Erde Can
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Erde Can has a total of 32 co-authors. Here are the top co-authors by number of shared publications:
- Gamze Torun Köse
Department of Genetics and Bioengineering, Faculty of Engineering and Natural Sciences, Yeditepe University, Istanbul 34755, Türkiye
4 shared publications S. Küsefoğlu
Department of Chemistry, Polymer Research Center, Bogaziçi University, Istanbul, Turkey
4 shared publications- Giuseppe R. Palmese
Department of Chemical Engineering, Rowan University, Glassboro, NJ 08028, USA
3 shared publications - Richard P. Wool
Department of Chemical Engineering University of Delaware 19716 Newark Delaware
3 shared publications - Emre Kinaci
Department of Chemical and Biological Engineering, Drexel University, Philadelphia, PA 19104, USA
2 shared publications Gokce Udenir
Yeditepe University
2 shared publications
Latest Publications
- 12 August 2023
- Published by Springer Nature in Journal of Polymer Research
- Vol. 30 (9) , 1-12
In vitro investigation of poly(propylene fumarate) cured with phosphonic acid based monomers as scaffolds for bone tissue engineering
- 12 August 2023
- Published by Springer Nature in Journal of Polymer Research
- Vol. 30 (9) , 1-12
In vitro investigation of poly(propylene fumarate) cured with phosphonic acid based monomers as scaffolds for bone tissue engineering
- Open Access
Epoxidation of Cardanol’s Terminal Double Bond
In this investigation, the terminal double bonds of the side chain epoxidized cardanol glycidyl ether (SCECGE) molecule were further epoxidized in the presence of Oxone® (potassium peroxomonosulfate) and fluorinated acetone. Regular methods for the double bond epoxidation are not effective on the terminal double bonds because of their reduced electronegativity with respect to internal double bonds. The terminal double bond functionality of the SCECGE was epoxidized to nearly 70%, increasing the epoxy functionality of SCECGE from 2.45 to 2.65 epoxies/molecule as measured using proton magnetic nuclear resonance (1H-NMR). This modified material—side chain epoxidized cardanol glycidyl ether with terminal epoxies (TE-SCECGE)—was thermally cured with cycloaliphatic curing agent 4-4′-methylenebis(cyclohexanamine) (PACM) at stoichiometry, and the cured polymer properties, such as glass transition temperature (Tg) and tensile modulus, were compared with SCECGE resin cured with PACM. The Tg of the material was increased from 52 to 69 °C as obtained via a dynamic mechanical analysis (DMA) while the tensile modulus of the material increased from 0.88 to 1.24 GPa as a result of terminal double bond epoxidation. In addition to highlighting the effects of dangling side groups in an epoxy network, this modest increase in Tg and modulus could be sufficient to significantly expand the potential uses of amine-cured cardanol-based epoxies for fiber reinforced composite applications.
Open AccessEpoxidation of Cardanol’s Terminal Double Bond
In this investigation, the terminal double bonds of the side chain epoxidized cardanol glycidyl ether (SCECGE) molecule were further epoxidized in the presence of Oxone® (potassium peroxomonosulfate) and fluorinated acetone. Regular methods for the double bond epoxidation are not effective on the terminal double bonds because of their reduced electronegativity with respect to internal double bonds. The terminal double bond functionality of the SCECGE was epoxidized to nearly 70%, increasing the epoxy functionality of SCECGE from 2.45 to 2.65 epoxies/molecule as measured using proton magnetic nuclear resonance (1H-NMR). This modified material—side chain epoxidized cardanol glycidyl ether with terminal epoxies (TE-SCECGE)—was thermally cured with cycloaliphatic curing agent 4-4′-methylenebis(cyclohexanamine) (PACM) at stoichiometry, and the cured polymer properties, such as glass transition temperature (Tg) and tensile modulus, were compared with SCECGE resin cured with PACM. The Tg of the material was increased from 52 to 69 °C as obtained via a dynamic mechanical analysis (DMA) while the tensile modulus of the material increased from 0.88 to 1.24 GPa as a result of terminal double bond epoxidation. In addition to highlighting the effects of dangling side groups in an epoxy network, this modest increase in Tg and modulus could be sufficient to significantly expand the potential uses of amine-cured cardanol-based epoxies for fiber reinforced composite applications.
