John Campbell
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
John Campbell has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
B. B. Nyichomba
Department of Mechanical Engineering, Dar es Salaam University, Tanzania
2 shared publications- Xinjin Cao
National Research Council Canada - Aerospace
2 shared publications A. K. M. B. Rashid
Bangladesh University of Engineering and Technology
1 shared publication- Christian Nyahumwa
Department of Mechanical Engineering, Dar es Salaam Institute of Technology, Dar es Salaam, Tanzania
1 shared publication I. M. Cheya
Faculty of Engineering, University of Dar es Salaam, Tanzania
1 shared publicationJ. Mi
School of Metallurgy and Materials, The University of Birmingham, Edgbaston, Birmingham B15 2TT United Kingdom
1 shared publication
Latest Publications
- 28 February 2011
- Published by Wiley
- p. 137-148
Fracture Surface Facets and Fatigue Life Potential of Castings
- 28 February 2011
- Published by Wiley
- p. 137-148
Fracture Surface Facets and Fatigue Life Potential of Castings
- 1 July 2004
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 35 (7) , 2063-2071
Oxide defects in a vacuum investment-cast ni-based turbine blade
- 1 July 2004
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 35 (7) , 2063-2071
Oxide defects in a vacuum investment-cast ni-based turbine blade
- 1 April 2004
- Published by Springer Nature in Journal of Materials Science
- Vol. 39 (7) , 2303-2314
Effect of iron and manganese contents on convection-free precipitation and sedimentation of primary α-Al(FeMn)Si phase in liquid Al-11.5Si-0.4Mg alloy
- 1 April 2004
- Published by Springer Nature in Journal of Materials Science
- Vol. 39 (7) , 2303-2314
Effect of iron and manganese contents on convection-free precipitation and sedimentation of primary α-Al(FeMn)Si phase in liquid Al-11.5Si-0.4Mg alloy
- 1 July 2003
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 15 (6) , 595-608
Effect of melt superheating on convection-free precipitation and sedimentation of primary α-Fe phase in liquid Al-11.5Si-0.4Mg alloy
The effect of melts superheated at 760, 850 and 900 °C on the precipitation and sedimentation of primary α-Fe phase has been investigated at 600 °C for 4 hours in convection-free conditions. Compared with normal melting at 760 °C, an intermediate superheating temperature of 850 °C may facilitate the nucleation of primary °-Fe phase and/or hinder its growth, causing clear increases in precipitated particle weight and number, and a decrease in particle size. No significant variations in the precipitated weight, number and size of primary α-Fe particles were found at a superheating temperature of 900 °C. The profound influence of superheating temperatures on the crystallisation behaviour of primary α-Fe particles might be related to the transformation of oxides from α or η- to α-Al2O3. The possibility of α-Fe phase (primary or script type) being nucleated on oxide films was assessed by planar disregistry. Good matching planes were found between the α-Fe phase and main oxide films in cast Al-Si-Mg alloys. It seems that α- or η-Al2O3, α-Al2O3, MgO.Al2O3 and MgO films could all be good substrates for the nucleation and growth of α-Fe phase. After sedimentation processing at 600 °C, approximately 50% Fe and 70% Mn has been removed from the nominal Al-11.5Si-0.4Mg-1.2Fe-1.1Mn alloy.
- 1 July 2003
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 15 (6) , 595-608
Effect of melt superheating on convection-free precipitation and sedimentation of primary α-Fe phase in liquid Al-11.5Si-0.4Mg alloy
The effect of melts superheated at 760, 850 and 900 °C on the precipitation and sedimentation of primary α-Fe phase has been investigated at 600 °C for 4 hours in convection-free conditions. Compared with normal melting at 760 °C, an intermediate superheating temperature of 850 °C may facilitate the nucleation of primary °-Fe phase and/or hinder its growth, causing clear increases in precipitated particle weight and number, and a decrease in particle size. No significant variations in the precipitated weight, number and size of primary α-Fe particles were found at a superheating temperature of 900 °C. The profound influence of superheating temperatures on the crystallisation behaviour of primary α-Fe particles might be related to the transformation of oxides from α or η- to α-Al2O3. The possibility of α-Fe phase (primary or script type) being nucleated on oxide films was assessed by planar disregistry. Good matching planes were found between the α-Fe phase and main oxide films in cast Al-Si-Mg alloys. It seems that α- or η-Al2O3, α-Al2O3, MgO.Al2O3 and MgO films could all be good substrates for the nucleation and growth of α-Fe phase. After sedimentation processing at 600 °C, approximately 50% Fe and 70% Mn has been removed from the nominal Al-11.5Si-0.4Mg-1.2Fe-1.1Mn alloy.
