Elena Y. Liberman
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Elena Y. Liberman has a total of 74 co-authors. Here are the top co-authors by number of shared publications:
A. I. Mikhailichenko
Mendeleev University of Chemical Technology
7 shared publicationsT. V. Kon’KOva
Mendeleev University of Chemical Technology of Russia, Moscow, Russia
7 shared publications- Tatiana V. Kon’kOva
Research and Design Institute of Chemical Engineering, Moscow 127015, Russia
6 shared publications A. V. Naumkin
Nesmeyanov Institute of Organoelement Compounds, Russian Academy of Sciences, Moscow, Russia
4 shared publicationsB. S. Kleusov
AO NIIgrafit, Moscow, Russia
4 shared publicationsM. V. Tsodikov
Topchiev Institute of Petrochemical Synthesis, Russian Academy of Sciences
4 shared publications
Latest Publications
- 1 February 2025
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 16 (1) , 10-15
Synthesis, Thermal Stability, and Catalytic Activity of Ce0.72Zr0.18Pr0.1O2 – δ Nanodispersed Solid Solution in CO Oxidation Reaction
A Ce0.72Zr0.18Pr0.1O2 – δ nanodispersed solid solution is synthesized by codeposition followed by thermal treatment. The identification of the material is performed by X-ray diffraction, X-ray fluorescence analysis, X-ray photoelectron spectroscopy, transmission electron microscopy, low-temperature adsorption of nitrogen, and gas chromatography. It is found that the synthesized Ce0.72Zr0.18Pr0.1O2 – δ solid solution is superior to CeO2 and Ce0.8Zr0.2O2 in catalytic activity and thermal stability as a result of doping with Pr3+ ions.
- 1 February 2025
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 16 (1) , 10-15
Synthesis, Thermal Stability, and Catalytic Activity of Ce0.72Zr0.18Pr0.1O2 – δ Nanodispersed Solid Solution in CO Oxidation Reaction
A Ce0.72Zr0.18Pr0.1O2 – δ nanodispersed solid solution is synthesized by codeposition followed by thermal treatment. The identification of the material is performed by X-ray diffraction, X-ray fluorescence analysis, X-ray photoelectron spectroscopy, transmission electron microscopy, low-temperature adsorption of nitrogen, and gas chromatography. It is found that the synthesized Ce0.72Zr0.18Pr0.1O2 – δ solid solution is superior to CeO2 and Ce0.8Zr0.2O2 in catalytic activity and thermal stability as a result of doping with Pr3+ ions.
- 4 September 2024
- Published by Springer Nature in Catalysis Letters
- Vol. 154 (11) , 6144-6156
Low Ag concentration Ag/CeO2 catalysts prepared with various CeO2 precursors in carbon monoxide oxidation reaction
- 4 September 2024
- Published by Springer Nature in Catalysis Letters
- Vol. 154 (11) , 6144-6156
Low Ag concentration Ag/CeO2 catalysts prepared with various CeO2 precursors in carbon monoxide oxidation reaction
- 18 July 2024
- Published by The Russian Academy of Sciences in Žurnal prikladnoj himii
- Vol. 97 (1) , 31-36
Каталитическая активность высокодисперсных твердых растворов Ce 0.85 Zr 0.10 MЕ 0.05 O 2–δ , где Mе — La, Nd, Gd, в реакции полного окисления метана
Высокодисперсные твердые растворы Ce0.85Zr0.10Mе0.05O2–δ, где Mе — La, Nd, Gd, синтезированы методом соосаждения с последующей термообработкой. Материалы охарактезированы методами рентгенофазового анализа, рентгеновской флуоресцентной спектроскопии, низкотемпературной адсорбции азота, просвечивающей электронной микроскопии и газовой хроматографии. Синтезированные материалы проявляют высокую активность в реакции полного окисления метана. Каталитическая активность твердых растворов зависит от ионного радиуса редкоземельного допанта и уменьшается в ряду La → Nd → Gd. Показана перспективность применения Ce0.85Zr0.10La0.05O2–δ в качестве носителя палладия. Каталитическая активность 0.5% PdО/Ce0.85Zr0.10La0.05O2–δ превосходит активность образца сравнения 0.5% PdО/γ-Al2O3, что демонстрирует целесообразность применения синтезированного твердого раствора в качестве носителя активного компонента.
