Mojgan Vaziri
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Mojgan Vaziri has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
Dick Sandberg
Wood Science and Engineering , Luleå University of Technology , Forskargatan 1, 931 87 Skellefteå , Sweden
7 shared publicationsLars Abrahamsson
Vattenfall AB, BU Fuel, Engineering & Projects , Evenemangsgatan 13, 169 79 Solna , Sweden
5 shared publications- Antonio Pizzi
LERMAB-ENSTIB, University of Lorraine, 27 rue Philippe Seguin, 88000 Epinal, France
4 shared publications Owe Lindgren
Department of Wood Science and Technology , Luleå University of Technology , Forskargatan 1, 931 87, Skellefteå , Sweden
4 shared publicationsChristopher Dreimol
Wood Materials Science , Institute for Building Materials , ETH Zürich, 8093 Zürich , Switzerland
2 shared publicationsOlov Karlsson
Luleå University of Technology , Wood Science and Engineering , Forskargatan 1 , Skellefteå , 931 87 , Sweden
2 shared publications
Latest Publications
- Open Access
- 31 May 2023
- Published by Walter de Gruyter GmbH in Holzforschung
- Vol. 77 (7) , 515-526
Parameter estimation and model selection for water vapour sorption of welded bond-line of European beech and Scots pine
The single exponential kinetics (SEK) and parallel exponential kinetics (PEK) models were fitted to kinetic sorption data of welded and unwelded Scots pine (Pinus sylvestris L.) and European beech (Fagus sylvatica L.). Furthermore, diffusion coefficients of water vapour in wood were determined using two different Fickian diffusion solutions. The objective was to identify how well these models could represent the moisture contents of the specimens and to characterize differences between the sorption behaviour of welded and unwelded wood. This knowledge can be used to enhance the moisture resistance of welded wood, develop drying schedules, and improve the quality of timbers. The PEK and SEK models provided the most precise and the second most precise fits to the sorption kinetic data, respectively. The two Fickian models are equivalent when both the infinite series are truncated at n = 10 $n=10$ . The Fickian models also exhibited the highest discrepancy with the experimental data. Nevertheless, the Fickian models fit relatively better to the sorption data of the welded wood than to that of the unwelded wood. This behaviour may be due to the rigid and less-swelling structure of the welded bond line.- 31 May 2023
- Published by Walter de Gruyter GmbH in Holzforschung
- Vol. 77 (7) , 515-526
Open AccessParameter estimation and model selection for water vapour sorption of welded bond-line of European beech and Scots pine
The single exponential kinetics (SEK) and parallel exponential kinetics (PEK) models were fitted to kinetic sorption data of welded and unwelded Scots pine (Pinus sylvestris L.) and European beech (Fagus sylvatica L.). Furthermore, diffusion coefficients of water vapour in wood were determined using two different Fickian diffusion solutions. The objective was to identify how well these models could represent the moisture contents of the specimens and to characterize differences between the sorption behaviour of welded and unwelded wood. This knowledge can be used to enhance the moisture resistance of welded wood, develop drying schedules, and improve the quality of timbers. The PEK and SEK models provided the most precise and the second most precise fits to the sorption kinetic data, respectively. The two Fickian models are equivalent when both the infinite series are truncated at n = 10 $n=10$ . The Fickian models also exhibited the highest discrepancy with the experimental data. Nevertheless, the Fickian models fit relatively better to the sorption data of the welded wood than to that of the unwelded wood. This behaviour may be due to the rigid and less-swelling structure of the welded bond line. - Open Access
- 26 May 2023
- Published by Walter de Gruyter GmbH in Holzforschung
- Vol. 77 (7) , 500-514
Water-vapour sorption of welded bond-line of European beech and Scots pine