- Open Access
Influence of Epoxidized Cardanol Functionality and Reactivity on Network Formation and Properties
Cardanol is a renewable resource based on cashew nut shell liquid (CNSL), which consists of a phenol ring with a C15 long aliphatic side chain in the meta position with varying degrees of unsaturation. Cardanol glycidyl ether was chemically modified to form side-chain epoxidized cardanol glycidyl ether (SCECGE) with an average epoxy functionality of 2.45 per molecule and was cured with petroleum-based epoxy hardeners, 4-4′-methylenebis(cyclohexanamine) and diethylenetriamine, and a cardanol-based amine hardener. For comparison, cardanol-based diphenol diepoxy resin, NC514 (Cardolite), and a petroleum-based epoxy resin, diglycidyl ether of bisphenol-A (DGEBA) were also evaluated. Chemical and thermomechanical analyses showed that for SCECGE resins, incomplete cure of the secondary epoxides led to reduced cross-link density, reduced thermal stability, and reduced elongation at break when compared with difunctional resins containing only primary epoxides. However, because of functionality greater than two, amine-cured SCECGE produced a Tg very similar to that of NC514 and thus could be useful in formulating epoxy with renewable cardanol content.
Open AccessInfluence of Epoxidized Cardanol Functionality and Reactivity on Network Formation and Properties
Cardanol is a renewable resource based on cashew nut shell liquid (CNSL), which consists of a phenol ring with a C15 long aliphatic side chain in the meta position with varying degrees of unsaturation. Cardanol glycidyl ether was chemically modified to form side-chain epoxidized cardanol glycidyl ether (SCECGE) with an average epoxy functionality of 2.45 per molecule and was cured with petroleum-based epoxy hardeners, 4-4′-methylenebis(cyclohexanamine) and diethylenetriamine, and a cardanol-based amine hardener. For comparison, cardanol-based diphenol diepoxy resin, NC514 (Cardolite), and a petroleum-based epoxy resin, diglycidyl ether of bisphenol-A (DGEBA) were also evaluated. Chemical and thermomechanical analyses showed that for SCECGE resins, incomplete cure of the secondary epoxides led to reduced cross-link density, reduced thermal stability, and reduced elongation at break when compared with difunctional resins containing only primary epoxides. However, because of functionality greater than two, amine-cured SCECGE produced a Tg very similar to that of NC514 and thus could be useful in formulating epoxy with renewable cardanol content.
- 1 July 2020
- Published by Wiley in Polymer International
- Vol. 69 (12) , 1283-1296
Biodegradable polymeric networks of poly(propylene fumarate) and phosphonic acid‐based monomers
Poly(propylene fumarate) (PPF) was crosslinked with vinyl phosphonic acid (VPA) and vinyl phosphonic acid diethyl ester (VPES) to prepare biodegradable and biocompatible polymers with a network structure. Intended for this purpose, the PPF pre‐polymer was synthesized through a polycondensation reaction of propylene glycol and fumaric acid in an excess of propylene glycol. The PPF pre‐polymer was then thermally cured with various ratios of VPA and VPES in the presence of benzoyl peroxide initiator via radical polymerization. Complete cure of PPF/VPA and PPF/VPES copolymers was confirmed by differential scanning calorimetry, crosslink density was determined via swelling experiments, and thermomechanical properties and thermal degradation profiles were characterized by dynamic mechanical and thermogravimetric analyses, respectively. Various compositions of the PPF/VPA and PPF/VPES copolymers exhibited compressive modulus values in the wide range 10–836 MPa and compressive strength values in the range 14–119 MPa. The equilibrium water content of the PPF/VPA and PPF/VPES copolymers ranged from 4 to 20.5 wt%. Biodegradation rate of the polymers in buffer solution at 37 °C, examined via both weight loss and pH measurements, was significantly influenced by the co‐monomer and initiator compositions. Combining the results of these studies indicated that PPF/VPA and PPF/VPES copolymers show potential for applications as bone tissue engineering scaffolds. Moreover, just varying PPF and co‐monomer ratio and initiator amount provides adjustable and controllable characteristics of the end product. © 2020 Society of Industrial Chemistry
- 1 July 2020
- Published by Wiley in Polymer International
- Vol. 69 (12) , 1283-1296
Biodegradable polymeric networks of poly(propylene fumarate) and phosphonic acid‐based monomers
