Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Masatoshi Takahashi has a total of 49 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Surface Modification of Gutta-Percha for the Use of Intact MTA as a Root Canal Sealer

    by Nastiti Sarilaksmi, Futami Nagano-Takebe, Masatoshi Takahashi, Takashi Kado, Kazuhiko Endo, Takashi Nezu

    This study aimed to use intact mineral trioxide aggregate (MTA) as a root canal sealer by hydrophilizing the gutta-percha (GP) surface. The GP specimens were treated with atmospheric air plasma, cetylpyridinium chloride (CPC), or a combination of both. The wettability and surface chemical properties were evaluated using contact angle measurements and X-ray photoelectron spectroscopy (XPS). The physicochemical properties of MTA mixed with water or 100 mM of CPC solution were evaluated using setting time, flowability, compressive strength, and X-ray diffraction (XRD) analyses. Sealing ability was assessed by evaluating the dye penetration in obturated single-rooted teeth. Combined plasma and CPC treatment significantly decreased the contact angle of GP compared to that of the untreated group (p < 0.05) and showed the least hydrophobic recovery after 8 weeks. The XPS analysis confirmed the adsorption of CPC onto the GP surface. The XRD and compressive strength results indicated that the CPC did not interfere with the setting reaction of intact MTA, although the setting time was prolonged (p < 0.05). Dye penetration was significantly reduced in the plasma- and CPC-treated GP groups compared to the untreated GP group (p < 0.05), with a sealing ability comparable to that of the zinc oxide-based sealer.

  • Open Access

    Bone Compatibility of Experimental Ti–Ag and Ti–Cu Alloy Dental Implants in a Beagle Dog Model

    by Yasumitsu Ohtsuka, Taichi Tenkumo, Masatoshi Takahashi, Yasuhiro Nakanishi, Hiroaki Takebe, Takashi Nezu

    Titanium–silver (Ti–Ag) and titanium–copper (Ti–Cu) alloys have been developed to improve the mechanical properties and machinability of titanium (Ti) for dental applications while maintaining corrosion resistance comparable to that of pure Ti. Herein, cylindrical dental implants composed of experimental Ti–20Ag, Ti–30Ag, Ti–5Cu, and Ti–10Cu (mass%) alloys were fabricated and implanted into the jawbones of beagle dogs to evaluate bone compatibility. Pure Ti and Ti–6Al–4V alloy implants were used as controls. Because the implant surfaces were mechanically polished, the experimental alloys, which exhibited higher hardness than Ti, showed lower surface roughness than Ti. Radiographic observations revealed no remarkable bone resorption around any implants during the experimental period. Histological evaluation demonstrated new bone formation and partial bone contact around implants at 1 and 3 months post-implantation. Although the bone–implant contact ratio was relatively low owing to the cylindrical implant design and limited initial stability, no significant differences were observed between the experimental alloys and Ti. These results indicate that Ti–Ag and Ti–Cu alloys improve mechanical properties while maintaining bone compatibility comparable to that of Ti, suggesting their potential as candidate materials for dental implant applications, particularly for narrow dental implants.

  • Open Access

    Ultrasound Microscopy-Based Identification of Enamel and Restorative Materials: An Ex Vivo Acoustic Impedance Study

    by Yukihiro Naganuma, Masatoshi Takahashi, Yoshifumi Saijo, Masahiro Iikubo, Atsushi Takahashi

  • Open Access

    Thermal effects on the optical properties of dental composite resins and glass ionomer cements in forensic contexts

    by Moe Kosaka, Masatoshi Takahashi, Yuka Hatano, Toshihiko Suzuki

    Purpose: This study investigated the fluorescence intensity and color changes of tooth-colored dental materials under experimental conditions similar to those of charred bodies, from which dental evidence can be obtained.Methods: Among 160 composite resin (CR) and glass ionomer cement samples, the fluorescence intensity was measured using a spectrofluorometer. CIELAB color space (L*a*b*), difference in lightness (ΔL*), and CIEDE2000 color difference (ΔE00) were calculated for all samples.Results: The fluorescence intensity of CR was significantly higher in the flow type than in the paste type, and the A1 shade showed significantly higher intensity than the A3 before and after heating. The flow and paste type of the universal shade type CRs showed similar fluorescence to the A1 of conventional CRs before heating and tended to lose its fluorescence and transparency upon heating more easily than the conventional CRs. CR fluorescence intensity decreased significantly after 10 min of heating at 300°C, and many samples lost their fluorescence after 30 min. In contrast, glass ionomer cement fluorescence intensity increased with heating. ΔL* and ΔE00 were consistent with the macroscopic findings.Conclusion: The findings of this study provide updated information on tooth-colored dental materials and help us understand the circumstances in charred cases.

  • Open Access

    The Effect of Electroless Nickel–Polytetrafluoroethylene Coating on the Frictional Properties of Orthodontic Wires

    by Kento Numazaki, Masatoshi Takahashi, Arata Ito, Yukyo Takada, Itaru Mizoguchi

    In orthodontic treatment, to achieve efficient tooth movement, it is important to reduce the frictional force between the wire and the bracket, especially the binding friction that occurs when the angle between the wire and the bracket is large. Electroless nickel–polytetrafluoroethylene (Ni-PTFE) coating is a coating technology used to deposit PTFE particles with a low coefficient of friction on the coating surface to provide a low-friction surface for metallic materials. The purpose of this study was to investigate the effect of Ni-PTFE-coated orthodontic wires on the frictional force between brackets. The surface morphology, surface roughness, and frictional properties of Ni-PTFE-coated stainless steel wires and Ni-Ti wires were evaluated. The results demonstrate that the Ni-PTFE coating reduced the frictional force between the orthodontic wires and brackets, despite the increased surface roughness. Even when the angle between the wire and bracket was increased, assuming binding friction, the frictional force was reduced by the Ni-PTFE coating. This suggests that the friction between the wire and the bracket was suppressed by the PTFE particles deposited on the wire surface in contact with the bracket.