- 1 July 2002
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 15 (1) , 17-24
Effect of Mn and Sr on intermetallics in Fe-rich eutectic Al-Si alloy
The effect of Mn and Sr on the precipitation of iron intermetallics from A413 aluminium alloy melts has been studied. A high concentration of iron (2.5% Fe) was selected to facilitate the identification of the intermetallic compounds. As usual for the iron-rich intermetallic particles, many were observed to be cracked, often precisely down their central axis. Mn additions above 0.9 per cent, in the absence of strontium, refines the beta-phase from large plates (needles in 2-D section) to a more numerous, compact, and polyhedral form. This phenomenon, often known as the “fragmentation” of the alphaphase intermetallics, is identified as a conversion from plate to dendritic morphology, plus an effect deriving from the non-straightening of double oxide films (bifilms) on which the intermetallics grow. Sr addition at 0.03 per cent produced the expected modification of eutectic silicon, but in the presence of Mn, Sr had negligible influence on altering the plate-like form of the primary beta-phase. However, the use of higher levels of Sr (more than 0.1%) was found to be a powerful factor in changing the morphology of the intermetallics from plate to star-like (i.e. dendritic). Sr was also observed to expand the central bifilms in intermetallics, converting the central cracks into open porosity. This was interpreted as the result of an increased hydrogen content opening bifilms.
- 1 July 2002
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 15 (1) , 17-24
Effect of Mn and Sr on intermetallics in Fe-rich eutectic Al-Si alloy
The effect of Mn and Sr on the precipitation of iron intermetallics from A413 aluminium alloy melts has been studied. A high concentration of iron (2.5% Fe) was selected to facilitate the identification of the intermetallic compounds. As usual for the iron-rich intermetallic particles, many were observed to be cracked, often precisely down their central axis. Mn additions above 0.9 per cent, in the absence of strontium, refines the beta-phase from large plates (needles in 2-D section) to a more numerous, compact, and polyhedral form. This phenomenon, often known as the “fragmentation” of the alphaphase intermetallics, is identified as a conversion from plate to dendritic morphology, plus an effect deriving from the non-straightening of double oxide films (bifilms) on which the intermetallics grow. Sr addition at 0.03 per cent produced the expected modification of eutectic silicon, but in the presence of Mn, Sr had negligible influence on altering the plate-like form of the primary beta-phase. However, the use of higher levels of Sr (more than 0.1%) was found to be a powerful factor in changing the morphology of the intermetallics from plate to star-like (i.e. dendritic). Sr was also observed to expand the central bifilms in intermetallics, converting the central cracks into open porosity. This was interpreted as the result of an increased hydrogen content opening bifilms.
- 1 May 2002
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 14 (6) , 335-340
Liquid metal quality
Castings are now becoming commonplace in highly demanding and safety critical applications, for example in the aerospace and automotive industries. It is, therefore, imperative that internal defect structures and potential failure mechanisms are fully understood if reliable castings are to be produced consistently by the foundry. Many alloy systems, such as those based on aluminium, magnesium, zinc and certain copper- and iron- and steel-based alloys suffer from the entrainment of double oxide films and dissolved gases. However, the presence of damaging oxide films is often only detected when a casting leaks or fractures at such inclusions. The ubiquitous presence of these very thin double films has not been widely accepted because no single metal quality test has been able to resolve such thin but extensive defects. We have developed a novel reduced pressure test that allows a detailed assessment of metal quality through the simultaneous visualisation of double oxide films and gas content. The technique will be demonstrated for use on aluminium alloys as this system provides clear examples and contains only a single dissolved gas.
- 1 May 2002
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 14 (6) , 335-340
Liquid metal quality
Castings are now becoming commonplace in highly demanding and safety critical applications, for example in the aerospace and automotive industries. It is, therefore, imperative that internal defect structures and potential failure mechanisms are fully understood if reliable castings are to be produced consistently by the foundry. Many alloy systems, such as those based on aluminium, magnesium, zinc and certain copper- and iron- and steel-based alloys suffer from the entrainment of double oxide films and dissolved gases. However, the presence of damaging oxide films is often only detected when a casting leaks or fractures at such inclusions. The ubiquitous presence of these very thin double films has not been widely accepted because no single metal quality test has been able to resolve such thin but extensive defects. We have developed a novel reduced pressure test that allows a detailed assessment of metal quality through the simultaneous visualisation of double oxide films and gas content. The technique will be demonstrated for use on aluminium alloys as this system provides clear examples and contains only a single dissolved gas.