Poly(propylene fumarate) (PPF) was crosslinked with vinyl phosphonic acid (VPA) and vinyl phosphonic acid diethyl ester (VPES) to prepare biodegradable and biocompatible polymers with a network structure. Intended for this purpose, the PPF pre‐polymer was synthesized through a polycondensation reaction of propylene glycol and fumaric acid in an excess of propylene glycol. The PPF pre‐polymer was then thermally cured with various ratios of VPA and VPES in the presence of benzoyl peroxide initiator via radical polymerization. Complete cure of PPF/VPA and PPF/VPES copolymers was confirmed by differential scanning calorimetry, crosslink density was determined via swelling experiments, and thermomechanical properties and thermal degradation profiles were characterized by dynamic mechanical and thermogravimetric analyses, respectively. Various compositions of the PPF/VPA and PPF/VPES copolymers exhibited compressive modulus values in the wide range 10–836 MPa and compressive strength values in the range 14–119 MPa. The equilibrium water content of the PPF/VPA and PPF/VPES copolymers ranged from 4 to 20.5 wt%. Biodegradation rate of the polymers in buffer solution at 37 °C, examined via both weight loss and pH measurements, was significantly influenced by the co‐monomer and initiator compositions. Combining the results of these studies indicated that PPF/VPA and PPF/VPES copolymers show potential for applications as bone tissue engineering scaffolds. Moreover, just varying PPF and co‐monomer ratio and initiator amount provides adjustable and controllable characteristics of the end product. © 2020 Society of Industrial Chemistry
- 2 February 2018
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 56 (7) , 558-575
Cross‐linked poly(aryl ether sulfone) membranes for direct methanol fuel cell applications
Partially sulfonated poly(aryl ether sulfone) (PESS) was synthesized and methacrylated via reaction with glycidyl methacrylate (PESSGMA) and cross‐linked via radical polymerization with styrene and vinyl‐phosphonic acid (VPA). The chemical structures of the synthesized pre‐polymers were characterized via FTIR and 1H NMR spectroscopic methods and molecular weight was determined via GPC. Membranes of these polymers were prepared via solution casting method. The crosslinking of the PESS polymer reduced IEC, proton conductivity, swelling in water, and methanol permeability of the membranes while increasing the modulus and the glass transition temperature. However, the introduction of the VPA comonomer increased the proton conductivity while maintaining excellent resistance to methanol cross‐over, which was significantly higher as compared with both PESS and the commercial Nafion membranes. Membranes of PESSGMA copolymers incorporating VPA, exhibited proton conductivity values at 60 °C in the range of 16–32 mS cm−1 and methanol permeability values in the range of 6.52 × 10−9 – 1.92 × 10−8 cm2 s−1. © 2018 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2018, 56, 558–575
- 2 February 2018
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 56 (7) , 558-575
Cross‐linked poly(aryl ether sulfone) membranes for direct methanol fuel cell applications
Partially sulfonated poly(aryl ether sulfone) (PESS) was synthesized and methacrylated via reaction with glycidyl methacrylate (PESSGMA) and cross‐linked via radical polymerization with styrene and vinyl‐phosphonic acid (VPA). The chemical structures of the synthesized pre‐polymers were characterized via FTIR and 1H NMR spectroscopic methods and molecular weight was determined via GPC. Membranes of these polymers were prepared via solution casting method. The crosslinking of the PESS polymer reduced IEC, proton conductivity, swelling in water, and methanol permeability of the membranes while increasing the modulus and the glass transition temperature. However, the introduction of the VPA comonomer increased the proton conductivity while maintaining excellent resistance to methanol cross‐over, which was significantly higher as compared with both PESS and the commercial Nafion membranes. Membranes of PESSGMA copolymers incorporating VPA, exhibited proton conductivity values at 60 °C in the range of 16–32 mS cm−1 and methanol permeability values in the range of 6.52 × 10−9 – 1.92 × 10−8 cm2 s−1. © 2018 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2018, 56, 558–575
- 1 November 2015
- Published by Elsevier in European Polymer Journal
- Vol. 72, 129-147
Preparation and characterization of novel vinyl ester formulations derived from cardanol
- 1 November 2015
- Published by Elsevier in European Polymer Journal
- Vol. 72, 129-147
Preparation and characterization of novel vinyl ester formulations derived from cardanol
- 14 July 2014
- Published by Taylor & Francis in Polymer-Plastics Technology and Engineering
- Vol. 53 (11) , 1178-1193
Polybutylene Succinate (PBS) – Polycaprolactone (PCL) Blends Compatibilized with Poly(ethylene oxide)-block-poly(propylene oxide)-block-poly(ethylene oxide) (PEO-PPO-PEO) Copolymer for Biomaterial Applications
This study reports the preparation and characterization of Polybutylene Succinate (PBS)-Polycaprolactone (PCL) melt blends (10–40 wt.% PCL) in the presence of a compatibilizer, in order to explore their potential use as a biomaterial. The thermal transitions, as well as the crystallinity of the polymer blends were analyzed by Differential Scanning Calorimetry, the thermomechanical properties were analyzed via Dynamic Mechanical Analysis and phase morphologies were characterized by Scanning Electron Microscopy. Degradation profiles of the blends were analyzed in PBS buffer solution at pH 7.4 at 37°C via pH measurements. Cytotoxicity of the PBS/PCL films were tested by MTS assay.
