  • Experimental Investigation into Liquid and Solid Separation by an Industrial Mesh-Vane-Type Separator on Natural Gas at 4–5 MPa, Different Liquid Loadings and Gas Flows

    by K.K. Botros, N. Chan, J. Geerligs, K. Leong, B. Hickey, I. Gong

    Inline vertical separators are commonly employed in natural gas transmission facilities (e.g., receipt stations) to filter liquid contaminants such as compressor oil, glycol, and free water from the gas stream. Manufacturers of these separators have claimed liquid removal efficiencies of 98–99% for droplet sizes ≥ 8 μm. However, these contaminants have been found invariably in piping systems downstream of these separators, suggesting inadequate separator performance. Currently, there is a lack of ability to verify manufacturer claims due to difficulties in quantifying liquid contaminants and droplet characteristics. The potential consequences of having such contaminants include lower gas quality, impaired gas metering accuracy, corrosion and damage to equipment/instrumentation, and adverse impacts on industrial and residential end users. This paper presents performance testing of a mesh-vane-type vertical separator conducted on high pressure, pipeline quality, natural gas in the range of 4–5 MPa and flow velocity in the range of 1.3–13 m/s in the DN150 separator inlet (hence turndown ratio of 10:1). Four different spray nozzles were used to inject and atomize industrial compressor oil with a liquid-to-gas mass loading ratio of 0.06–1.8%. Test results revealed that the average bulk efficiency separation performance for this separator is approximately 90.34%. This was found to be independent of the liquid-to-gas mass loading ratio. The effective Souders–Brown K-factor was found to be 0.15 m/s. This is below literature published data in the range of 0.27–0.3 m/s for horizontal flow, vane-pack-type separators. Liquid separation tests were also conducted following the injection of solid glass beads. Liquid separation efficiency decreased by approximately 9%, following the injection of 7 kg of industrial glass beads over a period of approximately 4 h. This was attributed to accumulation of solids in the vane pack.

  • Insight Into the Interaction Between Flow Field and Acoustic Field of Turning Flow Into a Side Branch Against a Deadleg

    by K. K. Botros, Eric Clavelle, Hemanth Satish

    Acoustic resonances in internal flows can cause noise, vibration, and even equipment damage. One geometry prone to acoustic resonance is a deadleg at the point where the main flow turns into a side branch. Here, we report experimental and computational fluid dynamics (CFD) studies of flow-generated pulsation in such a geometry over a wide range of mean flow velocities. Experimental results of the normalized pulsation pressure amplitudes (P*) versus Strouhal number characterized the flow–acoustic field for acoustically tuned and detuned systems and for branch to main pipe diameter ratio of 1.0. The unsteady CFD simulations revealed the characteristic volume integral of the cross-product of the vorticity field and the velocity field (ω×U) in the vicinity of the T-junction which helped in quantifying the acoustic source power for different conditions. In addition, the cross-product (ω×U) in the direction along the main line is almost exactly out of phase with the acoustic velocity at the T-junction. The pressure amplitude at the closed end of the deadleg reaches maximum when two conditions are met: (i) the system overall acoustic resonance frequency matches closely the frequency of the oscillating component of the cross-product (ω×U) characterized by a Strouhal number and (ii) the deadleg length is tuned to an odd number of ¼ wavelength of this frequency such that maximum acoustic velocity is reached at the T-junction. Synchronized images generated from the unsteady CFD simulations revealed valuable insight into the velocity and vorticity field in the region of the T-junction in support of Howe's acoustic source power equation.