The wood–water interactions of welded bond-lines of European beech (Fagus sylvatica L.) and Scots pine (Pinus sylvestris L.) were in this paper studied for the first time with dynamic vapour sorption equipment. The aim of this study was to characterize the water sorption in the welded bond-line and to define to which extent it deviates from water sorption of the unwelded wood. The objective was to provide deepened knowledge about water sorption of the welded bond-line, which could be used to improve the moisture resistance of welded wood in the future. The welded wood generally had lower equilibrium moisture contents than the unwelded wood. The welded bond-lines of beech and pine showed greater hysteresis than the unwelded wood from 0 to 55 % relative humidity. All specimens showed faster adsorption than desorption. However, the welded wood showed slower adsorption but faster desorption than unwelded wood. The time to complete half of the fractional change in moisture content (E(t) = 0.5) increased as the moisture content increased. The adsorption diffusion coefficients of beech and welded beech were higher than those of pine and welded pine up to 50 % and 40 % RH, respectively. In desorption, pine had a higher diffusion coefficient than beech in the whole range of 85–0 % RH. Analogously, welded pine had a higher diffusion coefficient than welded beech in the range of 85–5 % RH. In contrast to the desorption, the welded wood always had lower adsorption diffusion coefficients than the corresponding unwelded wood. The diffusion coefficients showed irregular patterns in some ranges of the RH. Therefore, it was hard to make a clear conclusion about the water-sorption behaviour of the specimens based on the defined diffusion coefficients.
- 26 May 2023
- Published by Walter de Gruyter GmbH in Holzforschung
- Vol. 77 (7) , 500-514
Open AccessWater-vapour sorption of welded bond-line of European beech and Scots pine
The wood–water interactions of welded bond-lines of European beech (Fagus sylvatica L.) and Scots pine (Pinus sylvestris L.) were in this paper studied for the first time with dynamic vapour sorption equipment. The aim of this study was to characterize the water sorption in the welded bond-line and to define to which extent it deviates from water sorption of the unwelded wood. The objective was to provide deepened knowledge about water sorption of the welded bond-line, which could be used to improve the moisture resistance of welded wood in the future. The welded wood generally had lower equilibrium moisture contents than the unwelded wood. The welded bond-lines of beech and pine showed greater hysteresis than the unwelded wood from 0 to 55 % relative humidity. All specimens showed faster adsorption than desorption. However, the welded wood showed slower adsorption but faster desorption than unwelded wood. The time to complete half of the fractional change in moisture content (E(t) = 0.5) increased as the moisture content increased. The adsorption diffusion coefficients of beech and welded beech were higher than those of pine and welded pine up to 50 % and 40 % RH, respectively. In desorption, pine had a higher diffusion coefficient than beech in the whole range of 85–0 % RH. Analogously, welded pine had a higher diffusion coefficient than welded beech in the range of 85–5 % RH. In contrast to the desorption, the welded wood always had lower adsorption diffusion coefficients than the corresponding unwelded wood. The diffusion coefficients showed irregular patterns in some ranges of the RH. Therefore, it was hard to make a clear conclusion about the water-sorption behaviour of the specimens based on the defined diffusion coefficients.
- 1 February 2021
- Published by BioResources in BioResources
- Vol. 16 (2) , 3224-3234
Welding of thermally modified wood and thermal modification of the welded wood: Effects on the shear strength under climatic conditions
- 1 February 2021
- Published by BioResources in BioResources
- Vol. 16 (2) , 3224-3234
Welding of thermally modified wood and thermal modification of the welded wood: Effects on the shear strength under climatic conditions
- Open Access
- 3 August 2020
- Published by Walter de Gruyter GmbH in Holzforschung
- Vol. 75 (1) , 65-74
Wettability of welded wood-joints investigated by the Wilhelmy method: part 1. Determination of apparent contact angles, swelling, and water sorption
This study presents a novel application of the Wilhelmy plate method on welded joints of Scots pine sapwood and beech. Welding resulted in an increase in the contact angle (increased hydrophobicity) as well as a decrease in the water uptake and swelling of the welded pine-joint compared to non-welded pine. When the welding time was extended from 4 to 5 s, these properties were further pronounced. Welding of beech, on the other hand, led to an increase in the contact angle and a decrease in the water uptake, but an increase in the swelling. Fourier Transform Infrared spectroscopy showed that welding increased the aliphatic C–H and unsaturated C=C stretching absorption bands in pine and beech. Scanning electron microscopy showed a dense structure at the welded joints of the both species, giving evidence of a lower porosity that leads to a lower permeability as a result of the welding.
