Xingguo Feng

Xingguo Feng

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Xingguo Feng has a total of 45 co-authors. Here are the top co-authors by number of shared publications:

  • Xiangyu Lu

    Jiangsu University of Science and Technology

    10 shared publications
  • Da Chen

    3 shared publications
  • Ning Zhuang

    Key Laboratory of Coastal Disaster and Defence, Ministry of Education, College of Harbour, Coastal and Offshore Engineering , 12462 Hohai University , Nanjing , 210024 , Jiangsu , China

    3 shared publications
  • Yu Zuo

    Key Laboratory of Carbon Fiber and Functional Polymer, Ministry of Education, Beijing University of Chemical Technology, Beijing 100029, China

    3 shared publications
  • Xiangyu Lu

    Key Laboratory of Coastal Disaster and Defence, Ministry of Education, College of Harbour, Coastal and Offshore Engineering , 12462 Hohai University , Nanjing , 210024 , Jiangsu , China

    2 shared publications
  • Yang Zhao

    Key Laboratory of Coastal Disaster and Defence, Ministry of Education, Hohai University, Nanjing 210024 Jiangsu, People’s Republic of China

    2 shared publications

Latest Publications

  • Open Access

    Long-Lifetime Ag/AgCl Electrodes Prepared by Pulse Current Electrodeposition for Chloride Monitoring in the Concrete Environment

    by Xiangyu Lu, Jing Hu, Xingguo Feng, Qiyan Zhou, Zhanqing Qu, Jisheng Zhang, Ruihu Zhu, Huaqing Zhang, Songgui Chen

    Lifetimes of Ag/AgCl electrodes determine whether it is possible to monitor the concentration of chloride ions in marine concrete structures. A novel manufacturing method, pulse current electrodeposition at a low current density, was proposed to prepare the long-lifetime Ag/AgCl electrode. Influences of electrodeposition duration were investigated on the Nernst response, exchange current density, and lifetime of Ag/AgCl electrodes, and the properties were also compared to those of the ones electrodeposited by applying constant currents. Ag/AgCl electrodes prepared with the pulse current exhibited a wider potential response, a higher exchange current density, and a longer lifetime than those prepared by the constant current under the same equivalent charge transfer conditions. AgCl film on the electrode prepared with the pulse current displayed a thicker layer, a lower density of micropores, a higher Cl/O ratio, and a lower Ag/Cl ratio than those of its counterpart electrodeposited by applying the constant current. The lifetime of the Ag/AgCl electrode was mainly determined by the thickness of AgCl films in the concrete environment. The lifetimes of the Ag/AgCl electrode, which was prepared with a 0.1 mA cm−2 pulse current for 15 h, were 420 h in pore solution and more than 3500 h in mortar, respectively. In addition, the potential of this Ag/AgCl electrode did not show any significant decrease after 3500 h in the mortar without Cl−. The results suggest that pulse current electrodeposition is an effective method to improve the lifetimes of Ag/AgCl electrodes in concrete.


  • Investigation of SDS on Corrosion Behavior and Discharge Performance of AZ31B Magnesium Alloys in Aqueous Magnesium Air Batteries

    by Xiangyu Lu, Yang Zhao, Zhiteng Zheng, Jing Hu, Xingguo Feng

    To address the issue of high self-corrosion rate of Mg anodes in seawater batteries leading to low discharge efficiency, the green inhibitor, sodium dodecyl sulfate (SDS), was utilized to enhance the discharging performance of AZ31B alloy. The addition of SDS in a 3.5% NaCl solution led to a reduction in the corrosion rate of AZ31B alloy due to the formation of S-containing compounds. During the continuous-discharging period, the addition of 0.05 M SDS increased the anodic utilization efficiency from 64% to 81% and the specific energy density of the entire battery elevated from 1280 to 1912 mAh g−1 (an increase of 49%). The enhancement of the discharge performance of AZ31B Mg alloy in a 3.5% NaCl solution by SDS can be attributed to three aspects: reducing the negative difference effect of the Mg alloy, decreasing the accumulation of corrosion products on the surface of the Mg alloy, and promoting a more uniform dissolution of the Mg alloy.


  • Repassivation characteristics of carbon steel in chloride-free pore solution after thermal cycles of simulated tropical marine environments

    by Tong Wu, Xingguo Feng, Xiangyu Lu, Ning Zhuang, Shuai Qu

    Repassivation characteristics of carbon steel experienced thermal cycles in tropical marine environments were investigated in a simulated concrete pore solution (SCPS). The results suggested that the damage of passive films on the carbon steel mainly occurred during the cooling process in thermal cycles. The damaged passive films gradually recovered in the SCPS, and the duration of repassivation extended with the amplitude of thermal cycles and cyclic number in the high-amplitude thermal cycles (20–60 °C and 20–70 °C), while it was not significantly affected by the cyclic number in the low-amplitude thermal cycles (20–40 °C and 20–50 °C).


  • Pitting initiation on 304 stainless steel in a chloride-contaminated pore solution under alternating temperature conditions

    by Xingguo Feng, Tianyi Zhang, Ruihu Zhu, Zheng Chen, Xiangyu Lu

    Pitting initiation on 304 stainless steel grades was investigated in alternating temperature pore solutions to simulate pitting on stainless steel rebar in a tropical marine environment. The results suggested that a larger amplitude of alternating temperature heavily doped the passive film, reduced the film’s thickness and increased the (Fe 3+ ox + Fe 3+ hy)/Fe 2+ ox and Cr 3+ hy/Cr 3+ ox ratios in the film. Alternating temperatures more significantly degraded the passive film and intensified the pitting sensitivity on the stainless steel when compared with the average temperatures of the alternating temperature cycles. More pitting initiation sites were observed on the samples that experienced the 22–60 °C and 22–70 °C alternating temperature cycles than their counterparts in 50 °C and 60 °C solutions, respectively.


