Erik Asmussen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Erik Asmussen has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
A Peutzfeldt
9 shared publicationsA Sahafi
Department of Dental Materials, School of Dentistry, University of Copenhagen, Denmark
2 shared publicationsAnne Peutzfeldt
Department of Dental Materials, School of Dentistry, Faculty of Health Sciences, University of Copenhagen, Copenhagen, Denmark
2 shared publicationsE K Hansen
2 shared publications- Erik Christian Munksgaard
Department of Dental Materials, School of Dentistry, Faculty of Health Sciences, University of Copenhagen, Denmark
1 shared publication Erik Keith Hansen
Department of Dental Materials, School of Dentistry, University of Copenhagen, Denmark
1 shared publication
Latest Publications
- 1 January 2002
- Published by Medical Journals Sweden AB in Acta Odontologica Scandinavica
- Vol. 60 (3) , 146-150
Influence of composition on rate of polymerization contraction of light-curing resin composites
A slow contraction may result in reduced gap formation when a restorative resin polymerizes in a dental cavity. It was the aim in the present work to investigate the rate of contraction in relation to composition of experimental light-curing resin composites. The monomer of the resin composites consisted of mixtures of BisGMA, TEGDMA, and in one series HEMA. The resins contained varying amounts of initiators, co-initiators, and inhibitor, and were made composite by adding a silanized glass filler to a content of 74% by weight of the composite paste. The polymerization contraction up to 120 sec was determined by means of the bonded-disk method. Within the ranges studied, the concentration of initiator and co-initiator in the monomer mixture had only an insignificant influence on rate of polymerization. In comparison to camphorquinone, the initiators 1-phenyl-1,2-propanedione and benzil reduced the rate of polymerization without affecting the final contraction. In comparison to N,N-dimethyl- p -aminobenzoic acid ethyl ester, N,N-cyanoethyl methylaniline was as effective, while N,N-diethanol- p -toluidine was less effective as co-initiator. A relatively high content of the inhibitor methoxyhydroquinone reduced the initial rate but not the final polymerization contraction. The rate of polymerization increased with the level of HEMA and TEGDMA in the monomer mixture. It was concluded that intrinsic slow cure may be obtained with certain compositions of resin composites without impairing the final extent of polymerization.
- 1 January 2002
- Published by Medical Journals Sweden AB in Acta Odontologica Scandinavica
- Vol. 60 (3) , 146-150
Influence of composition on rate of polymerization contraction of light-curing resin composites
A slow contraction may result in reduced gap formation when a restorative resin polymerizes in a dental cavity. It was the aim in the present work to investigate the rate of contraction in relation to composition of experimental light-curing resin composites. The monomer of the resin composites consisted of mixtures of BisGMA, TEGDMA, and in one series HEMA. The resins contained varying amounts of initiators, co-initiators, and inhibitor, and were made composite by adding a silanized glass filler to a content of 74% by weight of the composite paste. The polymerization contraction up to 120 sec was determined by means of the bonded-disk method. Within the ranges studied, the concentration of initiator and co-initiator in the monomer mixture had only an insignificant influence on rate of polymerization. In comparison to camphorquinone, the initiators 1-phenyl-1,2-propanedione and benzil reduced the rate of polymerization without affecting the final contraction. In comparison to N,N-dimethyl- p -aminobenzoic acid ethyl ester, N,N-cyanoethyl methylaniline was as effective, while N,N-diethanol- p -toluidine was less effective as co-initiator. A relatively high content of the inhibitor methoxyhydroquinone reduced the initial rate but not the final polymerization contraction. The rate of polymerization increased with the level of HEMA and TEGDMA in the monomer mixture. It was concluded that intrinsic slow cure may be obtained with certain compositions of resin composites without impairing the final extent of polymerization.
- 1 October 2001
- Vol. 14 (5) , 295-6
Effect of pulse-delay curing on in vitro wall-to-wall contraction of composite in dentin cavity preparations.
