Michael Reich
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Michael Reich has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
- Olaf Kessler
Faculty of Mechanical Engineering and Marine Technology, Chair of Material Science, University of Rostock, Rostock, Germany
8 shared publications - Hannes Fröck
Faculty of Mechanical Engineering and Marine Technology, Chair of Materials Science, University of Rostock, Rostock, Germany
5 shared publications - Benjamin Milkereit
Chair of Materials Science, Faculty of Mechanical Engineering and Marine Technology, University of Rostock, Justus-von-Liebig-Weg 2, 18059 Rostock, Germany
4 shared publications - Armin Springer
Department Life, Light & Matter, University of Rostock, Rostock, Germany
2 shared publications - Manuela Sander
Institute of Structural Mechanics, Faculty of Mechanical Engineering and Marine Technology, University of Rostock, Albert Einstein-Str. 2, 18059 Rostock, Germany
2 shared publications - Marion Merklein
Institute of Manufacturing Technology, Friedrich-Alexander-Universität Erlangen-Nürnberg, Erlangen, Germany
2 shared publications
Latest Publications
- Open Access
Development of Precipitation Hardening Parameters for High Strength Alloy AA 7068
The mechanical properties after age hardening heat treatment and the kinetics of related phase transformations of high strength AlZnMgCu alloy AA 7068 were investigated. The experimental work includes differential scanning calorimetry (DSC), differential fast scanning calorimetry (DFSC), sophisticated differential dilatometry (DIL), scanning electron microscopy (SEM), as well as hardness and tensile tests. For the kinetic analysis of quench induced precipitation by dilatometry new metrological methods and evaluation procedures were established. Using DSC, dissolution behaviour during heating to solution annealing temperature was investigated. These experiments allowed for identification of the appropriate temperature and duration for the solution heat treatment. Continuous cooling experiments in DSC, DFSC, and DIL determined the kinetics of quench induced precipitation. DSC and DIL revealed several overlapping precipitation reactions. The critical cooling rate for a complete supersaturation of the solid solution has been identified to be 600 to 800 K/s. At slightly subcritical cooling rates quench induced precipitation results in a direct hardening effect resulting in a technological critical cooling rate of about 100 K/s, i.e., the hardness after ageing reaches a saturation level for cooling rates faster than 100 K/s. Maximum yield strength of above 600 MPa and tensile strength of up to 650 MPa were attained.
Open AccessDevelopment of Precipitation Hardening Parameters for High Strength Alloy AA 7068
The mechanical properties after age hardening heat treatment and the kinetics of related phase transformations of high strength AlZnMgCu alloy AA 7068 were investigated. The experimental work includes differential scanning calorimetry (DSC), differential fast scanning calorimetry (DFSC), sophisticated differential dilatometry (DIL), scanning electron microscopy (SEM), as well as hardness and tensile tests. For the kinetic analysis of quench induced precipitation by dilatometry new metrological methods and evaluation procedures were established. Using DSC, dissolution behaviour during heating to solution annealing temperature was investigated. These experiments allowed for identification of the appropriate temperature and duration for the solution heat treatment. Continuous cooling experiments in DSC, DFSC, and DIL determined the kinetics of quench induced precipitation. DSC and DIL revealed several overlapping precipitation reactions. The critical cooling rate for a complete supersaturation of the solid solution has been identified to be 600 to 800 K/s. At slightly subcritical cooling rates quench induced precipitation results in a direct hardening effect resulting in a technological critical cooling rate of about 100 K/s, i.e., the hardness after ageing reaches a saturation level for cooling rates faster than 100 K/s. Maximum yield strength of above 600 MPa and tensile strength of up to 650 MPa were attained.
