Antti Forsström
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Antti Forsström has a total of 21 co-authors. Here are the top co-authors by number of shared publications:
Hannu Hänninen
Department of Mechanical Engineering Aalto University School of Engineering Aalto Finland
5 shared publicationsYuriy Yagodzinskyy
Department of Mechanical Engineering Aalto University School of Engineering Aalto Finland
4 shared publicationsH. Hänninen
Aalto University
3 shared publicationsSebastian Lindqvist
2 shared publicationsBruno Reinaldo Goncalves
1 shared publicationG. Scotti
Aalto University
1 shared publication
Latest Publications
- Open Access
- 25 June 2025
- Published by Elsevier in Theoretical and Applied Fracture Mechanics
- Vol. 139
Assessment of full-field J-integrals through digital image correlation using stress estimation based on measured strains
- 25 June 2025
- Published by Elsevier in Theoretical and Applied Fracture Mechanics
- Vol. 139
Open AccessAssessment of full-field J-integrals through digital image correlation using stress estimation based on measured strains
- Open Access
- 10 December 2024
- Published by Elsevier in Theoretical and Applied Fracture Mechanics
- Vol. 136
Fracture toughness of additively manufactured 316L stainless steel measured with miniature C(T) specimens − compliance versus normalization technique
- 10 December 2024
- Published by Elsevier in Theoretical and Applied Fracture Mechanics
- Vol. 136
Open AccessFracture toughness of additively manufactured 316L stainless steel measured with miniature C(T) specimens − compliance versus normalization technique
- Open Access
- 22 July 2020
- Published by Wiley in Materials and Corrosion
- Vol. 72 (1-2) , 245-254
Hydrogen embrittlement of nodular cast iron
Ferritic nodular cast iron, intended for use as the material for inserts of canisters for long‐term geological disposal of spent nuclear fuel, was studied for hydrogen sensitivity. In the canisters, the insert provides the mechanical strength against external loads. Hydrogen was charged from 0.1 N H2SO4 solution in free‐corrosion tests and under controlled cathodic potential. Hydrogen uptake and trapping were then measured using thermal desorption spectroscopy. The hydrogen desorption rate after hydrogen charging manifests two distinct peaks. Plastic deformation during hydrogen charging increases the hydrogen uptake considerably. Hydrogen reduces the elongation to fracture and time to fracture in slow strain rate testing and constant load testing (CLT), respectively. Especially, the strain rate in CLT is dramatically increased. The appearance of hydrogen‐induced cracking in the ferrite phase changes from ductile dimple fracture to brittle cleavage fracture due to hydrogen charging, which initiates from the interphases of the graphite nodules. The results are discussed in terms of the role of hydrogen and the graphite nodules in hydrogen embrittlement of ductile cast iron.
- 22 July 2020
- Published by Wiley in Materials and Corrosion
- Vol. 72 (1-2) , 245-254
Open AccessHydrogen embrittlement of nodular cast iron
Ferritic nodular cast iron, intended for use as the material for inserts of canisters for long‐term geological disposal of spent nuclear fuel, was studied for hydrogen sensitivity. In the canisters, the insert provides the mechanical strength against external loads. Hydrogen was charged from 0.1 N H2SO4 solution in free‐corrosion tests and under controlled cathodic potential. Hydrogen uptake and trapping were then measured using thermal desorption spectroscopy. The hydrogen desorption rate after hydrogen charging manifests two distinct peaks. Plastic deformation during hydrogen charging increases the hydrogen uptake considerably. Hydrogen reduces the elongation to fracture and time to fracture in slow strain rate testing and constant load testing (CLT), respectively. Especially, the strain rate in CLT is dramatically increased. The appearance of hydrogen‐induced cracking in the ferrite phase changes from ductile dimple fracture to brittle cleavage fracture due to hydrogen charging, which initiates from the interphases of the graphite nodules. The results are discussed in terms of the role of hydrogen and the graphite nodules in hydrogen embrittlement of ductile cast iron.
