Kanghua Chen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Kanghua Chen has a total of 67 co-authors. Here are the top co-authors by number of shared publications:
- Songyi Chen
Light Alloy Research Institute, Central South University, Changsha 410083, China
8 shared publications - Changjun Zhu
Light Alloy Research Institute, Central South University, Changsha 410083, China
3 shared publications - Jin Lou
Light Alloy Research Institute, Central South University, Changsha 410083, China
3 shared publications Chengfu Xu
Central South University
2 shared publications- Daofen Xu
National Key Laboratory of Science and Technology for National Defence on High-Strength Structural Materials, Central South University, Changsha 410083, China
2 shared publications Gang Cheng
Guilin University of Electronic Technology
2 shared publications
Latest Publications
- Open Access
Dependence of Tensile Ductility and Impact Toughness on Constituent Particles in 2014 Aluminum Alloy
In contemporary engineering applications, deficiencies in dynamic mechanical properties, particularly impact toughness, are the leading cause of fracture incidents. Consequently, inadequate dynamic mechanical properties have emerged as the primary constraint limiting the further commercial application of precipitation-strengthened high-strength aluminum (Al) alloys, exemplified by the 2014 aluminum alloy. Since the dynamic mechanical properties of the 2014 wrought aluminum alloy are fundamentally governed by the decohesion and cracking of coarse second-phase constituent particles, it is necessary to quantify the correlation between microstructure and mechanical properties. Meanwhile, the size and volume fraction of constituent particles are largely dictated by the concentration of main and impurity alloying elements. Experimental results revealed that the volume fraction of coarse constituents increased with increasing Cu, Si, and Fe content, and that tensile ductility and impact toughness decreased following an inverse exponential relationship with the volume fraction of constituents. The aim of this study is to establish a quantitative relation to correlate the characteristics of coarse constituents with the tensile ductility and impact toughness of the 2014 aluminum alloy. A mathematical model was developed by regarding the coarse constituents as ellipsoidal inclusions. Their volume fraction and aspect ratio were considered in the model. Model predictions show broad agreement with experimental data. These properties are more sensitive to the volume fraction when it is low. Conversely, a larger aspect ratio leads to higher ductility and toughness. The sensitivity is also greater at a small aspect ratio. The model further indicates that reducing the volume fraction when it is high yields limited improvement, whereas further reduction at a low volume fraction leads to significant enhancement of ductility and toughness. This study correlates coarse constituent characteristics with tensile ductility and impact toughness quantitatively, and provides a theoretical framework for predicting and optimizing the mechanical properties of 2014 aluminum alloy.
Open AccessDependence of Tensile Ductility and Impact Toughness on Constituent Particles in 2014 Aluminum Alloy
In contemporary engineering applications, deficiencies in dynamic mechanical properties, particularly impact toughness, are the leading cause of fracture incidents. Consequently, inadequate dynamic mechanical properties have emerged as the primary constraint limiting the further commercial application of precipitation-strengthened high-strength aluminum (Al) alloys, exemplified by the 2014 aluminum alloy. Since the dynamic mechanical properties of the 2014 wrought aluminum alloy are fundamentally governed by the decohesion and cracking of coarse second-phase constituent particles, it is necessary to quantify the correlation between microstructure and mechanical properties. Meanwhile, the size and volume fraction of constituent particles are largely dictated by the concentration of main and impurity alloying elements. Experimental results revealed that the volume fraction of coarse constituents increased with increasing Cu, Si, and Fe content, and that tensile ductility and impact toughness decreased following an inverse exponential relationship with the volume fraction of constituents. The aim of this study is to establish a quantitative relation to correlate the characteristics of coarse constituents with the tensile ductility and impact toughness of the 2014 aluminum alloy. A mathematical model was developed by regarding the coarse constituents as ellipsoidal inclusions. Their volume fraction and aspect ratio were considered in the model. Model predictions show broad agreement with experimental data. These properties are more sensitive to the volume fraction when it is low. Conversely, a larger aspect ratio leads to higher ductility and toughness. The sensitivity is also greater at a small aspect ratio. The model further indicates that reducing the volume fraction when it is high yields limited improvement, whereas further reduction at a low volume fraction leads to significant enhancement of ductility and toughness. This study correlates coarse constituent characteristics with tensile ductility and impact toughness quantitatively, and provides a theoretical framework for predicting and optimizing the mechanical properties of 2014 aluminum alloy.