- Open Access
A Phenomenological Mechanical Material Model for Precipitation Hardening Aluminium Alloys
Age hardening aluminium alloys obtain their strength by forming precipitates. This precipitation-hardened state is often the initial condition for short-term heat treatments, like welding processes or local laser heat treatment to produce tailored heat-treated profiles (THTP). During these heat treatments, the strength-increasing precipitates are dissolved depending on the maximum temperature and the material is softened in these areas. Depending on the temperature path, the mechanical properties differ between heating and cooling at the same temperature. To model this behavior, a phenomenological material model was developed based on the dissolution characteristics and experimental flow curves were developed depending on the current temperature and the maximum temperature. The dissolution characteristics were analyzed by calorimetry. The mechanical properties at different temperatures and peak temperatures were recorded by thermomechanical analysis. The usual phase transformation equations in the Finite Element Method (FEM) code, which were developed for phase transformation in steels, were used to develop a phenomenological model for the mechanical properties as a function of the relevant heat treatment parameters. This material model was implemented for aluminium alloy 6060 T4 in the finite element software LS-DYNA (Livermore Software Technology Corporation).
Open AccessA Phenomenological Mechanical Material Model for Precipitation Hardening Aluminium Alloys
Age hardening aluminium alloys obtain their strength by forming precipitates. This precipitation-hardened state is often the initial condition for short-term heat treatments, like welding processes or local laser heat treatment to produce tailored heat-treated profiles (THTP). During these heat treatments, the strength-increasing precipitates are dissolved depending on the maximum temperature and the material is softened in these areas. Depending on the temperature path, the mechanical properties differ between heating and cooling at the same temperature. To model this behavior, a phenomenological material model was developed based on the dissolution characteristics and experimental flow curves were developed depending on the current temperature and the maximum temperature. The dissolution characteristics were analyzed by calorimetry. The mechanical properties at different temperatures and peak temperatures were recorded by thermomechanical analysis. The usual phase transformation equations in the Finite Element Method (FEM) code, which were developed for phase transformation in steels, were used to develop a phenomenological model for the mechanical properties as a function of the relevant heat treatment parameters. This material model was implemented for aluminium alloy 6060 T4 in the finite element software LS-DYNA (Livermore Software Technology Corporation).
- Open Access
Scanning Rate Extension of Conventional DSCs through Indirect Measurements
In this work, a method is presented which allows the determination of calorimetric information, and thus, information about the precipitation and dissolution behavior of aluminum alloys during heating rates that could not be previously measured. Differential scanning calorimetry (DSC) is an established method for in-situ recording of dissolution and precipitation reactions in various aluminum alloys. Diverse types of DSC devices are suitable for different ranges of scanning rates. A combination of the various available commercial devices enables heating and cooling rates from 10−4 to 5 Ks−1 to be covered. However, in some manufacturing steps of aluminum alloys, heating rates up to several 100 Ks−1 are important. Currently, conventional DSC cannot achieve these high heating rates and they are still too slow for the chip-sensor based fast scanning calorimetry. In order to fill the gap, an indirect measurement method has been developed, which allows the determination of qualitative information, regarding the precipitation state, at various points of any heat treatment. Different rapid heat treatments were carried out on samples of an alloy EN AW-6082 in a quenching dilatometer and terminated at defined temperatures. Subsequent reheating of the samples in the DSC enables analysis of the precipitation state of the heat-treated samples. This method allows for previously un-measurable heat treatments to get information about the occurring precipitation and dissolution reactions during short-term heat treatments.