- Open Access
- 29 June 2020
- Published by Wiley in Materials and Corrosion
- Vol. 72 (1-2) , 317-332
Sulphide‐induced stress corrosion cracking and hydrogen absorption of copper in deoxygenated water at 90°C
Stress corrosion cracking (SCC) of oxygen‐free phosphorous‐alloyed copper was investigated in sulphide‐ and chloride‐containing deoxygenated water at 90°C with sulphide concentrations of 0.001 and 0.00001 M. Several intergranular defects were found in the specimen exposed to the high sulphide environment. Similar defects were not found in the low sulphide environment, where only slight corrosion on grain boundaries and slip lines occurred. Hydrogen content measurements show an increase in hydrogen uptake of the plastically deformed specimens, which is dependent on the sulphide concentration and on plastic deformation of copper. However, the highest hydrogen content was measured in friction stir welds, welded in air without shielding gas, and tested in the high sulphide environment. The embedded oxide particles in the weld metal act as local hydrogen trapping sites and selectively react with the sulphide solution. A relatively thick air‐formed oxide film covers the copper canisters when deposited, which transforms into a sulphide film in the repository conditions. Thus, some of the coupon specimens were pre‐oxidised. The conversion of the pre‐existing Cu2O film into Cu2S film occurs quickly and the transformation is almost 100% efficient. The structure and properties of the Cu2S films, susceptibility of copper to sulphide‐induced SCC and hydrogen uptake of copper in reducing, anoxic repository conditions are discussed.
- 29 June 2020
- Published by Wiley in Materials and Corrosion
- Vol. 72 (1-2) , 317-332
Open AccessSulphide‐induced stress corrosion cracking and hydrogen absorption of copper in deoxygenated water at 90°C
Stress corrosion cracking (SCC) of oxygen‐free phosphorous‐alloyed copper was investigated in sulphide‐ and chloride‐containing deoxygenated water at 90°C with sulphide concentrations of 0.001 and 0.00001 M. Several intergranular defects were found in the specimen exposed to the high sulphide environment. Similar defects were not found in the low sulphide environment, where only slight corrosion on grain boundaries and slip lines occurred. Hydrogen content measurements show an increase in hydrogen uptake of the plastically deformed specimens, which is dependent on the sulphide concentration and on plastic deformation of copper. However, the highest hydrogen content was measured in friction stir welds, welded in air without shielding gas, and tested in the high sulphide environment. The embedded oxide particles in the weld metal act as local hydrogen trapping sites and selectively react with the sulphide solution. A relatively thick air‐formed oxide film covers the copper canisters when deposited, which transforms into a sulphide film in the repository conditions. Thus, some of the coupon specimens were pre‐oxidised. The conversion of the pre‐existing Cu2O film into Cu2S film occurs quickly and the transformation is almost 100% efficient. The structure and properties of the Cu2S films, susceptibility of copper to sulphide‐induced SCC and hydrogen uptake of copper in reducing, anoxic repository conditions are discussed.
- 29 November 2019
- Published by Walter de Gruyter GmbH in Corrosion Reviews
- Vol. 38 (1) , 99
Corrigendum to: Hydrogen effects on mechanical performance of nodular cast iron
Article Corrigendum to: Hydrogen effects on mechanical performance of nodular cast iron was published on February 1, 2020 in the journal Corrosion Reviews (volume 38, issue 1).
- 29 November 2019
- Published by Walter de Gruyter GmbH in Corrosion Reviews
- Vol. 38 (1) , 99
Corrigendum to: Hydrogen effects on mechanical performance of nodular cast iron
Article Corrigendum to: Hydrogen effects on mechanical performance of nodular cast iron was published on February 1, 2020 in the journal Corrosion Reviews (volume 38, issue 1).
