JMJeong-Tak Moon

Jeong-Tak Moon

*This is an algorithmically generated author record based on publicly available information.

Jeong-Tak Moon has a total of 21 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Influence of HCl Concentration on Corrosion Behavior between Au or Cu Bonding Wires and the Bond Pad for Semiconductor Packaging

    by Young-Ran Yoo, Gyubinn Kim, Sung-Min Jeon, Hyun-Jun Park, Won-Wook Seo, Jeong-Tak Moon, Young-Sik Kim

    Wire bonding, one of the methods for electrically connecting a semiconductor chip with a substrate, involves attaching thin metal wires to pads. It is the oldest electrical connection method that exhibits high compatibility with other processes. The metal wires used for electrical connection in wire bonding are mainly made of Au, Cu, and Ag. After the wire bonding, molding is performed using the epoxy molding compound (EMC). However, EMC inevitably contains ions such as halogen elements. In addition, it absorbs moisture due to its hydrophilicity, creating a corrosive environment with electrolytes. In this study, we evaluated the influence of hydrochloric acid concentration on corrosion behavior between Au or Cu bonding wires and sputtered Al bond pads. The electrochemical factors such as corrosion potential difference (ΔE), galvanic corrosion current density (ig), and anodic and cathodic Tafel slopes were found to influence galvanic corrosion behavior. Galvanic corrosion tendency in first bond and second bond areas of PCB unit specimen was confirmed.


  • Open Access

    Al2O3-Coated Si-Alloy Prepared by Atomic Layer Deposition as Anodes for Lithium-Ion Batteries

    by Kikang Lee, Sungho Yoon, Sunghoon Hong, Hyunmi Kim, Kyuhwan Oh, Jeongtak Moon

    Silicon-based anodes can increase the energy density of Li-ion batteries (LIBs) owing to their large weights and volumetric capacities. However, repeated charging and discharging can rapidly deteriorate the electrochemical properties because of a large volume change in the electrode. In this study, a commercial Fe-Si powder was coated with Al2O3 layers of different thicknesses via atomic layer deposition (ALD) to prevent the volume expansion of Si and suppress the formation of crack-induced solid electrolyte interfaces. The Al2O3 content was controlled by adjusting the trimethyl aluminum exposure time, and higher Al2O3 contents significantly improved the electrochemical properties. In 300 cycles, the capacity retention rate of a pouch full-cell containing the fabricated anodes increased from 69.8% to 72.3% and 79.1% depending on the Al2O3 content. The powder characterization and coin and pouch cell cycle evaluation results confirmed the formation of an Al2O3 layer on the powder surface. Furthermore, the expansion rate observed during the charging/discharging of the pouch cell indicated that the deposited layer suppressed the powder expansion and improved the cell stability. Thus, the performance of an LIB containing Si-alloy anodes can be improved by coating an ALD-synthesized protective Al2O3 layer.


  • Open Access

    Properties of Fe–Si Alloy Anode for Lithium-Ion Battery Synthesized Using Mechanical Milling

    by Kikang Lee, Jejun Jeong, Yeoneyi Chu, Jongbeom Kim, Kyuhwan Oh, Jeongtak Moon

    Silicon (Si)-based anode materials can increase the energy density of lithium (Li)-ion batteries owing to the high weight and volume capacity of Si. However, their electrochemical properties rapidly deteriorate due to large volume changes in the electrode resulting from repeated charging and discharging. In this study, we manufactured structurally stable Fe–Si alloy powders by performing high-energy milling for up to 24 h through the reduction of the Si phase size and the formation of the α-FeSi2 phase. The cause behind the deterioration of the electrochemical properties of the Fe–Si alloy powder produced by over-milling (milling for an increased time) was investigated. The 12 h milled Fe–Si alloy powder showed the best electrochemical properties. Through the microstructural analysis of the Fe–Si alloy powders after the evaluation of half/full coin cells, powder resistance tests, and charge/discharge cycles, it was found that this was due to the low electrical conductivity and durability of β-FeSi2. The findings provide insight into the possible improvements in battery performance through the commercialization of Fe–Si alloy powders produced by over-milling in a mechanical alloying process.


  • Simplifying Reliability Testing of Wire Bonds Using On-Chip Heater and Pad Resistance Method

    by S. Kim, M. Mayer, J. Persic, J. T. Moon

    In situ sensors can measure wire bond reliability nondestructively during thermal aging. Conventional thermal aging of ball bonds requires ovens heating the entire microchip along with the wire bonds, also affecting interconnects for in situ sensors. To protect the interconnects and on-chip logic components of in situ sensor chips, conventional thermal aging is kept below a safe temperature limit of 200 °C. At higher temperatures, the doped Si components change their characteristics and transistors stop working. Localized on-chip heating is introduced to circumvent these drawbacks using a new microheater to increase the safe temperature limit for nondestructive reliability assessment with in situ sensors. The effect of temperature on surrounding components is reduced. The microheater is a rectangular design resistive heater made from N+ silicon. In addition, a pad resistance measurement is introduced that indicates bond aging more conveniently than previously reported bond resistance measurements.


  • Concurrent Optimization of Crescent Bond Pull Force and Tail Breaking Force in a Thermosonic Cu Wire Bonding Process

    by J. Lee, M. Mayer, Y. Zhou, S. J. Hong, J. T. Moon

    In conventional wire bonding process optimization, the crescent bond is tested by destructive pulling the loop and measure the pull force (PF) required to break the bond. While this method assures the final quality, it does not necessarily minimize production stoppages which can reduce throughput significantly. Many stoppages are caused by short-tail and tail-lift errors which in turn are caused by reduced tail bond strength. The tail breaking force (TBF) is a measure for tail bond strength. A consistent tail breaking operation is needed for robust Cu wire bond production with little operator assistance required to restart stopped machines. We report the concurrent (simultaneous) optimization of PF and TBF using standard pull testing and a method that directly measures the tail bond strength in-process, respectively. The example process uses standard 25-mum-diameter Cu wire on standard Ag-plated leadframe diepads and wire loops oriented perpendicular to the ultrasonic horn. The optimization consists of (1) finding the factors to obtain a symmetrical bond shape, (2) choosing fixed values for bond time (25 ms) and heater stage temperature (220degC), and (3) adding the new optimization step of maximizing the TBF by iteratively optimizing the impact force (IF), bonding force (BF), and ultrasound (US) parameters. Among these parameters, the US and BF are the most significant. A process window (PW) is defined as the set of US/BF parameter combinations that result in a response being inside a previously defined range. PWs for PF and TBF are determined and compared with each other. There is only a partial overlap of these PWs. To increase the process capability index (cpk) for TBF, it is recommended to first carry out conventional PF optimization followed by a minimization of the bonding force parameter to the lowest value still fulfilling the PF cpk requirement.