- 18 July 2024
- Published by The Russian Academy of Sciences in Žurnal prikladnoj himii
- Vol. 97 (1) , 31-36
Каталитическая активность высокодисперсных твердых растворов Ce 0.85 Zr 0.10 MЕ 0.05 O 2–δ , где Mе — La, Nd, Gd, в реакции полного окисления метана
Высокодисперсные твердые растворы Ce0.85Zr0.10Mе0.05O2–δ, где Mе — La, Nd, Gd, синтезированы методом соосаждения с последующей термообработкой. Материалы охарактезированы методами рентгенофазового анализа, рентгеновской флуоресцентной спектроскопии, низкотемпературной адсорбции азота, просвечивающей электронной микроскопии и газовой хроматографии. Синтезированные материалы проявляют высокую активность в реакции полного окисления метана. Каталитическая активность твердых растворов зависит от ионного радиуса редкоземельного допанта и уменьшается в ряду La → Nd → Gd. Показана перспективность применения Ce0.85Zr0.10La0.05O2–δ в качестве носителя палладия. Каталитическая активность 0.5% PdО/Ce0.85Zr0.10La0.05O2–δ превосходит активность образца сравнения 0.5% PdО/γ-Al2O3, что демонстрирует целесообразность применения синтезированного твердого раствора в качестве носителя активного компонента.
- 30 June 2024
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- No. 6,p. 34-39
Prospects for processing deactivated Co – Mо/Al2O3 catalyst of diesel hydrotreating
Deactivated catalysts of diesel hydrotreating are regarded as hazardous wastes and cannot be buried in the ground; therefore, this results in a significant volume of hazardous wastes with a high content of non-ferrous metals. Developing methods of recovery and recycling of deactivated hydro treating catalysts is a currently relevant field of research in modern chemical technology. The article presents the results of studies on partial processing of deactivated Co – Mo/Al2O3 catalyst of diesel hydrotreating to apply it in processes of gas and waste water cleaning from toxic impurities. The authors studied nature of a leaching agent and a method of extracting molybdenum from the catalyst. A more efficient and selective leaching of molybdenum with a leaching degree of 90% or more requires treatment with a sodium carbonate solution after preliminary annealing of the deactivated catalyst to remove carbon deposits from the surface. Calcium molybdate will be separated from the leaching solution, which may be used as an alloying addition to steels. Extraction of molybdenum to the solution as sodium molybdate resulted in producing a Сo/Al2O3 material, whose composition was characterized by a method of energy-dispersive X-ray spectroscopy, and a porous structure — by a method of low-temperature nitrogen adsorption. Со/Al2O3 showed high activity and stability as a catalyst in an oxidative degradation of carmoisine azo dyes in a water solution (the dye bleeding rate was 95–97% in 30 minutes of contact), and catalytic activity in the medium-temperature degradation of carbon monoxide (temperature of 100% CO degradation was 475 oС). Thus, the material is promising for oxidative processes of ecological catalysis, namely degradation of toxic impurities in waste water and gas emissions. Research was funded by the Ministry of Education and Science of the Russian Federation as part of state order No. FSSM-2023-0004.
- 30 June 2024
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- No. 6,p. 34-39
Prospects for processing deactivated Co – Mо/Al2O3 catalyst of diesel hydrotreating
Deactivated catalysts of diesel hydrotreating are regarded as hazardous wastes and cannot be buried in the ground; therefore, this results in a significant volume of hazardous wastes with a high content of non-ferrous metals. Developing methods of recovery and recycling of deactivated hydro treating catalysts is a currently relevant field of research in modern chemical technology. The article presents the results of studies on partial processing of deactivated Co – Mo/Al2O3 catalyst of diesel hydrotreating to apply it in processes of gas and waste water cleaning from toxic impurities. The authors studied nature of a leaching agent and a method of extracting molybdenum from the catalyst. A more efficient and selective leaching of molybdenum with a leaching degree of 90% or more requires treatment with a sodium carbonate solution after preliminary annealing of the deactivated catalyst to remove carbon deposits from the surface. Calcium molybdate will be separated from the leaching solution, which may be used as an alloying addition to steels. Extraction of molybdenum to the solution as sodium molybdate resulted in producing a Сo/Al2O3 material, whose composition was characterized by a method of energy-dispersive X-ray spectroscopy, and a porous structure — by a method of low-temperature nitrogen adsorption. Со/Al2O3 showed high activity and stability as a catalyst in an oxidative degradation of carmoisine azo dyes in a water solution (the dye bleeding rate was 95–97% in 30 minutes of contact), and catalytic activity in the medium-temperature degradation of carbon monoxide (temperature of 100% CO degradation was 475 oС). Thus, the material is promising for oxidative processes of ecological catalysis, namely degradation of toxic impurities in waste water and gas emissions. Research was funded by the Ministry of Education and Science of the Russian Federation as part of state order No. FSSM-2023-0004.