- 1 May 2002
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 14 (6) , 325-334
The tilt casting process
Tilt casting is a process with the unique feature that, in principle, liquid metal can be transferred into a mould by simple mechanical means under the action of gravity, but without surface turbulence. It therefore has the potential to produce very high quality castings. Even so, the process is not often optimised in the industrial environment. This investigation represents an attempt to investigate some fundamental problems associated with the process. A computer controlled, programmable roll-over casting wheel with a diameter of 1 m was used to produce sand castings in an Al-4.5% Cu alloy. The filling of the mould was studied using realtime X-ray radiography. Real-time X-ray radiography revealed that the molten metal could exhibit tranquil, turbulent or chaotic flow into the mould during tilt casting, depending on (i) the angle of tilt of the mould at the start of casting, and (ii) the tilting speed. Essentially horizontal transfer of the melt could achieve tranquil filling of the mould with minimum surface turbulence by a tilt starting position above the horizontal. The tensile properties of castings made using various starting conditions and rotation rates were measured and the results analysed using Weibull statistics to quantify reliability. Results are summarised on a map of the various operating regimes for tilt casting. An operational window for the production of reliable castings has been defined for the first time.
- 1 May 2002
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 14 (6) , 325-334
The tilt casting process
Tilt casting is a process with the unique feature that, in principle, liquid metal can be transferred into a mould by simple mechanical means under the action of gravity, but without surface turbulence. It therefore has the potential to produce very high quality castings. Even so, the process is not often optimised in the industrial environment. This investigation represents an attempt to investigate some fundamental problems associated with the process. A computer controlled, programmable roll-over casting wheel with a diameter of 1 m was used to produce sand castings in an Al-4.5% Cu alloy. The filling of the mould was studied using realtime X-ray radiography. Real-time X-ray radiography revealed that the molten metal could exhibit tranquil, turbulent or chaotic flow into the mould during tilt casting, depending on (i) the angle of tilt of the mould at the start of casting, and (ii) the tilting speed. Essentially horizontal transfer of the melt could achieve tranquil filling of the mould with minimum surface turbulence by a tilt starting position above the horizontal. The tensile properties of castings made using various starting conditions and rotation rates were measured and the results analysed using Weibull statistics to quantify reliability. Results are summarised on a map of the various operating regimes for tilt casting. An operational window for the production of reliable castings has been defined for the first time.
- 29 November 1998
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 11 (3) , 179-186
Linear contraction of ductile iron castings
The effect of casting design on the linear contraction of ductile iron castings produced in clay- and silicate-bonded sand moulds has been studied. The designs included free and restrained square bar castings. Free contraction of very thin sections of ductile iron in sand moulds was found to approach 1.35%. As sections increased to 25 mm thick, the contraction decreased linearly to 1.08% in silicate-bonded sand moulds, but to 0.90% in clay-bonded sand moulds. For test pieces with end flanges which stimulated various degrees of constraint as would be experienced in a shaped casting, the contraction was found to be sensitive to the third power of the relative cooling time of the flange and the cast section. In conditions of high constraint, contraction could fall as low as 0.55%. The data from this study represent a first attempt to provide a designer and toolmaker with realistic contraction allowances for shaped castings.
- 29 November 1998
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 11 (3) , 179-186
Linear contraction of ductile iron castings
The effect of casting design on the linear contraction of ductile iron castings produced in clay- and silicate-bonded sand moulds has been studied. The designs included free and restrained square bar castings. Free contraction of very thin sections of ductile iron in sand moulds was found to approach 1.35%. As sections increased to 25 mm thick, the contraction decreased linearly to 1.08% in silicate-bonded sand moulds, but to 0.90% in clay-bonded sand moulds. For test pieces with end flanges which stimulated various degrees of constraint as would be experienced in a shaped casting, the contraction was found to be sensitive to the third power of the relative cooling time of the flange and the cast section. In conditions of high constraint, contraction could fall as low as 0.55%. The data from this study represent a first attempt to provide a designer and toolmaker with realistic contraction allowances for shaped castings.
