Phillip Haslberger
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Phillip Haslberger has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Ronald Schnitzer
Christian Doppler Laboratory for Knowledge‐based Design of Advanced Steels Department of Materials Science Montanuniversität Leoben Leoben Austria
7 shared publications Wolfgang Ernst
Voestalpine Stahl GmbH
5 shared publicationsSylvia Holly
Voestalpine Böhler Welding Austria GmbH
3 shared publicationsChristian Schneider
Graz University of Technology
1 shared publicationChristoph Turk
Montanuniversitaet Leoben
1 shared publicationDevrim Caliskanoglu
Buderus Edelstahl GmbH
1 shared publication
Latest Publications
- Open Access
- 13 August 2018
- Published by Springer Nature in Welding in the World
- Vol. 62 (6) , 1153-1158
Influence of inhomogeneity on several length scales on the local mechanical properties in V-alloyed all-weld metal
- 13 August 2018
- Published by Springer Nature in Welding in the World
- Vol. 62 (6) , 1153-1158
Open AccessInfluence of inhomogeneity on several length scales on the local mechanical properties in V-alloyed all-weld metal
- Open Access
- 3 April 2018
- Published by Springer Nature in Welding in the World
- Vol. 62 (4) , 713-719
Precipitates in microalloyed ultra-high strength weld metal studied by atom probe tomography
- 3 April 2018
- Published by Springer Nature in Welding in the World
- Vol. 62 (4) , 713-719
Open AccessPrecipitates in microalloyed ultra-high strength weld metal studied by atom probe tomography
- Open Access
- 24 January 2018
- Published by Springer Nature in Journal of Materials Science
- Vol. 53 (9) , 6968-6979
Microstructure and mechanical properties of high-strength steel welding consumables with a minimum yield strength of 1100 MPa
Welded high-strength steel components have great potential for use in lightweight constructions or highly loaded structures. Welding of steels with a yield strength of more than 1100 MPa is particularly challenging because of the toughness requirements for the weld metal. Currently, a new generation of welding consumables with a minimum yield strength of 1100 MPa has been developed. Based on electron backscatter diffraction and atom probe tomography, a concept for toughening and strengthening of all-weld metal samples was deployed. Starting from a martensitic all-weld metal sample with an approximate yield strength of 1000 MPa, a reduction in manganese and silicon content resulted in a refined microstructure with a lower prior austenite grain size and effective grain size. Furthermore, a higher average grain boundary misorientation was measured, which influences the toughness positively. An addition of vanadium caused the formation of vanadium-rich clusters, which increased the strength of the all-weld metal significantly. With a combination of these two mechanisms, it was possible to produce an all-weld metal sample with the required yield strength of more than 1100 MPa and an acceptable toughness.
- 24 January 2018
- Published by Springer Nature in Journal of Materials Science
- Vol. 53 (9) , 6968-6979
Open AccessMicrostructure and mechanical properties of high-strength steel welding consumables with a minimum yield strength of 1100 MPa
Welded high-strength steel components have great potential for use in lightweight constructions or highly loaded structures. Welding of steels with a yield strength of more than 1100 MPa is particularly challenging because of the toughness requirements for the weld metal. Currently, a new generation of welding consumables with a minimum yield strength of 1100 MPa has been developed. Based on electron backscatter diffraction and atom probe tomography, a concept for toughening and strengthening of all-weld metal samples was deployed. Starting from a martensitic all-weld metal sample with an approximate yield strength of 1000 MPa, a reduction in manganese and silicon content resulted in a refined microstructure with a lower prior austenite grain size and effective grain size. Furthermore, a higher average grain boundary misorientation was measured, which influences the toughness positively. An addition of vanadium caused the formation of vanadium-rich clusters, which increased the strength of the all-weld metal significantly. With a combination of these two mechanisms, it was possible to produce an all-weld metal sample with the required yield strength of more than 1100 MPa and an acceptable toughness.
- 1 August 2017
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 22 (6) , 536-543
Influence of alloying elements on the mechanical properties of high-strength weld metal
High-strength lightweight constructions are a crucial part of transportation systems and steel constructions optimised for low energy consumption. In this investigation, the aim is to understand the influence of different alloying elements on the mechanical properties of all-weld metal samples of high-strength filler metals. Metal-cored wires with adjusted chemistry were produced and the measured yield strength is compared with calculated values which were obtained by thermodynamic and kinetic simulations. By increasing the content of the matrix alloying elements, no increase in strength could be achieved, but compared to that, higher strength was obtained by the addition of Ti, Nb and Al in combination. Furthermore, the influence of different Ti, Al and N contents is presented and discussed.
