Valery P. Privalko
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Valery P. Privalko has a total of 37 co-authors. Here are the top co-authors by number of shared publications:
Eleonora G. Privalko
Institute of Macromolecular Chemistry , National Academy of Sciences of Ukraine , Kyiv , Ukraine
3 shared publications- Victor Yu. Kramarenko
RNatl Tech Univ, Kharkiv Polytech Inst, 2 Kyrpychova St, UA-61002 Kharkov, Ukraine
3 shared publications E. G. Privalko
Institute of Macromolecular Chemistry, National Academy of Sciences ofUkraine , Kyiv , Ukraine
2 shared publicationsE.G. Privalko
Institute of Macromolecular Chemistry, National Academy of Sciences of Ukraine,02160 Kyiv Ukraine
2 shared publicationsIngo Alig
Deutsches Kunststoff‐Institut, Department of Physics , Darmstadt , Germany
2 shared publications- Sergiy M. Ponomarenko
Institute of Macromolecular Chemistry, National Academy of Sciences of Ukraine, Kharkiv Chaussee 48, 02160 Kyiv, Ukraine
2 shared publications
Latest Publications
- 1 September 2005
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 44 (5) , 749-759
Structure/Property Relationships for Poly(Vinylidene Fluoride)/Doped Polyaniline Blends
Poly(vinylidene fluoride) (PVDF) and its blends with polyaniline (PANI) doped with dodecylbenzene sulfonic acid (DBSA) were characterized by electrical conductivity, differential scanning calorimetry (DSC) and X‐ray scattering techniques. The onset of an infinite cluster (InC) of conducting, highly anisometric PANI/DBSA particles in PVDF/(PANI/DBSA) blends was observed at the percolation threshold as low as w*≈3.5 wt.%. The small angle X‐ray scattering (SAXS) data confirmed the expected spatial organization of PANI/DBSA needles into fractal‐like structures above w*. A slight decrease of both the DSC and the wide‐angle X‐ray scattering (WAXS) degrees of crystallinity of PVDF with the PANI/DBSA mass content w was explained by strong interactions at the PVDF/(PANI/DBSA) interface resulting in the loss of crystallizability of a fraction of sterically immobilized chains of PVDF in boundary layers around PANI/DBSA particles. The available data suggest that the conductive paths within InC of PANI/DBSA in PVDF/(PANI/DBSA) blends were formed primarily by the end‐to‐end contacts of PANI/DBSA fibrils.
- 1 September 2005
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 44 (5) , 749-759
Structure/Property Relationships for Poly(Vinylidene Fluoride)/Doped Polyaniline Blends
Poly(vinylidene fluoride) (PVDF) and its blends with polyaniline (PANI) doped with dodecylbenzene sulfonic acid (DBSA) were characterized by electrical conductivity, differential scanning calorimetry (DSC) and X‐ray scattering techniques. The onset of an infinite cluster (InC) of conducting, highly anisometric PANI/DBSA particles in PVDF/(PANI/DBSA) blends was observed at the percolation threshold as low as w*≈3.5 wt.%. The small angle X‐ray scattering (SAXS) data confirmed the expected spatial organization of PANI/DBSA needles into fractal‐like structures above w*. A slight decrease of both the DSC and the wide‐angle X‐ray scattering (WAXS) degrees of crystallinity of PVDF with the PANI/DBSA mass content w was explained by strong interactions at the PVDF/(PANI/DBSA) interface resulting in the loss of crystallizability of a fraction of sterically immobilized chains of PVDF in boundary layers around PANI/DBSA particles. The available data suggest that the conductive paths within InC of PANI/DBSA in PVDF/(PANI/DBSA) blends were formed primarily by the end‐to‐end contacts of PANI/DBSA fibrils.
- 1 September 2005
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 44 (5) , 739-748
Structure‐Property Relationships for Model Heterocyclic Polymer Networks: Effect of Monomer Functionality
The effect of initial monomer functionality on the final properties of densely cross‐linked heterocyclic polymer networks (HPN) was evaluated from comparative studies of the viscoelastic behavior and enthalpy relaxation in the glass transition range of polyisocyanurates prepared from a bifunctional monomer D (1,6‐hexamethylene diisocyanate, HDI) and a trifunctional monomer T (the isocyanurate of HDI). Quantitative analysis of these data suggested that an HPN prepared from the monomer T was chemically more heterogeneous and possessed a lower effective network density (presumably, as a result of a lower mobility of the initial monomer T compared to monomer D).