- 29 November 1998
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 11 (3) , 163-177
Linear contraction and residual stress of aluminium alloy sand castings
Variations in the linear contraction of unconstrained and constrained rectangular and round bar castings of aluminium alloys have been studied. The processing variables included test bar design and dimensions, alloy composition and mould and core materials. The results show that the largest effects on linear contraction were due to constraint by enclosed cores in round bars and/or the flanges at the ends of bars. The results also indicate that the size of the constraint effects can be numerically related, for a given mould material, to the geometry of the bar and its constraint. The contraction was found to be a function of the relative modulus and relative areas of the bar and its restraining flange. Measurements of AlSi5Cu3 and AlSi11 castings in sand moulds indicate that residual stress in these light alloys does not seem to vary significantly with alloy type. However, it is sensitive to (i) mould restraint, and thus is affected by the type of binder, greensand giving much higher stresses than furan, and (ii) the geometrical constraint provided by the shape of the casting. Residual stress is reduced by shaking out the casting from the mould at an early stage after casting. It was found that the residual stress could vary between values as low as 0 to 10 MPa and as high as 110 MPa. The high level of stress appears to approximate to yield stress of the alloys, indicating that the castings are in a plastic yielding condition when emerging at near room temperature from the mould.
- 29 November 1998
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 11 (3) , 163-177
Linear contraction and residual stress of aluminium alloy sand castings
Variations in the linear contraction of unconstrained and constrained rectangular and round bar castings of aluminium alloys have been studied. The processing variables included test bar design and dimensions, alloy composition and mould and core materials. The results show that the largest effects on linear contraction were due to constraint by enclosed cores in round bars and/or the flanges at the ends of bars. The results also indicate that the size of the constraint effects can be numerically related, for a given mould material, to the geometry of the bar and its constraint. The contraction was found to be a function of the relative modulus and relative areas of the bar and its restraining flange. Measurements of AlSi5Cu3 and AlSi11 castings in sand moulds indicate that residual stress in these light alloys does not seem to vary significantly with alloy type. However, it is sensitive to (i) mould restraint, and thus is affected by the type of binder, greensand giving much higher stresses than furan, and (ii) the geometrical constraint provided by the shape of the casting. Residual stress is reduced by shaking out the casting from the mould at an early stage after casting. It was found that the residual stress could vary between values as low as 0 to 10 MPa and as high as 110 MPa. The high level of stress appears to approximate to yield stress of the alloys, indicating that the castings are in a plastic yielding condition when emerging at near room temperature from the mould.
- 1 July 1998
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 11 (1) , 1-12
Liquid metal flow in moulds with off-set sprue
Two different geometries of sprue/runner junctions have been investigated for their effects on the flow behaviour of molten aluminium alloys during mould filling. In the present work, three-dimensional computer simulations of mould filling for (i) conventional in-line and (ii) sprue off-set relative to the runner (i.e. the sprue located at the side of the runner), have been carried out and compared with real-time X-ray radiographic observation experiments. The example modelled is the cast plate which was adopted in the Benchmark test,10 where the conventional sprue/runner junction presented an ingate velocity in the range 0.5 to 0.7 m/s, generally above the critical value 0.5 m/s in which surface turbulence phenomena were clearly observed, in agreement with the prediction. In contrast, it was shown that the ingate velocity when the sprue was sited offset relative to the runner is in the range 0.3 to 0.4 m/s, reducing surface turbulence in the casting cavity itself, although some initial surface turbulence at the sprue/runner junction was noted. Experimental studies including 3-point bend tests demonstrate greater strength and consistency, illustrating the overall reduction in damage for the castings produced with the off-set sprue.
- 1 July 1998
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 11 (1) , 1-12
Liquid metal flow in moulds with off-set sprue
Two different geometries of sprue/runner junctions have been investigated for their effects on the flow behaviour of molten aluminium alloys during mould filling. In the present work, three-dimensional computer simulations of mould filling for (i) conventional in-line and (ii) sprue off-set relative to the runner (i.e. the sprue located at the side of the runner), have been carried out and compared with real-time X-ray radiographic observation experiments. The example modelled is the cast plate which was adopted in the Benchmark test,10 where the conventional sprue/runner junction presented an ingate velocity in the range 0.5 to 0.7 m/s, generally above the critical value 0.5 m/s in which surface turbulence phenomena were clearly observed, in agreement with the prediction. In contrast, it was shown that the ingate velocity when the sprue was sited offset relative to the runner is in the range 0.3 to 0.4 m/s, reducing surface turbulence in the casting cavity itself, although some initial surface turbulence at the sprue/runner junction was noted. Experimental studies including 3-point bend tests demonstrate greater strength and consistency, illustrating the overall reduction in damage for the castings produced with the off-set sprue.