- Open Access
A Novel Sodium–Potassium Anode Supported by Fluorinated Aluminum Foam
Sodium–potassium (NaK) liquid alloy is a promising candidate for use as an anode material in sodium batteries because of its fluidity, which effectively suppresses the growth of sodium or potassium dendrites. However, the poor wettability of NaK alloy on conventional metal substrates is unfavorable for cell fabrication due to its strong surface tension. In this paper, low-density and low-cost fluorinated aluminum foam is used as a substrate support material for NaK liquid alloy. By combining low-surface-tension NaKC with fluorinated aluminum foam, we obtain a uniformly distributed and structurally stable electrode material. The composite electrode has a cycling stability of more than 3000 h in a symmetrical cell. Furthermore, when coupled with a sulfurized polyacrylonitrile cathode in carbonate electrolyte, it maintains excellent stability even after 800 cycles, with 72% of capacity retention.
Open AccessA Novel Sodium–Potassium Anode Supported by Fluorinated Aluminum Foam
Sodium–potassium (NaK) liquid alloy is a promising candidate for use as an anode material in sodium batteries because of its fluidity, which effectively suppresses the growth of sodium or potassium dendrites. However, the poor wettability of NaK alloy on conventional metal substrates is unfavorable for cell fabrication due to its strong surface tension. In this paper, low-density and low-cost fluorinated aluminum foam is used as a substrate support material for NaK liquid alloy. By combining low-surface-tension NaKC with fluorinated aluminum foam, we obtain a uniformly distributed and structurally stable electrode material. The composite electrode has a cycling stability of more than 3000 h in a symmetrical cell. Furthermore, when coupled with a sulfurized polyacrylonitrile cathode in carbonate electrolyte, it maintains excellent stability even after 800 cycles, with 72% of capacity retention.
- Open Access
- 26 October 2023
- Published by MDPI AG in Preprints.org
A Novel Sodium-Potassium Anode Supported by Fluorinated Aluminum Foam
Sodium-potassium (NaK) liquid alloy is a promising candidate for use as anode material in sodium batteries because of its fluidity, which effectively suppresses the growth of sodium or potassium dendrites. However, the poor wettability of the NaK liquid alloy on conventional metal substrates is unfavorable for cell fabrication due to its strong surface tension. In this paper, low-density and low-cost fluorinated aluminum foam is used as a substrate support material for NaK liquid alloy. By combining low surface tension NaK@C with fluorinated aluminum foam, we obtain a uniformly distributed and structurally stable electrode material. The composite electrode has a cycling stability of more than 3000 hours in a symmetrical cell. Furthermore, when coupled with a sulfurized polyacrylonitrile cathode in carbonate electrolyte, it maintains excellent stability even after 800 cycles, with 72% of capacity retention.
- 26 October 2023
- Published by MDPI AG in Preprints.org
Open AccessA Novel Sodium-Potassium Anode Supported by Fluorinated Aluminum Foam
Sodium-potassium (NaK) liquid alloy is a promising candidate for use as anode material in sodium batteries because of its fluidity, which effectively suppresses the growth of sodium or potassium dendrites. However, the poor wettability of the NaK liquid alloy on conventional metal substrates is unfavorable for cell fabrication due to its strong surface tension. In this paper, low-density and low-cost fluorinated aluminum foam is used as a substrate support material for NaK liquid alloy. By combining low surface tension NaK@C with fluorinated aluminum foam, we obtain a uniformly distributed and structurally stable electrode material. The composite electrode has a cycling stability of more than 3000 hours in a symmetrical cell. Furthermore, when coupled with a sulfurized polyacrylonitrile cathode in carbonate electrolyte, it maintains excellent stability even after 800 cycles, with 72% of capacity retention.