- 1 September 2005
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 44 (5) , 739-748
Structure‐Property Relationships for Model Heterocyclic Polymer Networks: Effect of Monomer Functionality
The effect of initial monomer functionality on the final properties of densely cross‐linked heterocyclic polymer networks (HPN) was evaluated from comparative studies of the viscoelastic behavior and enthalpy relaxation in the glass transition range of polyisocyanurates prepared from a bifunctional monomer D (1,6‐hexamethylene diisocyanate, HDI) and a trifunctional monomer T (the isocyanurate of HDI). Quantitative analysis of these data suggested that an HPN prepared from the monomer T was chemically more heterogeneous and possessed a lower effective network density (presumably, as a result of a lower mobility of the initial monomer T compared to monomer D).
- 1 September 2005
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 44 (5) , 697-709
Structure‐Property Relationships for Model Heterocyclic Polymer Networks: Effect of Network Density
Chain motion dynamics around and through the glass transition region of a series of heterocyclic polymer networks (HPN) were characterized by dynamic mechanical spectroscopy and differential scanning calorimetry. The effective network densities of those HPN prepared by simultaneous trimerization of a bifunctional (1,6‐hexamethylene diisocyanate, HDI) and a monofunctional (hexyl isocyanate, HI) monomers were systematically varied by changing the HDI/HI ratio in the reaction mixture, whereas their overall chemical structure remained essentially unchanged. The increasing difference between the experimental and theoretical values of the mean molar masses of chain strands between network junctions, the lower the HDI/HI ratio, was assumed to be the result of deviations from the exact chemical stoichiometry due to subsidiary reactions between isocyanate groups of the same monomer. The increase of the effective network density was accompanied by narrowing of the glass transition interval and by its systematic shift to higher temperatures concomitant with the increase of cooperativity and fragility indexes. The characteristic linear dimension of a kinetic unit involved in the dielectric and the mechanical α‐relaxations of studied HPNs proved to be of the same order of magnitude as the size of one isocyanurate heterocycle.
- 1 September 2005
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 44 (5) , 697-709
Structure‐Property Relationships for Model Heterocyclic Polymer Networks: Effect of Network Density
Chain motion dynamics around and through the glass transition region of a series of heterocyclic polymer networks (HPN) were characterized by dynamic mechanical spectroscopy and differential scanning calorimetry. The effective network densities of those HPN prepared by simultaneous trimerization of a bifunctional (1,6‐hexamethylene diisocyanate, HDI) and a monofunctional (hexyl isocyanate, HI) monomers were systematically varied by changing the HDI/HI ratio in the reaction mixture, whereas their overall chemical structure remained essentially unchanged. The increasing difference between the experimental and theoretical values of the mean molar masses of chain strands between network junctions, the lower the HDI/HI ratio, was assumed to be the result of deviations from the exact chemical stoichiometry due to subsidiary reactions between isocyanate groups of the same monomer. The increase of the effective network density was accompanied by narrowing of the glass transition interval and by its systematic shift to higher temperatures concomitant with the increase of cooperativity and fragility indexes. The characteristic linear dimension of a kinetic unit involved in the dielectric and the mechanical α‐relaxations of studied HPNs proved to be of the same order of magnitude as the size of one isocyanurate heterocycle.
- 1 September 2005
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 44 (5) , 641-650
Thermoelastic Behavior of Polyurethanes Reinforced with the In situ‐Generated Sodium Silica‐Polyphosphate Nanophase
Segmented polyurethane‐based nanocomposites prepared by reaction between the organic precursor (macrodiisocyanate, MDIC) and the inorganic precursor (sodium silica‐polyphosphate, SSP) were characterized by differential calorimetry, wide‐angle and small‐angle X‐ray diffraction, and stretching calorimetry techniques. Steric restrictions on the mobility of soft MDIC chain segments by a spatial network of self‐associated stiff segments were assumed responsible for the overshoot of experimental values of the glass transition temperature above that expected for completely miscible components. The initial spatial network of self‐associated stiff segments of the MDIC was destroyed by the randomly distributed SSP particles, giving rise to their own fractal‐like structure. Low reinforcement efficiency of the SSP nanophase was tentatively attributed to the relatively large size of its spatial aggregates. The scale of particle displacements within an infinite cluster during stretching is likely to be negligibly small.