- 3 August 2020
- Published by Walter de Gruyter GmbH in Holzforschung
- Vol. 75 (1) , 65-74
Open AccessWettability of welded wood-joints investigated by the Wilhelmy method: part 1. Determination of apparent contact angles, swelling, and water sorption
This study presents a novel application of the Wilhelmy plate method on welded joints of Scots pine sapwood and beech. Welding resulted in an increase in the contact angle (increased hydrophobicity) as well as a decrease in the water uptake and swelling of the welded pine-joint compared to non-welded pine. When the welding time was extended from 4 to 5 s, these properties were further pronounced. Welding of beech, on the other hand, led to an increase in the contact angle and a decrease in the water uptake, but an increase in the swelling. Fourier Transform Infrared spectroscopy showed that welding increased the aliphatic C–H and unsaturated C=C stretching absorption bands in pine and beech. Scanning electron microscopy showed a dense structure at the welded joints of the both species, giving evidence of a lower porosity that leads to a lower permeability as a result of the welding.
- Open Access
- 20 July 2020
- Published by Walter de Gruyter GmbH in Holzforschung
- Vol. 75 (1) , 79-86
Wettability of welded wood-joints investigated by the Wilhelmy method: part 2. Effect of wollastonite additive
The effect of wollastonite on the wetting properties of welded Scots pine-joints was studied using the multicycle Wilhelmy plate method and by observation of the chemical composition of the welded joints. Welding pine with wollastonite for 5 s resulted in a decrease in the water uptake and the swelling, and an increase in the contact angle of the welded joint compared to welded wood without wollastonite. High-performance liquid chromatography and gas chromatography/mass spectrometry showed the presence of dehydration products such as furfural, 5-hydroxymethylfurfural, and levoglucosan in methanol extracts from welded joints of specimens welded with and without wollastonite. Phenols were also found by analysis using the Folin-Ciocalteu method and High-performance liquid chromatography. The importance of such compounds in relation to the wetting properties of the welded joint is discussed.
- 20 July 2020
- Published by Walter de Gruyter GmbH in Holzforschung
- Vol. 75 (1) , 79-86
Open AccessWettability of welded wood-joints investigated by the Wilhelmy method: part 2. Effect of wollastonite additive
The effect of wollastonite on the wetting properties of welded Scots pine-joints was studied using the multicycle Wilhelmy plate method and by observation of the chemical composition of the welded joints. Welding pine with wollastonite for 5 s resulted in a decrease in the water uptake and the swelling, and an increase in the contact angle of the welded joint compared to welded wood without wollastonite. High-performance liquid chromatography and gas chromatography/mass spectrometry showed the presence of dehydration products such as furfural, 5-hydroxymethylfurfural, and levoglucosan in methanol extracts from welded joints of specimens welded with and without wollastonite. Phenols were also found by analysis using the Folin-Ciocalteu method and High-performance liquid chromatography. The importance of such compounds in relation to the wetting properties of the welded joint is discussed.
- 17 January 2020
- Published by BioResources in BioResources
- Vol. 15 (1) , 1617-1628
Welding of wood in the presence of wollastonite
The use of wollastonite as a natural additive for the welding of Scots pine improved the water resistance and shear strength of the welded joint. The X-ray computed tomography images revealed that the welding of Scots pine with wollastonite could postpone crack formation in the welded joints. The specimens welded for a longer time (5 s) had a more uniform distribution of wollastonite particles in welded joints. The microstructure of the wood and the thickness of the wood cell walls also had a great influence on the thickness and strength of the welded joints. Water immersion tests showed that the use of wollastonite in wood joints was able to meet the requirement of resistance to frequent short-term and long-term exposure to water.