- 14 July 2014
- Published by Taylor & Francis in Polymer-Plastics Technology and Engineering
- Vol. 53 (11) , 1178-1193
Polybutylene Succinate (PBS) – Polycaprolactone (PCL) Blends Compatibilized with Poly(ethylene oxide)-block-poly(propylene oxide)-block-poly(ethylene oxide) (PEO-PPO-PEO) Copolymer for Biomaterial Applications
This study reports the preparation and characterization of Polybutylene Succinate (PBS)-Polycaprolactone (PCL) melt blends (10–40 wt.% PCL) in the presence of a compatibilizer, in order to explore their potential use as a biomaterial. The thermal transitions, as well as the crystallinity of the polymer blends were analyzed by Differential Scanning Calorimetry, the thermomechanical properties were analyzed via Dynamic Mechanical Analysis and phase morphologies were characterized by Scanning Electron Microscopy. Degradation profiles of the blends were analyzed in PBS buffer solution at pH 7.4 at 37°C via pH measurements. Cytotoxicity of the PBS/PCL films were tested by MTS assay.
- 25 October 2011
- Published by Springer Nature in AAPS PharmSciTech
- Vol. 12 (4) , 1442-1453
Investigation of PLLA/PCL Blends and Paclitaxel Release Profiles
Blends of poly (l-lactide) (PLLA) and poly (ε-caprolactone) (PCL) with and without paclitaxel were prepared via solution casting. DSC analysis as well as SEM analysis of the PLLA/PCL blend solution cast films showed that these blends are all phase separated.%PLLA crystallinity was found to increase with increasing PCL content (up till 15 wt.%). The PCL phase is found to homogeneously disperse in the PLLA matrix as spherical domains where the pore diameters of the PCL domains significantly increased with increasing PCL content. The degradation profiles matched with the slower degrading component PCL rather than PLLA and also increasing PCL content of the blends increased the degradation rate relatively. The increased crystallinity of the PLLA phase with increasing PCL contents confirmed that the degradation occurred through PCL phase. Cell proliferation on PLLA/PCL blends showed that all these blends were suitable for the support of cellular growth. Apoptosis assay with the paclitaxel-loaded PLLA/PCL blends showed an increase in cell death throughout 7 days of incubation where the cell death was increased with increasing PCL contents. This was attributed to the faster release of paclitaxel which was at least partially affected by the faster degradation rate at increasing PCL contents. The paclitaxel release was shown to be degradation controlled in the initial stages followed by a faster diffusion-controlled release in the later stages. These polymer blends were found to be very suitable paclitaxel release agents for which the paclitaxel release times can be altered with the composition of the blend and the film thickness.
- 25 October 2011
- Published by Springer Nature in AAPS PharmSciTech
- Vol. 12 (4) , 1442-1453
Investigation of PLLA/PCL Blends and Paclitaxel Release Profiles
Blends of poly (l-lactide) (PLLA) and poly (ε-caprolactone) (PCL) with and without paclitaxel were prepared via solution casting. DSC analysis as well as SEM analysis of the PLLA/PCL blend solution cast films showed that these blends are all phase separated.%PLLA crystallinity was found to increase with increasing PCL content (up till 15 wt.%). The PCL phase is found to homogeneously disperse in the PLLA matrix as spherical domains where the pore diameters of the PCL domains significantly increased with increasing PCL content. The degradation profiles matched with the slower degrading component PCL rather than PLLA and also increasing PCL content of the blends increased the degradation rate relatively. The increased crystallinity of the PLLA phase with increasing PCL contents confirmed that the degradation occurred through PCL phase. Cell proliferation on PLLA/PCL blends showed that all these blends were suitable for the support of cellular growth. Apoptosis assay with the paclitaxel-loaded PLLA/PCL blends showed an increase in cell death throughout 7 days of incubation where the cell death was increased with increasing PCL contents. This was attributed to the faster release of paclitaxel which was at least partially affected by the faster degradation rate at increasing PCL contents. The paclitaxel release was shown to be degradation controlled in the initial stages followed by a faster diffusion-controlled release in the later stages. These polymer blends were found to be very suitable paclitaxel release agents for which the paclitaxel release times can be altered with the composition of the blend and the film thickness.