- 1 September 2005
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 44 (5) , 641-650
Thermoelastic Behavior of Polyurethanes Reinforced with the In situ‐Generated Sodium Silica‐Polyphosphate Nanophase
Segmented polyurethane‐based nanocomposites prepared by reaction between the organic precursor (macrodiisocyanate, MDIC) and the inorganic precursor (sodium silica‐polyphosphate, SSP) were characterized by differential calorimetry, wide‐angle and small‐angle X‐ray diffraction, and stretching calorimetry techniques. Steric restrictions on the mobility of soft MDIC chain segments by a spatial network of self‐associated stiff segments were assumed responsible for the overshoot of experimental values of the glass transition temperature above that expected for completely miscible components. The initial spatial network of self‐associated stiff segments of the MDIC was destroyed by the randomly distributed SSP particles, giving rise to their own fractal‐like structure. Low reinforcement efficiency of the SSP nanophase was tentatively attributed to the relatively large size of its spatial aggregates. The scale of particle displacements within an infinite cluster during stretching is likely to be negligibly small.
- 1 July 2005
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 44 (4) , 421-430
Enthalpy Relaxation in the Cooling/Heating Cycles of Polyamide 6/Organoclay Nanocomposites. I. Nonisothermal Crystallization
Neat polyamide 6 homopolymer (PA 6) and a series of commercial polymer nanocomposites (PNC) containing up to 7.5 wt. % of exfoliated organoclay nanoparticles were characterized by the exothermic ef...
- 1 July 2005
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 44 (4) , 421-430
Enthalpy Relaxation in the Cooling/Heating Cycles of Polyamide 6/Organoclay Nanocomposites. I. Nonisothermal Crystallization
Neat polyamide 6 homopolymer (PA 6) and a series of commercial polymer nanocomposites (PNC) containing up to 7.5 wt. % of exfoliated organoclay nanoparticles were characterized by the exothermic ef...
- 2 February 2004
- Published by Wiley in Polymers for Advanced Technologies
- Vol. 15 (3) , 144-148
Polyimides reinforced with the sol‐gel derived organosilicon nanophase as low dielectric permittivity materials
Polyimide (PI) nanocomposites prepared by thein situgeneration of crosslinked organosilicon nanophase (ON) through the sol‐gel process were characterized by densities, thermally stimulated depolarization currents and dielectric relaxation spectroscopy.Both a looser molecular packing of PI chain fragments adjacent to the ON and a loose inner structure of the spatial aggregates of ON were assumed to be responsible for a non‐additive decrease of the experimental values of dielectric permittivity for the nanocomposites. The pattern of composition dependence of the apparent dielectric permittivity of the ON suggested a probability of a morphological change around the composition PAAS/MTS = 100/16 (presumably, a sort of percolation transition from small‐size, individual clusters into large‐size, infinite clusters). Thus, PI reinforced with the sol‐gel derived nanophase may have a reasonably good potential as low dielectric permittivity materials. Copyright © 2004 John Wiley & Sons, Ltd.
- 2 February 2004
- Published by Wiley in Polymers for Advanced Technologies
- Vol. 15 (3) , 144-148
Polyimides reinforced with the sol‐gel derived organosilicon nanophase as low dielectric permittivity materials
Polyimide (PI) nanocomposites prepared by thein situgeneration of crosslinked organosilicon nanophase (ON) through the sol‐gel process were characterized by densities, thermally stimulated depolarization currents and dielectric relaxation spectroscopy.Both a looser molecular packing of PI chain fragments adjacent to the ON and a loose inner structure of the spatial aggregates of ON were assumed to be responsible for a non‐additive decrease of the experimental values of dielectric permittivity for the nanocomposites. The pattern of composition dependence of the apparent dielectric permittivity of the ON suggested a probability of a morphological change around the composition PAAS/MTS = 100/16 (presumably, a sort of percolation transition from small‐size, individual clusters into large‐size, infinite clusters). Thus, PI reinforced with the sol‐gel derived nanophase may have a reasonably good potential as low dielectric permittivity materials. Copyright © 2004 John Wiley & Sons, Ltd.