To determine the effect of pulse-delay curing of resin composite on marginal gap formation in dentin cavity preparations. Cylindrical cavities were prepared in extracted human molar dentin and were distributed into 8 groups (A-H). The cavity preparations were treated with a dentin-bonding agent (Prime & Bond NT) and filled with a light-cured resin composite (Z100). The restorations were irradiated initially for 1, 2 or 3 seconds at a power density of 425 mW/cm2. Following water storage for varying time intervals, the restorations were re-exposed for 10 seconds at 750 mW/cm2. Marginal gap formation was measured by light microscopy after 20 minutes of water-storage, and the wall-to-wall contraction was calculated as the widest gap in percent of cavity diameter. Pulse-delay curing in combination with a waiting time of at least 1 minute between exposures reduced wall-to-wall contraction in dentin cavities compared to continuous-cure control.
- 1 October 2001
- Vol. 14 (5) , 295-6
Effect of pulse-delay curing on in vitro wall-to-wall contraction of composite in dentin cavity preparations.
To determine the effect of pulse-delay curing of resin composite on marginal gap formation in dentin cavity preparations. Cylindrical cavities were prepared in extracted human molar dentin and were distributed into 8 groups (A-H). The cavity preparations were treated with a dentin-bonding agent (Prime & Bond NT) and filled with a light-cured resin composite (Z100). The restorations were irradiated initially for 1, 2 or 3 seconds at a power density of 425 mW/cm2. Following water storage for varying time intervals, the restorations were re-exposed for 10 seconds at 750 mW/cm2. Marginal gap formation was measured by light microscopy after 20 minutes of water-storage, and the wall-to-wall contraction was calculated as the widest gap in percent of cavity diameter. Pulse-delay curing in combination with a waiting time of at least 1 minute between exposures reduced wall-to-wall contraction in dentin cavities compared to continuous-cure control.
- 1 June 2001
- Vol. 14 (3) , 145-7
Soft-start polymerization and marginal gap formation in vitro.
To determine the effect of soft-start polymerization of resin-based composites on the marginal gap formation in dentin cavities. Cylindrical cavities were prepared in dentin in extracted human molars. The cavities were distributed into 8 groups. The teeth in groups 1-4 were treated with Scotchbond Multi-Purpose and restored with Z100, and the teeth in groups 5-8 were treated with OptiBond FL and restored with Herculite XRV. The restorations were light-cured for 40 s by four different curing modes. The marginal gap formation was measured in a light microscope after a 20 min water-storage, and the wall-to-wall contraction was calculated as the widest gap in percent of the cavity diameter. Soft-start light curing did not influence wall-to-wall contraction in dentin cavities. OptiBond FL and Herculite XRV showed less wall-to-wall contraction than did Scotchbond Multi-Purpose and Z100. The soft-start polymerization procedures studied did not improve the marginal adaptation of two resin composites bonded to dentin cavities compared with conventional polymerization.
- 1 June 2001
- Vol. 14 (3) , 145-7
Soft-start polymerization and marginal gap formation in vitro.
To determine the effect of soft-start polymerization of resin-based composites on the marginal gap formation in dentin cavities. Cylindrical cavities were prepared in dentin in extracted human molars. The cavities were distributed into 8 groups. The teeth in groups 1-4 were treated with Scotchbond Multi-Purpose and restored with Z100, and the teeth in groups 5-8 were treated with OptiBond FL and restored with Herculite XRV. The restorations were light-cured for 40 s by four different curing modes. The marginal gap formation was measured in a light microscope after a 20 min water-storage, and the wall-to-wall contraction was calculated as the widest gap in percent of the cavity diameter. Soft-start light curing did not influence wall-to-wall contraction in dentin cavities. OptiBond FL and Herculite XRV showed less wall-to-wall contraction than did Scotchbond Multi-Purpose and Z100. The soft-start polymerization procedures studied did not improve the marginal adaptation of two resin composites bonded to dentin cavities compared with conventional polymerization.