- 1 September 2011
- Published by Elsevier in Current Opinion in Biotechnology
- Vol. 22, S150
Paclitaxel release from poly(l,l-lactide) (PLLA)/poly(ɛ-caprolactone) (PCL) blends
- 1 September 2011
- Published by Elsevier in Current Opinion in Biotechnology
- Vol. 22, S150
Paclitaxel release from poly(l,l-lactide) (PLLA)/poly(ɛ-caprolactone) (PCL) blends
- 4 September 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 106 (6) , 3833-3842
The synthesis of 9–10 Dibromo stearic acid glycidyl methacrylate and its use in vinyl ester resins
In this study, 9–10 dibromo stearic acid glycidyl methacrylate (Di‐BrSAGMA) was synthesized from oleic acid and used as a replacement for styrene in vinyl ester (bisphenol A type VE (VE 828) and Novalac type VE (VE160)) to introduce fire retardance to these systems and to decrease the volatile organic compound (VOC) emissions caused by styrene. When the Di‐BrSAGMA was used as the comonomer, these resins exhibited too high viscosities, reduced modulus and glass transition temperature (Tg) values compared to those of the styrene based systems. Thus, the Di‐BrSAGMA was used in the presence of styrene in these resins. The viscosities of the resins with various Di‐BrSAGMA contents were determined and the modulus and the Tg values of the resulting polymers were measured via dynamic mechanical analysis (DMA) to determine the ideal formulations for each resin system. Similar analysis was performed, with similar oleic acid glycidyl methacrylate (OAGMA) contents, to determine the effect of the introduction of the bromine groups onto the network. Reactive diluent blends of the fatty acid based monomers with styrene, at styrene contents as low as 15–20 wt % at 35–45 wt % total comonomer content, in VE formulations were shown to have processable viscosities for liquid molding processes, and modulus and Tg values that are comparable to those of the commercial VE‐styrene systems. The effect of the replacement of styrene by the Di‐BrSAGMA monomer on the thermal degradation behavior of the VE 828 and VE 160 networks was also explored by thermal gravimetric analysis (TGA). © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007
- 4 September 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 106 (6) , 3833-3842
The synthesis of 9–10 Dibromo stearic acid glycidyl methacrylate and its use in vinyl ester resins
In this study, 9–10 dibromo stearic acid glycidyl methacrylate (Di‐BrSAGMA) was synthesized from oleic acid and used as a replacement for styrene in vinyl ester (bisphenol A type VE (VE 828) and Novalac type VE (VE160)) to introduce fire retardance to these systems and to decrease the volatile organic compound (VOC) emissions caused by styrene. When the Di‐BrSAGMA was used as the comonomer, these resins exhibited too high viscosities, reduced modulus and glass transition temperature (Tg) values compared to those of the styrene based systems. Thus, the Di‐BrSAGMA was used in the presence of styrene in these resins. The viscosities of the resins with various Di‐BrSAGMA contents were determined and the modulus and the Tg values of the resulting polymers were measured via dynamic mechanical analysis (DMA) to determine the ideal formulations for each resin system. Similar analysis was performed, with similar oleic acid glycidyl methacrylate (OAGMA) contents, to determine the effect of the introduction of the bromine groups onto the network. Reactive diluent blends of the fatty acid based monomers with styrene, at styrene contents as low as 15–20 wt % at 35–45 wt % total comonomer content, in VE formulations were shown to have processable viscosities for liquid molding processes, and modulus and Tg values that are comparable to those of the commercial VE‐styrene systems. The effect of the replacement of styrene by the Di‐BrSAGMA monomer on the thermal degradation behavior of the VE 828 and VE 160 networks was also explored by thermal gravimetric analysis (TGA). © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007