- 1 August 2017
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 22 (6) , 536-543
Influence of alloying elements on the mechanical properties of high-strength weld metal
High-strength lightweight constructions are a crucial part of transportation systems and steel constructions optimised for low energy consumption. In this investigation, the aim is to understand the influence of different alloying elements on the mechanical properties of all-weld metal samples of high-strength filler metals. Metal-cored wires with adjusted chemistry were produced and the measured yield strength is compared with calculated values which were obtained by thermodynamic and kinetic simulations. By increasing the content of the matrix alloying elements, no increase in strength could be achieved, but compared to that, higher strength was obtained by the addition of Ti, Nb and Al in combination. Furthermore, the influence of different Ti, Al and N contents is presented and discussed.
- 31 July 2017
- Published by Walter de Gruyter GmbH in Practical Metallography
- Vol. 54 (8) , 513-532
Microstructural Characterization of Martensitic All-Weld Metal Samples
The development of welding consumables is permanently challenged with matching the increasing strength and toughness of thermomechanically treated or quenched and tempered steels. A martensitic microstructure offers promising prospects to guarantee such requirements in the all-weld metal as well. A thorough characterization of the microstructure is indispensable to understand its effects on the mechanical properties. This paper shall summarize how light optical microscopy and electron backscatter diffraction can be used to deepen the understanding of fully martensitic weld metal. It was found that electron backscatter diffraction offers a variety of information that light optical microscopy cannot deliver, particularly regarding the prior austenite grain structure. Grain sizes of the primary dendrites, the prior austenite grains and the martensitic structure can be measured with a combination of these techniques.
- 31 July 2017
- Published by Walter de Gruyter GmbH in Practical Metallography
- Vol. 54 (8) , 513-532
Microstructural Characterization of Martensitic All-Weld Metal Samples
The development of welding consumables is permanently challenged with matching the increasing strength and toughness of thermomechanically treated or quenched and tempered steels. A martensitic microstructure offers promising prospects to guarantee such requirements in the all-weld metal as well. A thorough characterization of the microstructure is indispensable to understand its effects on the mechanical properties. This paper shall summarize how light optical microscopy and electron backscatter diffraction can be used to deepen the understanding of fully martensitic weld metal. It was found that electron backscatter diffraction offers a variety of information that light optical microscopy cannot deliver, particularly regarding the prior austenite grain structure. Grain sizes of the primary dendrites, the prior austenite grains and the martensitic structure can be measured with a combination of these techniques.
- 1 May 2017
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 22 (4) , 336-342
High resolution imaging of martensitic all-weld metal
Martensitic steel welds show promising results regarding their strength while they may tend to be brittle. As martensite is a quite complex microstructure, high resolution techniques like electron backscatter diffraction (EBSD) and atom probe tomography (APT) are valuable tools for an in-depth characterisation. In this study, the average block size and misorientation distribution of martensitic all-weld samples were evaluated with EBSD. A lower carbon content led to a smaller block size and consequently a higher toughness of the all-weld sample. Furthermore, APT revealed a concentration fluctuation of the main alloying elements and particles with a high carbon content. It is discussed how these methods can be used in the future to design the microstructure to achieve optimum properties.
- 1 May 2017
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 22 (4) , 336-342
High resolution imaging of martensitic all-weld metal
Martensitic steel welds show promising results regarding their strength while they may tend to be brittle. As martensite is a quite complex microstructure, high resolution techniques like electron backscatter diffraction (EBSD) and atom probe tomography (APT) are valuable tools for an in-depth characterisation. In this study, the average block size and misorientation distribution of martensitic all-weld samples were evaluated with EBSD. A lower carbon content led to a smaller block size and consequently a higher toughness of the all-weld sample. Furthermore, APT revealed a concentration fluctuation of the main alloying elements and particles with a high carbon content. It is discussed how these methods can be used in the future to design the microstructure to achieve optimum properties.
- Open Access
- 20 June 2016
- Published by Springer Nature in BHM Berg- und Hüttenmännische Monatshefte
- Vol. 161 (7) , 321-324
Mikrostrukturielle Charakterisierung von ultra-hochfesten Schweißgütern
- 20 June 2016
- Published by Springer Nature in BHM Berg- und Hüttenmännische Monatshefte
- Vol. 161 (7) , 321-324
Open AccessMikrostrukturielle Charakterisierung von ultra-hochfesten Schweißgütern
- 20 March 2015
- Published by Springer Nature in BHM Berg- und Hüttenmännische Monatshefte
- Vol. 160 (5) , 204-208
Boron Grain Boundary Segregation in a Heat Treatable Steel
- 20 March 2015
- Published by Springer Nature in BHM Berg- und Hüttenmännische Monatshefte
- Vol. 160 (5) , 204-208
Boron Grain Boundary Segregation in a Heat Treatable Steel