Open AccessScanning Rate Extension of Conventional DSCs through Indirect Measurements
In this work, a method is presented which allows the determination of calorimetric information, and thus, information about the precipitation and dissolution behavior of aluminum alloys during heating rates that could not be previously measured. Differential scanning calorimetry (DSC) is an established method for in-situ recording of dissolution and precipitation reactions in various aluminum alloys. Diverse types of DSC devices are suitable for different ranges of scanning rates. A combination of the various available commercial devices enables heating and cooling rates from 10−4 to 5 Ks−1 to be covered. However, in some manufacturing steps of aluminum alloys, heating rates up to several 100 Ks−1 are important. Currently, conventional DSC cannot achieve these high heating rates and they are still too slow for the chip-sensor based fast scanning calorimetry. In order to fill the gap, an indirect measurement method has been developed, which allows the determination of qualitative information, regarding the precipitation state, at various points of any heat treatment. Different rapid heat treatments were carried out on samples of an alloy EN AW-6082 in a quenching dilatometer and terminated at defined temperatures. Subsequent reheating of the samples in the DSC enables analysis of the precipitation state of the heat-treated samples. This method allows for previously un-measurable heat treatments to get information about the occurring precipitation and dissolution reactions during short-term heat treatments.
- Open Access
Combined Calorimetry, Thermo-Mechanical Analysis and Tensile Test on Welded EN AW-6082 Joints
Wide softening zones are typical for welded joints of age hardened aluminium alloys. In this study, the microstructure evolution and distribution of mechanical properties resulting from welding processes of the aluminium alloy EN AW-6082 (AlSi1MgMn) was analysed by both in-situ and ex-situ investigations. The in-situ thermal analyses included differential scanning calorimetry (DSC), which was used to characterise the dissolution and precipitation behaviour in the heat affected zone (HAZ) of welded joints. Thermo-mechanical analysis (TMA) by means of compression tests was used to determine the mechanical properties of various states of the microstructure after the welding heat input. The necessary temperature–time courses in the HAZ for these methods were measured using thermocouples during welding. Additionally, ex-situ tensile tests were done both on specimens from the fusion zone and on welded joints, and their in-depth analysis with digital image correlation (DIC) accompanied by finite element simulations serve for the description of flow curves in different areas of the weld. The combination of these methods and the discussion of their results make an essential contribution to understand the influence of welding heat on the material properties, particularly on the softening behaviour. Furthermore, the distributed strength characteristic of the welded connections is required for an applicable estimation of the load-bearing capacity of welded aluminium structures by numerical methods.
Open AccessCombined Calorimetry, Thermo-Mechanical Analysis and Tensile Test on Welded EN AW-6082 Joints
Wide softening zones are typical for welded joints of age hardened aluminium alloys. In this study, the microstructure evolution and distribution of mechanical properties resulting from welding processes of the aluminium alloy EN AW-6082 (AlSi1MgMn) was analysed by both in-situ and ex-situ investigations. The in-situ thermal analyses included differential scanning calorimetry (DSC), which was used to characterise the dissolution and precipitation behaviour in the heat affected zone (HAZ) of welded joints. Thermo-mechanical analysis (TMA) by means of compression tests was used to determine the mechanical properties of various states of the microstructure after the welding heat input. The necessary temperature–time courses in the HAZ for these methods were measured using thermocouples during welding. Additionally, ex-situ tensile tests were done both on specimens from the fusion zone and on welded joints, and their in-depth analysis with digital image correlation (DIC) accompanied by finite element simulations serve for the description of flow curves in different areas of the weld. The combination of these methods and the discussion of their results make an essential contribution to understand the influence of welding heat on the material properties, particularly on the softening behaviour. Furthermore, the distributed strength characteristic of the welded connections is required for an applicable estimation of the load-bearing capacity of welded aluminium structures by numerical methods.
- Open Access
Influence of Solution-Annealing Parameters on the Continuous Cooling Precipitation of Aluminum Alloy 6082
We use a systematic approach to investigate the influence of the specific solution condition on quench-induced precipitation of coarse secondary phase particles during subsequent cooling for a wide range of cooling rates. Commercially produced plate material of aluminum alloy EN AW-6082 was investigated and the applied solution treatment conditions were chosen based on heating differential scanning calorimetry experiments of the initial T651 condition. The kinetics of the quench-induced precipitation were investigated by in situ cooling differential scanning calorimetry for a wide range of cooling rates. The nature of those quench-induced precipitates was analyzed by electron microscopy. The experimental data was evaluated with respect to the detrimental effect of incomplete dissolution on the age-hardening potential. We show that if the chosen solution temperature and soaking duration are too low or short, the solution treatment results in an incomplete dissolution of secondary phase particles. This involves precipitation during subsequent cooling to start concurrently with the onset of cooling, which increases the quench sensitivity. However, if the solution conditions allow the formation of a complete solid solution, precipitation will start after a certain degree of undercooling, thus keeping the upper critical cooling rate at the usual alloy-specific level.