  • Pneumatic Testing of Piping Assemblies: Criteria for Stored Energy and Pinhole Leak Detectability

    by K. K. Botros, Vivian Liu, Jason Lu

    Pneumatic testing is beneficial as an alternative to hydrotesting particularly in remote areas where access to hydrotest fluids becomes logistically difficult or impossible. In some cases, above-ground pipe supports cannot hold the water weight, or that the pipe is coated/lined with materials that would degrade with water/methanol/glycol mixtures, or the system cannot be fully dried and the remaining hydrotest fluids are detrimental to the service application once the system is commissioned. Additionally, the elevation profile of the piping is such that an excessive number of test sections would be required for hydrotesting according to most codes. The present work is aimed at addressing two salient questions often faced with pneumatic testing. The first is related to the appropriate piping volume to consider for calculating the stored energy in use with ASME Post Construction Committee (PCC)-2 calculation for determining the safe exclusion distance for a given piping geometry and test conditions. It was found that the 8D criteria specified in ASME PCC-2 cannot be generalized for all pipe sizes, different material toughness, grades, wall thicknesses, and test conditions. A criterion is developed based on the ductile fracture arrest length that considers all these factors combined. The second criterion is related to the ability to detect a pinhole leak from the pneumatic test data, again for a given geometry and test conditions, and what constitutes the minimum pinhole effective area in relation to the system total volume, measured uncertainties in the test pressure and temperature over the duration of the test. A seminormalized physics-based parameter is suggested that can be applied to determine the effective pinhole leak size. The methodology is applied to a pneumatic field test on DN200, 12.2 km pipeline lateral.


  • Measurements of Blowdown Thrust Loading in Natural Gas Facilities

    by K. K. Botros, H. Charette, M. Martens, M. Beckel, G. Szuch

    The thrust loading on a vertical blowdown stack during a natural gas blowdown was investigated using a combined experimental and modeling approach. A gravimetric vessel initially at 4000 kPa-g was blown down through two geometrically different stack assemblies. Thrust loads were measured using a dynamic weigh scale typically used for gravimetric calibration of gas flow meters. A one-dimensional (1D) compressible flow model, calibrated using the experimental data, revealed stagnation pressure losses at the entrance to the riser, resulting in lower thrust loads. A comparison between thrust loading obtained from the measurements and the 1D compressible flow model is presented. This work shows that the analytical flow model predicts the blowdown thrust loads within ±30%.

  • Effects of Argon as the primary impurity in anthropogenic carbon dioxide mixtures on the decompression wave speed

    by Kamal K. Botros, John Geerligs, Brian Rothwell, Thomas Robinson

    In order to determine the material fracture resistance necessary to provide adequate control of the propagation of ductile fracture in a pipeline, a knowledge of the decompression wave speed (W) following the quasi‐instantaneous formation of an unstable, full‐bore rupture is necessary. The thermodynamic and fluid dynamics background of such calculations is understood, but predictions based on specific equations of state need to be validated against experimental measurements. A program of tests has been conducted using a specially constructed shock tube to determine the impact of impurities on W in carbon dioxide (CO2), so that the results can be compared to two existing theoretical models. In this paper, data and analysis results are presented for four tests involving simulated anthropogenic CO2 mixtures containing Argon (Ar) as the primary impurity. These mixtures represent typical oxy‐fuel CO2 capture technology with or without a purification train. Comparisons of the experimentally obtained W with predictions by two commonly used equation of state (EOS) models were also made. Generally, the GERG‐2008 EOS exhibits better overall performance than the Peng‐Robinson (PR) EOS when compared to the experimental results. The bubble point curve as predicted by GERG‐2008 was always at a higher pressure than that predicted by PR for these mixtures. This resulted in the plateau pressure prediction by GERG‐2008 being higher in cases where the isentropes intersect the phase envelope on the bubble point side. An example of pipeline material toughness required to arrest ductile fracture is presented which shows that prediction by GERG‐2008 is more conservative, and is therefore recommended.


