Sabine Decker
Research Subjects
Sabine Decker has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
Lutz Krüger
Institute of Materials Engineering, Gustav-Zeuner-Straße, Freiberg, Germany
4 shared publicationsKatja Lange
Institute of Materials Engineering Gustav‐Zeuner‐Straße 5 Freiberg 09599 Germany
2 shared publications- Stefan Martin
Institute of Materials Science TU Bergakademie Freiberg Freiberg Germany
2 shared publications Tobias Dubberstein
Institute of Iron and Steel Technology Leipziger Straße 34 Freiberg 09599 Germany
2 shared publications- Lutz Krüger
Institute of Materials Engineering, TU Bergakademie Freiberg, 09599 Freiberg, Germany
1 shared publication Sarah Richter
Institute of Materials Science, TU Bergakademie Freiberg, Freiberg, Germany
1 shared publication
Latest Publications
- 30 July 2015
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 50 (13) , 1829-1836
Improved mechanical properties by high-energy milling and Spark Plasma Sintering of a TRIP-matrix composite
A composite reinforced with 5 vol% MgO partially stabilized zirconia and a high-alloyed TRIP-steel matrix (16% Cr, 6% Ni, 6% Mn) was processed. The objective was to trigger a phase transformation under mechanical stresses within the steel and the ceramic. Therefore, the composite was processed by both mixing (110 r/min) and dispersing by intense milling (250 r/min) of the initial powders, and subsequent Spark Plasma Sintering. During Spark Plasma Sintering, the dwell time was varied (5 min, 10 min). The steel/MgO partially stabilized zirconia interfaces were improved through the intense milling and the 10 min dwell time. Furthermore, 50% of the MgO partially stabilized zirconia transformed to the monoclinic phase under quasi-static compressive loading (10−3 s−1) and the composite had a 1% offset compressive yield strength of 665 MPa. Independent from the processing route, 65% of the steel transformed to α′-martensite.
- 30 July 2015
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 50 (13) , 1829-1836
Improved mechanical properties by high-energy milling and Spark Plasma Sintering of a TRIP-matrix composite
A composite reinforced with 5 vol% MgO partially stabilized zirconia and a high-alloyed TRIP-steel matrix (16% Cr, 6% Ni, 6% Mn) was processed. The objective was to trigger a phase transformation under mechanical stresses within the steel and the ceramic. Therefore, the composite was processed by both mixing (110 r/min) and dispersing by intense milling (250 r/min) of the initial powders, and subsequent Spark Plasma Sintering. During Spark Plasma Sintering, the dwell time was varied (5 min, 10 min). The steel/MgO partially stabilized zirconia interfaces were improved through the intense milling and the 10 min dwell time. Furthermore, 50% of the MgO partially stabilized zirconia transformed to the monoclinic phase under quasi-static compressive loading (10−3 s−1) and the composite had a 1% offset compressive yield strength of 665 MPa. Independent from the processing route, 65% of the steel transformed to α′-martensite.
- 11 March 2015
- Published by Wiley in Advanced Engineering Materials
- Vol. 17 (9) , 1351-1356
Influence of the Sulfur Content on the Mechanical Properties of a TRIP/TWIP‐Matrix Composite Reinforced with 10 vol% Mg‐PSZ
The influence of the sulfur content (0.02 wt%, 0.1 wt%) within the steel phase (16 wt% Cr, 6 wt% Mn, 9 wt% Ni) of a TRIP/TWIP‐matrix composite, reinforced with 10 vol% MgO‐partially stabilized zirconia (Mg‐PSZ), produced by spark plasma sintering (SPS) is investigated. By increasing the sulfur content of the steel phase, the powder particle size after gas atomization is reduced. Hence, the steel/Mg‐PSZ‐particle size ratio decreases and the distribution of the Mg‐PSZ is improved. Within this study, the effect of the sulfur content on microstructure and flow behavior under compressive loading are determined. With increasing sulfur content, the 1% compressive yield strength increases by 40 MPa. The sulfur forms precipitations with chromium and manganese especially at the steel/Mg‐PSZ interfaces, which cause a destabilization of the Mg‐PSZ during sintering. The destabilization prevents a possible stress‐induced phase transformation of the Mg‐PSZ.
- 11 March 2015
- Published by Wiley in Advanced Engineering Materials
- Vol. 17 (9) , 1351-1356
Influence of the Sulfur Content on the Mechanical Properties of a TRIP/TWIP‐Matrix Composite Reinforced with 10 vol% Mg‐PSZ
The influence of the sulfur content (0.02 wt%, 0.1 wt%) within the steel phase (16 wt% Cr, 6 wt% Mn, 9 wt% Ni) of a TRIP/TWIP‐matrix composite, reinforced with 10 vol% MgO‐partially stabilized zirconia (Mg‐PSZ), produced by spark plasma sintering (SPS) is investigated. By increasing the sulfur content of the steel phase, the powder particle size after gas atomization is reduced. Hence, the steel/Mg‐PSZ‐particle size ratio decreases and the distribution of the Mg‐PSZ is improved. Within this study, the effect of the sulfur content on microstructure and flow behavior under compressive loading are determined. With increasing sulfur content, the 1% compressive yield strength increases by 40 MPa. The sulfur forms precipitations with chromium and manganese especially at the steel/Mg‐PSZ interfaces, which cause a destabilization of the Mg‐PSZ during sintering. The destabilization prevents a possible stress‐induced phase transformation of the Mg‐PSZ.