- 31 May 2019
- Published by Walter de Gruyter GmbH in Corrosion Reviews
- Vol. 37 (5) , 441-454
Hydrogen effects on mechanical performance of nodular cast iron
The KBS-3 method for long-term disposal of spent nuclear fuel is designed with an external self-standing copper shell, which provides the most important barrier against corrosion and escape of radionuclides, and an internal nodular cast iron insert, which provides the load-bearing structure against external loads. The material intended for the load-bearing insert is ferritic nodular cast iron EN 1563 grade EN-GJS-400-15U. In this paper, hydrogen uptake and sensitivity to hydrogen-induced cracking of the cast iron were studied using tensile testing under continuous electrochemical charging in 1 N H 2 SO 4 solution. Hydrogen uptake was measured by using the thermal desorption method. It was found that the hydrogen desorption profile manifests three distinct peaks at initial locations of 400, 500, and 700 K with a heating rate of 6 K/min. Plastic deformation results in a remarkable increase of the 400 K peak, which indicates hydrogen uptake during deformation. In the constant extension rate tests (CERT) and the constant load tests (CLT), electrochemical hydrogen charging reduced markedly the elongation to fracture and time to fracture, respectively. In CLT, hydrogen charging increased dramatically the creep rate at the applied load of about 0.7 yield stress. Ligaments between the graphite nodules exhibit brittle cleavage facets in the presence of hydrogen, while the ligaments show a characteristic ductile appearance of shear and small dimples when testing in air or distilled water. The obtained results are discussed in terms of the known mechanisms of hydrogen-induced cracking and the role of the graphite nodules in the embrittlement of ductile cast iron.
- 31 May 2019
- Published by Walter de Gruyter GmbH in Corrosion Reviews
- Vol. 37 (5) , 441-454
Hydrogen effects on mechanical performance of nodular cast iron
The KBS-3 method for long-term disposal of spent nuclear fuel is designed with an external self-standing copper shell, which provides the most important barrier against corrosion and escape of radionuclides, and an internal nodular cast iron insert, which provides the load-bearing structure against external loads. The material intended for the load-bearing insert is ferritic nodular cast iron EN 1563 grade EN-GJS-400-15U. In this paper, hydrogen uptake and sensitivity to hydrogen-induced cracking of the cast iron were studied using tensile testing under continuous electrochemical charging in 1 N H 2 SO 4 solution. Hydrogen uptake was measured by using the thermal desorption method. It was found that the hydrogen desorption profile manifests three distinct peaks at initial locations of 400, 500, and 700 K with a heating rate of 6 K/min. Plastic deformation results in a remarkable increase of the 400 K peak, which indicates hydrogen uptake during deformation. In the constant extension rate tests (CERT) and the constant load tests (CLT), electrochemical hydrogen charging reduced markedly the elongation to fracture and time to fracture, respectively. In CLT, hydrogen charging increased dramatically the creep rate at the applied load of about 0.7 yield stress. Ligaments between the graphite nodules exhibit brittle cleavage facets in the presence of hydrogen, while the ligaments show a characteristic ductile appearance of shear and small dimples when testing in air or distilled water. The obtained results are discussed in terms of the known mechanisms of hydrogen-induced cracking and the role of the graphite nodules in the embrittlement of ductile cast iron.
- Open Access
- 30 April 2019
- Published by Springer Nature in Experimental Mechanics
- Vol. 60 (1) , 3-12
Quantifying the Effectiveness of Patterning, Test Conditions, and DIC Parameters for Characterization of Plastic Strain Localization
- 30 April 2019
- Published by Springer Nature in Experimental Mechanics
- Vol. 60 (1) , 3-12
Open AccessQuantifying the Effectiveness of Patterning, Test Conditions, and DIC Parameters for Characterization of Plastic Strain Localization
- 1 June 2017
- Published by SAGE Publications in Materials Science and Technology
- Vol. 33 (9) , 1119-1129
Localisation of plastic deformation in friction stir and electron beam copper welds
Optical strain measurement through digital image correlation during tensile testing was utilised to study the effect of strain rate and welding defects on localisation of plastic deformation in friction stir welded and electron beam welded phosphorous-alloyed oxygen-free copper. Welds cut from full-size nuclear waste copper canisters and additionally made defective welds were studied. Optical strain measurement represents a new way of studying deformation of materials and obtaining local material data. The data was used to construct strain maps and estimate local true stress–strain curves. Using Gini coefficients to quantify strain localisation, it appears that the lower strain rate resulted in slightly faster localisation of plastic deformation with lower stress level.