- 30 June 2024
- Published by Ore and Metals Publishing House in CIS Iron and Steel Review
- Vol. 27, 113-117
Recycling of red mud in iron-containing catalyst for oxidizing organic impurities in waste water
Red mud is a solid waste of the industrial process of natural bauxite processing in aluminum production by the Bayer method. Currently, there is no effective and profitable technology for industrial red mud processing, and most of it is placed for permanent storage in specialized sludge storage facilities, and therefore development of the recycling technologies for this man-made waste into functional materials for various purposes is extremely relevant, since it will allow both to use its potential raw material resource and to solve environmental problems. This paper presents the results of investigations of the red mud recycling possibility at the Bogoslovsky aluminum plant into an ironcontaining catalyst for waste water purification with removal of organic impurities by their oxidizing destruction using hydrogen peroxide. Identification of the initial and obtained samples was carried out by methods of energy dispersive X-ray spectroscopy,s canning electron microscopy, low-temperature nitrogen adsorption, atomic absorption spectroscopy. It is shown that use of hydrochloric acid treatment of red mud with subsequent precipitation of dissolved compounds with ammonium carbonate and calcination of the precipitate allows to obtain the material with the iron content 55.17 wt. %. The sample has a developed specific surface area of 98.4 m2/g and porosity of 0.174 cm3/g, and consists of particles having a shape close to spherical with an average size of about 0.2–0.3 μm. The obtained material showed high catalytic activity and stability in the oxidation reaction of organic substances (on the example of the azo dye carmoisine) in an aqueous solution with hydrogen peroxide. The degree of discoloration of the dye solution during 30 minutes of contact was at least 94 % during 20 cycles of using the catalyst.
- 30 June 2024
- Published by Ore and Metals Publishing House in CIS Iron and Steel Review
- Vol. 27, 113-117
Recycling of red mud in iron-containing catalyst for oxidizing organic impurities in waste water
Red mud is a solid waste of the industrial process of natural bauxite processing in aluminum production by the Bayer method. Currently, there is no effective and profitable technology for industrial red mud processing, and most of it is placed for permanent storage in specialized sludge storage facilities, and therefore development of the recycling technologies for this man-made waste into functional materials for various purposes is extremely relevant, since it will allow both to use its potential raw material resource and to solve environmental problems. This paper presents the results of investigations of the red mud recycling possibility at the Bogoslovsky aluminum plant into an ironcontaining catalyst for waste water purification with removal of organic impurities by their oxidizing destruction using hydrogen peroxide. Identification of the initial and obtained samples was carried out by methods of energy dispersive X-ray spectroscopy,s canning electron microscopy, low-temperature nitrogen adsorption, atomic absorption spectroscopy. It is shown that use of hydrochloric acid treatment of red mud with subsequent precipitation of dissolved compounds with ammonium carbonate and calcination of the precipitate allows to obtain the material with the iron content 55.17 wt. %. The sample has a developed specific surface area of 98.4 m2/g and porosity of 0.174 cm3/g, and consists of particles having a shape close to spherical with an average size of about 0.2–0.3 μm. The obtained material showed high catalytic activity and stability in the oxidation reaction of organic substances (on the example of the azo dye carmoisine) in an aqueous solution with hydrogen peroxide. The degree of discoloration of the dye solution during 30 minutes of contact was at least 94 % during 20 cycles of using the catalyst.
- 1 January 2024
- Published by Science & Technology in Materials Science
Synthesis, thermal stability and catalytic activity of Ce0.72Zr0.18Pr0.1O2-δ nanodispersed solid solution in CO oxidation reaction
????? ??????????, ?????????? ??????????????, ?????????? ??????????, ??????? ???????, ?????? ?? ????????, ?????????? ????????, ???????? ??????????, ??????????? ???????, ????? ? ??????????, ?????????? ??????????, ??????? ??????????