- 1 September 2014
- Published by Wiley in Steel Research International
- Vol. 86 (5) , 544-549
Influence of the Sulfur Content on the Sintering Behavior and the Mechanical Properties of a CrMnNi‐TWIP‐Steel
The aim of the present study is the investigation of the influence of the sulfur content within the range of 0.02–0.1 wt% and the combined decrease of the particle size on the mechanical properties of a highly alloyed TWIP‐steel (TWinning Induced Plasticity; 16% Cr, 7% Mn, 9% Ni). Samples were processed by spark plasma sintering (SPS) and tested by quasi‐static compressive deformation (10−3 s−1). An increase of the surface‐active sulfur in TWIP‐steel is decreasing the surface tension (σ) of the liquid steel phase at a constant spraying parameter. The surface tension as a thermo‐physical property has a major impact on the particle size distribution of a metal powder in atomization. With a decrease in σ, the mass median particle size (d50) in steel powder is shifted to finer particles. Through the increased sulfur content, the compressive yield strength increases slightly about 40 MPa. A sulfur content of 0.05 wt% within the steel turned out to be optimal for the compressive properties by causing a high strength and work hardening through a fine grained microstructure, while the sulfur precipitations showed no pronounced negative influence. The mechanical properties were not negatively affected due to the increase of the sulfur content within the samples.
- 1 September 2014
- Published by Wiley in Steel Research International
- Vol. 86 (5) , 544-549
Influence of the Sulfur Content on the Sintering Behavior and the Mechanical Properties of a CrMnNi‐TWIP‐Steel
The aim of the present study is the investigation of the influence of the sulfur content within the range of 0.02–0.1 wt% and the combined decrease of the particle size on the mechanical properties of a highly alloyed TWIP‐steel (TWinning Induced Plasticity; 16% Cr, 7% Mn, 9% Ni). Samples were processed by spark plasma sintering (SPS) and tested by quasi‐static compressive deformation (10−3 s−1). An increase of the surface‐active sulfur in TWIP‐steel is decreasing the surface tension (σ) of the liquid steel phase at a constant spraying parameter. The surface tension as a thermo‐physical property has a major impact on the particle size distribution of a metal powder in atomization. With a decrease in σ, the mass median particle size (d50) in steel powder is shifted to finer particles. Through the increased sulfur content, the compressive yield strength increases slightly about 40 MPa. A sulfur content of 0.05 wt% within the steel turned out to be optimal for the compressive properties by causing a high strength and work hardening through a fine grained microstructure, while the sulfur precipitations showed no pronounced negative influence. The mechanical properties were not negatively affected due to the increase of the sulfur content within the samples.
- 25 April 2012
- Published by Wiley in Steel Research International
- Vol. 83 (6) , 521-528
Strain‐Rate‐Dependent Flow Stress and Failure of an Mg‐PSZ Reinforced TRIP Matrix Composite Produced by Spark Plasma Sintering
A composite consisting of 5 vol% MgO‐partially stabilized ZrO2 particles (Mg‐PSZ) and a TRIP‐steel‐matrix (CrNiMn steel; transformation induced plasticity) was produced through Spark Plasma Sintering. The processed material was tested under compression at various nominal strain rates (4 × 10−4 s−1; 10−3 s−1; 1 s−1, 102 s−1). Both, the pure steel and the composite showed a considerable plasticity and high strength due to the very fine grained steel matrix. The addition of 5 vol% ceramic particles led to a rise in the offset yield strength of 60 MPa till 90 MPa according to the applied strain rate. Up to a strain rate of 1 s−1, no change in offset yield strength was measured. A strain‐rate of 100 s−1 leads to a rise in the offset yield strength of approx. 100 MPa. Both, the ceramic and an increase in the strain rate implicate to an early generation of microdeterioration. Limited by the interfacial strength of steel and Mg‐PSZ, failure occurs early at the interfaces, which is shown in a decrease in the work hardening. During the compression, especially at higher strain‐rates, adiabatic heating occurred and counteracted to the martensitic transformation.
- 25 April 2012
- Published by Wiley in Steel Research International
- Vol. 83 (6) , 521-528
Strain‐Rate‐Dependent Flow Stress and Failure of an Mg‐PSZ Reinforced TRIP Matrix Composite Produced by Spark Plasma Sintering
A composite consisting of 5 vol% MgO‐partially stabilized ZrO2 particles (Mg‐PSZ) and a TRIP‐steel‐matrix (CrNiMn steel; transformation induced plasticity) was produced through Spark Plasma Sintering. The processed material was tested under compression at various nominal strain rates (4 × 10−4 s−1; 10−3 s−1; 1 s−1, 102 s−1). Both, the pure steel and the composite showed a considerable plasticity and high strength due to the very fine grained steel matrix. The addition of 5 vol% ceramic particles led to a rise in the offset yield strength of 60 MPa till 90 MPa according to the applied strain rate. Up to a strain rate of 1 s−1, no change in offset yield strength was measured. A strain‐rate of 100 s−1 leads to a rise in the offset yield strength of approx. 100 MPa. Both, the ceramic and an increase in the strain rate implicate to an early generation of microdeterioration. Limited by the interfacial strength of steel and Mg‐PSZ, failure occurs early at the interfaces, which is shown in a decrease in the work hardening. During the compression, especially at higher strain‐rates, adiabatic heating occurred and counteracted to the martensitic transformation.