- 1 June 2017
- Published by SAGE Publications in Materials Science and Technology
- Vol. 33 (9) , 1119-1129
Localisation of plastic deformation in friction stir and electron beam copper welds
Optical strain measurement through digital image correlation during tensile testing was utilised to study the effect of strain rate and welding defects on localisation of plastic deformation in friction stir welded and electron beam welded phosphorous-alloyed oxygen-free copper. Welds cut from full-size nuclear waste copper canisters and additionally made defective welds were studied. Optical strain measurement represents a new way of studying deformation of materials and obtaining local material data. The data was used to construct strain maps and estimate local true stress–strain curves. Using Gini coefficients to quantify strain localisation, it appears that the lower strain rate resulted in slightly faster localisation of plastic deformation with lower stress level.
- Open Access
- 14 June 2016
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 47 (8) , 3956-3970
Effects of Thermal Aging on Material Properties, Stress Corrosion Cracking, and Fracture Toughness of AISI 316L Weld Metal
- 14 June 2016
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 47 (8) , 3956-3970
Open AccessEffects of Thermal Aging on Material Properties, Stress Corrosion Cracking, and Fracture Toughness of AISI 316L Weld Metal
- 8 July 2014
- Published by Wiley in Materials and Corrosion
- Vol. 66 (2) , 95-104
Grain boundary engineering of metastable 204Cu, 301, and 301LN austenitic stainless steels to improve their sensitization resistance
Grain boundary engineering (GBE) of 304 and 316 austenitic stainless steels has been widely researched but studies on other grades of austenitic stainless steels are less common. In this study, application of GBE on metastable austenitic stainless steels 204Cu, 301, and 301LN was assessed. Thermomechanical processing parameters were obtained for each of the tested steel grades by varying cold rolling reduction and annealing temperature, and analyzing the acquired grain boundary character distributions (GBCD) in scanning electron microscope (SEM) with electron backscatter diffraction (EBSD). A high fraction of about 80% low‐Σ CSL boundaries was attained in all of the tested steels. Effect of the GBE‐treatments on sensitization and intergranular corrosion properties was studied with Streicher and DL‐EPR tests. GBE‐treating was found to beneficially decrease the rate of intergranular corrosion and sensitization in 204Cu and 301 steels, but in low‐carbon 301LN steel no improvement was observed.
- 8 July 2014
- Published by Wiley in Materials and Corrosion
- Vol. 66 (2) , 95-104
Grain boundary engineering of metastable 204Cu, 301, and 301LN austenitic stainless steels to improve their sensitization resistance
Grain boundary engineering (GBE) of 304 and 316 austenitic stainless steels has been widely researched but studies on other grades of austenitic stainless steels are less common. In this study, application of GBE on metastable austenitic stainless steels 204Cu, 301, and 301LN was assessed. Thermomechanical processing parameters were obtained for each of the tested steel grades by varying cold rolling reduction and annealing temperature, and analyzing the acquired grain boundary character distributions (GBCD) in scanning electron microscope (SEM) with electron backscatter diffraction (EBSD). A high fraction of about 80% low‐Σ CSL boundaries was attained in all of the tested steels. Effect of the GBE‐treatments on sensitization and intergranular corrosion properties was studied with Streicher and DL‐EPR tests. GBE‐treating was found to beneficially decrease the rate of intergranular corrosion and sensitization in 204Cu and 301 steels, but in low‐carbon 301LN steel no improvement was observed.