- 1 January 2024
- Published by Science & Technology in Materials Science
Synthesis, thermal stability and catalytic activity of Ce0.72Zr0.18Pr0.1O2-δ nanodispersed solid solution in CO oxidation reaction
????? ??????????, ?????????? ??????????????, ?????????? ??????????, ??????? ???????, ?????? ?? ????????, ?????????? ????????, ???????? ??????????, ??????????? ???????, ????? ? ??????????, ?????????? ??????????, ??????? ??????????
- 1 October 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (5-6) , 1435-1440
Synthesis and Catalytic Activity of Highly Dispersed Solid Solutions Ce0.9Sn0.1O2 and Ce0.8Sn0.1Zr0.1O2 in CO Oxidation
Fluorite-like solid solutions of Ce0.9Sn0.1O2 and Ce0.8Sn0.1Zr0.1O2 were synthesized by coprecipitation using ammonium carbonate as a precipitant. The samples were characterized by X-ray powder diffraction analysis, scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy, low-temperature nitrogen adsorption, and gas chromatography. It was shown that the solid solutions are formed already at an annealing temperature of 550°C. In this process, platelike particles are formed, the size of which, according to SEM data, is 4 μm. The synthesized materials have a mesoporous structure. The specific surface areas of Ce0.9Sn0.1O2 and Ce0.8Zr0.1Sn0.1O2 samples are 80.6 and 76.3 m2/g, respectively. Calcination at a temperature of 800°C leads to an increase in the particle size up to 8–10 μm. The specific surface area after calcination is the highest (15.3 m2/g) for the Ce0.8Zr0.1Sn0.1O2 sample, which is due to the presence of zirconium ions in its composition. The synthesized materials demonstrated high activity in CO oxidation. The maximum catalytic activity was observed for the two-component system Ce0.9Sn0.1O2: T50% at 180°C and T90% at 236°C. Of the samples calcined at a temperature of 800°C, Ce0.8Zr0.1Sn0.1O2 is the most active, which is due to the formation of a more heat-resistant system in comparison with cerium dioxide and Ce0.9Sn0.1O2. To increase the thermal stability, it is advisable to dope the two-component material Ce0.9Sn0.1O2 with Zr+4 ions.
- 1 October 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (5-6) , 1435-1440
Synthesis and Catalytic Activity of Highly Dispersed Solid Solutions Ce0.9Sn0.1O2 and Ce0.8Sn0.1Zr0.1O2 in CO Oxidation
Fluorite-like solid solutions of Ce0.9Sn0.1O2 and Ce0.8Sn0.1Zr0.1O2 were synthesized by coprecipitation using ammonium carbonate as a precipitant. The samples were characterized by X-ray powder diffraction analysis, scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy, low-temperature nitrogen adsorption, and gas chromatography. It was shown that the solid solutions are formed already at an annealing temperature of 550°C. In this process, platelike particles are formed, the size of which, according to SEM data, is 4 μm. The synthesized materials have a mesoporous structure. The specific surface areas of Ce0.9Sn0.1O2 and Ce0.8Zr0.1Sn0.1O2 samples are 80.6 and 76.3 m2/g, respectively. Calcination at a temperature of 800°C leads to an increase in the particle size up to 8–10 μm. The specific surface area after calcination is the highest (15.3 m2/g) for the Ce0.8Zr0.1Sn0.1O2 sample, which is due to the presence of zirconium ions in its composition. The synthesized materials demonstrated high activity in CO oxidation. The maximum catalytic activity was observed for the two-component system Ce0.9Sn0.1O2: T50% at 180°C and T90% at 236°C. Of the samples calcined at a temperature of 800°C, Ce0.8Zr0.1Sn0.1O2 is the most active, which is due to the formation of a more heat-resistant system in comparison with cerium dioxide and Ce0.9Sn0.1O2. To increase the thermal stability, it is advisable to dope the two-component material Ce0.9Sn0.1O2 with Zr+4 ions.