  • Measurements of Decompression Wave Speed in Simulated Anthropogenic Carbon Dioxide Mixtures Containing Hydrogen

    by K. K. Botros, J. Geerligs, B. Rothwell, T. Robinson

    In order to determine the material fracture resistance necessary to provide adequate control of ductile fracture propagation in a pipeline, a knowledge of the decompression wave speed following the quasi-instantaneous formation of an unstable, full-bore rupture is necessary. The thermodynamic and fluid dynamics background of such calculations is understood, but predictions based on specific equations of state (EOS) need to be validated against experimental measurements. A program of tests has been conducted using a specially constructed shock tube to determine the impact of impurities on the decompression wave speed in carbon dioxide (CO2), so that the results can be compared to two existing theoretical models. In this paper, data and analysis results are presented for three shock tube tests involving anthropogenic CO2 mixtures containing hydrogen as the primary impurity. The first mixture was intended to represent a typical scenario of precombustion carbon capture and storage (CCS) technology, where typically the concentration of CO2 is around 95–97% (mole). The second mixture represents a worst case scenario of this technology with high level of impurities (with CO2 concentration around 85%). The third test represents a typical chemical-looping combustion process. It was found that the extent of the plateau on the decompression wave speed curves in these tests depends on the location of the phase boundary crossing along the bubble-point curve. The closer the phase boundary crossing to the critical point, the shorter the plateau. This is primarily due to the change in magnitude of the drop in the speed of sound at phase boundary crossing. For the most part, the predictions of the plateau pressure by both of the EOS that were evaluated, GERG-2008 and Peng–Robinson (PR), are in good agreement with measurements by the shock tube. This by no means reflects overall good performance of either EOS, but was rather due to the fact that the isentropes intersected the phase envelope near the critical point, or that the concentration of H2 was relatively low, either in absolute terms or relative to other impurity constituents. Hence, its influence in causing inaccurate prediction of the plateau pressure is lessened. An example of pipeline material toughness required to arrest ductile fracture is presented which shows that predictions by GERG-2008 are more conservative and are therefore recommended.


  • Measurements of Decompression Wave Speed in Binary Mixtures of Carbon Dioxide and Impurities

    by K. K. Botros, J. Geerligs, B. Rothwell, T. Robinson

    Shock tube tests were conducted on a number of binary CO2 mixtures with N2, O2, CH4, H2, CO, and Ar impurities, from a range of initial pressures and temperatures. This paper provides examples of results from these tests. The resulting decompression wave speeds are compared with predictions made utilizing different equations of state (EOS). It was found that, for the most part (except for binaries with H2), the GERG-2008 EOS shows much better performance than the Peng–Robinson (PR) EOS. All binaries showed a very long plateau in the decompression wave speed curves. It was also shown that tangency of the fracture propagation speed curve would normally occur on the pressure plateau, and hence, the accuracy of the calculated arrest toughness for pipelines transporting these binary mixtures is highly dependent on the accuracy of the predicted plateau pressure. Again, for the most part, GERG-2008 predictions of the plateau are in good agreement with the measurements in binary mixtures with N2, O2, and CH4. An example of the determination of pipeline material toughness required to arrest ductile fracture is presented, which shows that prediction by GERG-2008 is generally more conservative and is therefore recommended. However, both GERG-2008 and PR EOS show much worse performance for the other three binaries: CO2 + H2, CO2 + CO, and CO2 + Ar, with CO2 + H2 being the worst. This is likely due to the lack of experimental data for these three binary mixtures that were used in the development of these EOS.


  • Interfacial Contamination Between Batches of Crude Oil Due to Dead-Legs in Pump Station Piping

    by K. K. Botros, E. J. Clavelle, G. M. Vogt

    Some oil pump station design layouts may contain multiple dead-legs. During the transportation of heavy crude through the pump station, these dead-legs will be filled with this crude. When a light crude batch is introduced next into the pipeline, following the heavy crude ahead, two phenomena will occur. First, contamination between batches at the interface of the two crudes will occur due to axial turbulent diffusion along the length of the pipeline itself. Second, as the light crude flows through the pump station and passes by each dead-leg containing still heavy crude from the preceding batch, the heavy crude trapped in these dead-legs will start to drain out into the passing light crude in the main run. This causes further contamination and spreading of the mixing zone between the two batches. These two different sources of contamination are addressed in this paper with the objective of accurately quantifying the extent of the contamination, with particular emphasis on the second phenomenon which could cause appreciable contamination particularly for large size and number of these dead-legs. A computational fluid dynamics (CFD) model has been developed to quantify the drainage rate of the contaminating crude into the main stream and its impact on widening the mixed zone (contamination spread) between the two batches. Two drainage mechanisms of the heavy crude in the dead-legs into the main stream of the light crude have been identified and quantified. The initial phase is a gravity-current-induced outflow of the initially stagnant fluid in the dead-leg, followed by a subsequent draining mechanism primarily induced by turbulent mixing and diffusion at the mouth of the dead-leg penetrating slightly into the dead-leg. It was found that the second mechanism takes a much longer time to drain the first, and that the break point in time where drainage switches from a predominantly gravity current to a turbulent diffusion appears to be at a specific time normalized with respect to the length of the dead-leg and the gravity current speed. The results show a consistent trend with actual interface contamination data obtained from the Keystone 2982 km pipeline from Hardisty (Canada) to the Patoka Terminal (U.S.A.).


