Maria Åkerfeldt
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Maria Åkerfeldt has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- Erik Nilsson
Materials Department Swerea IVF Box 104, SE‐431 22 Mölndal Sweden
1 shared publication Martin Strååt
Department of Textiles and Plastics, Swerea IVF, Sweden
1 shared publicationPernilla Walkenström
Department of Textiles and Plastics, Swerea IVF, Sweden
1 shared publication- Pernilla Walkenström
Textiles and Plastics Department
1 shared publication - Philip Gillgard
Textiles and Plastics Department
1 shared publication
Latest Publications
- Open Access
- 25 September 2014
- Published by Springer Nature in Fashion and Textiles
- Vol. 1 (1) , 1-17
Textile piezoelectric sensors – melt spun bi-component poly(vinylidene fluoride) fibres with conductive cores and poly(3,4-ethylene dioxythiophene)-poly(styrene sulfonate) coating as the outer electrode
The work presented here addresses the outer electroding of a fully textile piezoelectric strain sensor, consisting of bi-component fibre yarns of β-crystalline poly(vinylidene fluoride) (PVDF) sheath and conductive high density polyethylene (HDPE)/carbon black (CB) core as insertions in a woven textile, with conductive poly(3,4-ethylene dioxythiophene)-poly(styrene sulfonate) (PEDOT:PSS) coatings developed for textile applications. Two coatings, one with a polyurethane binder and one without, were compared for the application and evaluated as electrode material in piezoelectric testing, as well as tested for surface resistivity, tear strength, abrasion resistance and shear flexing. Both coatings served their function as the outer electrodes in the system and no difference in this regard was detected between them. Omission of the binder resulted in a surface resistivity one order of magnitude less, of 12.3 Ω/square, but the surface resistivity of these samples increased more upon abrasion than the samples coated with binder. The tear strength of the textile coated with binder decreased with one third compared to the uncoated substrate, whereas the tear strength of the coated textile without binder increased with the same amount. Surface resistivity measurements and scanning electron microscopy (SEM) images of the samples subjected to shear flexing showed that the coatings without the binder did not withstand this treatment, and that the samples with the binder managed this to a greater extent. In summary, both of the PEDOT:PSS coatings could be used as outer electrodes of the piezoelectric fibres, but inclusion of binder was found necessary for the durability of the coating.
- 25 September 2014
- Published by Springer Nature in Fashion and Textiles
- Vol. 1 (1) , 1-17
Open AccessTextile piezoelectric sensors – melt spun bi-component poly(vinylidene fluoride) fibres with conductive cores and poly(3,4-ethylene dioxythiophene)-poly(styrene sulfonate) coating as the outer electrode
The work presented here addresses the outer electroding of a fully textile piezoelectric strain sensor, consisting of bi-component fibre yarns of β-crystalline poly(vinylidene fluoride) (PVDF) sheath and conductive high density polyethylene (HDPE)/carbon black (CB) core as insertions in a woven textile, with conductive poly(3,4-ethylene dioxythiophene)-poly(styrene sulfonate) (PEDOT:PSS) coatings developed for textile applications. Two coatings, one with a polyurethane binder and one without, were compared for the application and evaluated as electrode material in piezoelectric testing, as well as tested for surface resistivity, tear strength, abrasion resistance and shear flexing. Both coatings served their function as the outer electrodes in the system and no difference in this regard was detected between them. Omission of the binder resulted in a surface resistivity one order of magnitude less, of 12.3 Ω/square, but the surface resistivity of these samples increased more upon abrasion than the samples coated with binder. The tear strength of the textile coated with binder decreased with one third compared to the uncoated substrate, whereas the tear strength of the coated textile without binder increased with the same amount. Surface resistivity measurements and scanning electron microscopy (SEM) images of the samples subjected to shear flexing showed that the coatings without the binder did not withstand this treatment, and that the samples with the binder managed this to a greater extent. In summary, both of the PEDOT:PSS coatings could be used as outer electrodes of the piezoelectric fibres, but inclusion of binder was found necessary for the durability of the coating.
- 3 June 2013
- Published by SAGE Publications in Textile Research Journal
- Vol. 83 (20) , 2164-2176
Influence of coating parameters on textile and electrical properties of a poly(3,4-ethylene dioxythiophene):poly(styrene sulfonate)/polyurethane-coated textile
Textile coatings with electrical conductivity were obtained by the addition of poly(3,4-ethylene dioxythiophene)-poly(styrene sulfonate) (PEDOT:PSS) and ethylene glycol (EG) to a polyurethane (PU)-based coating formulation. Variations of the coating formulation, the coating amount and the drying conditions, as well as the absence of an annealing step, were investigated. The coated fabrics were evaluated for tear strength and bending rigidity as well as surface resistivity and appearance before and after Martindale abrasion. A high proportion of PEDOT:PSS dispersion in the formulation and the presence of EG provided low surface resistivity. This composition resulted in softer samples with higher tear strength than those containing more PU-binder. All coatings proved to withstand abrasion to a similar extent. The surface resistivity increased gradually with the abrasion, about one half order of magnitude, except for those coatings that had been subjected to a faster drying process, where the surface resistivity increased somewhat faster.
- 3 June 2013
- Published by SAGE Publications in Textile Research Journal
- Vol. 83 (20) , 2164-2176
Influence of coating parameters on textile and electrical properties of a poly(3,4-ethylene dioxythiophene):poly(styrene sulfonate)/polyurethane-coated textile
Textile coatings with electrical conductivity were obtained by the addition of poly(3,4-ethylene dioxythiophene)-poly(styrene sulfonate) (PEDOT:PSS) and ethylene glycol (EG) to a polyurethane (PU)-based coating formulation. Variations of the coating formulation, the coating amount and the drying conditions, as well as the absence of an annealing step, were investigated. The coated fabrics were evaluated for tear strength and bending rigidity as well as surface resistivity and appearance before and after Martindale abrasion. A high proportion of PEDOT:PSS dispersion in the formulation and the presence of EG provided low surface resistivity. This composition resulted in softer samples with higher tear strength than those containing more PU-binder. All coatings proved to withstand abrasion to a similar extent. The surface resistivity increased gradually with the abrasion, about one half order of magnitude, except for those coatings that had been subjected to a faster drying process, where the surface resistivity increased somewhat faster.