- 17 January 2020
- Published by BioResources in BioResources
- Vol. 15 (1) , 1617-1628
Welding of wood in the presence of wollastonite
The use of wollastonite as a natural additive for the welding of Scots pine improved the water resistance and shear strength of the welded joint. The X-ray computed tomography images revealed that the welding of Scots pine with wollastonite could postpone crack formation in the welded joints. The specimens welded for a longer time (5 s) had a more uniform distribution of wollastonite particles in welded joints. The microstructure of the wood and the thickness of the wood cell walls also had a great influence on the thickness and strength of the welded joints. Water immersion tests showed that the use of wollastonite in wood joints was able to meet the requirement of resistance to frequent short-term and long-term exposure to water.
- 5 August 2014
- Published by Taylor & Francis in Wood Material Science & Engineering
- Vol. 10 (4) , 368-372
Nano X-ray tomography analysis of the cell-wall density of welded beech joints
This paper reports the results of a novel approach using nano X-ray computed tomography (CT) for the non-invasive determination of the weld-line density profile of welded wood joints. As a case study, wood samples with a dimension of 2 mm × 2 mm × 20 mm were cut from a board of welded beech (Fagus sylvatica L.). The spatial resolution of the X-ray scan was 500 nm. Densitometry results showed that welding was accompanied by a considerable increase in the bulk density and a decrease in the cell-wall density at the weld-line. The cell-wall density in the weld-line was almost 33% less than that of the unaffected wood. As an additional application of nano computed tomography, the 3D imaging also revealed details of the internal structure of the welded sample. This study showed that nano-CT is a powerful tool for the descriptive and quantitative study of welded wood.
- 5 August 2014
- Published by Taylor & Francis in Wood Material Science & Engineering
- Vol. 10 (4) , 368-372
Nano X-ray tomography analysis of the cell-wall density of welded beech joints
This paper reports the results of a novel approach using nano X-ray computed tomography (CT) for the non-invasive determination of the weld-line density profile of welded wood joints. As a case study, wood samples with a dimension of 2 mm × 2 mm × 20 mm were cut from a board of welded beech (Fagus sylvatica L.). The spatial resolution of the X-ray scan was 500 nm. Densitometry results showed that welding was accompanied by a considerable increase in the bulk density and a decrease in the cell-wall density at the weld-line. The cell-wall density in the weld-line was almost 33% less than that of the unaffected wood. As an additional application of nano computed tomography, the 3D imaging also revealed details of the internal structure of the welded sample. This study showed that nano-CT is a powerful tool for the descriptive and quantitative study of welded wood.
- 13 January 2014
- Published by Taylor & Francis in Wood Material Science & Engineering
- Vol. 9 (2) , 102-109
Three-dimensional finite element modelling of heat transfer for linear friction welding of Scots pine
Finite element numerical analyses were performed to determine three-dimensional heat flux generated by friction to wood pieces during linear friction welding. The objective was to develop a computational model to explain the thermal behaviour of welded wood material rather than experimental methods, which are usually expensive and time consuming. This model serves as a prediction tool for welding parameters, leading to optimal thermo-mechanical performance of welded joints. The energy produced by the friction welding of small wood specimens of Scots pine (Pinus sylvestris L.) was determined by thermocouples and used as input data in the model. The model is based on anisotropic elasticity and the thermal properties were modelled as isotropic. This numerical simulation gave information on the distribution of the temperature in the welding interface during the entire welding process. A good agreement between the simulation and experimental results showed the appropriateness of the model for planning welded wood manufacture and prediction of thermal behaviour of wood during other mechanically induced vibration processes. The specimens presented in this model required a heat flux of 11 kW/m2 to achieve a satisfactory welding joint.