- 27 January 2022
- Published by Springer Nature in Metals and Materials International
- Vol. 28 (10) , 2472-2482
Forming Limit and Mechanical Properties of 2024-O Aluminum Alloy Under Electromagnetic Forming
- 27 January 2022
- Published by Springer Nature in Metals and Materials International
- Vol. 28 (10) , 2472-2482
Forming Limit and Mechanical Properties of 2024-O Aluminum Alloy Under Electromagnetic Forming
- 28 August 2021
- Published by Springer Nature in Metals and Materials International
- Vol. 28 (2) , 433-447
Influence of Forging Temperature on the Microstructures and Mechanical Properties of a Multi-Directionally Forged Al–Cu–Li Alloy
- 28 August 2021
- Published by Springer Nature in Metals and Materials International
- Vol. 28 (2) , 433-447
Influence of Forging Temperature on the Microstructures and Mechanical Properties of a Multi-Directionally Forged Al–Cu–Li Alloy
- Open Access
Microstructures and Tensile Fracture Behavior of 2219 Wrought Al–Cu Alloys with Different Impurity of Fe
The Fe-rich intermetallic phases have a broadly detrimental effect on the mechanical properties of Al–Cu alloy. In this paper, the continuous evolution of Fe-rich intermetallics and their effects on mechanical properties, especially the tensile fracture behavior of 2219 wrought Al–Cu alloys as a function of Fe content against different processing approaches (i.e., as-cast, homogenization, multidirectional forging, and solution-peak aging treatment) were investigated using optical microscopy, scanning electron microscopy, and tensile tests. The results indicated that needle-like Al7Cu2Fe or Al7Cu2(Fe, Mn) intermetallics mainly presented in the final microstructures of all alloys with various Fe contents. The size and number of Al7Cu2Fe/Al7Cu2(Fe, Mn) intermetallics increased with the increase of Fe content. The increase of Fe content had little influence on the ultimate tensile strength and yield strength, while obvious deterioration in the elongation, because fracture initiators mainly occurred at the Al7Cu2Fe/Al7Cu2(Fe, Mn) particles or particles–matrix interface. Therefore, the 2219 Al–Cu alloy with 0.2 wt.% Fe content presented relatively low tensile ductility. The tensile fracture mechanism has been discussed in detail.
Open AccessMicrostructures and Tensile Fracture Behavior of 2219 Wrought Al–Cu Alloys with Different Impurity of Fe
The Fe-rich intermetallic phases have a broadly detrimental effect on the mechanical properties of Al–Cu alloy. In this paper, the continuous evolution of Fe-rich intermetallics and their effects on mechanical properties, especially the tensile fracture behavior of 2219 wrought Al–Cu alloys as a function of Fe content against different processing approaches (i.e., as-cast, homogenization, multidirectional forging, and solution-peak aging treatment) were investigated using optical microscopy, scanning electron microscopy, and tensile tests. The results indicated that needle-like Al7Cu2Fe or Al7Cu2(Fe, Mn) intermetallics mainly presented in the final microstructures of all alloys with various Fe contents. The size and number of Al7Cu2Fe/Al7Cu2(Fe, Mn) intermetallics increased with the increase of Fe content. The increase of Fe content had little influence on the ultimate tensile strength and yield strength, while obvious deterioration in the elongation, because fracture initiators mainly occurred at the Al7Cu2Fe/Al7Cu2(Fe, Mn) particles or particles–matrix interface. Therefore, the 2219 Al–Cu alloy with 0.2 wt.% Fe content presented relatively low tensile ductility. The tensile fracture mechanism has been discussed in detail.