  • Corrosion Performance of 201 low-Nickel Stainless Steel Anchor in Cl – Contaminated Underground Water with Various Concentrations of SO 4 2− and HCO 3 −

    by Xingguo Feng, Qixiang Yan, Chao Zhu, Zheng Chen, Xiangyu Lu, Sheng Lu

    Corrosion behavior of 201 low-nickel stainless steel was studied in Cl − -contaminated underground water with various concentrations of HCO 3 − and SO 4 2− at different pHs to investigate the durability of stainless-steel anchors. The charge-transfer resistance increased, whereas the carrier densities and corrosion current density decreased with an increase in concentration of HCO 3 − and SO 4 2− , and solution pH. A parameter that was termed the composite corrosiveness index ( CCI ) was proposed to assess the corrosivity of underground waters to stainless steels. The CCI exhibited a monotonic relationship with charge-transfer resistance, carrier density, and corrosion current density, and it was more suitable for stainless steels compared with previous corrosiveness indexes in underground waters.


  • Open Access

    Electrochemical Study of Stainless Steel Anchor Bolt Corrosion Initiation in Corrosive Underground Water

    by Fangping Ma, Qing Zeng, Xiangyu Lu, Tong Wu, Xiao Lu, Tianyi Zhang, Xingguo Feng

    Application of low-nickel stainless steel anchor was one of the economical and effective methods to solve the durability problem of slope engineering. At present, there are scarce reports about corrosion characteristics of low-nickel stainless steel in various underground waters. For investigating the corrosion initiation of stainless steel anchor bolt in corrosive underground water, the effect of SO42−, HCO3− and pH value on the corrosion behavior of 201 low-nickel stainless steel was studied via electrochemical methods. As the SO42− concentration, HCO3− concentration or pH value increase, the open circuit potential and polarization resistance increase, while the double-layer capacitance, donor density and passive current density decrease. The results indicate that corrosion is inhibited by SO42−, HCO3− and OH− in underground water. In addition, the inhibitive efficiency of SO42− and HCO3− increases with the SO42− and HCO3− concentration.


  • Effect of interaction between two single-particle-impingements on the repassivation behavior of 304 stainless steel in a simulated groundwater

    by Xingguo Feng, Yang Zhao, Xiangyu Lu, Vahidoddin Fattahpour, Morteza Roostaei, Mahdi Mahmoudi, Hongbo Zeng, Jing-Li Luo

    To investigate the effect of interaction between two single-Si 3 N 4 particle-impingements on the repassivation of 304 stainless steel in a simulated groundwater, the corrosion current peaks of the samples during the impingement were recorded, and the micro-hardness of the substrate around the crater was tested. The results indicated that significant interactions between the two impingements were observed only when the value of distance-diameter ratio ( L/d ) was less than 1.5. With L/d being less than 1.5, the corrosion current peaks and mass losses due to the second impingements were higher than those of the first ones, and the re-passivation rates of samples during the second impingements were lower than those of the first impingements. Simultaneously, the microhardness of the substrate between the two craters was higher than that of the surface around one single crater with the same distance-diameter ratio. The mechanisms of how the L/d ratio influenced the interaction between the two impingements are also discussed.


  • Open Access

    Investigation of Protective Performance of a Mg-Rich Primer Containing Aluminum Tri-Polyphosphate on AZ91D Magnesium Alloy in Simulated Acid Rain

    by Xiangyu Lu, Sichen Sun, Qiqi Fan, Xiangjun Pei, Yuchao Dun, Xingguo Feng, Chen Zou, Wang Lu

    Mg-rich primer (MRP) containing aluminum tri-polyphosphate functions via a galvanic mechanism to protect AZ91D alloy from corrosion in the 3 wt % NaCl solution. However, its protective performance can be strongly affected by the testing environment. Therefore, it is important to investigate the performance of the primer on magnesium alloys in an acid rain environment. In the present study, the protective performance of MRP with or without aluminum tri-polyphosphate was investigated via open circuit potential (OCP), electrochemical impedance spectroscopy (EIS), scanning electronic microscopy (SEM) and X-ray photoelectron spectroscopy (XPS) in the simulated acid rain. Compared to the primer without aluminum tri-polyphosphate, the MRP containing aluminum tri-polyphosphate pigments exhibited better protective performance in the simulated acid rain condition. In the initial stage, the acidic condition prompted the aluminum tri-polyphosphate pigments to release phosphates and H+ to form magnesium phosphates on Mg particles, retarding their consumption rate. The Mg-rich primer with aluminum tri-polyphosphate can provide cathodic protection to AZ91D alloy for about 49 days in the simulated acid rain solution. Simultaneously, the corrosion products of Mg particles, magnesium oxides and phosphates, precipitated on the Mg particles and improved the stability of the primer. In addition, a protective film, consisting of magnesium oxides and phosphates, formed on the AZ91D substrate. Consequently, all these factors contributed to the long cathodic protection and improved corrosion resistance of MRP containing aluminum tri-polyphosphate in the simulated acid rain.