H2 plasma and the influence of the methane concentration on growth on type Ib (100) HPHT synthetic diamonds were investigated. By controlling step flow growth we were able to prepare optical quality thick diamond films, free of hillocks and unepitaxial crystallites, with a relatively high growth rate of 4 to 5 µm/h using higher pressures and methane concentrations than standard growth conditions in combination with a modified substrate holder. All diamond films were characterized by optical microscopy, SEM, AFM and Raman spectroscopy. The mean roughness (Rms) of the films grown with a thickness of 120 µm was approximately 0.5 to 0.8 nm for scanning regions of 5 × 5 µm2. For the first time nearatomically flat films thicker than 200 µm could be prepared.