- Open Access
Evolution of the Second-Phase Particles and Their Effect on Tensile Fracture Behavior of 2219 Al-xCu Alloys
In this study, the continuous evolution of the second-phase particles across as-cast, homogenization, multi-directional forging (MDF), and solution-aging treatment and their effect on tensile fracture behavior of 2219 aluminum alloys with different Cu contents was examined by optical microscopy (OM), scanning electron microscopy (SEM), and tensile tests. The results showed that the microstructure of as-cast 2219 aluminum alloy consisted of the α-Al matrix, Al2Cu coarse phase, and Fe-rich impurity phase. Severe segregation of Cu existed, and eutectic networks can be observed in the ingot. With an increase in Cu content, the eutectic networks became coarsen and thicker. During the complex improved process, the refinement mechanisms were fragmentation, dissolution, and diffusion of Al2Cu particles. Most fine Al2Cu particles were fully dissolved into the matrix and partial coarse particles were still retained after solution-aging treatment. Thus, the elongations of all the samples, undergoing solution treatment followed by water quenching, increased evidently. Then, the elongations decreased slightly due to the increase of precipitates. The fractography analysis of peak aged condition samples indicated that the fracture mode was diverted from a typical inter-granular fracture to a mainly trans-granular fracture with increase in Cu content from 5.56% to 6.52%. Fracture initiation mainly occurred by original microcrack propagation and microvoid nucleation at the coarse constituents.
Open AccessEvolution of the Second-Phase Particles and Their Effect on Tensile Fracture Behavior of 2219 Al-xCu Alloys
In this study, the continuous evolution of the second-phase particles across as-cast, homogenization, multi-directional forging (MDF), and solution-aging treatment and their effect on tensile fracture behavior of 2219 aluminum alloys with different Cu contents was examined by optical microscopy (OM), scanning electron microscopy (SEM), and tensile tests. The results showed that the microstructure of as-cast 2219 aluminum alloy consisted of the α-Al matrix, Al2Cu coarse phase, and Fe-rich impurity phase. Severe segregation of Cu existed, and eutectic networks can be observed in the ingot. With an increase in Cu content, the eutectic networks became coarsen and thicker. During the complex improved process, the refinement mechanisms were fragmentation, dissolution, and diffusion of Al2Cu particles. Most fine Al2Cu particles were fully dissolved into the matrix and partial coarse particles were still retained after solution-aging treatment. Thus, the elongations of all the samples, undergoing solution treatment followed by water quenching, increased evidently. Then, the elongations decreased slightly due to the increase of precipitates. The fractography analysis of peak aged condition samples indicated that the fracture mode was diverted from a typical inter-granular fracture to a mainly trans-granular fracture with increase in Cu content from 5.56% to 6.52%. Fracture initiation mainly occurred by original microcrack propagation and microvoid nucleation at the coarse constituents.
- Open Access
Prediction and Experimental of Yield Strengths of As-Quenched 7050 Aluminum Alloy Thick Plates after Continuous Quench Cooling
The aim of this study was to predict the yield strength of as-quenched aluminum alloys according to their continuous quench cooling path. Our model was established within the framework of quench factor analysis (QFA) by representing a quenching curve as a series of consecutive isothermal transformation events and adding the yield strength increments after each isothermal step to predict the yield strength after continuous quench cooling. For simplification; it was considered that the effective hardeners during quenching were the nanosized solute clusters formed at low temperatures, whereas the other coarse precipitates were neglected. In addition, quenching tests were conducted on aluminum plates with different thicknesses. The predictions were compared with the experimental measurements, and the results showed that the predictions fit the measurements well for the 40- and 80-mm-thick plates but overestimated the as-quenched yield strength at the mid-thickness of the 115-mm-thick plates.
Open AccessPrediction and Experimental of Yield Strengths of As-Quenched 7050 Aluminum Alloy Thick Plates after Continuous Quench Cooling
The aim of this study was to predict the yield strength of as-quenched aluminum alloys according to their continuous quench cooling path. Our model was established within the framework of quench factor analysis (QFA) by representing a quenching curve as a series of consecutive isothermal transformation events and adding the yield strength increments after each isothermal step to predict the yield strength after continuous quench cooling. For simplification; it was considered that the effective hardeners during quenching were the nanosized solute clusters formed at low temperatures, whereas the other coarse precipitates were neglected. In addition, quenching tests were conducted on aluminum plates with different thicknesses. The predictions were compared with the experimental measurements, and the results showed that the predictions fit the measurements well for the 40- and 80-mm-thick plates but overestimated the as-quenched yield strength at the mid-thickness of the 115-mm-thick plates.