- 18 June 2021
- Published by Pleiades Publishing Ltd in Petroleum Chemistry
- Vol. 61 (7) , 748-761
Effects of Support on the Formation and Activity of Gold Catalysts for Ethanol Conversion to Butanol
Using a combination of physicochemical methods, such as TEM, SEM, EDS, XPS, NH3–TPD, and N2 adsorption, the study investigates the structure of a number of supports (Al2O3, SiO2, TiO2, ZrO2, and C) and of Au/support catalyst samples (Au = 0.5%). The concentration of highly active 2–4 nm gold particles in Au catalysts is influenced by the support’s texture; this concentration increases in the following order: Au/TiO2 < Au/ZrO2 < Au/C < Au/SiO2 << Au/Al2O3. The acidity of Au catalysts is influenced by the support’s nature; this acidity decreases in the following order: Al2O3 > TiO2 > ZrO2 > SiO2 >> Au/C. At 275°C, a carbon support is inactive in ethanol conversion to butanol. In the presence of oxide supports, the target reaction occurs at a relatively low rate by a bimolecular condensation mechanism. Over Au/Al2O3, Au/SiO2, Au/TiO2, or Au/ZrO2, the reaction occurs more rapidly by an aldol condensation mechanism. At an ethanol conversion of 14–18%, the butanol selectivity increases in the following order: Au/C(0) << Au/SiO2 (0.4%) < Au/ZrO2 (1.5%) < Au/TiO2 (2%) << Au/Al2O3 (78%). The high efficiency of Au/Al2O3 stems from the high density of the Aln+–O2– sites located on the support’s surface, and of the coordination-unsaturated Au0(KH) atoms located on the surface of 2–4 nm gold particles.
- 18 June 2021
- Published by Pleiades Publishing Ltd in Petroleum Chemistry
- Vol. 61 (7) , 748-761
Effects of Support on the Formation and Activity of Gold Catalysts for Ethanol Conversion to Butanol
Using a combination of physicochemical methods, such as TEM, SEM, EDS, XPS, NH3–TPD, and N2 adsorption, the study investigates the structure of a number of supports (Al2O3, SiO2, TiO2, ZrO2, and C) and of Au/support catalyst samples (Au = 0.5%). The concentration of highly active 2–4 nm gold particles in Au catalysts is influenced by the support’s texture; this concentration increases in the following order: Au/TiO2 < Au/ZrO2 < Au/C < Au/SiO2 << Au/Al2O3. The acidity of Au catalysts is influenced by the support’s nature; this acidity decreases in the following order: Al2O3 > TiO2 > ZrO2 > SiO2 >> Au/C. At 275°C, a carbon support is inactive in ethanol conversion to butanol. In the presence of oxide supports, the target reaction occurs at a relatively low rate by a bimolecular condensation mechanism. Over Au/Al2O3, Au/SiO2, Au/TiO2, or Au/ZrO2, the reaction occurs more rapidly by an aldol condensation mechanism. At an ethanol conversion of 14–18%, the butanol selectivity increases in the following order: Au/C(0) << Au/SiO2 (0.4%) < Au/ZrO2 (1.5%) < Au/TiO2 (2%) << Au/Al2O3 (78%). The high efficiency of Au/Al2O3 stems from the high density of the Aln+–O2– sites located on the support’s surface, and of the coordination-unsaturated Au0(KH) atoms located on the surface of 2–4 nm gold particles.
- 1 April 2021
- Published by Pleiades Publishing Ltd in Petroleum Chemistry
- Vol. 61 (4) , 498-503
Regeneration of a Porous Iron-Containing Carbon Adsorbent under Plasma-Catalytic Conditions Assisted by Microwave Irradiation
This article reports experimental data on a double-step technology for processing a model organic contaminant (m-cresol) adsorbed in the pores of an iron-containing carbon adsorbent (specific surface area 616 m2/g) under microwave irradiation. The first step comprised the decomposition of cresol into a hydrogen-containing gas and a carbon residue under plasma-catalytic conditions assisted by microwave irradiation at an induced temperature of 600°C. Cresol was completely converted after 25 min of the MW irradiation. The second step consisted of adsorbent regeneration (by CO2 treatment under MW irradiation to remove the carbon residue) followed by thermal shock treatment (by decomposition of a pre-adsorbed ammonium hydroxide). After the regeneration, the specific surface area was 500 m2/g. The regenerated adsorbent exhibited almost the same cresol adsorption capacity as the starting material.
