P. K. Singh
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
P. K. Singh has a total of 26 co-authors. Here are the top co-authors by number of shared publications:
A.K. Ghosh
Bhabha Atom Res Ctr, Bombay 400085, Maharashtra, India
1 shared publication- Ashish Ghosh
International Institute of Information Technology Bhubaneswar
1 shared publication B.B. Rupani
Bhabha Atom Res Ctr, Bombay 400085, Maharashtra, India
1 shared publicationB.K. Gaur
Bhabha Atom Res Ctr, Bombay 400085, Maharashtra, India
1 shared publicationD. M. Pukazhendi
Fatigue Testing Laboratory, Structural Engineering Research Centre, Chennai-600113, India
1 shared publicationD. S. R. Murthy
Fatigue Testing Laboratory, Structural Engineering Research Centre, Chennai-600113, India
1 shared publication
Latest Publications
- 22 March 2024
- Published by Springer Nature in Journal of Failure Analysis and Prevention
- Vol. 24 (3) , 1-15
Fatigue Crack Growth and Fracture Studies on Stainless Steel Straight Pipes Having Circumferential Surface Crack
- 22 March 2024
- Published by Springer Nature in Journal of Failure Analysis and Prevention
- Vol. 24 (3) , 1-15
Fatigue Crack Growth and Fracture Studies on Stainless Steel Straight Pipes Having Circumferential Surface Crack
- 1 April 2018
- Published by Elsevier in Nuclear Engineering and Design
- Vol. 330, 303-316
Round robin exercise on ball indentation technique in India: Indian nuclear reactor materials
- 1 April 2018
- Published by Elsevier in Nuclear Engineering and Design
- Vol. 330, 303-316
Round robin exercise on ball indentation technique in India: Indian nuclear reactor materials
- 7 September 2015
- Published by ASME International in Journal of Pressure Vessel Technology
- Vol. 138 (1) , 011403
Mechanical Properties Variations and Comparative Analysis of Dissimilar Metal Pipe Welds in Pressure Vessel System of Nuclear Plants
The experimental investigations of two dissimilar metal weld (DMW) joints between SA508Gr.3Cl.1 ferritic steel and SS304LN austenitic stainless steel using Inconel 82/182 (ERNiCr-3/ENiCrFe-3) and Inconel 52/152 (ERNiCrFe-7/ENiCrFe-7) filler metals have been conducted in the present work. The integrity assessment of DMW joints and the mechanical properties variations has made pertaining to ASME Section-III and Section-IX. Mechanical tests comprising bend test, transverse tensile test (TTT), tensile test, Charpy impact test, microhardness measurement have been carried out along with microstructural evolution using the standard test specimens according to respective ASTM standards. Bend tests have shown that interfaces of the SA508–Inconel, Inconel–Inconel, and Inconel–SS304LN are free from any lack of fusion or cracks. TTTs have shown that failures of the specimens are from the SS304LN indicating integrity of the weld joint. Tensile tests confirm that tensile strength of the different regions agreed the required strength as per ASME Section-II. The weld strength mismatch and plastic instability strength (PIS) are found to be important factors during integrity assessment of joints. Based on the comparative investigations, owing to better mechanical properties, Inconel 82/182 filler metals could be an optimum choice over Inconel 52/152 filler metals for present DMW joints required in pressure vessel system of nuclear plants.
- 7 September 2015
- Published by ASME International in Journal of Pressure Vessel Technology
- Vol. 138 (1) , 011403
Mechanical Properties Variations and Comparative Analysis of Dissimilar Metal Pipe Welds in Pressure Vessel System of Nuclear Plants
The experimental investigations of two dissimilar metal weld (DMW) joints between SA508Gr.3Cl.1 ferritic steel and SS304LN austenitic stainless steel using Inconel 82/182 (ERNiCr-3/ENiCrFe-3) and Inconel 52/152 (ERNiCrFe-7/ENiCrFe-7) filler metals have been conducted in the present work. The integrity assessment of DMW joints and the mechanical properties variations has made pertaining to ASME Section-III and Section-IX. Mechanical tests comprising bend test, transverse tensile test (TTT), tensile test, Charpy impact test, microhardness measurement have been carried out along with microstructural evolution using the standard test specimens according to respective ASTM standards. Bend tests have shown that interfaces of the SA508–Inconel, Inconel–Inconel, and Inconel–SS304LN are free from any lack of fusion or cracks. TTTs have shown that failures of the specimens are from the SS304LN indicating integrity of the weld joint. Tensile tests confirm that tensile strength of the different regions agreed the required strength as per ASME Section-II. The weld strength mismatch and plastic instability strength (PIS) are found to be important factors during integrity assessment of joints. Based on the comparative investigations, owing to better mechanical properties, Inconel 82/182 filler metals could be an optimum choice over Inconel 52/152 filler metals for present DMW joints required in pressure vessel system of nuclear plants.
- 9 August 2006
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 29 (11) , 901-915
Crack resistance of austenitic stainless steel pipe and pipe welds with a circumferential crack under monotonic loading
This paper describes the experimental studies carried out on cracked austenitic stainless steel pipe and pipe welds under bending loads. Pipe welds were produced by gas tungsten arc welding (GTAW) and shielded metal arc welding (SMAW). Fracture resistance curves for pipe and pipe welds were compared. Results indicate that the fracture resistance of pipe and pipe weld (GTAW) is comparable but that of pipe weld (GTAW+SMAW) is inferior. Cracks do not deviate from their original plane during propagation as observed in the cases of carbon steel pipe and pipe welds. The fracture resistance of pipe welds does not depend on the loading histories to which it has been subjected prior to fracture test. Initiation and crack propagation were observed prior to the maximum moment. An existing limit load expression is applicable for the pipe base material but gives non‐conservative results for the pipe welds. Multiplication factors have been suggested for the pipe welds for evaluation of limit loads using the existing expression. Fracture resistance for the pipe and compact tension specimens have also been compared for base material and welds.
- 9 August 2006
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 29 (11) , 901-915
Crack resistance of austenitic stainless steel pipe and pipe welds with a circumferential crack under monotonic loading
This paper describes the experimental studies carried out on cracked austenitic stainless steel pipe and pipe welds under bending loads. Pipe welds were produced by gas tungsten arc welding (GTAW) and shielded metal arc welding (SMAW). Fracture resistance curves for pipe and pipe welds were compared. Results indicate that the fracture resistance of pipe and pipe weld (GTAW) is comparable but that of pipe weld (GTAW+SMAW) is inferior. Cracks do not deviate from their original plane during propagation as observed in the cases of carbon steel pipe and pipe welds. The fracture resistance of pipe welds does not depend on the loading histories to which it has been subjected prior to fracture test. Initiation and crack propagation were observed prior to the maximum moment. An existing limit load expression is applicable for the pipe base material but gives non‐conservative results for the pipe welds. Multiplication factors have been suggested for the pipe welds for evaluation of limit loads using the existing expression. Fracture resistance for the pipe and compact tension specimens have also been compared for base material and welds.