- Open Access
- 1 December 2003
- Published by Walter de Gruyter GmbH in e-Polymers
- Vol. 3 (1) , 491-496
Interfacial interactions-controlled thermoelastic behaviour of synthetic rubber/organoclay nanocomposites
Thermoelastic measurements of synthetic rubber/organoclay nanocomposites provided the first experimental evidence for the dramatic dependence on interfacial interactions of the scale of nanoparticle displacements within filler aggregates of synthetic rubber/organoclay nanocomposites at high uniaxial extensions.
- 1 December 2003
- Published by Walter de Gruyter GmbH in e-Polymers
- Vol. 3 (1) , 491-496
Open AccessInterfacial interactions-controlled thermoelastic behaviour of synthetic rubber/organoclay nanocomposites
Thermoelastic measurements of synthetic rubber/organoclay nanocomposites provided the first experimental evidence for the dramatic dependence on interfacial interactions of the scale of nanoparticle displacements within filler aggregates of synthetic rubber/organoclay nanocomposites at high uniaxial extensions.
- Open Access
- 1 January 2003
- Published by Taylor & Francis in Science and Technology of Advanced Materials
- Vol. 4 (2) , 115-119
Synthesis and thermomechanical characterization of polyimides reinforced with the sol–gel derived nanoparticles
Polyimide-based nanocomposites prepared by the in situ generation of inorganic nanoparticles (silica) through the sol–gel process were characterized by kinetics of water uptake, thermogravimetry and dynamic mechanical analysis.Silica particles turned out to possess a rather loose inner structure characterized by enhanced water diffusivities and by dynamic elasticity moduli comparable to that of the pristine, glassy PI. Thermal stability and thermomechanical properties of nanocomposites in the glassy state remained nearly the same as those of the pristine PI, while a significant reinforcement effect was observed for the rubbery PI matrix.
- 1 January 2003
- Published by Taylor & Francis in Science and Technology of Advanced Materials
- Vol. 4 (2) , 115-119
Open AccessSynthesis and thermomechanical characterization of polyimides reinforced with the sol–gel derived nanoparticles
Polyimide-based nanocomposites prepared by the in situ generation of inorganic nanoparticles (silica) through the sol–gel process were characterized by kinetics of water uptake, thermogravimetry and dynamic mechanical analysis.Silica particles turned out to possess a rather loose inner structure characterized by enhanced water diffusivities and by dynamic elasticity moduli comparable to that of the pristine, glassy PI. Thermal stability and thermomechanical properties of nanocomposites in the glassy state remained nearly the same as those of the pristine PI, while a significant reinforcement effect was observed for the rubbery PI matrix.
- Open Access
- 1 January 2002
- Published by Taylor & Francis in Science and Technology of Advanced Materials
- Vol. 3 (2) , 111-116
Viscoelasticity and flow behavior of irradiation grafted nano-inorganic particle filled polypropylene composites in the melt state
Nanoparticles (mean size about 7 nm) of the standard pyrogenic Aerosil 1380 (Degussa) pregrafted by g-irradiation with styrene were melt-compounded with the general purpose isotactic polypropylene homopolymer to prepare four nanocomposites with ®ller volume contents up to 4.68%. Storage G 0 (v) and loss G 00 (v) shear moduli in the melt state (measured in the range of linear viscoelasticity at three temperatures in the frequency window spanning about three decades) were treated to derive the relaxation times spectra h(t) using the nlreg computer program based on Tikhonov's method of non-linear regularization. The experimental data were interpreted in terms of the tentative model highlighting the structural signi®cance of the ratio of mean thickness of polymer interlayer between neighboring ®ller particles, kLl, to the mean radius of gyration of a polymer coil, kR g l. In the range of very low ®ller loadings characterized by large scaled distances, kLl/kR g l $ 1, all nanocomposites behaved as Newtonian liquids in which the self-diffusion of macromolecular coils was, however, slowed down. The onset of plastic yield phenomenon for a nanocomposite with the ®ller volume content as low as 4.68% was regarded as the experimental evidence for the shear-resistant, in®nite cluster of ®ller particles coated with polymer boundary interphase when the scaled distance approached the `critical' value, kLl/kR g l # 1.
