  • Microstructure of ball milled and compacted Co–Ni–Al alloys from the β range

    by W. Maziarz, J. Dutkiewicz, Ł. Rogal, J. Grzonka, E. Cesari

    Two powder alloys from the beta phase region of compositions Co(28.5)Ni(36.5)Al(35) and Co(35)Ni(30)Al(35) were ball milled for 80 h in a high energy ball mill. The formation of amorphous structure was observed after 40 h of milling and further milling did not change their structure. The analytical and high-resolution transmission electron microscopy (TEM, HREM) examination of powder structure showed that nanoparticles of L1(0) phase of size of about 5 nm were present within the amorphous matrix. The vacuum hot pressing of the milled powders under pressure of 400 MPa at 700 degrees C for 12 min resulted in the formation of compacts with density of about 70% of the theoretical one. The additional heat treatment at 1300 degrees C for 6 h followed by water quenching, led to significant improvement of density and induced the martensitic transformation manifested by a broad heat effect. The characteristic temperatures of the transformation were determined using DSC measurements, which revealed only small differences within the examined alloys compositions. TEM structure studies of heat-treated alloys allowed to identify the structure of an ordered beta (B2) phase and L1(0) martrensite.


  • HRTEM studies of NiNbZr + Ag amorphous‐nanocrystalline composites

    by J. Dutkiewicz, L. Lityńska‐Dobrzyńska, A. Kovacova, Ł. Rogal, W. Maziarz

    Amorphous powder of composition corresponding to Ni60Ti20Zr20 (in at%) was obtained by ball milling in a high-energy mills starting from pure elements. Formation of the amorphous structure was observed already after 20 h of milling, although complete amorphization occurred after 40 h. The microhardness of powders increased from about 30 HV for pure elements to above 400 HV (1290 MPa) after 40 h of milling. Transmission electron microscopy (TEM) allowed to identify nanocrystalline inclusions of intermetallic phases of size 2-10 nm. Uniaxial hot pressing was performed in vacuum at temperature below the crystallization T(x) it is 510 degrees C and pressure of 600 MPa, Mixed amorphous powders and nanocrystalline silver powders were used to form a composite, in which microhardness was near 970 MPa HV and 400 HV for the amorphous phase and nanocrystalline silver, respectively. The compression strength of the composite containing 20 wt% of nanocrystalline Ag powder was equal to 600 MPa and plastic strain was 2%. Microstructure studies showed low porosity of composites of less than 1%, uniform distribution of the silver phase and a transition zone between both components, about 150 nm thick, where diffusion of nickel, niobium and zirconium into silver was observed. High-resolution TEM allowed identifying the structure of nanocrystalline inclusions in the amorphous matrix after hot pressing as either Ni(3)Zr or Ni(17)Nb(3). The identification was performed basing on measurements of angles and interatomic distances using inverse Fourier transformed images with enhanced contrast using Digital Micrograph computer program.