Jiacan Su
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Jiacan Su has a total of 25 co-authors. Here are the top co-authors by number of shared publications:
Jie Wei
Key Laboratory for Ultrafine Materials of Ministry of Education, East China University of Science and Technology, Shanghai 200237, China
2 shared publicationsJung-Woog Shin
Department of Biomedical Engineering, Inje University, Gimhae, 621749, Republic of Korea
2 shared publicationsSongchao Tang
Key Laboratory for Ultrafine Materials of Ministry of Education, East China University of Science and Technology, Shanghai, China
2 shared publicationsBaoqin Yu
Department of Orthopaedics Trauma, Changhai Hospital, Second Military Medical University, Shanghai, People's Republic of China
1 shared publicationBaoqing Yu
Department of Orthopaedics, Changhai Hospital, Second Military Medical University, Shanghai 200433, People's Republic of China
1 shared publicationDonghui Fan
Key Laboratory for Ultrafine Materials of Ministry of Education and The State Key Laboratory of Bioreactor Engineering, East China University of Science and Technology, Shanghai
1 shared publication
Latest Publications
- Open Access
- 1 July 2016
- Published by Taylor & Francis in International Journal of Nanomedicine
- Vol. ume 11, 3545-3555
Degradability, cytocompatibility, and osteogenesis of porous scaffolds of nanobredigite and PCL–PEG–PCL composite
Biocomposite scaffolds were fabricated by incorporation of nanobredigite (n-BD) into the polymer of poly(ε-caprolactone)–poly(ethyleneglycol)–poly(ε-caprolactone) (PCL–PEG–PCL). The results revealed that the addition of n-BD into PCL–PEG–PCL significantly improved water absorption, compressive strength, and degradability of the scaffolds of n-BD/PCL–PEG–PCL composite (n-BPC) compared with PCL–PEG–PCL scaffolds alone. In addition, the proliferation and alkaline phosphatase activity of MG63 cells cultured on n-BPC scaffolds were obviously higher than that cultured on PCL–PEG–PCL scaffolds. Moreover, the results of the histological evaluation from the animal model revealed that the n-BPC scaffolds significantly improved new bone formation compared with the PCL–PEG–PCL scaffolds, indicating good osteogenesis. The n-BPC scaffolds with good biocompatibility could stimulate cell proliferation, differentiation, and bone tissue regeneration and would be an excellent candidate for bone defect repair.
- 1 July 2016
- Published by Taylor & Francis in International Journal of Nanomedicine
- Vol. ume 11, 3545-3555
Open AccessDegradability, cytocompatibility, and osteogenesis of porous scaffolds of nanobredigite and PCL–PEG–PCL composite
Biocomposite scaffolds were fabricated by incorporation of nanobredigite (n-BD) into the polymer of poly(ε-caprolactone)–poly(ethyleneglycol)–poly(ε-caprolactone) (PCL–PEG–PCL). The results revealed that the addition of n-BD into PCL–PEG–PCL significantly improved water absorption, compressive strength, and degradability of the scaffolds of n-BD/PCL–PEG–PCL composite (n-BPC) compared with PCL–PEG–PCL scaffolds alone. In addition, the proliferation and alkaline phosphatase activity of MG63 cells cultured on n-BPC scaffolds were obviously higher than that cultured on PCL–PEG–PCL scaffolds. Moreover, the results of the histological evaluation from the animal model revealed that the n-BPC scaffolds significantly improved new bone formation compared with the PCL–PEG–PCL scaffolds, indicating good osteogenesis. The n-BPC scaffolds with good biocompatibility could stimulate cell proliferation, differentiation, and bone tissue regeneration and would be an excellent candidate for bone defect repair.
- Open Access
- 6 October 2015
- Published by The Royal Society in Journal of The Royal Society Interface
- Vol. 12 (111) , 20150779
In vitro degradability, bioactivity and primary cell responses to bone cements containing mesoporous magnesium–calcium silicate and calcium sulfate for bone regeneration
Mesoporous calcium sulfate-based bone cements (m-CSBC) were prepared by introducing mesoporous magnesium–calcium silicate (m-MCS) with specific surface area (410.9 m² g −1 ) and pore volume (0.8 cm³ g −1 ) into calcium sulfate hemihydrate (CSH). The setting time of the m-CSBC was longer with the increase of m-MCS content while compressive strength decreased. The degradation ratio of m-CSBC increased from 48.6 w% to 63.5 w% with an increase of m-MCS content after soaking in Tris–HCl solution for 84 days. Moreover, the m-CSBC containing m-MCS showed the ability to neutralize the acidic degradation products of calcium sulfate and prevent the pH from dropping. The apatite could be induced on m-CSBC surfaces after soaking in SBF for 7 days, indicating good bioactivity. The effects of the m-CSBC on vitamin D 3 sustained release behaviours were investigated. It was found that the cumulative release ratio of vitamin D 3 from the m-CSBC significantly increased with the increase of m-MCS content after soaking in PBS (pH = 7.4) for 25 days. The m-CSBC markedly improved the cell-positive responses, including the attachment, proliferation and differentiation of MC3T3-E1 cells, suggesting good cytocompatibility. Briefly, m-CSBC with good bioactivity, degradability and cytocompatibility might be an excellent biocement for bone regeneration.
- 6 October 2015
- Published by The Royal Society in Journal of The Royal Society Interface
- Vol. 12 (111) , 20150779
Open AccessIn vitro degradability, bioactivity and primary cell responses to bone cements containing mesoporous magnesium–calcium silicate and calcium sulfate for bone regeneration
Mesoporous calcium sulfate-based bone cements (m-CSBC) were prepared by introducing mesoporous magnesium–calcium silicate (m-MCS) with specific surface area (410.9 m² g −1 ) and pore volume (0.8 cm³ g −1 ) into calcium sulfate hemihydrate (CSH). The setting time of the m-CSBC was longer with the increase of m-MCS content while compressive strength decreased. The degradation ratio of m-CSBC increased from 48.6 w% to 63.5 w% with an increase of m-MCS content after soaking in Tris–HCl solution for 84 days. Moreover, the m-CSBC containing m-MCS showed the ability to neutralize the acidic degradation products of calcium sulfate and prevent the pH from dropping. The apatite could be induced on m-CSBC surfaces after soaking in SBF for 7 days, indicating good bioactivity. The effects of the m-CSBC on vitamin D 3 sustained release behaviours were investigated. It was found that the cumulative release ratio of vitamin D 3 from the m-CSBC significantly increased with the increase of m-MCS content after soaking in PBS (pH = 7.4) for 25 days. The m-CSBC markedly improved the cell-positive responses, including the attachment, proliferation and differentiation of MC3T3-E1 cells, suggesting good cytocompatibility. Briefly, m-CSBC with good bioactivity, degradability and cytocompatibility might be an excellent biocement for bone regeneration.