Open AccessInfluence of Solution-Annealing Parameters on the Continuous Cooling Precipitation of Aluminum Alloy 6082
We use a systematic approach to investigate the influence of the specific solution condition on quench-induced precipitation of coarse secondary phase particles during subsequent cooling for a wide range of cooling rates. Commercially produced plate material of aluminum alloy EN AW-6082 was investigated and the applied solution treatment conditions were chosen based on heating differential scanning calorimetry experiments of the initial T651 condition. The kinetics of the quench-induced precipitation were investigated by in situ cooling differential scanning calorimetry for a wide range of cooling rates. The nature of those quench-induced precipitates was analyzed by electron microscopy. The experimental data was evaluated with respect to the detrimental effect of incomplete dissolution on the age-hardening potential. We show that if the chosen solution temperature and soaking duration are too low or short, the solution treatment results in an incomplete dissolution of secondary phase particles. This involves precipitation during subsequent cooling to start concurrently with the onset of cooling, which increases the quench sensitivity. However, if the solution conditions allow the formation of a complete solid solution, precipitation will start after a certain degree of undercooling, thus keeping the upper critical cooling rate at the usual alloy-specific level.
- 17 June 2016
- Published by Springer Nature in Production Engineering
- Vol. 10 (4-5) , 383-389
Influence of short-term heat treatment on the microstructure and mechanical properties of EN AW-6060 T4 extrusion profiles: Part A
- 17 June 2016
- Published by Springer Nature in Production Engineering
- Vol. 10 (4-5) , 383-389
Influence of short-term heat treatment on the microstructure and mechanical properties of EN AW-6060 T4 extrusion profiles: Part A
- 16 June 2016
- Published by Springer Nature in Production Engineering
- Vol. 10 (4-5) , 391-398
Influence of short-term heat treatment on the microstructure and mechanical properties of EN AW-6060 T4 extrusion profiles—Part B
- 16 June 2016
- Published by Springer Nature in Production Engineering
- Vol. 10 (4-5) , 391-398
Influence of short-term heat treatment on the microstructure and mechanical properties of EN AW-6060 T4 extrusion profiles—Part B
- 10 December 2013
- Published by Walter de Gruyter GmbH in HTM Journal of Heat Treatment and Materials
- Vol. 68 (6) , 274-282
Kalorimetrische und dilatometrische Analyse des Anlassverhaltens in der Wärmeeinflusszone von Schweißnähten des Stahls T24
Kurzfassung: Der Werkstoff 7CrMoVTiB10-10 (T24) wurde als warmfester Stahl für den Einsatz in der Membranwand neuer Kohlekraftwerke der 600/620°C-Klasse entwickelt. Trotz seiner umfangreichen Qualifizierung kam es zu Schäden bei der Inbetriebnahme durch Spannungsrisskorrosion. Zur Reduzierung der Spannungsrisskorrosionsempfindlichkeit wurden verschiedene Anlassbehandlungen durchgeführt. Grundlegende Untersuchungen sollen nun die Prozesse beleuchten, die bei diesen Glühbehandlungen ablaufen. Für die geplanten Untersuchungen wurde Probenmaterial aus zwei nahtlosen Rohren (aus unterschiedlichen Schmelzen) des Stahls T24 entnommen. In den Proben wurde anhand von Wärmebehandlungen