- 13 January 2014
- Published by Taylor & Francis in Wood Material Science & Engineering
- Vol. 9 (2) , 102-109
Three-dimensional finite element modelling of heat transfer for linear friction welding of Scots pine
Finite element numerical analyses were performed to determine three-dimensional heat flux generated by friction to wood pieces during linear friction welding. The objective was to develop a computational model to explain the thermal behaviour of welded wood material rather than experimental methods, which are usually expensive and time consuming. This model serves as a prediction tool for welding parameters, leading to optimal thermo-mechanical performance of welded joints. The energy produced by the friction welding of small wood specimens of Scots pine (Pinus sylvestris L.) was determined by thermocouples and used as input data in the model. The model is based on anisotropic elasticity and the thermal properties were modelled as isotropic. This numerical simulation gave information on the distribution of the temperature in the welding interface during the entire welding process. A good agreement between the simulation and experimental results showed the appropriateness of the model for planning welded wood manufacture and prediction of thermal behaviour of wood during other mechanically induced vibration processes. The specimens presented in this model required a heat flux of 11 kW/m2 to achieve a satisfactory welding joint.
- 17 May 2012
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 26 (18-19) , 2189-2197
Influence of Machine Setting and Wood Parameters on Crack Formation in Scots Pine Joints Produced by Linear Friction Welding
Previous investigations on linear welded woods have shown that the connections are not sufficiently resistant to water for use in outdoor conditions. Therefore, they are utilized mainly for non-structural use, with only short time exposure to varying humidity. Influences of some welding and wood parameters such as welding pressure, welding time and heartwood or sapwood on crack formation in the weldline of Scots pine (Pinus sylvestris) were investigated. Axial samples measuring 200 mm × 20 mm × 20 mm from Scots pine were welded, placed vertically in 5-mm-deep tap water and were taken out of the water one at a time after each 10 min of water absorption. Then they were scanned and put back into water until the first crack appeared in the weldline. An X-ray Computer Tomography (CT-) scanner was used to monitor water movement and density change in the weldlines during water absorption–desorption. CT-scanning enabled to detect the cracks as they formed in the weldline and could be used in wood welding studies. Data evaluation showed that all the three studied parameters had significant effects on crack formation and that crack occurrence could be postponed by using heartwood samples with 1.3 MPa welding pressure and 1.5 s welding time.
- 17 May 2012
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 26 (18-19) , 2189-2197
Influence of Machine Setting and Wood Parameters on Crack Formation in Scots Pine Joints Produced by Linear Friction Welding
Previous investigations on linear welded woods have shown that the connections are not sufficiently resistant to water for use in outdoor conditions. Therefore, they are utilized mainly for non-structural use, with only short time exposure to varying humidity. Influences of some welding and wood parameters such as welding pressure, welding time and heartwood or sapwood on crack formation in the weldline of Scots pine (Pinus sylvestris) were investigated. Axial samples measuring 200 mm × 20 mm × 20 mm from Scots pine were welded, placed vertically in 5-mm-deep tap water and were taken out of the water one at a time after each 10 min of water absorption. Then they were scanned and put back into water until the first crack appeared in the weldline. An X-ray Computer Tomography (CT-) scanner was used to monitor water movement and density change in the weldlines during water absorption–desorption. CT-scanning enabled to detect the cracks as they formed in the weldline and could be used in wood welding studies. Data evaluation showed that all the three studied parameters had significant effects on crack formation and that crack occurrence could be postponed by using heartwood samples with 1.3 MPa welding pressure and 1.5 s welding time.
- 1 January 2012
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 26 (1-3) , 109-119
Optimization of Tensile-Shear Strength for Linear Welded Scots Pine
The mechanical performance of welded wood has a decisive role in its applications. This study was performed to determine the welding conditions that optimized the tensile-shear strength of welded S...
- 1 January 2012
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 26 (1-3) , 109-119
Optimization of Tensile-Shear Strength for Linear Welded Scots Pine
The mechanical performance of welded wood has a decisive role in its applications. This study was performed to determine the welding conditions that optimized the tensile-shear strength of welded S...