Nataša Čuk
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Nataša Čuk has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
Matjaž Kunaver
Laboratory for Polymer Chemistry and Technology, National Institute of Chemistry, Hajdrihova 19, SI-1001, Ljubljana, Slovenia
2 shared publicationsAleš Ugovšek
Biotechnical Faculty, Department of Wood Science and Technology, University of Ljubljana, Rožna dolina C VIII/34, SI-1000, Ljubljana, Slovenia; M SORA d.d., Trg svobode 2, SI-4226 Žiri, Slovenia
1 shared publicationEma Fabjan
Center of Excellence PoliMaT Tehnološki park 24 SI‐1001 Ljubljana Slovenia
1 shared publicationIda Poljanšek
Biotechnical Faculty, Department of Wood Science and Technology, University of Ljubljana, Rožna dolina C VIII/34, SI-1000, Ljubljana, Slovenia
1 shared publicationMilan Šernek
Biotechnical Faculty, Department of Wood Science and Technology, University of Ljubljana, Rožna dolina C VIII/34, SI-1000, Ljubljana, Slovenia
1 shared publicationPetra Grželj
Center of Excellence PoliMaT Tehnološki park 24 SI‐1001 Ljubljana Slovenia
1 shared publication
Latest Publications
- 24 April 2015
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 29 (15) , 1553-1562
Properties of liquefied wood modified melamine-formaldehyde (MF) resin adhesive and its application for bonding particleboards
In this study, we modified melamine-formaldehyde (MF) resin adhesive with liquefied wood (LW) and determined the properties of MF–LW adhesive mixtures. Furthermore, we produced particleboards using prepared MF–LW mixtures and evaluated their mechanical and physical properties. Results showed that with increasing content of LW in the adhesive mixture gel time and peak temperature increased while reaction enthalpy decreased. With increasing substitution of MF resin adhesive with LW the thermal stability of adhesive mixture reduced, namely thermal degradation started at lower temperature and weight loss increased. Properties of particleboards improved with increasing amount of LW in the adhesive mixture up to 20% and then deteriorated. Nevertheless, the properties of particleboard with 30% LW in the adhesive mixture were comparable to the properties of particleboard without LW while they worsen at greater portion of LW. Consequently, MF resin adhesive with 30% LW substitution could be used to produce particleboards with suitable mechanical properties and reduced formaldehyde release content.
- 24 April 2015
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 29 (15) , 1553-1562
Properties of liquefied wood modified melamine-formaldehyde (MF) resin adhesive and its application for bonding particleboards
In this study, we modified melamine-formaldehyde (MF) resin adhesive with liquefied wood (LW) and determined the properties of MF–LW adhesive mixtures. Furthermore, we produced particleboards using prepared MF–LW mixtures and evaluated their mechanical and physical properties. Results showed that with increasing content of LW in the adhesive mixture gel time and peak temperature increased while reaction enthalpy decreased. With increasing substitution of MF resin adhesive with LW the thermal stability of adhesive mixture reduced, namely thermal degradation started at lower temperature and weight loss increased. Properties of particleboards improved with increasing amount of LW in the adhesive mixture up to 20% and then deteriorated. Nevertheless, the properties of particleboard with 30% LW in the adhesive mixture were comparable to the properties of particleboard without LW while they worsen at greater portion of LW. Consequently, MF resin adhesive with 30% LW substitution could be used to produce particleboards with suitable mechanical properties and reduced formaldehyde release content.
- 4 October 2014
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 132 (8)
Water‐blown polyurethane/polyisocyanurate foams made from recycled polyethylene terephthalate and liquefied wood‐based polyester polyol
Depolymerized polyethylene terephthalate and liquefied wood polyesters can be used as a polyol for the production of polyurethane/polyisocyanurate foams. In this research, liquefied wood was synthesized by using a combination of diethylene glycol and glycerol and due to the possibility of using glycerol that is a by‐product in biodiesel production, our goal was to use as much glycerol in the liquefaction reagent as possible. We determined the properties of the polyols, properties of produced foams, and explained their correlation. Greater amount of glycerol in the liquefaction reagent resulted in higher OH number, molecular weight, functionality, and viscosity of the polyol, as well as in longer cream time and tack free time in foam preparation. Glass transition temperature, density, and water absorption of the foam increased with increasing amount of glycerol in liquefied wood. Compressive stress increased up to 30% of the glycerol in the reagent and then reduced, while thermal conductivity was not affected. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015, 132, 41522.
- 4 October 2014
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 132 (8)
Water‐blown polyurethane/polyisocyanurate foams made from recycled polyethylene terephthalate and liquefied wood‐based polyester polyol
Depolymerized polyethylene terephthalate and liquefied wood polyesters can be used as a polyol for the production of polyurethane/polyisocyanurate foams. In this research, liquefied wood was synthesized by using a combination of diethylene glycol and glycerol and due to the possibility of using glycerol that is a by‐product in biodiesel production, our goal was to use as much glycerol in the liquefaction reagent as possible. We determined the properties of the polyols, properties of produced foams, and explained their correlation. Greater amount of glycerol in the liquefaction reagent resulted in higher OH number, molecular weight, functionality, and viscosity of the polyol, as well as in longer cream time and tack free time in foam preparation. Glass transition temperature, density, and water absorption of the foam increased with increasing amount of glycerol in liquefied wood. Compressive stress increased up to 30% of the glycerol in the reagent and then reduced, while thermal conductivity was not affected. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015, 132, 41522.