  • Experimental Investigation Into the Relationship Between the Roughness Height in Use With Nikuradse or Colebrook Roughness Functions and the Internal Wall Roughness Profile for Commercial Steel Pipes

    by K. K. Botros

    The relationships between the sand grain roughness height (ks) in use with Nikuradse or Colebrook correlations for the roughness function (RF) and the internal pipe wall roughness element described by the root-mean-square (RMS) of the roughness profile (Rq) for turbulent flow in pipes are experimentally examined. Flow tests were conducted on a total of 13 commercial steel pipes of two sizes: 168.3 mm and 114.3 mm outer diameter (OD). The aim was to provide further insight into relationship between ks and Rq, for use with either RF correlations. The tests were conducted on high-pressure pipeline quality natural gas in the range of Reynolds number (based on pipe internal diameter) of 9 × 106–16 × 106. For commercial carbon steel pipes, the relationship between ks and Rq was found in the form ks=1.306  Rq+0.078  Rq2 and ks=2.294  Rq (both ks and Rq in μm), for use with Colebrook and Nikuradse RF correlations, respectively. These correlations cover a wide range of Rq from 2.7 μm to 12.5 μm which is typically found in commercial carbon steel pipes. For stainless steel (SS) pipes, preliminary results indicate that other surface roughness profile parameters need to be employed to better define the values of ks for these types of commercial steel pipes.


  • Measurements of Decompression Wave Speed in Pure Carbon Dioxide and Comparison With Predictions by Equation of State

    by K. K. Botros, J. Geerligs, B. Rothwell, T. Robinson

    Carbon dioxide capture and storage (CCS) is one of the technologies that have been proposed to reduce emissions of carbon dioxide (CO2) to the atmosphere. CCS will require the transportation of the CO2 from the “capture” locations to the “storage” locations via large-scale pipeline projects. One of the key requirements for the design and operation of pipelines in all jurisdictions is fracture control. Supercritical CO2 is a particularly challenging fluid from this point of view, because its thermodynamic characteristics are such that a very high driving force for fracture can be sustained for a long time. Even though CO2 is not flammable, it is an asphyxiating gas that is denser than air, and can collect in low-lying areas. Additionally, it is well known that any pipeline rupture, regardless of the nature of the fluid it is transporting, has a damaging reputational, commercial, logistic, and end user impact. Therefore, it is as important to control fracture in a CO2 pipeline as in one transporting a flammable fluid. With materials specified appropriately for the prevention of brittle failure, the key element is the control of propagating ductile (or tearing) fracture. The determination of the required toughness for the arrest of ductile fracture requires knowledge of the decompression behavior of the contained fluid, which in turn requires accurate knowledge of its thermodynamic characteristics along the decompression isentrope. While thermodynamic models based on appropriate EOS (equations of state) are available that will, in principle, allow determination of the decompression wave speed, they, in general, have not been fully validated for very rapid transients following a rupture. This paper presents experimental results of the decompression wave speed obtained from shock tube tests conducted on pure CO2 from different initial conditions, and comparison with predictions by models based on GERG-2008, Peng-Robinson, and BWRS equations of state (EOS). These tests were conducted as a baseline before introducing various impurities.