- 1 January 1998
- Published by Elsevier in Dental Materials
- Vol. 14 (1) , 51-56
Influence of UEDMA, BisGMA and TEGDMA on selected mechanical properties of experimental resin composites
- 1 January 1998
- Published by Elsevier in Dental Materials
- Vol. 14 (1) , 51-56
Influence of UEDMA, BisGMA and TEGDMA on selected mechanical properties of experimental resin composites
- 1 October 1997
- Published by Wiley in European Journal of Oral Sciences
- Vol. 105 (5P1) , 434-439
Improved efficacy of dentin‐bonding agents
Dentin cavities, prepared in extracted human teeth, were treated with various proprietary dentin‐bonding agents and then filled with a light‐cured restorative resin for posterior use. All bonding agents were either treated in accordance with the manufacturers' instructions or combined with Gluma, which is an aqueous solution of glutaraldehyde and HEMA, a hydrophilic monomer. 10 min after polymerization, the width and the extent of the marginal contraction gap was measured approximately 0.1 mm below the free surface of the filling, using a light microscope. With nearly all dentin‐bonding agents, the marginal contraction gap could be significantly reduced if Gluma was used after conditioning of the dentin. The reason for this improvement may be that glutaraldehyde cross‐links the collagen fibers and thereby strengthens the organic part of the hybrid layer, however, other mechanisms might also play a role in the improvement found.
- 1 October 1997
- Published by Wiley in European Journal of Oral Sciences
- Vol. 105 (5P1) , 434-439
Improved efficacy of dentin‐bonding agents
Dentin cavities, prepared in extracted human teeth, were treated with various proprietary dentin‐bonding agents and then filled with a light‐cured restorative resin for posterior use. All bonding agents were either treated in accordance with the manufacturers' instructions or combined with Gluma, which is an aqueous solution of glutaraldehyde and HEMA, a hydrophilic monomer. 10 min after polymerization, the width and the extent of the marginal contraction gap was measured approximately 0.1 mm below the free surface of the filling, using a light microscope. With nearly all dentin‐bonding agents, the marginal contraction gap could be significantly reduced if Gluma was used after conditioning of the dentin. The reason for this improvement may be that glutaraldehyde cross‐links the collagen fibers and thereby strengthens the organic part of the hybrid layer, however, other mechanisms might also play a role in the improvement found.
- 1 February 1997
- Vol. 10 (1) , 15-7
Surface hardness and wear of glass ionomers and compomers.
To determine the surface hardness and in vitro wear of glass ionomer cements (GIC) and compomers in comparison with a resin composite and to test for a possible correlation between the determined hardness and wear values. Samples were made of conventional GIC (Ketac-Fil, Fuji II, Fuji IX, Ketac-Prototype = Ketac-Molar), resin-modified GIC (Photac-Fil, Fuji II LC, Vitremer), compomers (Dyract, Compoglass) and resin composite (Z100) for the hardness test (n = 10) and for the wear test (n = 3). The materials were handled according to the manufacturers' instructions. The samples were stored in deionized water for 48 hours at 37 degrees C prior to the determination of Rockwell hardness and three-body in vitro wear. Hardness could not be measured on Ketac-Fil and Fuji II as the samples fractured before a reading was obtainable. Statistically significant differences were found in hardness and wear between brands and between the four types of material. Surface hardness: resin-modified GIC < conventional GIC = compomers < resin composite. In vitro wear: resin-modified GIC > compomers > conventional GIC > resin composite. A negative correlation between hardness and wear was recorded.
- 1 February 1997
- Vol. 10 (1) , 15-7
Surface hardness and wear of glass ionomers and compomers.