- 1 April 2021
- Published by Pleiades Publishing Ltd in Petroleum Chemistry
- Vol. 61 (4) , 498-503
Regeneration of a Porous Iron-Containing Carbon Adsorbent under Plasma-Catalytic Conditions Assisted by Microwave Irradiation
This article reports experimental data on a double-step technology for processing a model organic contaminant (m-cresol) adsorbed in the pores of an iron-containing carbon adsorbent (specific surface area 616 m2/g) under microwave irradiation. The first step comprised the decomposition of cresol into a hydrogen-containing gas and a carbon residue under plasma-catalytic conditions assisted by microwave irradiation at an induced temperature of 600°C. Cresol was completely converted after 25 min of the MW irradiation. The second step consisted of adsorbent regeneration (by CO2 treatment under MW irradiation to remove the carbon residue) followed by thermal shock treatment (by decomposition of a pre-adsorbed ammonium hydroxide). After the regeneration, the specific surface area was 500 m2/g. The regenerated adsorbent exhibited almost the same cresol adsorption capacity as the starting material.
- 1 March 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (2) , 468-476
Thermal Stability and Catalytic Activity of the MnOx–CeO2 and the MnOx–ZrO2–CeO2 Highly Dispersed Materials in the Carbon Monoxide Oxidation Reaction
Highly dispersed MnOx–CeO2 and MnOx–ZrO2–CeO2 catalysts for the carbon monoxide oxidation reaction are synthesized. Using the XRF and the XRD methods, the formation of the Mn–Ce–O and the Mn–Zr–Ce–O solid solutions, as well as the presence of Mn2O3 and Mn3O4, is established. The specific surface area of the synthesized materials is 121 and 155 m2/g, respectively, the particle size being equal to 8–10 nm. The X-ray photoelectron (XPS) spectra is deconvolved and the relative content of the ionic forms of Mn, the lattice oxygen Oα, and the high-energy forms Oβ are determined. Upon studying the thermal stability of catalysts, it is established that the two-component systems have low thermal stability, causing the particle size to increase to 32 nm, the specific surface area to decrease to 29 m2/g, and thus the catalytic activity to deteriorate. For MnOx–ZrO2–CeO2, less significant changes take place: the particle size is 27 nm, the specific surface area is 43 m2/g, and thus its catalytic activity is higher than that for MnOx–CeO2. Investigation of the state of the components of the near-surface layer of catalysts after isothermal aging makes it possible to ascertain the change in content of ionic forms of Mn, Oα, and Oβ. It is concluded that doping of the two-component MnOx–CeO2 systems with the Zr4+ ions is expedient. The resulting ZrO2–MnOx–CeO2 solid solution is more resistant to high temperatures.
- 1 March 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (2) , 468-476
Thermal Stability and Catalytic Activity of the MnOx–CeO2 and the MnOx–ZrO2–CeO2 Highly Dispersed Materials in the Carbon Monoxide Oxidation Reaction
Highly dispersed MnOx–CeO2 and MnOx–ZrO2–CeO2 catalysts for the carbon monoxide oxidation reaction are synthesized. Using the XRF and the XRD methods, the formation of the Mn–Ce–O and the Mn–Zr–Ce–O solid solutions, as well as the presence of Mn2O3 and Mn3O4, is established. The specific surface area of the synthesized materials is 121 and 155 m2/g, respectively, the particle size being equal to 8–10 nm. The X-ray photoelectron (XPS) spectra is deconvolved and the relative content of the ionic forms of Mn, the lattice oxygen Oα, and the high-energy forms Oβ are determined. Upon studying the thermal stability of catalysts, it is established that the two-component systems have low thermal stability, causing the particle size to increase to 32 nm, the specific surface area to decrease to 29 m2/g, and thus the catalytic activity to deteriorate. For MnOx–ZrO2–CeO2, less significant changes take place: the particle size is 27 nm, the specific surface area is 43 m2/g, and thus its catalytic activity is higher than that for MnOx–CeO2. Investigation of the state of the components of the near-surface layer of catalysts after isothermal aging makes it possible to ascertain the change in content of ionic forms of Mn, Oα, and Oβ. It is concluded that doping of the two-component MnOx–CeO2 systems with the Zr4+ ions is expedient. The resulting ZrO2–MnOx–CeO2 solid solution is more resistant to high temperatures.