- Open Access
Microstructure, Properties, and Titanium Cutting Performance of AlTiN–Cu and AlTiN–Ni Coatings
In this study, three kinds of coatings, AlTiN, AlTiN–Ni, and AlTiN–Cu were deposited via the cathodic arc evaporation method. The microstructure, mechanical properties, oxidation resistance, and cutting behavior of these coatings were then investigated. The incorporation of Cu(Ni) into AlTiN eliminated its columnar structure and led to an increase in the growth defects of its macroparticles. The addition of Cu and Ni decreased the hardness of the coatings, their elastic moduli, and their friction coefficients. All of the AlTiN, AlTiN–Ni, and AlTiN–Cu coatings presented sufficient adhesion strength values. The oxidation resistance of these three coatings was determined to be in the following order: AlTiN > AlTiN–Ni > AlTiN–Cu. Titanium turning experiments indicated that the cutting force was reduced and the tool life was improved through doping with Cu(Ni) elements, dependent on cutting speed. The AlTiN–Ni coating showed the best performance at a high cutting speed, whereas the AlTiN–Cu coating was more successful at a lower cutting speed.
Open AccessMicrostructure, Properties, and Titanium Cutting Performance of AlTiN–Cu and AlTiN–Ni Coatings
In this study, three kinds of coatings, AlTiN, AlTiN–Ni, and AlTiN–Cu were deposited via the cathodic arc evaporation method. The microstructure, mechanical properties, oxidation resistance, and cutting behavior of these coatings were then investigated. The incorporation of Cu(Ni) into AlTiN eliminated its columnar structure and led to an increase in the growth defects of its macroparticles. The addition of Cu and Ni decreased the hardness of the coatings, their elastic moduli, and their friction coefficients. All of the AlTiN, AlTiN–Ni, and AlTiN–Cu coatings presented sufficient adhesion strength values. The oxidation resistance of these three coatings was determined to be in the following order: AlTiN > AlTiN–Ni > AlTiN–Cu. Titanium turning experiments indicated that the cutting force was reduced and the tool life was improved through doping with Cu(Ni) elements, dependent on cutting speed. The AlTiN–Ni coating showed the best performance at a high cutting speed, whereas the AlTiN–Cu coating was more successful at a lower cutting speed.
- 1 June 2019
- Published by SAGE Publications in Surface Engineering
- Vol. 35 (6) , 501-506
Performance of AlTiBN and AlTiTaN coatings during milling of titanium
AlTiN, AlTiBN, and AlTiTaN coatings were deposited on cemented carbide substrate by cathodic arc evaporation. Scanning electron microscopy, X-ray diffraction, nanohardness testing, and scratch testing were used to examine the coating thickness, microstructure, hardness, adhesion strength, and oxidation resistance. The incorporation of B and Ta into the AlTiN coatings increased their hardness and oxidation resistance. In titanium-milling experiments using these three coatings, AlTiBN-coated carbide tools had the longest lifetime at cutting speed of 60 m/min. This is attributed to less delamination and chipping at the cutting edge, due to the coating's high hardness, good oxidation resistance, and sufficient adhesion strength. The major wear mechanisms of these coated tools are adhesive wear, oxidation, and chipping.
- 1 June 2019
- Published by SAGE Publications in Surface Engineering
- Vol. 35 (6) , 501-506
Performance of AlTiBN and AlTiTaN coatings during milling of titanium
AlTiN, AlTiBN, and AlTiTaN coatings were deposited on cemented carbide substrate by cathodic arc evaporation. Scanning electron microscopy, X-ray diffraction, nanohardness testing, and scratch testing were used to examine the coating thickness, microstructure, hardness, adhesion strength, and oxidation resistance. The incorporation of B and Ta into the AlTiN coatings increased their hardness and oxidation resistance. In titanium-milling experiments using these three coatings, AlTiBN-coated carbide tools had the longest lifetime at cutting speed of 60 m/min. This is attributed to less delamination and chipping at the cutting edge, due to the coating's high hardness, good oxidation resistance, and sufficient adhesion strength. The major wear mechanisms of these coated tools are adhesive wear, oxidation, and chipping.