To determine the surface hardness and in vitro wear of glass ionomer cements (GIC) and compomers in comparison with a resin composite and to test for a possible correlation between the determined hardness and wear values. Samples were made of conventional GIC (Ketac-Fil, Fuji II, Fuji IX, Ketac-Prototype = Ketac-Molar), resin-modified GIC (Photac-Fil, Fuji II LC, Vitremer), compomers (Dyract, Compoglass) and resin composite (Z100) for the hardness test (n = 10) and for the wear test (n = 3). The materials were handled according to the manufacturers' instructions. The samples were stored in deionized water for 48 hours at 37 degrees C prior to the determination of Rockwell hardness and three-body in vitro wear. Hardness could not be measured on Ketac-Fil and Fuji II as the samples fractured before a reading was obtainable. Statistically significant differences were found in hardness and wear between brands and between the four types of material. Surface hardness: resin-modified GIC < conventional GIC = compomers < resin composite. In vitro wear: resin-modified GIC > compomers > conventional GIC > resin composite. A negative correlation between hardness and wear was recorded.
- 1 April 1996
- Vol. 9 (2) , 65-6
Distortion of alloy by sandblasting.
To measure distortion of alloy plates caused by sandblasting, and to determine the influence on degree of distortion of type of alloy, plate thickness, and sandblasting conditions i.e. particle size of alumina, air pressure, and duration of blasting period. Plates were cast in a noble alloy and in a Co-Cr alloy. One end of the plates was fastened in a device, and the projecting 20 mm of the plates was sandblasted. Distortion was determined as the deflection of the plates at a distance of 20 mm from the mounting device. The mean deflections varied between 0.37 mm and 1.72 mm. Plates of Co-Cr alloy showed less deflection than did plates of noble alloy. Deflection was increased by an increase in duration of the blasting, pressure, particle size of the alumina, and by a decrease in plate thickness.
- 1 April 1996
- Vol. 9 (2) , 65-6
Distortion of alloy by sandblasting.
To measure distortion of alloy plates caused by sandblasting, and to determine the influence on degree of distortion of type of alloy, plate thickness, and sandblasting conditions i.e. particle size of alumina, air pressure, and duration of blasting period. Plates were cast in a noble alloy and in a Co-Cr alloy. One end of the plates was fastened in a device, and the projecting 20 mm of the plates was sandblasted. Distortion was determined as the deflection of the plates at a distance of 20 mm from the mounting device. The mean deflections varied between 0.37 mm and 1.72 mm. Plates of Co-Cr alloy showed less deflection than did plates of noble alloy. Deflection was increased by an increase in duration of the blasting, pressure, particle size of the alumina, and by a decrease in plate thickness.
- 1 August 1991
- Vol. 95 (11) , 469-72
[Retention of composite inlays in enamel-dentin cavities].
The retention of composite inlays depends on acid-etching of marginal enamel of the preparation. In many cases, only little marginal enamel is available, making loss of retention a liability. The present study evaluated the retention of three brands of composite inlays under various conditions. Inlays were fabricated and cemented in standardized enamel/dentin cavities prepared in extracted human teeth. The force necessary to extract a cemented inlay was used to express the retention of the inlay. The effects of thermocycling and choice of dentin-bonding agent on inlay retention were also determined. Inlays made of Estilux posterior C VS were more retentive than inlays of either Brilliant Dentin or SR-Isosit. The latter two products were found to provide similar retentive strengths. The retention of Estilux posterior C VS and SR-isosit inlays declined when samples were thermocycled. Treatment with Gluma increased retention of inlays, resulting in retentive strengths of the same magnitude for all three inlay systems. The choice of dentin-bonding agent was found to affect composite inlay retention to a greater extent than the choice of either composite brand, mode of inlay curing, or effect of thermocycling.
- 1 August 1991
- Vol. 95 (11) , 469-72
[Retention of composite inlays in enamel-dentin cavities].
