Ping Zhu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ping Zhu has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
Yun Liu
Hubei Biomass Fibers and Eco-dyeing & Finishing Key Laboratory, College of Chemistry and Chemical Engineering, State Key Laboratory of New Textile Materials and Advanced Processing Technologies, Wuhan Textile University, Wuhan, China
2 shared publicationsChuan-Jie Zhang
Hubei Biomass Fibers and Eco-dyeing & Finishing Key Laboratory, College of Chemistry and Chemical Engineering, State Key Laboratory of New Textile Materials and Advanced Processing Technologies, Wuhan Textile University, Wuhan, China
1 shared publicationChuanjie Zhang
College of Chemistry and Chemical Engineering, Wuhan Textile University, Wuhan, China
1 shared publication- De-Yi Wang
IMDEA Materials Institute Madrid Spain
1 shared publication Hu Ji
College of Chemistry and Chemical Engineering, Wuhan Textile University, Wuhan, China
1 shared publicationJin-Chao Zhao
Hubei Biomass Fibers and Eco-dyeing & Finishing Key Laboratory, College of Chemistry and Chemical Engineering, State Key Laboratory of New Textile Materials and Advanced Processing Technologies, Wuhan Textile University, Wuhan, China
1 shared publication
Latest Publications
- 16 September 2015
- Published by Springer Nature in Journal of Materials Science
- Vol. 51 (2) , 1052-1065
Effect of manganese and cobalt ions on flame retardancy and thermal degradation of bio-based alginate films
- 16 September 2015
- Published by Springer Nature in Journal of Materials Science
- Vol. 51 (2) , 1052-1065
Effect of manganese and cobalt ions on flame retardancy and thermal degradation of bio-based alginate films
- 14 February 2014
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 53 (6) , 1074-1089
The Flame Retardancy, Thermal Properties, and Degradation Mechanism of Zinc Alginate Films
The coordination structure, flame retardancy, thermal stabilities, and degradation mechanism of zinc alginate films were studied by Fourier transform infrared spectroscopy (FTIR), limiting oxygen index (LOI), vertical burning (UL-94), and thermogravimetric analysis (TGA) tests. The FTIR results showed that the structure of zinc alginate was correlated to its bidentate bridging coordination. The LOI (49.3) and UL-94 (V-0 rating) results indicated that zinc alginate was an inherent flame retardant material. The TG results showed that zinc alginate had better thermal stabilities than sodium alginate in the lower temperature zones; however, the thermal stabilities of zinc alginate were worse than those of sodium alginate at higher temperatures because of the decomposition of zinc oxalate formed in the degradation process of zinc alginate. Based on the TG results and FTIR of the residues at different temperatures, the effect of zinc ions on the degradation process of alginate was different from that of sodium ions. The zinc ions can catalyze alginate to form the residues and increase the amount of the residues, finally forming zinc oxide. Further, it could decrease the release of flammable gases and increase the flame retardancy of alginate.
- 14 February 2014
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 53 (6) , 1074-1089
The Flame Retardancy, Thermal Properties, and Degradation Mechanism of Zinc Alginate Films
The coordination structure, flame retardancy, thermal stabilities, and degradation mechanism of zinc alginate films were studied by Fourier transform infrared spectroscopy (FTIR), limiting oxygen index (LOI), vertical burning (UL-94), and thermogravimetric analysis (TGA) tests. The FTIR results showed that the structure of zinc alginate was correlated to its bidentate bridging coordination. The LOI (49.3) and UL-94 (V-0 rating) results indicated that zinc alginate was an inherent flame retardant material. The TG results showed that zinc alginate had better thermal stabilities than sodium alginate in the lower temperature zones; however, the thermal stabilities of zinc alginate were worse than those of sodium alginate at higher temperatures because of the decomposition of zinc oxalate formed in the degradation process of zinc alginate. Based on the TG results and FTIR of the residues at different temperatures, the effect of zinc ions on the degradation process of alginate was different from that of sodium ions. The zinc ions can catalyze alginate to form the residues and increase the amount of the residues, finally forming zinc oxide. Further, it could decrease the release of flammable gases and increase the flame retardancy of alginate.