in einem Dilatometer ein Schweißgefüge eingestellt, wie es in der Wärmeeinflusszone (WEZ) der Schweißverbindungen auftritt. An diesem Probenmaterial erfolgten anschließend unterschiedliche Anlassbehandlungen. Die sich einstellenden Gefügeveränderungen wurden in Abhängigkeit von der Erwärmrate bzw. Anlasstemperatur und -dauer durch kalorimetrische und dilatometrische Analysen charakterisiert. Hierzu wurden Proben kontinuierlich in verschiedenen DSC-Geräten und in einem Dilatometer mit Heizraten zwischen 0,02 K/s und 100 K/s erwärmt. Zusätzlich erfolgten isotherme Glühbehandlungen dieser Proben mit Temperaturen zwischen 450 °C und 700 °C im Dilatometer. Die Ergebnisse der Dilatometrie und Kalorimetrie lassen auf mehrere Anlassreaktionen schließen. Die Ergebnisse erlauben eine Zuordnung der beobachteten Reaktionen zu den in der Literatur beschriebenen Anlassstufen und somit eine gezielte Gestaltung der Anlassbehandlung der geschweißten T24-Verbindungen zur Reduzierung ihrer Rissanfälligkeit im laufenden Betrieb.
- 10 December 2013
- Published by Walter de Gruyter GmbH in HTM Journal of Heat Treatment and Materials
- Vol. 68 (6) , 274-282
Kalorimetrische und dilatometrische Analyse des Anlassverhaltens in der Wärmeeinflusszone von Schweißnähten des Stahls T24
Kurzfassung: Der Werkstoff 7CrMoVTiB10-10 (T24) wurde als warmfester Stahl für den Einsatz in der Membranwand neuer Kohlekraftwerke der 600/620°C-Klasse entwickelt. Trotz seiner umfangreichen Qualifizierung kam es zu Schäden bei der Inbetriebnahme durch Spannungsrisskorrosion. Zur Reduzierung der Spannungsrisskorrosionsempfindlichkeit wurden verschiedene Anlassbehandlungen durchgeführt. Grundlegende Untersuchungen sollen nun die Prozesse beleuchten, die bei diesen Glühbehandlungen ablaufen. Für die geplanten Untersuchungen wurde Probenmaterial aus zwei nahtlosen Rohren (aus unterschiedlichen Schmelzen) des Stahls T24 entnommen. In den Proben wurde anhand von Wärmebehandlungen in einem Dilatometer ein Schweißgefüge eingestellt, wie es in der Wärmeeinflusszone (WEZ) der Schweißverbindungen auftritt. An diesem Probenmaterial erfolgten anschließend unterschiedliche Anlassbehandlungen. Die sich einstellenden Gefügeveränderungen wurden in Abhängigkeit von der Erwärmrate bzw. Anlasstemperatur und -dauer durch kalorimetrische und dilatometrische Analysen charakterisiert. Hierzu wurden Proben kontinuierlich in verschiedenen DSC-Geräten und in einem Dilatometer mit Heizraten zwischen 0,02 K/s und 100 K/s erwärmt. Zusätzlich erfolgten isotherme Glühbehandlungen dieser Proben mit Temperaturen zwischen 450 °C und 700 °C im Dilatometer. Die Ergebnisse der Dilatometrie und Kalorimetrie lassen auf mehrere Anlassreaktionen schließen. Die Ergebnisse erlauben eine Zuordnung der beobachteten Reaktionen zu den in der Literatur beschriebenen Anlassstufen und somit eine gezielte Gestaltung der Anlassbehandlung der geschweißten T24-Verbindungen zur Reduzierung ihrer Rissanfälligkeit im laufenden Betrieb.
- 1 May 2009
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 40 (5-6) , 473-478
Similarities and differences in heat treatment simulation of aluminium alloys and steels
- 1 May 2009
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 40 (5-6) , 473-478
Similarities and differences in heat treatment simulation of aluminium alloys and steels