The retention of composite inlays depends on acid-etching of marginal enamel of the preparation. In many cases, only little marginal enamel is available, making loss of retention a liability. The present study evaluated the retention of three brands of composite inlays under various conditions. Inlays were fabricated and cemented in standardized enamel/dentin cavities prepared in extracted human teeth. The force necessary to extract a cemented inlay was used to express the retention of the inlay. The effects of thermocycling and choice of dentin-bonding agent on inlay retention were also determined. Inlays made of Estilux posterior C VS were more retentive than inlays of either Brilliant Dentin or SR-Isosit. The latter two products were found to provide similar retentive strengths. The retention of Estilux posterior C VS and SR-isosit inlays declined when samples were thermocycled. Treatment with Gluma increased retention of inlays, resulting in retentive strengths of the same magnitude for all three inlay systems. The choice of dentin-bonding agent was found to affect composite inlay retention to a greater extent than the choice of either composite brand, mode of inlay curing, or effect of thermocycling.
- 1 May 1991
- Vol. 96 (7) , 291-3
[Color stability of three composite resins used in the inlay/onlay technique].
The color stability of three composite resins used in the inlay/onlay technique was determined by means of irradiation with UV-light and by water storage. Generally, water storage resulted in greater changes in color than did UV-light, but no correlation was found between the results of the two chromogenic procedures. The microfilled composite resin was the least color stable, but none of the resins had alarmingly low color stability.
- 1 May 1991
- Vol. 96 (7) , 291-3
[Color stability of three composite resins used in the inlay/onlay technique].
The color stability of three composite resins used in the inlay/onlay technique was determined by means of irradiation with UV-light and by water storage. Generally, water storage resulted in greater changes in color than did UV-light, but no correlation was found between the results of the two chromogenic procedures. The microfilled composite resin was the least color stable, but none of the resins had alarmingly low color stability.
- 1 April 1991
- Vol. 95 (6) , 243-6
[A comparison of accuracy in seating and gap formation for three inlay/onlay techniques].
The accuracy (fit) of MOD inlays of three brands of composite resin was determined by measuring the axial discrepancy (marginal opening in the approximal area). The axial discrepancy varied between 17 and 121 microns. Directly manufactured inlays were more accurate (axial discrepancy: 17-26 microns) than indirectly manufactured inlays (axial discrepancy: 40-121 microns). Inlays of a microfilled resin, SR-Isosit, were less accurate than inlays of two hybrid materials, Brilliant Dentin and Estilux posterior C VS (axial discrepancy: 121 microns vs 44 and 41 microns respectively). There was a tendency for 24-hour-old inlays to be less accurate than 10-min-old inlays. The formation of marginal gaps due to contraction of the resin cement was assessed in a light microscope on cemented single-surfaced inlays. Gaps were not formed when enamel margins were etched or dentin margins treated with a dentin-bonding agent of high efficacy. Gaps (2.4-5.6 microns) were formed, however, at untreated dentin margins and at margins treated with dentin-bonding agents of low efficacy.
- 1 April 1991
- Vol. 95 (6) , 243-6
[A comparison of accuracy in seating and gap formation for three inlay/onlay techniques].
The accuracy (fit) of MOD inlays of three brands of composite resin was determined by measuring the axial discrepancy (marginal opening in the approximal area). The axial discrepancy varied between 17 and 121 microns. Directly manufactured inlays were more accurate (axial discrepancy: 17-26 microns) than indirectly manufactured inlays (axial discrepancy: 40-121 microns). Inlays of a microfilled resin, SR-Isosit, were less accurate than inlays of two hybrid materials, Brilliant Dentin and Estilux posterior C VS (axial discrepancy: 121 microns vs 44 and 41 microns respectively). There was a tendency for 24-hour-old inlays to be less accurate than 10-min-old inlays. The formation of marginal gaps due to contraction of the resin cement was assessed in a light microscope on cemented single-surfaced inlays. Gaps were not formed when enamel margins were etched or dentin margins treated with a dentin-bonding agent of high efficacy. Gaps (2.4-5.6 microns) were formed, however, at untreated dentin margins and at margins treated with dentin-bonding agents of low efficacy.