- 1 January 2002
- Published by Taylor & Francis in Science and Technology of Advanced Materials
- Vol. 3 (2) , 111-116
Open AccessViscoelasticity and flow behavior of irradiation grafted nano-inorganic particle filled polypropylene composites in the melt state
Nanoparticles (mean size about 7 nm) of the standard pyrogenic Aerosil 1380 (Degussa) pregrafted by g-irradiation with styrene were melt-compounded with the general purpose isotactic polypropylene homopolymer to prepare four nanocomposites with ®ller volume contents up to 4.68%. Storage G 0 (v) and loss G 00 (v) shear moduli in the melt state (measured in the range of linear viscoelasticity at three temperatures in the frequency window spanning about three decades) were treated to derive the relaxation times spectra h(t) using the nlreg computer program based on Tikhonov's method of non-linear regularization. The experimental data were interpreted in terms of the tentative model highlighting the structural signi®cance of the ratio of mean thickness of polymer interlayer between neighboring ®ller particles, kLl, to the mean radius of gyration of a polymer coil, kR g l. In the range of very low ®ller loadings characterized by large scaled distances, kLl/kR g l $ 1, all nanocomposites behaved as Newtonian liquids in which the self-diffusion of macromolecular coils was, however, slowed down. The onset of plastic yield phenomenon for a nanocomposite with the ®ller volume content as low as 4.68% was regarded as the experimental evidence for the shear-resistant, in®nite cluster of ®ller particles coated with polymer boundary interphase when the scaled distance approached the `critical' value, kLl/kR g l # 1.
- 1 January 2000
- Published by Taylor & Francis in Designed Monomers and Polymers
- Vol. 3 (3) , 363-379
Solution behavior of copoly(amide imide)s
Dimethyl acetamide (DMAA) solutions of copoly(amide imide)s (coPAIs) synthesized from the dichloro-dianhydride of trimellitimide-N-acetic acid and mixtures of diphenylmethane diamine (DPA) with cardo-9,9′-bis-phenylfluorene diamine (CDA) were characterized by measurements of the specific heat capacity in the temperature interval 150-370 K, of heats of dilution in DMAA at room temperature, and of the apparent viscosity in the temperature interval 288-373 K. It was established that the degree of inter-segment interactions in quiescent solutions of coPAIs increased, and the contribution of the shear-thickening flow mechanism of semi-dilute solutions decreased, the lower the DPA/CDA ratio. The regime cross-over from dilute solution to semi-dilute solution manifested itself as jump-like changes of the normalized solvent melting heats and of the activation energies for viscous flow, as well as breaks in the heats of dilution vs. concentration plots.
- 1 January 2000
- Published by Taylor & Francis in Designed Monomers and Polymers
- Vol. 3 (3) , 363-379
Solution behavior of copoly(amide imide)s
Dimethyl acetamide (DMAA) solutions of copoly(amide imide)s (coPAIs) synthesized from the dichloro-dianhydride of trimellitimide-N-acetic acid and mixtures of diphenylmethane diamine (DPA) with cardo-9,9′-bis-phenylfluorene diamine (CDA) were characterized by measurements of the specific heat capacity in the temperature interval 150-370 K, of heats of dilution in DMAA at room temperature, and of the apparent viscosity in the temperature interval 288-373 K. It was established that the degree of inter-segment interactions in quiescent solutions of coPAIs increased, and the contribution of the shear-thickening flow mechanism of semi-dilute solutions decreased, the lower the DPA/CDA ratio. The regime cross-over from dilute solution to semi-dilute solution manifested itself as jump-like changes of the normalized solvent melting heats and of the activation energies for viscous flow, as well as breaks in the heats of dilution vs. concentration plots.