Jun Xu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Jun Xu has a total of 22 co-authors. Here are the top co-authors by number of shared publications:
Dapeng Jiang
Key Laboratory of Transparent and Opto-functional Inorganic Materials, Shanghai Institute of Ceramics, Chinese Academy of Sciences, No.588 Heshuo Road, Shanghai 201899, China
2 shared publications- Liangbi Su
Key Laboratory of Transparent and Opto-functional Inorganic Materials, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 201800, China
2 shared publications Chun Li
Shandong Normal University, Sch Phys & Elect, Shandong Prov Key Lab Opt & Photon Device, Jinan 250014, China
1 shared publicationFei Tang
Key Laboratory of Transparent and Opto-functional Inorganic Materials, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 201800, PR China
1 shared publicationFengkai Ma
Key Laboratory of Transparent and Opto-functional Inorganic Materials, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 201800, PR China
1 shared publication- Jiangfeng Zhu
Xidian University
1 shared publication
Latest Publications
- Open Access
- 13 January 2016
- Published by Optica Publishing Group in Optical Materials Express
- Vol. 6 (2) , 409-415
Effect of erbium concentration on spectroscopic properties and 279 μm laser performance of Er:CaF_2 crystals
The effect of erbium concentration on spectroscopic properties of Er:CaF2 crystals was investigated. Two highest absorption cross-sections (σabs) at 967 nm were achieved in the 4at.% and 8at.% Er:CaF2 samples with the value of 0.22 × 10−20 cm2 and 0.23 × 10−20 cm2, respectively. And the 4at.% and 8at.% Er:CaF2 samples also had the highest emission cross-section (σem) at 2727 nm with the value about 0.67 × 10−20 cm2. Lifetime of 4I13/2 decreased faster than that of 4I11/2 with the increase of erbium concentration. Under laser diode (LD) pumping, the continuous-wave (CW) laser operations around 2.79 μm were demonstrated in the 4at.%, 8at.% and 11at.% Er:CaF2 samples. And the 4at.% Er:CaF2 sample had the best laser performance with a maximum output power of 0.282 W and a slop efficiency of 13.9%.
- 13 January 2016
- Published by Optica Publishing Group in Optical Materials Express
- Vol. 6 (2) , 409-415
Open AccessEffect of erbium concentration on spectroscopic properties and 279 μm laser performance of Er:CaF_2 crystals
The effect of erbium concentration on spectroscopic properties of Er:CaF2 crystals was investigated. Two highest absorption cross-sections (σabs) at 967 nm were achieved in the 4at.% and 8at.% Er:CaF2 samples with the value of 0.22 × 10−20 cm2 and 0.23 × 10−20 cm2, respectively. And the 4at.% and 8at.% Er:CaF2 samples also had the highest emission cross-section (σem) at 2727 nm with the value about 0.67 × 10−20 cm2. Lifetime of 4I13/2 decreased faster than that of 4I11/2 with the increase of erbium concentration. Under laser diode (LD) pumping, the continuous-wave (CW) laser operations around 2.79 μm were demonstrated in the 4at.%, 8at.% and 11at.% Er:CaF2 samples. And the 4at.% Er:CaF2 sample had the best laser performance with a maximum output power of 0.282 W and a slop efficiency of 13.9%.
- Open Access
- 15 October 2015
- Published by MDPI AG in Applied Sciences
- Vol. 5 (4) , 817-824
Kerr-Lens Mode-Locked Femtosecond Yb:GdYSiO5 Laser Directly Pumped by a Laser Diode
We demonstrate the first Kerr-lens mode-locked operation in a diode-pumped Yb:GdYSiO5 oscillator. Under a diode pump power of 5 W, 141 fs pulses with an average power of 237 mW were obtained at a repetition rate of 118 MHz. The central wavelength was at 1094 nm with a bandwidth of 10.1 nm. Shorter pulses were obtained by adjusting the cavity to operate at a shorter wavelength, resulting in 55 fs pulse duration at the central wavelength of 1054 nm with a bandwidth of 23.5 nm.
- 15 October 2015
- Published by MDPI AG in Applied Sciences
- Vol. 5 (4) , 817-824
Open AccessKerr-Lens Mode-Locked Femtosecond Yb:GdYSiO5 Laser Directly Pumped by a Laser Diode
We demonstrate the first Kerr-lens mode-locked operation in a diode-pumped Yb:GdYSiO5 oscillator. Under a diode pump power of 5 W, 141 fs pulses with an average power of 237 mW were obtained at a repetition rate of 118 MHz. The central wavelength was at 1094 nm with a bandwidth of 10.1 nm. Shorter pulses were obtained by adjusting the cavity to operate at a shorter wavelength, resulting in 55 fs pulse duration at the central wavelength of 1054 nm with a bandwidth of 23.5 nm.
- 17 August 2015
- Published by Royal Society of Chemistry (RSC) in CrystEngComm
- Vol. 17 (38) , 7398-7405
Nd,Y:CaF2laser crystals: novel spectral properties and laser performance from a controlled local structure
A series of Nd,Y:CaF2 single crystals grown using the TGT method were studied systematically by absorption, excitation and luminescence spectroscopy, and the extended X-ray absorption fine structure (EXAFS) technique. The incorporation of Y3+ substantially manipulated the local structure of Nd ions in the CaF2 crystal lattice. Subsequently, the changes in the local structure of the Nd3+ ions induced substantial variations of the photoluminescence parameters, including FWHM, cross sections, lifetimes and quantum efficiency. Preliminary laser experiments were carried out with 0.5% Nd,10% Y:CaF2, 0.8% Nd,5% Y:CaF2 and 0.8% Nd,10% Y:CaF2 crystals under LD pumping; true CW laser operation was achieved with slope efficiencies of 30.1%, 19.3% and 24.9%, respectively.
- 17 August 2015
- Published by Royal Society of Chemistry (RSC) in CrystEngComm
- Vol. 17 (38) , 7398-7405
Nd,Y:CaF2laser crystals: novel spectral properties and laser performance from a controlled local structure
A series of Nd,Y:CaF2 single crystals grown using the TGT method were studied systematically by absorption, excitation and luminescence spectroscopy, and the extended X-ray absorption fine structure (EXAFS) technique. The incorporation of Y3+ substantially manipulated the local structure of Nd ions in the CaF2 crystal lattice. Subsequently, the changes in the local structure of the Nd3+ ions induced substantial variations of the photoluminescence parameters, including FWHM, cross sections, lifetimes and quantum efficiency. Preliminary laser experiments were carried out with 0.5% Nd,10% Y:CaF2, 0.8% Nd,5% Y:CaF2 and 0.8% Nd,10% Y:CaF2 crystals under LD pumping; true CW laser operation was achieved with slope efficiencies of 30.1%, 19.3% and 24.9%, respectively.