  • Open Access

    Development of Ternary Ti-Ag-Cu Alloys with Excellent Mechanical Properties and Antibiofilm Activity

    by Genichi Togawa, Masatoshi Takahashi, Hiroyuki Tada, Yukyo Takada

    Titanium-20 mass% Silver (Ti-20%Ag) alloy can suppress biofilm formation on the surface. Unlike bactericidal agents, it does not kill bacteria; therefore, the healthy oral microflora remains undisturbed. To utilize the unique functions of this alloy and enable its use in the fabrication of dental prostheses that require relatively high strength, we added copper (Cu) as an alloying element to improve strength. This study aimed to develop ternary Ti-Ag-Cu alloys with excellent mechanical properties and antibiofilm activity. As a result of investigating the mechanical properties of several experimental alloys, the tensile strength, yield strength, and hardness of Ti-20%Ag-1%Cu and Ti-20%Ag-2%Cu alloys were improved by the solid-solution strengthening or hardening of the αTi phase. In addition, these alloys had the same ability to suppress biofilm formation as the Ti-20Ag alloy. Thus, Ti-20%Ag-1–2%Cu alloys can be used for fabrication of narrow-diameter dental implants and prostheses subjected to extremely high force, and these prostheses are useful in preventing post-treatment oral diseases.


  • Open Access

    Mechanical Properties of Ti-Nb-Cu Alloys for Dental Machining Applications

    by Masatoshi Takahashi, Kotaro Sato, Genichi Togawa, Yukyo Takada

    Titanium has excellent biocompatibility and good corrosion resistance and is extensively used in dental implants and denture bases. However, pure titanium lacks the strength for use in dental prostheses that require relatively high strength. We developed 15 different types of Ti-Nb-Cu alloys and investigated their alloy phases and mechanical properties, including tensile and yield strength, elongation after fracture, and Vickers hardness. The alloy phases of Ti-8%Nb-2%Cu and Ti-13%Nb-2%Cu were α + β, while those of Ti-5%Nb-5%Cu and Ti-10%Nb-5%Cu were α + Ti2Cu. The tensile strength and hardness of these alloys were significantly higher than those of titanium; however, their elongation was less. In particular, the yield strength of these alloys was more than twice that of titanium. These differences in mechanical properties are attributable to solid–solution strengthening and precipitation strengthening. Other compositions with an alloy phase of α + β + Ti2Cu or β + Ti2Cu had high hardness but not high strength. These results suggest that the Ti-8%Nb-2%Cu, Ti-5%Nb-5%Cu, Ti-13%Nb-2%Cu, and Ti-10%Nb-5%Cu alloys can be applied to dental prostheses, which are subject to very high forces from accessories such as long-span bridges, clasps, implant-retained superstructures, and narrow-diameter implants.


  • Open Access

    Grindability of Ti−Nb−Cu Alloys for Dental Machining Applications

    by Masatoshi Takahashi, Masafumi Kikuchi, Yukyo Takada

    We developed high-strength Ti−Nb−Cu alloys and investigated their grindability. The grindability of each alloy was evaluated based on the volume of metal removed per minute (grinding rate) and on the ratio of the metal volume removed to the volume of the wheel material lost (grinding ratio). The grinding rate of the Ti-6%Nb-4%Cu, Ti-18%Nb-2%Cu, and Ti-24%Nb-1%Cu alloys significantly exceeded that of unalloyed titanium at high, medium, and low grinding speeds, respectively. Additionally, the Ti-6%Nb-4%Cu alloy exhibited an excellent grinding ratio. Generally, materials with high strength and hardness frequently exhibit poor machinability; however, the Ti−Nb−Cu alloys developed in our study presented favorable grindability characteristics and, therefore, demonstrated good potential for application as dental titanium alloys that can be subjected to computer-aided design/manufacturing processes.


  • Open Access

    Effects of Stabilizer Concentration on the Electrochemical Performance of Au-Pt Anode Catalysts for Direct Glucose Fuel Cell

    by Masatoshi Takahashi, Kazuki Iwabata, Kanjiro Torigoe, Takeshi Endo, Kengo Sakaguchi, Hideki Sakai, Masahiko Abe

    Effects of stabilizer (poly(N-vinyl-2-pyrrolidone), PVP) concentration on the electrochemical performance of Au-Pt bimetallic (Au4Pt) anode catalysts for direct glucose fuel cell (DGFC) have been investigated. In the cyclic voltammetry, the maximum current density was recorded at [PVP] / [metal] = 1 in molar ratio for the carbon supported metal nanoparticle catalysts at 5 wt% metal loading. At lower PVP concentrations, the current density decreased due to aggregation of metal nanoparticles, while at higher PVP concentrations, the current density also decreased, presumably due to loss of active surface area of the metal catalyst by passivating with the stabilizer. Also for the full cell systems, the maximum power density was recorded at [PVP] / [metal] = 1. When the optimal stabilizer condition was applied to the full cell system, the maximum power density of 12.7 mW cm-2 at 0.38 V vs Ag | AgCl and the open circuit voltage of 0.85 V were recorded. Furthermore, a set of 10 stacked cells was able to light 6 LED lamps of total 1 W for over 60 h without flowing the glucose fuel. These results demonstrate that the present DGFC system can be applied as a power supply for LED illuminating systems.